Abstract
In this paper, the permeability(${\mu}$$\sub$r′/, ${\mu}$$\sub$r"/), permittivity($\varepsilon$$\sub$r′/, $\varepsilon$$\sub$r"/) and absorption properties of Ferroxplana/Rubber composites were investigated. The composite specimens were prepared by molding and curing the mixtures of matrix rubber and Ni$_2$Y ferroxplana powders which were synthesized by coprecipitated method. The permeability(${\mu}$$\sub$r′/) of specimen was decreased in the range of 8∼12.5(GHz) and the permeability(${\mu}$$\sub$r"/) and Permittivity($\varepsilon$$\sub$r′/, $\varepsilon$$\sub$r"/) were increased. The optimum thickness of electromagnetic wave absorber (F/R=4, 1,200($^{\circ}C$) ), utilizing the Smith chart, was about 3.0(mm). The Figure of Merit was 93(%).