• 제목/요약/키워드: welding joint

검색결과 1,132건 처리시간 0.022초

외력을 고려한 양면 T-용접이음부의 음력해석 (Stress Analysis of Double T-Welded Joints Considering External Forces)

  • 김성환;방한서;방희선;송관형
    • Journal of Welding and Joining
    • /
    • 제19권2호
    • /
    • pp.215-220
    • /
    • 2001
  • In the T-joint welding, the complete penetration joint which is obtained by groove welding with edge preparation is generally required thor the safety and reliability of structures but this way have the some defects such as increase of working time, consumed welding electrode quantity and large welding deformation. If there is no probrem, in the strength, T-joint welding without edge preparation will be profitably understood in the economical and welding deformation side. In this paper, we performed the finite element analysis to understand the characteristics of welding residual stresses on two models, complete penetration joint have the edge preparation and incomplete penetration joint without edge preparation, respectively. Especially, we observed the relation between welding residual stress distributed on the notch of gap in the root and external force in the incomplete penetration joint without edge preparation.

  • PDF

390MPa급 고장력강판의 경치기 레이저 용접에서 부분용입 용접의 적용 가능성에 대한 연구 (A Study on the Feasibility of Partial Penetration Laser Welding for the Lap Joint of 390MPa High Strength Steel Sheets)

  • 이경돈;박기영;김주관
    • Journal of Welding and Joining
    • /
    • 제20권2호
    • /
    • pp.95-101
    • /
    • 2002
  • After high power lasers are avaliable in the commercial market, the number of applications of the laser welding has been increased in manufacturing industries. Although the tailored blank laser welding of butt jointed steel sheets is well known recently in the automotive industries, the lap joint laser welding is a new technology to the automotive manufacturing people as well as the design people. But the deep penetration laser welding seems to be preferred to the partial penetration welding for the lap joint welding in the automotive manufacturers because the partial penetration is a serious deflect for the butt joint. In this study, the feasibility of partial penetration welding fur the lap joint $CO_2$ laser welding was studied fur the 1mm thick 390MPa high strength steel sheets for automotive bodies. The process window of the lap joint partial penetration welding was obtained from experiments with the gap size and the welding speed as process parameters. The partial penetration welding was found excellent on the basis of the tensile shear strength and sectional geometry. The bead width, input energy Per volume, tensile-shear strength, deformation energy and the sectional geometries after tensile-shear tests of partial penetration welded specimens are compared with those of full penetration welded specimens with a series of gaps and welding speeds.

Friction Stir Welding Tool Geometries Affecting Tensile Strength of AA6063-T1 Aluminum Alloy Butt Joint

  • Kimapong, Kittipong;Kaewwichit, Jesada;Roybang, Waraporn;Poonnayom, Pramote;Chantasri, Sakchai
    • International journal of advanced smart convergence
    • /
    • 제4권1호
    • /
    • pp.145-153
    • /
    • 2015
  • Friction Stir Welding (FSW) is a solid state welding that could successfully weld the difficult-to-weldmaterials such as an aluminum alloy. In this welding process, the stirrer of the welding tool is one of the important factors for producing the perfect sound joint that indicates the higher joint strength. So, this report aims to apply the friction stir welding using various stirrer geometries to weld the AA6063-T1 aluminum alloy butt joint, investigates the mechanical properties of the joint and then compares the mechanical properties with the microstructure of the joint. An experiment was started by applying the friction stir welding process to weld a 6.3 mm thickness of AA6063-T1 aluminum alloy butt joint. A study of the stirrer geometries effect such as a cylindrical geometry, a cone geometry, a left screw geometry and a right screw geometry at a rotational speed of 2000 rpm and a welding speed of 50-200 mm/min was performed. The mechanical properties such as a tensile strength and a hardness of the joint were also investigated and compared with the microstructure of the joint. The results are as follows. A variation of FSW Stirrer shape directly affected the quality AA6063-T1 aluminum alloy butt joint. A cylindrical stirrer shape and a cone stirrer shape produced the void defect at the bottom part of the weld metal and initiated the failure of the joint when the joint was subjected to the load during the tensile test. Left and right screw stirrer shapes gave the sound joint with no void defect in the weld metal and affected to increase the joint strength that was higher than that of the aluminum base metal.

T형 평면용접이음재의 응력해석과 굽힘피로강도에 관한 연구 (A Study on Stree Analysis and Bending Fatigue Strength of One Side Fillet Welded T-joint)

  • 강성원;이태훈;전재목;김충희
    • 한국해양공학회지
    • /
    • 제13권2호통권32호
    • /
    • pp.51-57
    • /
    • 1999
  • In this study, one side fillet welded T-joint, used in box type girder and other welding structure, was investigated by stress analysis and bending fatigue test without edge preparation, with variation of joint shape. The purpose of this study is to give the welding condiltion and design standard on manufacturing one side fillet welded T-joint. As a result, the following conclusions were obtained. 1) In one side fillet welded T-joint, the larger the leg length and the penetration depth, the greater the bending fatigue strength because reduction of stress and strain on toe and root. The increase of the longitudinal leg length rather than vertical leg length contributed to the increase in bending fatigue strength. 2) In one side fillet welded T-joint without edge preparation, both general manual welding and general automatic welding were carried out with same condition. In this case, automatic welding showed deeper penetration and more increased longitudinal leg length than manual welding, so that automatic welding offers greater bending fatigue strength. 3) For one side fillet welded T-joint without edge preparation with automatic welding, the ratio(h/t) of the leg length(h) and the main plate thickness(t) in which toe crake can occur was 1.0 over.

  • PDF

저탄소강 SS41 연속파형 Nd:YAG 레이저 겹치기 용접의 기공제어 기술 (The Porosity Control Technology of Lap Joint Welding Using Continuous Wave Nd:YAG Laser of the Low Carbon Steel SS41)

  • 이가람;황찬연;양윤석;박은경;유영태
    • 한국생산제조학회지
    • /
    • 제22권4호
    • /
    • pp.665-672
    • /
    • 2013
  • With the development of advanced processing technology, laser processing systems, which require high-quality precision processing, have attracted considerable attention. Although laser equipment is expensive, it enables quick processing and less deformation of materials. This technology is often applied to secondary batteries, which has thus farinvolved the use of argon tungsten inert gas (TIG) welding. However, the welding characteristics of argon TIG welding are not yet good, and a laser is used for welding to address this problem. In this study, lap-joint welding was conducted, and the desired welding characteristics were obtained when the laser power was 1800W and the laser beam travel speed was 1.8 m/min. Lap-joint welding was conducted on Ni-coated SS41. Two cases were compared. No pores were observed in the Ni-coated SS41 lap-joint welding part, and cracks appeared from the lap-joints. Moreover, the pole rod and tap were welded together in a T-joint form to improve the output of the secondary battery. T-joint laser welding showed better welding characteristics than TIG welding.

Effect of Process Variables on the Flash Butt Welding of High Strength Steel

  • Kim, Y.S.;Kang, M.J.
    • International Journal of Korean Welding Society
    • /
    • 제3권2호
    • /
    • pp.24-28
    • /
    • 2003
  • This study was aimed to evaluate the quality of flash welded joints and optimize the welding process for flash butt welding of 780MPa grade high strength steel. And then the relationship between the welding process variables and the joint quality would be established. The effect of process variables between flashing and upsetting process was elucidated. Microstructure observation of the joint indicated that the decarburized band was mainly changed with upsetting process. Width of HAZ was also related to the upsetting conditions rather than the flashing conditions. Generally maximum hardness at HAZ was correlated with Ceq of steel and the empirical relationship was obtained to estimate the HAZ properties. Tensile elongation at the joint was usually decreased with increasing the initial clamping distance. Investigation of fracture surface after tensile and bending tests reveal that the origin of cracking at the joint was oxide inclusions composed of $SiO_2$, MnO, $Al_2O_3$, and/or FeO. The amount of inclusions was dependent on the composition ratio of Mn/Si in steel. If this ratio was above 4, the amount of inclusions was low and then the resistance to cracking at the joint was enough to maintain the joint performance. It was obtained that the flashing process influenced the conditions for the energy input to establish uniform or non­uniform molten layer, while the upsetting conditions influenced the joint strength. Heat input variable during flashing process was also discussed with the joint properties.

  • PDF

응력제거 열처리한 Mg-AZ31B 합금 TIG 용접부의 기계적 특성과 미세조직 변화에 미치는 용접조건의 영향 (The Influence of Welding Conditions on Mechanical Properties and Microstructural Change of TIG Welded Joint in Stress Relieve Heat Treated Mg-AZ31B Alloy)

  • 김용길;정동석;배차헌
    • 열처리공학회지
    • /
    • 제17권4호
    • /
    • pp.230-235
    • /
    • 2004
  • Present work was carried out to investigate the influence of welded conditions, such as welding current, diameter of welding wire on the microstructural change and mechanical properties of TIG welded joint in AZ31B Mg alloy. It was found that good and sound welded joint was achieved in all welding conditions. The grain size decreased with increasing welding current and decreasing diameter of welding wire. Also, the second phases were homogeneously distributed in the grain and grain boundary as decreasing welding current and diameter of welding wire. The ${\beta}$ discontinuos precipitates were observed in the welded joint, but this microstructure has not been reported by previous researchs in AZ31B Mg alloy. The hardness value is affected by the existence state of the second phase and the hardness of the welded joint region is lower than the other regions in welded AZ31B Mg alloy. The strength of the welded joint region was influenced by the grain size and has more than 90%, compared to that of ASTM standard specification.

루트부 갭이 있는 양면 필릿용접 이음부의 용접잔류응력 분포 (Distribution of Welding Residual Stresses in T-joint Weld with Root Gap)

  • 방한서;김성환;김영표;이창우
    • 대한조선학회논문집
    • /
    • 제39권3호
    • /
    • pp.81-88
    • /
    • 2002
  • 용접구조물의 루트부는 외력에 의한 응력 집중에 의해 파손되기 쉽다. 따라서 구조물의 안전성 및 신뢰성 측면에서 홈 가공한 그루브 용접에 의한 완전용입 용접이 일반적으로 요구되어진다. 하지만 필릿 T-이음부 용접은 루트부의 갭과 같은 불완전 용입부를 만들어내기 쉬움에도 불구하고 홈 가공 시간 및 용접봉 소모량을 줄이기 위해 이러한 필릿용접이 자주 행해지고 있다. 따라서, 본 연구에서는 필릿 용접구조물의 플래이트(또는 플랜지)와 웨브 부분에 발생하는 용접잔류 응력과, 특히 불완전 용입에 의한 루트부 갭을 갖는 양면 T-이음부의 노치부분에 발생하는 잔류응력 분포를 해석하고자 하였다. 해석을 위해서 서브머지드 아-크 용접에 의한 단층 및 다층패스용접 모델을 선정하였으며, 열전도 및 열탄소성 이론을 고려한 유한요소 프로그램을 사용하였다.

Effect of Resistance Spot Welding Parameters on AA1100 Aluminum Alloy and SGACD Zinc coated Lap Joint Properties

  • Chantasri, Sakchai;Poonnayom, Pramote;Kaewwichit, Jesada;Roybang, Waraporn;Kimapong, Kittipong
    • International Journal of Advanced Culture Technology
    • /
    • 제3권1호
    • /
    • pp.153-160
    • /
    • 2015
  • This article is aimed to study the effects of resistance spot welding (RSW) on the lap joint properties between AA1100 aluminum alloy and SGACD zinc coated steel and its properties. The summarized experimental results are as follows. The summarized experimental results are as follows. The optimum welding parameters that produced maximum tensile shear strength of 2200 N was a welding current of 95 kA, a holding time of 10 cycles, and a welding pressure of 0.10 MPa. Increasing of welding current, increased the tensile shear strength of the joint and also increased the amount of aluminum dispersion at the joint interface. The lap joint of steel over the aluminum (Type I) showed the higher joint tensile shear strength than a lap joint of aluminum over the steel (Type II). The indentation depth and the ratio of the indentation depth to the plate thickness decreased when the welding current was increased in the type I lap joint and also decreased when the welding current was decreased in the type II lap joint. The interface structure showed the formation of the brittle $FeAl_3$ intermetallic compound that deteriorated the joint strength.

외관검사를 통한 한국형 철근자동가스압접기의 압접성능 연구 (A study on the welding performance of korean automatic gas pressure welding machine by external appearance investigation)

  • 서덕석
    • 한국건축시공학회지
    • /
    • 제8권6호
    • /
    • pp.161-166
    • /
    • 2008
  • This study is focused on the welding performance of automatic gas pressure welding machine adapted to korean construction site by external appearance investigation. As gas pressure welding is more economical and has good performances compared with other steel bar jointing methods, as arc welding and mechanical joint etc, in Japan, the gas pressure welding is one of the typical connection of steel reinforcement when connecting the D29 and thicker steel bars, But in Korea, gas pressure welding joint method is not widely used caused by the shortage of skilled workers. so to activate the gas pressure welding in Korea, the automatic gas pressure welding machine is developed. In this study, the welding performances of gas pressure welding joint samples using korean automatic gas pressure welding machine are measured by external appearance investigation - blown diameters, blown length, welding face disagreement, central axis eccentric ratio, bending, sag and crack. The results of welding performances on the gas pressure welding joint samples show that samples are satisfied with the standard value regulated in KS D 0244 and JIS Z 3120.