• 제목/요약/키워드: wear life diagram

검색결과 5건 처리시간 0.021초

마모수명평가를 위한 TiN 경질박막의 마찰 및 마모특성에 관한 연구 (A Study on Friction and Wear of TiN Film for the Wear-life Prediction)

  • 정기훈;이영제
    • Tribology and Lubricants
    • /
    • 제13권3호
    • /
    • pp.28-32
    • /
    • 1997
  • Indentation, scratch and sliding tests were carried out in this paper to predict the critical loads and the failure modes of TiN-coated specimen. The test specimens were S20C steels with three different substrate hardness, roughness and coating thickness. The scratch test shows that the coating thickness has more dominant effect on the critical load of coated disk than the hardness and the roughness. Using the percent contact load, the ratio of sliding load to the critical scratch load, the cycles to failure are measured to predict the wear-life of TiN film. On the wear-life diagram the percent loads and the cycle to failure show the good linear relation on semi-log coordinate. With decreasing loads, the diagram shows the wear-limit at which the coated disk survives more than 4000 cycles.

TiN 박막 처리될 베어링 볼의 마모 수명 및 메커니즘에 관한 연구 (A Study on Wear Life and Mechanisms of TiN Coated Bearing Balls against Steel Disks)

  • 한지훈;조정우;이영제
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2000년도 제32회 추계학술대회 정기총회
    • /
    • pp.378-384
    • /
    • 2000
  • This paper presents the results of the repeated sliding tests to determine the wear-life of TiN coated AISI 52100 bearing balls deposited by PVD method and to show the wear mechanisms of those. The sliding tests were carried out using a ball-on-disk tribometer under ambient conditions. The coefficient of friction, wear volume and the cycles to failures of TiN coated bearing balls were measured with different normal loads and roughness of lower specimens. On the wear-life diagram, the normal loads and the cycles to failure showed the good linear relation on log-log coordinate. With a decreasing normal load, the diagram showed that the wear-limits, at which the coated bearing balls survived more than 4000cycles were under 0.1N of the normal load.

  • PDF

마찰 및 음향방출 신호를 이용한 CrN 코팅의 마모수명 평가 (Life Evaluation of CrN Coatings due to Wear Using Friction and Acoustic Emission Sensor)

  • 조정우;이영제
    • Tribology and Lubricants
    • /
    • 제15권4호
    • /
    • pp.328-334
    • /
    • 1999
  • Acoustic emission (AE) sensor was used to evaluate the wear-life of CrN-coated steel disks with 1 $\mu\textrm{m}$ and 4 $\mu\textrm{m}$ coating thickness. The relationship between Af and friction signal from scratch test and sliding test was investigated. The first spatting of CrN film was detected by AR signals in the early stage of coating failures, and overall failures by friction signals. Therefore, the conservative design for coating-life should be done using the results of AE signals. Using the percent contact load, the ratio of sliding normal load to the critical scratch load and the number of cycles to failure was measured to predict the wear-life of CrN film. On the wear-life dia-gram the percent contact loads and the number of cycles to failure showed a good linear relationship on the log coordinate. As the load percentage was decreased, the diagram showed that the wear-limits, at which the coated steels survived more than 35,000 cycles, were about 4∼5% of the critical scratch loads.

AE 센서를 이용한 CrN 코팅의 마찰특성에 관한 연구 (An Experimental Study on the Friction of CrN Coated Specimen using the Acoustic Emission Sensor)

  • 조정우;이영제
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1999년도 제29회 춘계학술대회
    • /
    • pp.215-219
    • /
    • 1999
  • One of the innovative physical methods that provide insight into the basic processes which determine friction and wear behavior of coated machine tools is acoustic emission (AE). In this study, an investigation of the relation between AE and friction signal produced during repeated sliding test is presented. The material of test specimens is CrN coated 0.2% plain carbon steel with 1 Um thickness. The obtained results demonstrate that AE signal is very related with friction, and AE signal is more sensitive than friction when CrN coated film come off the substrate.

  • PDF

HSS공구와 PVD 코팅기술의 영향 (Impact of PVD Coating Technology on HSS Tool)

    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.899-904
    • /
    • 2001
  • The impact of PVD coatings can be summed up in practical terms: this technology historically complements the best designed tool substrates to enhance cutting performance. PVD coatings are now incorporated in 25% of all HSS tools. The functionality is to extend the machining speed range, improve wear resistance at the cutting edge, and reduce friction at chip/tool contact areas to allow easier chip evacuation. These translate to a larger safe zone, as discussed in the failure mode diagram, for better productivity and higher reliability in machining operations of the customer. PVD coatings therefore represent an enabling technology that extends the application range of cutting tools in response to modern industrial needs. PVD coatings prolong the product life cycle of HSS tools and help this "mature" material to hold its territory against the advent of the newer hardmetal and ceramic tool materials. There is a lot of competitive life left particularly in PVD coated HSS endmills, drills, threading/tapping tools. PM HSS technology further increases the possibilities.ibilities.

  • PDF