• 제목/요약/키워드: unit weight of concrete

검색결과 334건 처리시간 0.027초

지역별 골재 품질변화가 콘크리트 물성에 미치는 영향 (Influence of Domestic Aggregates Quality on Concrete Properties)

  • 노재호;조일호;이선우;정재동
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1993년도 봄 학술발표회 논문집
    • /
    • pp.34-39
    • /
    • 1993
  • Recently inappropriate aggregates are used as a raw material for ready-mixed concretes, due to the shortage of natural aggregate resources and the prohibition of their extraction for the environmental protection. We, therefore, have conducted experiments to obtain some knowledge of properties of domestic aggregates and to investigate subsequent changes in the properties of the fresh and hardened concretes. To this end, aggregates currently used in 13 domestic ready-mixed concrete plants were collected. Most of aggregate used in this experiment satisfied the KS in density and unit weight. But some of the aggregates have the particle size distribution that can effect bad influence on concrete. In this experiment the aggregates are found to have a bad particle size distribution, resulting in high amount of a unit water content and a unit cement content in concrete.

  • PDF

Engineering Properties of Permeable Polymer Concrete Using Bottom Ash and Recycled Coarse Aggregate

  • Sung, Chan-Yong;Kim, Jong-Hyouk
    • 한국농공학회논문집
    • /
    • 제48권7호
    • /
    • pp.25-31
    • /
    • 2006
  • Permeable polymer concretes can be applied to roads, sidewalks, river embankment, drain pipes, conduits, retaining walls, yards, parking lots, plazas, interlocking blocks, etc. This study was to explore a possibility of using bottom ash as filler and recycled coarse aggregate of industrial by-products for permeable polymer concrete. The tests carried out at $20{\pm}1^{\circ}C$ and $60{\pm}2%$ relative humidity. At 7 days of curing, unit weight, void ratio, compressive and flexural strength and coefficient of permeability ranged between $1,652{\sim}1,828kgf/m^{3},\;15{\sim}29+%,\;18.2{\sim}24.5\;MPa,\;6.4{\sim}8.4\;MPa\;and\;6.8{\times}10^{-2}{\sim}1.7{\times}10^{-1}\;cm/s$, respectively. It was concluded that the bottom ash and recycled coarse .aggregate can be used in the permeable polymer concrete.

바텀애시를 활용하는 다공성 콘크리트의 열전도 특성에 관한 실험 연구 (An Experimental Study on Thermal Property of Porous Concrete Containing Bottom Ash)

  • 정승태;김범수;박지훈;양인환
    • 한국건설순환자원학회논문집
    • /
    • 제9권4호
    • /
    • pp.625-632
    • /
    • 2021
  • 본 논문에서는 화력발전소 산업부산물이 바텀애시의 활용성을 증대시키기 위해 다공성 콘크리트를 제작하여 단열 콘크리트로서의 적용 가능성을 연구하였다. 본 연구에서는 두 가지 입도의 골재를 사용하여 골재 특성을 파악한 후, 바텀애시를 다공성 콘크리트 골재로 활용하였다. 물-바인더 비를 0.25와 0.35로 사용하고, 컴펙션에 따른 다공성 콘크리트의 재료 특성을 파악하기 위해 0.5MPa, 1.5MPa, 3.0MPa로 콘크리트 시편을 제작하였다. 이후 28일의 수중양생을 진행한 후, 단위중량, 총 공극률 및 열전도율 실험을 수행하여 결과를 도출하였다. 측정된 실험 결과를 토대로 다공성 및 경량 특성을 갖는 바텀애시를 활용한 다공성 콘크리트의 단위중량, 총 공극률 및 열전도율과의 상관관계를 제시하였다.

팽창점토를 사용한 경량콘크리트의 특성에 관한 실험적 연구 (An Experimental Study on the Properties of Lightweight Concrete Using Expanded Clay)

  • 김종인;최영화;하상진
    • 한국산업융합학회 논문집
    • /
    • 제5권3호
    • /
    • pp.225-232
    • /
    • 2002
  • The purpose of this study is to find the mechanical properties of lightweight concrete using expanded clay. Thus, slump, air content, compressive strength, elastic modulus, tensile strength, length change ratio, unitweight change ratio and absorption of lightweight concrete have been investigated. The conclusions of this study are as follows ; 1. The loss of slump and air content of concrete increased as the expanded clay content increased and the size of coarse aggregate decreased. 2. The compressive strength of concrete using 100% expanded clay of 13, 19mm size at 28 days were respectively 282, $252kgf/cm^2$. 3. The elastic modulus and tensile strength of concrete decreased with increase of expanded clay content. 4. The length change ratio of concrete increased with the larger coarse aggregate size, and decreased with the increase of expanded clay content. 5. The unit weight of concrete decreased with the increase of expanded clay content, and the ratio of that was larger at the early age.

  • PDF

부순모래 콘크리트의 강도 특성에 관한 연구 (A Study on the Strength Characteristics of Crushed Sand Concrete)

  • 김상태;김태영;백동일;장희석;김명식
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(II)
    • /
    • pp.429-432
    • /
    • 2005
  • An investigation for long-term strength characteristics of crushed sand concrete using crushed sands produced in Yang-san, Kim-hae and Jin-hae that can assume to respectively represent eastern, middle and western suburb of Busan was carried out. Cases were divided as variation of blend ratio of crushed sand (50, 60, 70, 80, 90, 100$\%$) and area. Compressive strength, unit weight and strain in age of 28, 60, 90, 180, 356 days were measured in each case. Compressive strength, unit weight and modulus of elasticity were increased as time goes by and they are expected to keep on increasing in long-term age as well.

  • PDF

충전재가 투수용 폴리머 콘크리트의 공학적 성질에 미치는 영향 (Effects of Filler on Engineering Properties of Permeable Polymer Concrete)

  • 성찬용;정현정;민정기
    • 농업과학연구
    • /
    • 제23권1호
    • /
    • pp.51-60
    • /
    • 1996
  • This study was performed to evaluate the effects of filler on engineering properties of permeable polymer concrete with unsaturated polyester resin. The following conclusions were drawn; 1. The unit weight was in the range of $1.804{\sim}1.919t/m^3$, the weights of those concrete were decreased 17~22% than that of the normal cement concrete. 2. The highest strength was achieved by stone dust filled permeable polymer concrete, it was increased 17% by compressive, 147% by tensile and 188% by bending strength than that of the normal cement concrete, respectively. 3. The ultrasonic pulse velocity was in the range of 2,722~3,060m/sec, which was showed about the same compared to that of the normal cement concrete. Stone dust filled permeable polymer concrete was showed higher pulse velocity. 4. The water permeability was in the range of $3.076{\sim}4.152{\ell}/cm^2/h$, and it was larglely dependent upon the mix design. These concrete can be used to the structures which need water permeability. 5. The compressive strength, tensile strength, bending strength and ultrasonic pulse velocity were largely showed with the increase of unit weight. But, it was decreased with the increase of water permeability, respectively.

  • PDF

급결제를 사용한 외장재용 3D 프린팅 콘크리트의 강도 특성 (Strength Characteristics of 3D Printing Concrete for Exterior materials using Accelerating agent)

  • 서대석
    • 한국산학기술학회논문지
    • /
    • 제22권2호
    • /
    • pp.267-272
    • /
    • 2021
  • 본 연구는 최근 증가하고 있는 건축물의 다양한 외벽 형상에 따라 적용이 가능한 비정형 건축물에의 적용을 위해 3D 프린팅 기법을 적용한 외장재의 제조를 위한 기초 연구로서 진행하였다. 3D 프린팅 외장재의 출력성과 적층성의 확보를 위하여 3D 프린팅 콘크리트를 몰드에 타설한 시험체와 급결제를 사용한 출력물 시험체의 단위중량과 강도특성을 분석하였다. 몰드에 타설한 콘크리트의 단위중량에 비하여 급결제를 사용한 3D 프린팅 콘크리트의 단위중량이 3.5%~5.0% 정도 감소하는 경향을 나타내었고, 압축강도는 몰드에 타설한 콘크리트의 압축강도에 비하여 3D 프린팅을 통한 출력물의 압축강도는 36%~46%정도 감소하는 경향을 나타냈다. 휨강도의 경우 몰드에 타설한 콘크리트의 압축강도에 비하여 3D 프린팅을 통한 출력물의 압축강도는 36%~46%정도 감소하는 경향을 나타냈다. 급결제를 사용한 3D 프린팅 콘크리트의 강도 특성에 관한 영향은 2.0~5.8%정도 감소하는 경향을 나타냈다. 따라서, 3D 프린팅 출력시 급결제의 사용에 따른 강도 특성에 영향은 출력에 의한 강도 특성의 감소 보다 적은 것으로 나타나 3D 프린팅 외장재 제조시 급결제의 사용이 가능한 것으로 판단된다.

바텀애쉬골재 대체율에 따른 경량투수블록의 단위용적질량 및 강도특성 평가 (Evaluation of the Unit Weight and Strength Properties of Lightweight Porous Blocks according to Replacement Ratio of Bottom Ash Aggregate)

  • 이경수;오태규;정수빈;김영욱;최희용;최세진
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2019년도 춘계 학술논문 발표대회
    • /
    • pp.215-216
    • /
    • 2019
  • Recently, due to abnormal climate phenomena caused by greenhouse gas, flood damage such as local torrential rain has been emerging in Korea. Accordingly, there is a growing need for porous blocks capable of permeability in concrete, but there are limitations in commercialization due to problems such as high unit weight and flexural strength development limitations. This study investigates the unit weight and strength properties of porous blocks using bottom ash as an alternative to aggregate as part of a study to improve the light weight of porous blocks.

  • PDF

표면코팅된 경량골재를 사용한 콘크리트의 탄산화 저항성에 관한 연구 (A Study on Carbonation Resistance of Concrete Using Surface-coated Lightweight Aggregates)

  • 엄인혁;정의창;김영수
    • 한국건축시공학회지
    • /
    • 제14권1호
    • /
    • pp.21-28
    • /
    • 2014
  • 경량골재의 내부공극을 통한 탄산가스 유입으로 인해 경량골재콘크리트는 보통콘크리트에 비해 탄산화가 더 빠르게 진행되는 문제점을 극복하고자, 4가지 표면코팅제로 코팅된 경량골재를 사용한 콘크리트에 대하여 탄산화 저항성을 보통 경량골재콘크리트, 보통콘크리트와 비교 분석하였다. 코팅경량골재를 사용한 콘크리트가 보통 경량골재콘크리트보다 우수한 탄산화 저항성을 보였으며, 특히 발수제보다는 고분자계 코팅제를 사용하였을 때 더 우수한 저항성을 나타내었다.

고성능 감수제를 사용한 콘크리트의 품질 특성에 관한 연구 (A Study on the Quality Characteristics of Concrete Using Super Plasticizer)

  • 배수호;윤상대;정영수;김영의
    • 콘크리트학회지
    • /
    • 제6권6호
    • /
    • pp.135-142
    • /
    • 1994
  • 본 연구는 고유동성, 고강도 및 고내구성을 가진 고성능 콘크리트를 실용화시키기 위하여 국내에서 시판되고 있는 9종류의 고성능 감수제를 사용한 콘크리트의 품질 특성을 평가하였다. 이를 위하여 혼화제 첨가량에 따라서 굳지 않은 콘크리트의 슬럼프, 공기걍, 단위중량 및 감수율과 경화콘크리트의 압축강도비를 비교분석하였다. 본 시험결과, 국내 시판되는 고성능 감수제를 사용한 콘크리트의 공기연행 효과는 거의 없었으며 또한, 보통강도 및 고성능 콘크리트 각각에 대하여 최적혼화제 첨가량이 존재함을 알아냈다.