Behaviors of the interface cracks during an Al-Fe dissimilar joining

Al-Fe 이종재료 접합 계면에서의 크랙 거동

  • 강남현 (한국생산기술연구원 정밀접합팀) ;
  • 김철희 (한국생산기술연구원 정밀접합팀) ;
  • 김준기 (한국생산기술연구원 정밀접합팀) ;
  • 이창우 (한국생산기술연구원 정밀접합팀)
  • Published : 2006.05.01

Abstract

The $CO_2$ laser cladding was conducted on an AC2B alloy with feeding Fe-based powders. A powder feeding rate (PFR) and a travel velocity were related with the cracks adjacent to the Fe/Al interface. Preheating temperature was varied to study the interface crack. Preheating to $250^{\circ}C$ during the laser cladding suppressed the interface crack ratio (ICR). The ICR was limited for the single pass clad and the reciprocating test for the slide wear was conducted on an overlay cladding experiment. Comparing with no overlap overlay, the overlay clad with 50% overlap showed better wear resistance.