실험통계법을 이용한 마찰재의 고온 마찰특성에 대한 고찰 (High Temperature Fade Behavior of Brake Friction Materials at Extreme Braking Conditions)

  • 고길주;박상진;장호
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제34회 추계학술대회 개최
    • /
    • pp.117-126
    • /
    • 2001
  • Tribological properties of high temperature fade were investigated by changing relative amounts of ingredients in the brake friction material. Based on a simple experimental formulation containing 10 ingredients, friction materials were tested using a pad-on-disk type friction tester. Twenty-five friction material specimens with different relative amounts of the ingredients were manufactured according to the constrained mixture design .The difference ($\Delta$${\mu}$=${\mu}$$\sub$max/. -${\mu}$$\sub$min/. ) of friction coefficients was measured to represent the high temperature fade. Results from elevated temperature tests showed that five ingredients including cashew, graphite, Sb$_2$S$_3$, ZrSiO$_4$, and Cu fibers played important roles on $\Delta$${\mu}$. In order to find relative importance on fade phenomena among these ingredients, ANOVA(analysis of variance) was performed in this investigation. Thirty-two friction material specimens by changing ${\pm}$50vol.% of these five ingredients were tested to examine the relative importance. Results showed that cashew, graphite '||'&'||' Sb$_2$S$_3$, and cashew '||'&'||' graphite aggravated the fade behavior and Cu fibers improved on fade resistance.

  • PDF

PE-CVD방법을 이용한 DLC 박막의 기계적특성 평가 (Mechanical Property Evaluation of Diamond-like Carbon Coated by PE-CVD)

  • 강석주;이진우;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2003년도 학술대회지
    • /
    • pp.368-376
    • /
    • 2003
  • In this research, DLC thin films are produced as several hundred nm thickness by PE-CVD method. And then these thin films are estimated tribological characteristics to find out useful possibilities as a protecting film for high-quality function and life extension at MEMs by mechanical properties observation . These are measured thickness and residual stress of DLC coating. Compared after measuring friction coefficient, adhesion force, hardness, cohesive force of coating films. As results all test, we can decide several conclusions. First, friction coefficient decreased, as the load increased. otherwise, friction coefficient increased, as thickness of coating film increased under low load$(1\~50mN)$. Secod, adhesion force increased as thickness of coating films. Third, hardness of coating film is affected by substrate coating film when it is less than thickness of 300nm and it has general hardness of DLC coating film when it is more than thickness of 500nm. Fourth, cohesive force of coating film is complexly affected by hardness, adhesion force, residual stress, etc.

  • PDF

트라이볼로지 손상을 억제하기 위한 구조물 모서리부 설계: 제1부 - 설계공식 개발 (Design of Structure Corners Restraining Tribological Failures: Part I - Development of Design Formula)

  • 김형규
    • Tribology and Lubricants
    • /
    • 제31권4호
    • /
    • pp.163-169
    • /
    • 2015
  • This paper describes a design method for the corner radius of a contacting body using the theoretical approach of contact mechanics. A complete contact, as in the case of a sharp-cornered punch, produces singular contact traction: whereas, in an incomplete contact, the singular contact traction disappears because of the rounded corners, and the contact edges are within the rounded regions. The design method aims to determine the conditions of the contact force as well as the material properties in an incomplete contact. The incomplete contact changes into the complete contact again when the contact edges exceed the rounded regions owing to either an increased contact force or the compliance of the materials. The contact length of a rounded punch is used as a parameter to derive the required conditions. As a result, a design formula is obtained, which provides a minimum allowable radius when the materials, normal contact force, and the length of a flat region of the punch are predetermined. This work consists of two parts: Part I includes a theoretical background, design method, and formula, and Part II describes the actual process with the investigation of design parameters.

디젤엔진 피스톤 링 코팅 층의 경도에 따른 마찰특성 (Effect of Coating Layer Hardness on Frictional Characteristics of Diesel Engine Piston Ring)

  • 장정환;주병돈;이호진;김은화;문영훈
    • 소성∙가공
    • /
    • 제18권6호
    • /
    • pp.465-470
    • /
    • 2009
  • The frictional behaviors of Cermets/Cr-Ceramics and Cu-Al coatings of piston ring were investigated. Friction tests were carried out by pin-on-disk test and materials properties of coating layer were analyzed by nano indentation tester. The effect of surface roughness of cylinder liner on the friction coefficient was analyzed. This study provided tribological data of hard and soft piston ring coatings against cylinder liner. The surface roughness does exert an influence on the average friction coefficient, with smoother surfaces generally yielding lower friction coefficients. In case of hard-coating, the scratch depth, width and pile-up height had close relationship with hardness. So the scratch width, depth and pile-up height increases with decreasing friction coefficient. But in case of soft-coating, the friction coefficients are strongly dependent on the morphological characteristics such as, scratch depth, width, pile-up height and elastic modulus.

비정질 다이아몬드 코팅을 위한 자장여과 아크소스의 동작 특성에 관한 연구 (Operation Characteristic of Filtered Vacuum Arc Source for Amorphous Diamond Coating)

  • 김종국;이구현
    • 연구논문집
    • /
    • 통권30호
    • /
    • pp.147-157
    • /
    • 2000
  • The filtered vacuum arc source (FVAS), which is adopted by magnetic filtering methode to remove the macro-particle in vacuum arc plasma, was composed of a torus structure with bending angle of 60 degree. The radius of torus was 266 mm, the radius of plasma duct was 80 mm and the total length was 600 mm. The magnet parts were consisted of one permanent magnet, one magnetic yoke and five solenoid magnets. The plasma duct was electrically isolated from the ground so that a bias voltage could be applied. The baffles inside plasma duct were installed in order to prevent the recoil effect of macro-particles. Graphite was used as the cathode material to coat the amorphic diamond film and its diameter was 80 mm. The amorphic diamond film attracts much attention due to its excellent mechanical, optical and tribological properties suitable for wide range of applications. The effects of solenoid magnet in plasma extraction were studied by computer simulation and experiment using Taguchi's method. The source and extraction magnet affected the arc stabilization. The extraction beam current was maximized with low value of the source magnet current and high value of the filtering magnet current. Optimum deposition condition was obtained when the currents of arc discharge, source, extraction, bending, deflection and outlet magnet were 30 A, 1 A, 3 A, 5 A, and 5 A, respectively.

  • PDF

AlSiMg/TiC 복합 용사 피막 : 분말제조 및 피막 특성(I) (Thermal Sprayed AlSiMg/TiC Composite Coatings : Fabrication of Powder and Characteristics of Coatings (I))

  • 양병모;변응선;박경채
    • Journal of Welding and Joining
    • /
    • 제18권5호
    • /
    • pp.98-104
    • /
    • 2000
  • Aluminum alloys are being employed in automobile parts as strive to reduce overall vehicle weight to meet demands for improved fuel economy and reduction in vehicle emissions. Al-based composites reinforced with ceramic ($Al_2O_3,\;SiC,\;TiC\;and\;B_4C$) applications in a variety of components in automotive engines, such as liners, where the tribological properties of the material are important. In this study, Al-base composites reinforced with TiC particle powders has been developed for producing plasma spray coatings. The composite plasma spray powders were prepared Al-13Si-3Mg(wt%) alloy with TiC(40, 60 and 80wt%) particles ($0.2~5{\mu}textrm{m}$) by drum type ball milling. The composite powders ($36~76{\mu}textrm{m}$) were sprayed with plasma torch. Plasma sprayed coatings were heat-treated at $500^{\circ}C$ for 3 hours. The wear resistances of the plasma sprayed coatings were found to decrease with increasing TiC content and improved with heat treatment. AlSiMg-40% TiC heat-treated coatings were showed the best wear resistance in this study.

  • PDF

SM45C의 레이저 표면경화특성 (Laser surface hardening characterization of SM45C)

  • 신호준;유영태;안동규;임기건
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2005년도 춘계학술대회 논문집
    • /
    • pp.246-251
    • /
    • 2005
  • Laser surface hardening is an effective technique used to improve the tribological properties and also to increase the service life of automobile components such as camshafts, crankshatfs, lorry brake drums and gears. High power $CO_2$ lasers and Nd:YAG lasers are employed for localized hardening of materials and hence are of potential application in the automobile industries. The heat is conducted rapidly into the bulk of the specimen causing self-quenching to occur and the formation of martensitic structure. In this investigation, the microstructure features occurring in Nd:YAG laser hardening SM45C steel are discussed with the use of optical microscopic and scanning electron microscopic analysis. Moreover, This paper describes the optimism of the processing parameters for maximum hardened depth of SM45C steel specimens of 3mm thickness by using CW Nd:YAG laser. Travel speed was varied from 0.6m/min to 1.0m/min. The maximum hardness and case depth fo SM45C steel are 780Hv and 0.4mm by laser hardening.

  • PDF

Solid Lubrication Characteristics of DLC Coated Alumina Seals in High Temperature

  • 옥철호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.356-356
    • /
    • 2007
  • Plasma immersion ion beam deposition (PIIBD) technique is a cost-effective process for the deposition of diamond like carbon thin film, the possible solid lubricant on large surface and a complex shape. We used PIIB process for the preparation of DLC thin film on $Al_2O_3$ with deposition conditions of deposition temperature range $200^{\circ}C$, working gas pressure of 1.310-1Pa. DLC thin films were coated by $C_2H_2$ ion beam deposition on $Al_2O_3$ after the ion bombardment of SiH4 as the bonding layer. Energetic bombardment of $C_2H_2$ ions during the DLC deposition to ceramic materials generated mixed layers at the DLC-Si interface which enhanced the interface to be highly bonded. Wear test showed that the low coefficient of friction of around 0.05 with normal load 2.9N and proved the advantage of the low energy ion bombardment in PIIBD process which improved the tribological properties of DLC thin film coated alumina ceramic. Furthermore, PIIBD was recognized as a useful surface modification technique for the deposition of DLC thin film on the irregular shape components, such as molds, and for the improvement of wear and adhesion problems of the DLC thin film, high temperature solid lubricant.

  • PDF

두 종의 고체윤활제에 따른 마찰재의 마찰성능에 관한 실험적 고찰 (Experimental Investigation on Friction Performance of Brake Linings with Two Different Solid Lubricants)

  • 김성진;배은갑;윤호규;장호
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2001년도 제33회 춘계학술대회 개최
    • /
    • pp.72-78
    • /
    • 2001
  • An experimental investigation was conducted to examine the tribological behavior of NAO (non-asbestos organic) type brake linings containing different volume ratios of graphite and antimony trisulfide (Sb$_2$S$_3$). In order to investigate the effect of the solid lubricants on brake performance, three different friction tests (pressure, speed, and temperature sensitive tests) were carried out using a scale dynamometer. The test results showed that the friction characteristics were strongly affected by the type and the amount of solid lubricants in the brake lining. It was found that the brake linings with both solid lubricants were better in friction stability due to the complementary role of the two disparate lubricating properties at various pressure and speed conditions. In particular, the brake lining containing higher concentrations of graphite showed better fade resistance than others during high temperature friction test.

  • PDF

나노다이아몬드를 첨가한 오일의 트라이볼로지 특성 및 이에 미치는 표면 경도의 영향 (Tribological Characteristics of Paraffin Liquid Oil with Nanodiamond and Effects of Surface Hardness on Wear Properties)

  • 이규선;김현수;이정훈;박태희;이정석;이영제
    • Tribology and Lubricants
    • /
    • 제27권6호
    • /
    • pp.321-325
    • /
    • 2011
  • Nanodiamond was dispersed in paraffin liquid oil to investigate the effects of nanodiamond at the marginally lubricated condition. Scuffing test and immediate loading sliding wear test were conducted using the fabricated nanodiamond oil. As a result, dispersion of nanodiamond in oil leads to increase in scuffing life, and nanodiamond contents affects the scuffing life. In case of immediate loading sliding wear test, the result was different according to hardness of specimen. If hardness of specimen was low, abrasion of nanodiamond occurred actively. If hardness of specimen was increased, however, nanodiamond can act as a spacer or rolling between contacting surfaces.