• Title/Summary/Keyword: water to cement ratio

Search Result 1,097, Processing Time 0.028 seconds

Effect of Substituting Normal-Weight Coarse Aggregate on the Workability and Mechanical Properties of Heavyweight Magnetite Concrete (중량 자철석 콘크리트의 유동성 및 역학적 특성에 미치는 보통중량 굵은골재 치환율의 영향)

  • Mun, Jae-Sung;Mun, Ju-Hyun;Yang, Keun-Hyeok;Lee, Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.4
    • /
    • pp.439-446
    • /
    • 2013
  • The objective of this study is to evaluate the workability and various mechanical properties of heavyweight magnetite concrete and examine the reliability of the design equations specified in code provisions. The main parameters investigated were the water-to-cement ratio and substitution level of normal-weight coarse aggregate (granite) for magnetite. The oven-dried unit weight of concrete tested ranged between 2446 and $3426kg/m^3$. The measured mechanical properties included compressive strength development, stress-strain curve, splitting tensile strength, moduli of elasticity and rupture, and bond stress-slip relationship of concrete. Test results revealed that the initial slump of heavyweight magnetite concrete increased as the substitution level of normal-weight coarse aggregate increases. The substitution level of normal-weight coarse aggregate had little influence on the compressive strength and tensile resistance capacity of heavyweight concrete, while it significantly affected the modulus of elasticity and stress-strain curves of such concrete. The design equations of ACI 349-06 and CEB-FIP provisions mostly conservatively predicted the mechanical properties of heavyweight magnetite concrete, but the empirical equations for modulus of elasticity and splitting tensile strength need to be modified considering the unit weight of concrete.

Characteristics of sound absorption materials by using ecological aggregates (에코골재를 사용한 흡음재의 특성)

  • Kim, Kang-Duk;Ryu, Yu-Gwang;Kim, Yoo-Taek
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.18 no.6
    • /
    • pp.264-270
    • /
    • 2008
  • Ecological lightweight aggregates were made by using the wastes come from various industrial fields. Wastes were crushed and pulverized by mills and a certain portions of wastes were mixed and formed by pelletizer like small beads. The formed lightweight aggregates were finally sintered with $1125^{\circ}C$/15 min conditions by using rotary kiln. Lightweight concrete sound absorbers were made of ecological lightweight aggregates K73 (Coal bottom ash 70 wt%: Dredged soil 30 wt%) and K631 (Clay 60 wt%: Stone sludge 30 wt%: Spent bleaching clay 10 wt%). For the reference, lightweight concrete sound absorbers made of DL (German made 'L' company LWA) were also made under the same conditions. Sound absorption characteristics were observed and measured according to the kinds of aggregates, water/cement ratio (W/C=20, 25, and 30%), and designed pore rates (V=20, 25, and 30%). The pore rates of the lightweight concrete sound absorber were turned out to be 5 to 10% higher than designed ones. Absorption coefficient of the lightweight concrete sound absorber by using K631 aggregates with W/C=20% and V=25% conditions was 0.88 at 1000 and 3150 Hz from the measurement by the impedance tube.

Properties and Prediction Model for Ultra High Performance Fiber Reinforced Concrete (UHPFRC): (I) Evaluation of Setting and Shrinkage Characteristics and Tensile Behavior (초고성능 섬유보강 콘크리트(UHPFRC)의 재료 특성 및 예측모델: (I) 응결 및 수축 특성과 인장거동 평가)

  • Yoo, Doo-Yeol;Park, Jung-Jun;Kim, Sung-Wook;Yoon, Young-Soo
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.32 no.5A
    • /
    • pp.307-315
    • /
    • 2012
  • Recently, ultra high performance fiber reinforced concrete (UHPFRC) having over 180 MPa compressive strength and 10 MPa tensile strength has been developed in Korea. However, UHPFRC represents different material properties with normal concrete (NC) and conventional high performance concrete (HPC) such as a high early age autogenous shrinkage and a rapid dry on the surface, because it has a low water-binder ratio and high fineness admixtures without coarse aggregate. In this study, therefore, to propose suitable experimental methods and regulations, and to evaluate mechanical properties at a very early age for UHPFRC, setting, shrinkage and tensile tests were performed. From the setting test results, paraffin oil was an appropriate material to prevent drying effect on the surface, because if paraffin oil is applied on the surface, it can efficiently prevent the drying effect and does not disturb or catalyze the hydration of cement. From the ring-test results, it was defined that the shrinkage stress is generated at the time when the graph tendency of temperature and strain of inner steel ring is changed. By comparing with setting test result, the shrinkage stress was firstly occurred as the penetration resistance of 1.5 MPa was obtained, and it was about 0.6 and 2.1 hour faster than those of initial and final sets. So, the starting time of autogenous shrinkage measurement (time-zero) of UHPFRC was determined when the penetration resistance of 1.5 MPa was obtained. Finally, the tensile strength and elastic modulus of UHPFRC were measured from near initial setting time by using a very early age tensile test apparatus, and the prediction models for tensile strength and elastic modulus were proposed.

Fundamental Properties of Porous Concrete According to the Sizes of Aggregate (골재 크기에 따른 포러스콘크리트의 기초물성에 관한 실험적 연구)

  • 김무한;백용관;강석표;김용로;김재환
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.5
    • /
    • pp.438-446
    • /
    • 2001
  • Recently, porous concrete has been used for the purpose of decreasing the load of earth environment. It consists solely of cement, water and uniform-sized coarse aggregate. And its fundamental properties will be considerably affected by the physical properties of aggregate because the aggregate occupies for the most part in its mix proportion. For such a reason, this study was carried out to investigate the influence of the sizes and kinds of aggregate for the fundamental properties of porous concrete. It showed that the fundamental properties of porous concrete were the similar value in all sizes of aggregate except in the case of using the 2.5∼5㎜ aggregate and were varied according to the kinds of aggregate. In particular, compressive strength of porous concrete using 2.5∼5㎜ aggregate was more higher than that using other aggregate, and its void ratio and coefficient of permeability was lower. And the maintenance capacity of permeability of porous concrete was varied by the sizes and the kinds of aggregate. In particular, it was greatly decreased in case of using the 2.5∼5㎜ aggregate. And unlike dynamic modulus of elasticity of ordinary concrete, that of porous concrete was very high value in early ages and was slowly increased after that time.

Rapid Chloride Penetration Test for Concrete Based on the Electrochemical Method (전기 영동법에 기초한 콘크리트의 급속 염소이온 확산 특성 평가)

  • Oh, Sang-Gyun;Park, Dong-Cheon
    • Journal of Navigation and Port Research
    • /
    • v.34 no.10
    • /
    • pp.787-792
    • /
    • 2010
  • It is necessary to predict the penetration of chloride ions for designing RC construction in marine environments. However, it takes a long time to obtain chloride migration coefficients. Therefore, the rapid chloride penetration test (RCPT) is generally used to shorten the test time. But there is a difference between chloride migration coefficients determined by rapid chloride penetration tests and those based on exposure in marine environments. In this study, we evaluated the effect on the chloride ion migration coefficient caused by a change in voltage and NaCl concentration. We also compared the relationship between the chloride ion migration coefficient by RCPT and that by exposure in marine environments. As a result of the experiments, we found that there is only a small change in the experimental factors based on changes in voltage and NaCl concentration and since they are so small, we can conclude that they are in the range of experimental error and test results from chloride ion migration coefficients by RCPT and exposure were very different from each other. In the exposure experiments, when the water-cement ratio was increased, the smaller fine air gaps in concrete affected the chloride ion migration coefficient.

Effect of Artificial Granular Zeolite(AGZ) on Purification of Heavy Metals in Wastewater and Alleviation or Rice Seeding Growth Damage (입상 인공제올라이트를 이용한 중금속 폐수 정화와 벼 유묘 생육장해 경감)

  • Lee, Deog-Bae;Lee, Kyeong-Bo;Lee, Sang-Bok;Kim, Jae-Duk;Henmi, Teruo
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.32 no.4
    • /
    • pp.446-451
    • /
    • 1999
  • This study was carried out to investigate some mineralogical characteristics of Artificial Granular Zeolite (AGZ) and effect of AGZ on purification and alleviation of rice seedling damages of mine wastewater containing heavy metals. AGZ had mainly representative Na-P1 peaks and some $C_3S$ peaks of Portland cement in X-ray diffractogram. Differential thermal analysis represented that AGZ had weak endothermic peak around $130^{\circ}C$ and new deep endothermic peak around $750^{\circ}C$ as compared to powdery artificial zeolite. The ranking of heavy metals removals by AGZ, was lead> copper> cadmium> zinc in the synthetic wastewater. Root growth of rice seedling was greatly inhibited in the mine wastewater, and died after all. As AGZ treated into the mine wastewater with the ratio 1 : 50 (W : V) for one day or 1 : 100 for 4 days, the concentrations of heavy metals in the mine wastewater were decreased to below the critical concentration for agricultural use. And rice seedlings were grew with little damages in the purified water by AGZ.

  • PDF

Flow and Strength Characteristics of the Lightweight Foamed CLSM(Controlled Low-Strength Materials) with Coal Ash (석탄회를 활용한 경량기포유동화재의 플로우 및 강도 특성)

  • Lee, Seungjun;Lee, Jonghwi;Chae, Hwiyoung;Chun, Byungsik
    • Journal of the Korean GEO-environmental Society
    • /
    • v.12 no.10
    • /
    • pp.73-82
    • /
    • 2011
  • Coal ash of industial by-products was not recycled about 30% in total emissions. Moreover, it caused environmental pollution as well as wasted unnecessary expenses and time. Currently, fly ash(FA) is recycled as construction material however ponded ash(PA) is mostly buried. Lightweight foamed Controlled Low-Strength Materials(CLSM) evaluated in this study reduces unit weight by mixing foam in the traditional Controlled Low-Strength Material and has lightweight and flowability to be available for backfill materials in construction. Flow test, unconfined compressive strength test, and foamed-slurry unit weight test were performed in this study and the applicability of lightweight foamed CLSM for construction materials was evaluated. The results indicate that the mixture ratio(PA:FA) ranging from 70:30 to 50:50, cement of 7%, foam of 2~3%, and water content of 26.5~29.5% were required to satisfy the following standards such as flow value(i.e., 20cm), unconfined compressive strength(i.e., 0.8~1.2MPa), and foamed-slurry unit weight(i.e., $12{\sim}15kN/m^3$).

Engineering Characteristics of Wet-mixing Solidified Soil in Pavement Surfacing (습식 경화교반토 포장의 공학적 특성)

  • Yoo, Ji-Hyeung;Shu, Dong-Hyuk;Lee, Seong-Won
    • International Journal of Highway Engineering
    • /
    • v.6 no.3 s.21
    • /
    • pp.1-7
    • /
    • 2004
  • Roads, like bikeways, parkways and walks, are to be just capable of supporting light traffic and traveling public, but they are required to be human friendly and environmental-oriented. Lately soil-solidifier mixture, a kind of soil-cement, has developed and has been applied to the recycling and environment-oriented pavement as the surfacing material. Soil-solidifier pavement structure has been designed by only experience. To design this pavement mechanically, it is necessary to find out basic engineering properties of soil-solidifier mixture. This study focuses on finding out mechanical characteristics of the mixture according to mixture proportions and aging. Test molds with various mixture proportions are made, and then unconfined strength tests are performed for test molds with aging of the mixture. As the result of this study, it is found that the strength of the mixture increases with amount of cement and that maximum strength is achieved at 6%$\sim$8% of the ratio of solidifier and water. The strength increase rapidly until 14 days, after then slowly. After 28 days the strength of the mixture approaches to the constant value. The heat of hydration during curing of the mixture is measured no significantly. It also shows that temperature characteristics of the mixture is similar to that of soil. Since this mixture is mixed with soil and is able to improve engineering problems in pavement due to temperature, this mixture is expected to use effectively in the environment-oriented pavement for light traffic.

  • PDF

Influence of Temperature on Chloride Ion Diffusion of Concrete (콘크리트의 염화물이온 확산성상에 미치는 온도의 영향)

  • So, Hyoung-Seok;Choi, Seung-Hoon;Seo, Chung-Seok;Seo, Ki-Seog;So, Seung-Young
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.1
    • /
    • pp.71-78
    • /
    • 2014
  • The long term integrity of concrete cask is very important for spent nuclear fuel dry storage system. However, there are serious concerns about early deterioration of concrete cask from creaking and corrosion of reinforcing steel by chloride ion because the cask is usually located in seaside, expecially by combined deterioration such as chloride ion and heat, carbonation. This study is to investigate the relation between temperature and chloride ion diffusion of concrete. Immersion tests using 3.5% NaCl solution that were controlled in four level of temperature, i.e. 20, 40, 65, and $90^{\circ}C$, were conducted for four months. The chloride ion diffusion coefficient of concrete was predicted based on the results of profiles of Cl- ion concentration with the depth direction of concrete specimens using the method of potentiometric titration by $AgNO_3$. Test results indicate that the diffusion coefficient of chloride ion increases remarkably with increasing temperature, and there was a linear relation between the natural logarithm values of the diffusion coefficients and the reciprocal of the temperature from the Arrhenius plots. Activation energy of concrete in this study was about 46.6 (W/C = 40%), 41.7 (W/C = 50%), 30.7 (W/C = 60%) kJ/mol under a temperature of up to $90^{\circ}C$, and concrete with lower water-cement ratio has a tendency towards having higher temperature dependency.

Basic Research of Self Compacting Concrete Using Alkali-Activated Slag Binder (알칼리 활성 슬래그 결합재를 이용한 자기충전 콘크리트의 기초 연구)

  • Song, Keum-Il;Shin, Gyeong-Sik;Gong, Min-Ho;Song, Jin-Kyu
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.6
    • /
    • pp.657-665
    • /
    • 2013
  • The purpose of this study is the basic research of self-compacting concrete using Alkali-Activated Slag (AAS) binder in order to emphasize the durability of structures and facilitate casting the fresh concrete in field. The AAS binder emitted low carbon dioxide ($CO_2$) is eco friendly material of new concept because AAS products not only emit little $CO_2$ during production but also reuse the industrial by-products such as ground granulated blast-furnace slag (GGBS) of the steel mill. Until now, almost of domestic and foreign research are using Ordinary Portland Cement (OPC) for self-compacting concrete, and also, nonexistent research about AAS. The self-compacting concrete must get the performance of flowability, segregation resistance, filling and passing ability. Nine concrete mixes were prepared with the main parameter of unit amount of binder (400, 500, 600 $kg/m^3$) and 3 types of water-binder (W/B) ratio. The results of test were that fresh concretes were satisfied with flowability, segregation resistance, and filling ability of JSCE. But the passing ability was not meet the criteria of EFNARC because of higher viscosity of AAS paste than OPC. This high viscosity of AAS paste enables the manufacturing of self compacting concrete, segregation of which does not occur without the using of viscosity agent. It is necessary that the development of high fluidity AAS binders of higher strength and the study of better passing ability of AAS concrete mixes in order to use self compacting AAS concrete in field.