Evaluation of Chloride Behavior and Service Life in Long-Term Aged FA Concrete through Probabilistic Analysis (장기재령 FA 콘크리트에 대한 염화물 거동 및 확률론적 염해 내구수명 평가)

  • Yoon, Yong-Sik;Kwon, Seung-Jun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.3
    • /
    • pp.276-285
    • /
    • 2020
  • In this study, accelerated chloride diffusion tests were performed on OPC(Ordinary Portland Cement) and FA(Fly Ash) concrete considering three levels o f W/B(Water to Binder) ratio o n 1,095 curing days. The accelerated chloride diffusion coefficient and the passed charge were evaluated in accordance with Tang's method and ASTM C 1202, and the resistance performance to chloride attack improved over time. FA concrete showed excellent resistance performance against chloride penetration with help of pozzolanic reaction. As the result of the passed charge, FA concrete showed durability improvement, "low" grade to "very low" grade, but OPC concrete changed "moderate" grade to "low" grade at 1,095 curing days. After assuming the design variables used for durability design as normal distribution functions, the service life of each case was evaluated by the probabilistic analysis method based on MCS(Monte Carlo Simulation). In FA concrete, the increase of probability of durability failure was lower than that of OPC concrete with increasing time, because the time-dependent coefficient of FA concrete was up to 3.2 times higher than OPC concrete. In addition, the service life by probabilistic analysis was evaluated lower than the service life by deterministic analysis, since the target probability of durability failure was set to 10%. It is considered that more economical durability design will be possible if the mo re suitable target probability of durability failure is set for various structures through researches on actual conditions and indoor tests under various circumstances.

A Fundamental Research on Determining Segregation Boundary using Rheological Parameters for 21 and 24MPa grade of Normal Strength Concrete (레올로지 정수를 이용하여 21, 24MPa급 일반강도 콘크리트의 재료분리 경계를 판단하기 위한 기초연구)

  • Lee, You-Jung;Lee, Young-Jun;Han, Dongyeop
    • Journal of the Korea Institute of Building Construction
    • /
    • v.20 no.5
    • /
    • pp.399-407
    • /
    • 2020
  • The aim of the research is to provide the boundary conditions for segregation of normal strength grade and high fluidity concrete mixture (so called mid-fluidity concrete) with rheology parameters. Since the normal strength grade concrete mixture has a relatively high water-to-cement ratio and no SCMs, it is easy to be segregated when superplasticizer is added. Hence, to achieve the mid-fluidity concrete of normal strength grade and high fluidity, preventing segregation of the mixture is inevitable. In this research, using two superplasticizers with different solid concentrations, the flow behaviors and rheological behaviors were assessed by increasing fluidity until the segregation happened. According to the experiment in this research, an unusual behavior in rheology parameters was observed when the concrete mixture started to be segregated. From this results and report, it is expected to contribute on the definition of segregation with rheological test methods.

An Experimental Study on the Properties of Engineering and Shrinkage Cracking Reduction of Fiber Reinforced Concrete Using Recycled Fine Aggregate (섬유보강 순환잔골재 콘크리트의 공학적 특성 및 수축균열저감특성에 관한 실험적 연구)

  • Kim, Gyu-Yong;Nam, Jeong-Soo;Kim, Moo-Han;Lee, Do-Heun;Song, Ha-Young
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.3
    • /
    • pp.82-89
    • /
    • 2009
  • Recently, the study is progressing actively about manufacture skill of concrete for promoted recycled aggregate and concrete made into recycled aggregate in the construction production field. But, application and study about recycled fine aggregate insufficient compared to recycled coarse aggregate. So, in this study, it presents basic data for development of environmental load reduction fiber reinforcement recycled fine aggregate concrete by comparison and investigation about engineering properties and shrinkage cracking of fiber reinforcement recycled find aggregate concrete for increasing shrinkage cracking reduction and long term stability of environmental load reduction concrete used recycled fine aggregate. In the result of the study, compared to natural fine aggregate, a crack-extent increased by applying recycled fine aggregate, moreover, as a water cement ratio increased, the crack size increased, as well. In addition, it's shown that the specimen mixed with PVA and Nylon, among all kinds of fibers, showed the smallest crack size, so it's verified that the mix of fiber had an effect on decreasing crack-extent.

  • PDF

A Study on Correlation Between Cyclic Drying-Wetting Accelerated Corrosion Test and Long-term Exposure Test (건습반복 부식촉진시험 및 장기폭로시험의 상관성에 대한 연구)

  • Park, Sang-Soon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.20 no.4
    • /
    • pp.136-143
    • /
    • 2016
  • There are various method for evaluating the durability life of concrete structures due to salt damage. The best way is to perform a corrosion test for a rebar embedded in concrete specimen was exposure to marine environment. However, this method has the disadvantage that it takes a long period of time. Also, accelerated corrosion test which was complemented complements the time-consuming weakness is limited to apply because it could not reveal a correlation between long-term exposure test. Accordingly, the purpose of this study is to derive a correlation coefficient between cycle drying-wetting accelerated corrosion test and long-term exposure test. Corrosion initiation time was measured in four types of concrete samples, i.e., two samples mixed with fly ash(FA) and blast furnace slag(BS), and the other two samples having two water/cement ratio(W/C = 0.6, 0.35) without admixture(OPC 60 and OPC 35). The accelerated corrosion test was carried out by two case, i.e., one is a cyclic drying-wetting method(case 1), and the other is a artificial seawater ponding test method(case 2). Whether corrosion occurs, it was measures using half-cell potential method. The results indicated that case 1 is to accelerated the corrosion of rebar about 24~36% as compared with case 2, then the corrosion of rebar embedded in concrete occurred according to the order of OPC60, FA, BS, OPC35. Correlation coefficient between accelerated corrosion test and long-term exposure test, case 1 is 4.23 to 5.42, and case 2 is 6.54 to 7.82.

Box-Wilson Experimental Design-based Optimal Design Method of High Strength Self Compacting Concrete (Box-willson 실험계획법 기반 고강도 자기충전형 콘크리트의 최적설계방법)

  • Do, Jeong-Yun;Kim, Doo-Kie
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.5
    • /
    • pp.92-103
    • /
    • 2015
  • Box-Wilson experimental design method, known as central composite design, is the design of any information-gathering exercises where variation is present. This method was devised to gather as much data as possible in spite of the low design cost. This method was employed to model the effect of mixing factors on several performances of 60 MPa high strength self compacting concrete and to numerically calculate the optimal mix proportion. The nonlinear relations between factors and responses of HSSCC were approximated in the form of second order polynomial equation. In order to characterize five performances like compressive strength, passing ability, segregation resistance, manufacturing cost and density depending on five factors like water-binder ratio, cement content, fine aggregate percentage, fly ash content and superplasticizer content, the experiments were made at the total 52 experimental points composed of 32 factorial points, 10 axial points and 10 center points. The study results showed that Box-Wilson experimental design was really effective in designing the experiments and analyzing the relation between factor and response.

Effect of Artificial Granular Zeolite(AGZ) on Purification of Heavy Metals in Wastewater and Alleviation or Rice Seeding Growth Damage (입상 인공제올라이트를 이용한 중금속 폐수 정화와 벼 유묘 생육장해 경감)

  • Lee, Deog-Bae;Lee, Kyeong-Bo;Lee, Sang-Bok;Kim, Jae-Duk;Henmi, Teruo
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.32 no.4
    • /
    • pp.446-451
    • /
    • 1999
  • This study was carried out to investigate some mineralogical characteristics of Artificial Granular Zeolite (AGZ) and effect of AGZ on purification and alleviation of rice seedling damages of mine wastewater containing heavy metals. AGZ had mainly representative Na-P1 peaks and some $C_3S$ peaks of Portland cement in X-ray diffractogram. Differential thermal analysis represented that AGZ had weak endothermic peak around $130^{\circ}C$ and new deep endothermic peak around $750^{\circ}C$ as compared to powdery artificial zeolite. The ranking of heavy metals removals by AGZ, was lead> copper> cadmium> zinc in the synthetic wastewater. Root growth of rice seedling was greatly inhibited in the mine wastewater, and died after all. As AGZ treated into the mine wastewater with the ratio 1 : 50 (W : V) for one day or 1 : 100 for 4 days, the concentrations of heavy metals in the mine wastewater were decreased to below the critical concentration for agricultural use. And rice seedlings were grew with little damages in the purified water by AGZ.

  • PDF

Flow and Strength Characteristics of the Lightweight Foamed CLSM(Controlled Low-Strength Materials) with Coal Ash (석탄회를 활용한 경량기포유동화재의 플로우 및 강도 특성)

  • Lee, Seungjun;Lee, Jonghwi;Chae, Hwiyoung;Chun, Byungsik
    • Journal of the Korean GEO-environmental Society
    • /
    • v.12 no.10
    • /
    • pp.73-82
    • /
    • 2011
  • Coal ash of industial by-products was not recycled about 30% in total emissions. Moreover, it caused environmental pollution as well as wasted unnecessary expenses and time. Currently, fly ash(FA) is recycled as construction material however ponded ash(PA) is mostly buried. Lightweight foamed Controlled Low-Strength Materials(CLSM) evaluated in this study reduces unit weight by mixing foam in the traditional Controlled Low-Strength Material and has lightweight and flowability to be available for backfill materials in construction. Flow test, unconfined compressive strength test, and foamed-slurry unit weight test were performed in this study and the applicability of lightweight foamed CLSM for construction materials was evaluated. The results indicate that the mixture ratio(PA:FA) ranging from 70:30 to 50:50, cement of 7%, foam of 2~3%, and water content of 26.5~29.5% were required to satisfy the following standards such as flow value(i.e., 20cm), unconfined compressive strength(i.e., 0.8~1.2MPa), and foamed-slurry unit weight(i.e., $12{\sim}15kN/m^3$).

Injection Characteristics Evaluation of Conductive Grout Material According to Carbon Fiber Mixing Ratio (탄소섬유 배합비에 따른 전도성 그라우트 재료의 주입특성평가)

  • Hyojun Choi;Wanjei Cho;Hyungseok Heo;Teawan Bang;Chanyoung Yune
    • Journal of the Korean GEO-environmental Society
    • /
    • v.24 no.1
    • /
    • pp.15-23
    • /
    • 2023
  • The grouting method is a method of construction for the purpose of waterproofing and reinforcing soft ground. When grout is injected into the ground, there are various types of penetration and diffusion of grout depending on the shape of the ground, the size of soil, the porosity, and the presence or absence of groundwater. the current situation. Therefore, in this study, to investigate the penetration performance of the grouting to conductive material, laboratory tests were performed on the addition of the conductive material. In the injection test, 0%, 3%, and 5% of the mixed water were added as conductive materials to the grout, and the original ground condition was composed of various types of ground composed of gravel and silica sand. Conductive grout is injected by pressure into the model ground using a dedicated injection device, and the injection time (t), pressure (p), flow rate (v) and injection amount (q) are measured, and the hardened body injected in the model ground is collected. Penetration performance was evaluated. In the results of the grout injection experiment, the amount of conductive material used and the grout injection rate showed an inverse relationship, and it was confirmed that the penetration pattern was changed according to the size of the soil particles in the model ground. The grout containing the conductive material has relatively good penetration into the ground and excellent strength and durability of the hardened body, so it was judged that it could be used as an additive for measuring the penetration range of the grout.

A Study on Pullout-Resistance Increase in Soil Nailing due to Pressurized Grouting (가압 그라우팅 쏘일네일링의 인발저항력 증가 원인에 관한 연구)

  • Jeong, Kyeong-Han;Park, Sung-Won;Choi, Hang-Seok;Lee, Chung-Won;Lee, In-Mo
    • Journal of the Korean Geotechnical Society
    • /
    • v.24 no.4
    • /
    • pp.101-114
    • /
    • 2008
  • Pressurized grouting is a common technique in geotechnical engineering applications to increase the stiffness and strength of the ground mass and to fill boreholes or void space in a tunnel lining and so on. Recently, the pressurized grouting has been applied to a soil-nailing system which is widely used to improve slope stability. Because interaction between pressurized grouting paste and adjacent ground mass is complicated and difficult to analyze, the soil-nailing design has been empirically performed in most geotechnical applications. The purpose of this study is to analyze the ground behavior induced by pressurized grouting paste with the aid of laboratory model tests. The laboratory tests are carried out for four kinds of granitic residual soils. When injecting pressure is applied to grout, the pressure measured in the adjacent ground initially increases for a while, which behaves in the way of the membrane model. With the lapse of time, the pressure in the adjacent ground decreases down to a value of residual stress because a portion of water in the grouting paste seeps into the adjacent ground. The seepage can be indicated by the fact that the ratio of water/cement in the grouting paste has decreased from a initial value of 50% to around 30% during the test. The reduction of the W/C ratio should cause to harden the grouting paste and increase the stiffness of it, which restricts the rebound of out-moved ground into the original position, and thus increase the in-situ stress by approximately 20% of the injecting pressures. The measured radial deformation of the ground under pressure is in good agreement with the expansion of a cylindrical cavity estimated by the cavity expansion theory. In-situ test revealed that the pullout resistance of a soil nailing with pressurized grouting is about 36% larger than that with regular grouting, caused by grout radius increase, residual stress effect, and/or roughness increase.

Engineering Characteristics of Wet-mixing Solidified Soil in Pavement Surfacing (습식 경화교반토 포장의 공학적 특성)

  • Yoo, Ji-Hyeung;Shu, Dong-Hyuk;Lee, Seong-Won
    • International Journal of Highway Engineering
    • /
    • v.6 no.3 s.21
    • /
    • pp.1-7
    • /
    • 2004
  • Roads, like bikeways, parkways and walks, are to be just capable of supporting light traffic and traveling public, but they are required to be human friendly and environmental-oriented. Lately soil-solidifier mixture, a kind of soil-cement, has developed and has been applied to the recycling and environment-oriented pavement as the surfacing material. Soil-solidifier pavement structure has been designed by only experience. To design this pavement mechanically, it is necessary to find out basic engineering properties of soil-solidifier mixture. This study focuses on finding out mechanical characteristics of the mixture according to mixture proportions and aging. Test molds with various mixture proportions are made, and then unconfined strength tests are performed for test molds with aging of the mixture. As the result of this study, it is found that the strength of the mixture increases with amount of cement and that maximum strength is achieved at 6%$\sim$8% of the ratio of solidifier and water. The strength increase rapidly until 14 days, after then slowly. After 28 days the strength of the mixture approaches to the constant value. The heat of hydration during curing of the mixture is measured no significantly. It also shows that temperature characteristics of the mixture is similar to that of soil. Since this mixture is mixed with soil and is able to improve engineering problems in pavement due to temperature, this mixture is expected to use effectively in the environment-oriented pavement for light traffic.