• 제목/요약/키워드: wet abrasive wear

검색결과 7건 처리시간 0.02초

다이아몬드 연마재 입도가 초경 습식신선 다이스 수명에 미치는 영향 (The Influence of Diamond Abrasive Size on the Life of Tungsten Carbide Wet Drawing Dies)

  • 이상곤;김민안;고대철;김병민
    • 소성∙가공
    • /
    • 제15권7호
    • /
    • pp.518-523
    • /
    • 2006
  • Wet wire drawing of brass coated steel wire, used for tire reinforcement, is realized with Tungsten Carbide(WC) dies sintered with a cobalt(Co) binder. Dies wear represents an important limitation to the production process and cost savings. Several parameters, such as Co content, WC grain size of tungsten carbide, sintering conditions, and so on, affect on the wear of the drawing die. In this study, the effect of the diamond abrasive particle size on the life of the WC centered dies of the wet wire drawing was investigated. Wet wire drawing experiments were carried out on a wet wire drawing machine. From the experiments, the dies life, dies fracture, wire surface roughness, and wire breaks were investigated. From the results, it was found that the wear of the WC dies increased with the increase in the diamond abrasive particle size.

오일샌드 플랜트용 금속소재의 마모 특성에 대한 실험적 연구 (Experimental Study on Wear Characteristics of Metallic Materials used in Oil Sands Plants)

  • 원성재;조승현;강대경;허중식
    • Tribology and Lubricants
    • /
    • 제33권1호
    • /
    • pp.31-35
    • /
    • 2017
  • Recently, international attention has been focused on the development of non-traditional energy resources such as shale gas and oil sands, due to the steep increase in the demand for natural resources. The materials incorporated in an oil gas plant module experience extreme environments, and are prone to various problem such as fracture, corrosion and abrasion due to low-temperature brittleness. In order to improve the plant life, it is necessary to perform characteristics study and performance evaluation of the materials. In particular, this paper explains the main set of materials which are most frequently used in oil sands plant project. In order to investigate wear characteristics, the authors carried out abrasive wear tests of TP 316, stainless steel and SS 400, structural rolled steel. For the analysis of the abrasive wear resistance of an oil sands plant, the authors carried out the test according to ASTM G 105 "Standard Test Method for Conducting Wet Sand/Rubber Wheel Abrasion Test" standard guidelines. The authors have derived the results from the data associated with the loss of mass with respect to wear rate. During the test, for a given wear length for 10,000 revolutions, the rotational speed and applied force of the rubber wheel were varied.

알루미나 연삭숫돌의 마모에 관한 실험적 연구 (An Experimental Study on the Wear of Alumina Grinding Wheels)

  • 조기수;이종찬;최환
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1994년도 추계학술대회 논문집
    • /
    • pp.113-118
    • /
    • 1994
  • An experimental investigation on the wear of alumina grinding wheel is presented. The experiments consist of the measurements of fracture strength of the abrasive grains, grinding forces, and the area of wear flats of grinding wheels. Microscopic examinations of abrasive grains were also carried out to observe the progress of wheel wear. the results show that the 32A grain, which has relatively lower fracture strength, wears out faster than 5SS and 5SG. The wheel wear occurs much faster in wet grinding than in dry grinding. It has also been found that the grinding forces increase logarithmically with increasing wear flats.

  • PDF

고능률 연삭용 알루미나 연삭숫돌의 연삭성능 및 마멸에 관한 실험적 연구 (An Experimental Study on Grinding Performance and Wear of Alumina Grinding Wheels Developed for High Performance Grinding)

  • 조기수;이종찬
    • 한국정밀공학회지
    • /
    • 제13권12호
    • /
    • pp.38-45
    • /
    • 1996
  • A new grinding wheel was developed for the high performance grinding of difficult-to-grinding materials. The grinding performance of the newly developed wheel including grinding forces, grinding ratio, and surface roughness of ground surface was evaluated through experiments. Experimental results show that the performance of the newly developed wheel is superior to the conventional alumina wheel and comparable to the Sol-gel wheel. An experimental investigation on the wear of alumina grinding wheel was also carried out. The experiments consist of the measurements of fracture strength of the abrasive grains, grinding force, and the area of wear flats of grinding wheels. Microscopic examination of abrasive grains was executed to observe the progress of wheel wear. The results indicate that the 32A grain, which has relatively lower fracture strength, wears out faster than 5SS and 5SG. The wheel wear occurs much faster in wet grinding than in dry grinding. It has also been found that the grinding forces increase logarithmically with increasing wear flats.

  • PDF

세라믹 성형체의 미소구멍 가공 시 다이아몬드 입자 전착 드릴의 공구 수명 예측 모델 (Model for predicting tool life of diamond abrasive micro-drills during micro-drilling of ceramic green bodies)

  • 이학구;이대길
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2003년도 춘계학술대회 논문집
    • /
    • pp.593-598
    • /
    • 2003
  • Ceramic plates containing many micro-holes are used in diverse applications such as MCP (Microchannel Plate). catalytic converters, filters, electrical insulators in integrated circuits, and so on. One of the efficient methods for machining many holes in ceramic plates is wet drilling of ceramic green bodies followed by sintering them. Since the strength of ceramic green bodies is much lower than the strength of sintered ceramic plate, ceramic green bodies can be drilled with high feed rate. The axial force during micro-drilling of ceramic green bodies increases rapidly at high feed rate, which induces the crack in workpiece. Therefore, the tool lift of micro-drill with respect to feed rate may be determined by the predicting increase of axial force. In this work, the axial force during micro-drilling was calculated using the chip flow model on the micro-drill tip. from which the tool life of diamond abrasive micro-drill during micro-drilling of ceramic green bodies was calculated.

  • PDF

반도체 웨이퍼 다이싱용 나노 복합재료 블레이드의 제작 (Fabrication of Organic-Inorganic Nanocomposite Blade for Dicing Semiconductor Wafer)

  • 장경순;김태우;민경열;이정익;이기성
    • Composites Research
    • /
    • 제20권5호
    • /
    • pp.49-55
    • /
    • 2007
  • 반도체 쿼츠 웨이퍼 다이싱용 블레이드는 마이크로/나노 디바이스와 부품을 제조하기 위해 고정밀도의 가공성을 요구한다. 따라서 균일한 마이크로/나노 선폭의 가공을 위해서는 블레이드의 제작 단계에서 균일한 두께와 밀도를 유지하는 것이 중요하다. 기존의 실리콘웨이퍼 가공을 위해서는 금속의 블레이드가 사용되고 있지만 쿼츠 웨이퍼 가공을 위해서는 고분자 복합재가 사용된다. 이러한 복합재는 가공성, 전기전도성, 그리고 적절한 강도와 연성 및 마모저항성이 있어야 한다. 그러나 기존의 건식성형 공정으로는 균일성을 유지하기 위해 많은 공정과 비용이 소비되고 있다. 본 연구에서는 도전성 나노 세라믹스 분말, 연마재 세라믹스 분말에 열경화성 수지, 전도성 고분자를 혼합한 복합재 분말을 습식성형 공정에 의해 제조, 평가하는 연구를 수행하였다. 먼저 복합재 분말을 액상과 혼합하여 블레이드를 제작하였으며, 액상의 종류, 액상 건조공정의 영향을 고찰하였다. 평가는 마이크로미터 측정기와 현미경을 이용하여 두께를 측정하였다. 두께편차와 기공률, 밀도, 경도, 등의 특성을 비교, 평가하였다. 그 결과 습식성형에 의해 블레이드의 두께편차를 감소시킬 수 있었으며, 경도 등의 특성을 향상시킬 수 있었다.

차선재료의 내구성 향상을 위한 내마모성 시험 적용 연구 (Abrasion-Resistant Road Markings for Improved Durability Lane to Wear Simulators Test)

  • 이창근;박진환;오흥운
    • 한국도로학회논문집
    • /
    • 제13권3호
    • /
    • pp.75-82
    • /
    • 2011
  • 도로표지용 도료의 품질기준은 KS M 6080의 품질기준을 만족하는 제품들의 경우에도 시공 후 일정기간이 경과한 후에는 도료 자체의 부착력 문제로 교통량 증가에 따른 자동차 차륜에 의한 도료 자체의 마모 손실에 의하여 재귀반사 기능을 부여하는 유리알의 마모 및 탈리로 시인성이 급격히 저하되고 있다. 이에 따른 야간 교통 사고율 증가와 동시에 추가 교통 안전을 위한 부가 보완시공으로 안전시설 제비용이 직접비용으로 유발되고 있으며, 직접비용보다 추가공사로 인한 교통체증으로 사회간접 비용이 증가되고 있다. 특히, 차선의 품질 규격이 KS M 6080 제품에 만족한다 하더라도 빗물의 수막(水膜)에 의한 유리알의 굴절율 차로 재귀반사기능을 하는 차선 도료용 유리알의 기능을 발휘하지 못하여 운전자의 시인성은 열악함을 알 수 있다. 따라서, 국외에서 많이 사용되고 있는 마모성이 우수한 수용성 차선도료, 고성능 융착식 도료, 상온경화형 도료를 도입하여 성능을 비교 검토하였다. 본 연구에서는 차선재료의 내구성 향상을 위해 EN 1436규격에 의한 내마모성 시험을 수용성, 융착식, 상온경화형 도료에 실시하여, 재귀반사도 성능이 우수한 차선재료의 적용 가능성을 확인하였다.