틈새가 존재하는 이종강 레이저 용접부의 열유동에 관한연구 (A Study on Heat Flow of Laser-Welded Dissimilar Steel Joints with Gap)

  • 양해석
    • 한국군사과학기술학회지
    • /
    • 제10권3호
    • /
    • pp.5-15
    • /
    • 2007
  • A welding structures is generally composed of dissimilar steel materials in order to reduce weight cost, and has a gap to fill the welding agent. Also, heat flow analysis should be fulfilled for structure existing of gap to figure out residual stress which is generated after welding. Since mechanical properties of welding structure composed of dissimilar steel is more fragile than mechanical properties of welding structure consisted of same material, heat flow analysis verifying this should be fulfilled as well. Therefore, on this research, heat flow analysis about dissimilar steel weldment consisted of gap existing AISI304 and AISI630 is practiced so that it could be a basic data of research about mechanical properties of gap existing dissimilar steel welding part which is going to be studied later on. During heat flow analysis, heat input model which based on Gaussian profile and using volume heat flux was newly consisted and applied. In addition, for verifying of analysis on this research, gap existing dissimilar steel weldment which had gap of 0.25mm and was welded using Nd-YAG. The welding profile and temperature distribution for weldment during welding was compared to the result which was gotten through heat flow analysis. Both of those results corresponded each other.

박판 GMA 용접에서 단락 주파수를 이용한 이면비드의 제어에 관한 연구 (A Study on the Back Bead control by Using Short Circuit Frequency in GMA Welding of Sheet Metal)

  • 안재현;김재웅
    • Journal of Welding and Joining
    • /
    • 제13권4호
    • /
    • pp.75-84
    • /
    • 1995
  • In GMA welding of sheet metal, the short circuit metal transfer mdoe is preferred because of its low heat input and capability of bridging the root gap. The molten electrode is transferred to the workpiece during repectitive short circuit in the model. The waveform of welding current or voltage and the frequency of short circuiting are affected by a number of factors including: magnitude of welding current and voltage, root gap, electrode extension, power supply characteristics, and so on. In this study experimental models were proposed, which are able to determine the relationship between the root gap and short circuit frequency and the relationship between the root gap and appropriate welding speed that produces the good quality of back bead without burn through. Using the experimental models, the root gap can be obtained from measuring the short circuit frequency, and then the appropriate weldig speed to the root gap can be determined. Thus a back bead control system was constructed by controlling the welding speed for maintaining the quality of back bead. The developed system has shown the successful capability of back bead control.

  • PDF

조선용 강재의 $CO_2$레이저 GMA 하이브리드 용접에서 갭 브리징 능력 향상기술 개발 (Improvement of Gap Bridging Ability in $CO_2$ Laser-GMA Hybrid Welding)

  • 채현병;김철희;김정한;이세헌
    • Journal of Welding and Joining
    • /
    • 제24권5호
    • /
    • pp.49-56
    • /
    • 2006
  • For laser welding in shipbuilding industry, gap bridging capability is one of the most important characteristics to achieve the high productivity and good weld quality. Recently, laser-GMA hybrid welding process is regarded as a distinctive method to overcome the tight gap tolerance with improving the productivity. In this study, the influence of process parameters on the bead formation was experimentally analyzed and the relationship between the process parameters and geometric imperfections was investigated. It was revealed that undercut, excessive weld metal, excessive penetration and incompletely filled groove were the major geometric imperfections. The optimized wire feeding and arc pressure were necessary to ensure the gap bridging ability. The approach to select the process parameters was conducted for butt welding with up to 2mm joint gap, in which the sound weld beads were generated without changing the welding speed.

교량용 후판 다층용접시 잔류응력과 변형에 미치는 루트간격의 영향 (Effects of Root Gap on Residual Stresses and Deformation in the Multi-Pass Weld of Thick Plates for Steel Bridge)

  • 장경복;김하근;강성수
    • Journal of Welding and Joining
    • /
    • 제17권1호
    • /
    • pp.88-96
    • /
    • 1999
  • The effects of root gap on welding residual stress and deformation are dealt with the multi-pass weldment with three kinds(0, 6, 30mm) of root gap by F.E.M common code, and then compared with experiment data. In this analysis, an 100% ramp heat input model was used to avoid numerical convergence problem due to an instantaneous increase in temperature near the fusion zone, and the effect of a moving arc in a two dimensional plane was also included. During the analysis, a small time increment was applied in a period with instantaneous temperature fluctuation while a large time increment was used in the rest period. The residual stress is distributed as symmetric types and maximum value is also equivalent when the weldment with 0mm and 6mm root gap is welded. In the case of 30mm root gap welding, the distribution of the residual stress extends over a wide range as asymmetric types due to the built-up weld, and most of the residual stress is biased in the side of a built-up weld part. In case of 0mm gap welding and 6mm gap welding, a little angular distortion occurs, but the level of deformation is small. When the weldment with 30mm root gap is welded, the angular deformation of the asymmetric types, however, occurs larger than the other specimens. The experimental and the analytic results show good coincidence and indicate that the welding residual stress and deformation distribution of 30 mm root gap specimen may be asymmetric and the amplitude is larger than those of root gap specimen under standard.

  • PDF

하이드로포밍용 열연강재의 레이저 용접성 및 기계적 특성 (Laser weldability and mechanical behavior of hot rolled steels for hydroforming applications)

  • 이원범;이종봉
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2003년도 춘계학술발표대회 개요집
    • /
    • pp.84-86
    • /
    • 2003
  • The laser welding and its analysis of thin-sheet carbon steels were carried out with high power CO$_2$1aser. Bead on plate welding of thin sheet was examined to investigate the effect of weld variables of laser welding, and to obtain optimum welding condition. Butt-welding was also carried out to show the effect of gap on the laser weldability of thin sheet. At high welding speed, the partial penetration was obtained by low heat input. Otherwise, porosity was formed in the bead at low weld speed because of too many heat input. The maximum gap tolerance on laser welding was observed to be about 0.2mm. This gap size has good relationship with beam size of laser spot(about 0.3mm). The formability of welded sheet was about 80% value of base metal and the gap size has not affected on the formability, although weld quality is dependent on the gap size.

  • PDF

스테인레스강에 대한 전자빔용접과 협개선TIG 용접수축량 비교 (The comparison of weld shrinkage between Electron beam welding and Narrow-gap TIG welding for stainless steel)

  • 김용재;정원회;심덕남;정인철
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 추계학술발표대회 개요집
    • /
    • pp.76-78
    • /
    • 2004
  • The phenomenon of weld shrinkage mainly occurs owing to residual stress by heating, which largely effects on welding quality, Actually as the shrinkage rate depends on the weld deposit amount, so it is desired that the sectional area of weld joint shall be reduced. In this respect the Electron beam welding has more profitable position compare to Narrow-gap TIG welding which is even superior to other arc welding processes. In case of thick austenitic stainless steel the shrinkage rate of Electron beam welding has about $10\%$ of Narrow-gap TIG welding's, which means that residual stress is a lot less than that of Narrow-gap TIG welding. And heat input and welded section area also indicate large difference between two processes.

  • PDF

이종두께 강판의 $CO_2$ 레이저 용접 및 성형성 ($CO_2$ Laser Beam Welding and Formability of Steel Plates with Different Thicknesses)

  • 서정;한유희;김정오;이영신
    • Journal of Welding and Joining
    • /
    • 제14권1호
    • /
    • pp.82-91
    • /
    • 1996
  • The maximum butt-joint gap size in $CO_2$ laser beam welding of SAPH steel plates with different thicknesses and its bending formability were studied. In the range of the gap size$\geq$0.1mm, the optimal butt welding speed was faster than that of no gap (air gap) condition. This behaviour was independent on the difference of thickness at any combination. Also, the allowable gap size in steel plates with different thicknesses was larger than with same thicknesses. In the range of $T/T_0$(bead shape) $\geq$ 0.8, good bending formability was obtained at any combination of thickness. The formability was improved by reducing the hardness in weld bead using pre-heating process. Finally, FEM result of the laser beam welded underframe with different thicknesses was compared to that of the conventional spot welded underframe.

  • PDF

GMAW 루트패스 이면비드 용접에서 아크력제어에 의한 갭변동 극복 방법 (Method to Overcome Gap Variation by Control of Arc Force in Root Pass Welding for Back Bead by GMAW)

  • 손창희;조상명
    • Journal of Welding and Joining
    • /
    • 제29권6호
    • /
    • pp.77-81
    • /
    • 2011
  • In most industry, manual GTAW welding is preferred for formation of stable back bead in root weld of butt joint. However, manual GTAW welding has low productivity as compared with GMAW, also it has unstable bead quality which depend on skilled workers. So it is necessary to develop process of root pass welding by using automation GMAW that have stable back bead formation and high productivity. In this paper, the design of U-groove with 3mm root face was applied to extend the tolerance of misalignment in condition of standard root gap 1.5mm. Consequently, for the formation of stable back bead in root pass of butt welding, in case of the narrow root gap(0.5mm) the large arc force was applied by increasing the current and voltage. In case of the large root gap(2.5mm), the small arc force was applied by decreasing the current and voltage. Considering the various root gap, the required deposited metal was controlled by welding speed only.

루트간격이 용접부의 기계적 성질과 미세조직에 미치는 영향에 관한 연구 (A Study on the Effects of Root Gap on Mechanical Properties and Microstructure of Weldment)

  • 이원근;장경복;강성수
    • 한국정밀공학회지
    • /
    • 제16권10호
    • /
    • pp.187-193
    • /
    • 1999
  • Dimensional difference by welding deformation is usually occurred at steel bridge manufacturting or multi-pass welding used at joining of thick plates. Be this, root gap out of standard is frequently developed at butt weld joints. For example, although standard root gap below 6mm at butt weld joints of plates under 15mm thickness, maximum 30mm root opening is developed at the weld field. At this case, 24mm parts out of standard is generally built up. But, there are no accumulated data and restriction about this built up welding pars. In this study, therefore, the accumulation of data for built up parts and the verification of the mechanical properties of weld part as root gap is performed. It is included that tensile, bending, impact, hardness test and microstructural review for each welding specimen of 0mm, 6mm, 30mm root opening.

  • PDF

후판 자동용접을 위한 용접물의 갭 측정 (Recognition of Gap between base Plates for Automated Welding of Thick Plates)

  • 이화조
    • 한국정밀공학회지
    • /
    • 제16권4호통권97호
    • /
    • pp.37-45
    • /
    • 1999
  • Many automated welding equipment are used in the industry. However, there are some problems to get quality welds because of the geometric error, thermal distortion, and incorrect joint fit-up. These factors can make the gap between base plates in case of a thick plate welding. The welding product with the quality welds can not be obtained without consideration of the gap. In this paper, the robot path and welding conditions are modified to get the quality weld by detecting the position and size of the gap. In this work, a low-priced laser range sensor is used. The 3-dimensional information is obtained using the motion of a robot, which holds a laser range sensor. The position and size of the gap is calculated using signal processing of the measured 3-dimensional information of joint profile geometry. The data measured by a laser range sensor is segmented by an iterative end point method. The segmented data is optimized by the least square method. The existence of gap is detected by comparing the data with the segmented shape of template. The effects of robot measuring speed and gap size are also tested. The recognizability fo the gap is verified as good by comparing the real joint profile and the calculated joint profile using the signal processing.

  • PDF