Polarization properties of SBT capacitor with annealing temperatures

열처리에 따른 SBT 캐패시터의 분극특성

  • Published : 2001.09.21

Abstract

The $Sr_{0.8}Bi_{2.4}Ta_2O_9(SBT)$ thin films are deposited on Pt-coated electrode($Pt/TiO_2/SiO_2/Si$) using RF magnetron sputtering method. With increasing post-annealing temperature from $600[^{\circ}C]$ to $850[^{\circ}C]$, Bi-layered perovskite phase was crystallized above $650[^{\circ}C]$. The maximum remanent polarization and the coercive electric field is 11.60[${\mu}C/cm^{2}$] 48[kV/cm] respectively. The leakage current density of SBT capacitor at post-annealing temperature of $750[^{\circ}C]$ is $1.01{\times}10^{-8}A/cm^2$ at 100[kV/cm]