Effect of Cr Addition on the High Temperature Deformation Behavior of Fe-Al Intermetallics

Fe-Al 금속간 화합물의 고온변형거동에 미치는 Cr 첨가의 효과

  • 방원규 (포항공과대학교 항공재료연구센터) ;
  • 임현태 ((주)삼성테크윈) ;
  • 하태권 (포항공과대학교 항공재료연구센터) ;
  • 송진화 (포항산업과학연구원 금속코팅연구팀) ;
  • 장영원 (포항공과대학교 항공재료연구센터)
  • Published : 2001.05.01

Abstract

High temperature deformation behavior of Fe-28Al-5Cr alloy has been investigated known to show anomalous temperature dependence of yield strength. Specifically, the effect of Cr addition has been examined. A series of tensile and load relaxation tests have been carried out to obtain the flow behavior of Fe-28Al-5Cr alloy at the elevated temperatures. The flow curves have then been analyzed using the inelastic deformation theory recently proposed. Firstly, high temperature flow stress of iron aluminides can be resolved into internal stress and frictional stress. Secondly, the temperature corresponding to peak strength gets higher level at faster strain rate, which presumably due to the increased contribution of internal stress in observed flow stress. And thirdly, the alloying of Cr seems to cause solid-solution strengthening of frictional stress level and the elevation of 2nd order transition temperature. In this analogy, Fe-28Al-5Cr exhibits better strength especially at relatively higher temperature and lower strain rate than Fe-28Al.

Keywords