Microwave dielectric properties of $La_2O_3-CaO-B_2O_3$ glass-added alumina

$La_2O_3-CaO-B_2O_3$계 유리 첨가 알루미나 복합체의 유전특성

  • Published : 2007.06.21

Abstract

Influence of $La_2O_3$ addition to $CaO-B_2O_3$-based glass on the water leaching resistance of the glass was first investigated. The optimized $La_2O_3-CaO-B_2O_3$(LCB) glass was ball milled for varying time, followed by mixing with $Al_2O_3$ crystalline phase to form $Al_2O_3$-LCB glass composites at $875^{\circ}C$ for 1h. Microwave dielectric properties of the composites were investigated as a function of the ball milling time of the LCB glass. Dielectric constant and quality factor of the composites were 6.31 and 13856 GHz, respectively, when the LCB glass was ball milled for 2h prior to mixing with $Al_2O_3$.