• Title/Summary/Keyword: whisker

Search Result 287, Processing Time 0.029 seconds

A Study on Sintering and mechanical Properties of Sinter/HIPed SiC Whisker/$Al_2O_3$ Composite (Sinter/HIP 공정으로 제조한 SiC whisker/$Al_2O_3$ 복합재료의 소결 및 기계적 물성에 관한 연구)

  • Lee, Chae-Hyun;Kim, Jong-Ock;Kim, Chong-Hee
    • The Journal of Natural Sciences
    • /
    • v.8 no.1
    • /
    • pp.53-59
    • /
    • 1995
  • Effects of sintering additives and sintering temperatures on the sintering behavior and mechanical properties of SiC whisker reinforced alumina composites have been investigated in this study. Dense (>95% TD) composites were obtained by using 2 wt% $Y_2O_3$ as liquid phase sintering additive. But only porous composite could be obtained when the sintering additives were MgO and $TiO_2$, which were known as the sintering additives for solid state sintering of alumina. Bending strength and fracture toughness were enhanced by reinforcement of SiC whisker. It is belived from the microstructure investigation that the enhanced by strength and toughness could be attribute to the reinforcing and grain growth inhibition effects of SiC whisker. After HIP treatment, fully dense composites were obtained and further enhanced mechanical properties achieved.

  • PDF

Sintering Phenomena and Thermodynamic Analysis in the SiC Whisker-Reinforced Mullite Matrix Ceramic Composites During RF Plasma Sintering

  • Park, Youngsoo;:Michael J. MeNallan
    • The Korean Journal of Ceramics
    • /
    • v.2 no.4
    • /
    • pp.231-237
    • /
    • 1996
  • Mullite ceramics can be sintered by rf plasma sintering to densities as high as 97% compared to the theoretical density of the mullite, while SiC whisker-reinforced mullite matrix ceramic composites were not sintered by plasma sintering. Decomposition of mullite occurs in a superficial regins at the outside surface of the specimen by volatilization of SiO at elevated temperature by plasma. SiC whiskers were destroyed, and the matrix was converted to alumina from SiC-whisker reinforced mullite matrix ceramic composites during the plasma sintering. Accelerated volatilization from the SiC whisker in the mullite prevents sintering. The volatile species are mainly SiC and CO gas species. The effects of plasma on mullite and SiC-whisker reinforced mullite matrix composites are interpreted by thermodynamic simulation of the volatile species in the plasma environment. The thermodynamic results show that the decomposition will not occur during hot pressing.

  • PDF

Effect of Granule Characteristics of Mixed Powder on Mechanical Properties of Hot-Pressed SiC-Whisker/Alumina Composites (혼합분말의 과립특성이 가압소결 탄화규소 휘스커/알루미나 복합재료의 기계적 물성에 미치는 영향)

  • 이해원;송휴섭
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.12
    • /
    • pp.1513-1520
    • /
    • 1994
  • Mechanical properties of hot-pressed SiC whisker/Al2O3 composites were strongly dependent on the granular characteristics of mixed powder, which were controlled by co-dispersion condition, the existence of steric barrier on whisker surface, and granulating method, etc. Heat-treatment of SiC whiskers at $700^{\circ}C$ for 1 hr in air was very effective both for achieving dispersion stability of whiskers with PVA adsorption and for obtaining excellent mechanical properties of resulting composites. It is believed from the fractography of composites prepared with various whisker dispersion conditions that the most common fracture origin of Al2O3 agglomerate could be attributed to whisker clusters arising due to flocculation. Further improvement of mechanical properties of composites were achieved by hot pressing green tapes prepared by Doctor-blade process, which promoted two-dimensional random alignment of whiskers.

  • PDF

Synthesis of Mullite Whisker from Fly Ash (플라이 애쉬로부터 뮬라이트 휘스커의 합성)

  • Kim, Sung-Hwan;Bang, Hee-Gon;Park, Sang-Yeup
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.11 s.282
    • /
    • pp.753-757
    • /
    • 2005
  • In this study, we attempted to recycle the fly ash as a mullite whisker with addition of $Al_{2}O_{3}$ to obtain the high yield of mullite whisker. During the reaction process, mullite whisker was formed with the reaction of amorphous $\alpha$-Cristobalite and Anorthite above $1350^{\circ}C$. With increasing the heat treatment temperature and time, the mean length and aspect ratio of mullite whiskers was gradually increased.

Effect of Cold Cyclic Compaction on Densification of $Al_2O_3$ Powder/SiC Whisker Composite ($Al_2O_3$분말과 SiC 휘스커 복합체의 치밀화에 미치는 상온 반복 압축의 영향)

  • 최승완;김기태
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.3
    • /
    • pp.296-302
    • /
    • 1997
  • The effect of cold cyclic compaction on densification of SiC whisker/Al2O3 composite was investigated. Re-lative density of the compact increased as the number of cycle and the compaction pressure increased and the bias pressure decreased. The rate of loading and unloading and the frequency of cold cyclic compaction did not affect much on sliding and rearrangement of the particles. Fracture of SiC whisker was hardly ob-served during cold cyclic compaction and the direction of whisker was randomly oriented throughout the compact regardless of the direction of compaction. Thus, cold cyclic compaction may be an efficient method to densify SiC whisker/Al2O3 composite.

  • PDF

Toughening of SiC Whisker Reinforced Al2O3 Composite (SiC 휘스커 강화 Al2O3 복합재료의 고인화)

  • Kim Yon Jig;Song Jun Hee
    • Korean Journal of Materials Research
    • /
    • v.14 no.9
    • /
    • pp.649-654
    • /
    • 2004
  • In this paper, the fracture toughness and mechanisms of failure in a random SiC-whisker/$Al_{2}O_3$ ceramic composite were investigated using in situ observations during mode I(opening) loading. $SiC_{w}/Al_{2}O_3$ composite was obtained by hot press sintering of $Al_{2}O_3$ powder and SiC whisker as the matrix and reinforcement, respectively. The whisker and powder were mixed using a turbo mill. The composite was produced at SiC whisker volume fraction of $0.3\%$. Compared with monolithic $Al_{2}O_3$, fracture toughness enhancement was observed in $SiC_{w}/Al_{2}O_3$ composite. This improved fracture toughness was attributed to SiC whisker bridging and crack deflection. $SiC_{w}/Al_{2}O_3$ composite exhibited typically brittle fracture behavior, but a fracture process zone was observed in this composite. This means that the load versus load-line displacement curve of $SiC_{w}/Al_{2}O_3$ composite from a fracture test may involve a small non-linear region near the peak load.

Effects of the Whisker Orientation and Sintering Temperature on Mechanical Properties of the Si$_3$N$_4$ based Composites (Si$_3$N$_4$ Whisker의 배열방향과 소결온도가 Si$_3$N$_4$ 복합체의 기계적 성질에 미치는 영향)

  • 김창원;박동수
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.5
    • /
    • pp.483-489
    • /
    • 1999
  • Gas pressure sintered silicon nitride based composites with 3 wt% $\beta$-Si3N4 whiskers were prepared and change of properties according to the whisker orientation and sintering temperature was studied. The tapes with whiskers were fabricated by two different method ; conventional tape casting and a modified tape casting by using guide pins,. Orientations of the whiskers were controlled by different stacking sequences of the sheets cut from the tape. Samples were fully densified by gas pressure sintering at 2148-2273K. As the sintering temperature increased size of the large elongated grains increased. In case of unidirectional samples sintering shrinkage normal to the whisker alignment direction was larger than that of parallel to the direction and the shrinkage anisotropy increased slightly as sintering temperature increased. As sintering temperature increased the crack length parallel to whisker alignment direction became shorter but that normal to the direction did not depend on sintering temperature. In case of cross-plied samples the anisotropy of mechanical properties disappeared.

  • PDF

Mechanical Properties of the Pressureless Sintered Al2O3-SiC Composites(2) : Dispersion Effects of SiC Whisker (상압소결한 Al2O3-SiC계 소결체의 기계적 성질(2) : SiC Whisker의 분산효과)

  • 김경수;이홍림
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.6
    • /
    • pp.704-712
    • /
    • 1988
  • In order to investigate the effect of the second phase on Al2O3 matrix, SiC whisker was dispersed in Al2O3 matrix as a second phase over the content range of 5vol% to 20vol%. To this mixture, Y2O3 or TiO2 powder was added as a sintering additive before isostatically pressing and pressureless sintering at 1800-190$0^{\circ}C$ for 90min in N2 atmosphere. With increasing SiC whisker content, relative densities of composites were decreased and the grain growth of Al2O3 was restricted. When Y2O3 was added as a sintering aid the sintering temperature was 180$0^{\circ}C$, the maximum values of flexural strength, hardness and fracture toughness were 537MPa, 12.1GPa, 3.7MPa.m1/2, respectively. However, when the sintering temperature was elevated to 190$0^{\circ}C$, maximum values of flexural strength, hardness and fracture toughness were 453MPa, 17.5GPa, 4.9MPa.m1/2, respectively. Improved mechanical properties are assumed to be attributed to the crack deflection by the second phase SiC whisker and whisker pullout mechanism.

  • PDF

The Observation of Intermetallic Compound Microstructure Under Sn Whisker in Lead-free Finish

  • Yu, Chong-Hee
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.16 no.2
    • /
    • pp.27-31
    • /
    • 2009
  • Sn whiskers can grow from the pure Sn and high Sn-based finish and cause the electrical shorts and failures. Even with the wealth of information on whiskers, we have neither the clear understanding of whisker growth nor methods for its prevention. In this study, the whisker grain roots which connected with intermetallic layer were analyzed by high-resolution transmission electron microscopy (HR-TEM). In the Sn-Cu plated leadframe (LF) that was stored at ambient condition for 540 days, filament-shaped whiskers were grown on the Sn-plated surface and ${\eta}'-Cu_6Sn_5$ precipitates were widely distributed along the grain boundaries at the Sn matrix. The measured of the lattice fringes at the ${\eta}'-Cu_6Sn_5$ was $4.71{\AA}$ at the coarse grain and $2.91{\AA}$ at the fine grain. The $Cu_3Sn$ which generates the tensile stresses was not observed. The formation of $Cu_6Sn_5$ precipitates and intermetallic layer were strongly related to whisker growth, but, the whisker growth tendency does not closely relate with the geometric morphology of irregularly grown intermetallic compound (lMC).

  • PDF

Synthesis and characterization of potassium titanate whisker by hydrothermal process (수열합성법을 이용한 티탄산칼륨 휘스커의 합성과 특성)

  • Choi, Yeon-Bin;Son, Jeong-hun;Lee, Je Kyun;Bae, Dong-Sik
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.27 no.1
    • /
    • pp.9-17
    • /
    • 2017
  • $K_2Ti_6O_{13}$ whisker have been synthesized by hydrothermal process at low temperature and pressure condition. The average length of the synthesized $K_2Ti_6O_{13}$ whisker was about in the range of 300 nm to $1.5{\mu}m$. The average diameter of the synthesized $K_2Ti_6O_{13}$ whisker was 15 nm to 60 nm. The aspect ratio of the synthesized $K_2Ti_6O_{13}$ whisker was below 12. The average length and diameter of the synthesized $K_2Ti_6O_{13}$ whisker can be controlled by reaction temperature and time, KOH molar ratio. $K_2Ti_6O_{13}$ whisker was synthesized from more than $210^{\circ}C$ and 4 h at reaction temperature and time. The length of the whisker is increased with increasing reaction temperature. Characterization of the synthesized $K_2Ti_6O_{13}$ whisker was carried out using the XRD and FE-SEM.