Development of New Titanium Alloys for Castings (주조용 티타늄 신합금 개발)

  • Kim, Seung-Eon;Jeong, Hui-Won;Hyeon, Yong-Taek;Kim, Seong-Jun;Lee, Yong-Tae
    • 연구논문집
    • /
    • s.29
    • /
    • pp.163-171
    • /
    • 1999
  • A new titanium alloy system. Ti-xFe-ySi (x,y=0-4 wt%). was designed and characterized with the point at low cost and high strength for casting applications. Fe improved room and elevated temperature mechanical properties owing to solid solution hardening and beta phase stabilization. Si yielded titanium silicides and Si addition over 1 wt% resulted in poor ductility due to coarse silicide chains at prior beta boundaries. The optimum composition was found to be Ti-4Fe-(0.5-1)Si in the viewpoint of tensile strength and ductility which are comparable to the Ti-6Al-4V. The metal-mould reaction was also examined for Ti-xFe and Ti-xSi binary alloy system. The thickness of surface reaction layer w as not affected significantly with Fe content, while it was decreased with Si content. In the Ti-4Si alloy, no reaction layer was found. The depth of surface hardening layer was about $200\mum$ regardless of the mould materials.

  • PDF

Color Evolution in Anodized Titanium (열산화에 의한 티타늄의 발색효과)

  • 송오성;홍석배;이정임
    • Journal of the Korean institute of surface engineering
    • /
    • v.35 no.5
    • /
    • pp.325-329
    • /
    • 2002
  • We investigated the oxide thickness and color evolution with the oxidation temperatures between $370^{\circ}C$ and $950^{\circ}C$ for 30 minutes in an electric furnace. Oxide thickness and color index were determined by cross sectional field emission scanning electron microscopy (FESEM) images and digital camera images, respectively. We confirmed that thermal oxidation was suitable for the mass production of color-titanium products, while coloring process window was narrow compared with anodizing oxidation process.

Effect of atmospheric plasma versus conventional surface treatments on the adhesion capability between self-adhesive resin cement and titanium surface

  • Seker, Emre;Kilicarslan, Mehmet Ali;Deniz, Sule Tugba;Mumcu, Emre;Ozkan, Pelin
    • The Journal of Advanced Prosthodontics
    • /
    • v.7 no.3
    • /
    • pp.249-256
    • /
    • 2015
  • PURPOSE. The aim of this study was to evaluate the effects of atmospheric plasma (APL) versus conventional surface treatments on the adhesion of self-adhesive resin cement to Ti-6Al-4V alloy. MATERIALS AND METHODS. Sixty plates of machined titanium (Ti) discs were divided into five groups (n=12): 1) Untreated (CNT); 2) Sandblasted (SAB); 3) Tribochemically treated (ROC); 4) Tungsten CarbideBur (TCB); 5) APL treated (APL). SEM analysis and surface roughness (Ra) measurements were performed. Self-adhesive resin cement was bonded to the Ti surfaces and shear bond strength (SBS) tests, Ra and failure mode examinations were carried out. Data were analyzed by one-way analysis of variance and chi-squared test. RESULTS. The lowest SBS value was obtained with CNT and was significantly different from all other groups except for APL. The ROC showed the highest SBS and Ra values of all the groups. CONCLUSION. It was concluded that the effect of APL on SBS and Ra was not sufficient and it may not be a potential for promoting adhesion to titanium.

Investigation on nanoadhesive bonding of plasma modified titanium for aerospace application

  • Ahmed, Sabbir;Chakrabarty, Debabrata;Mukherjee, Subroto;Joseph, Alphonsa;Jhala, Ghanshyam;Bhowmik, Shantanu
    • Advances in aircraft and spacecraft science
    • /
    • v.1 no.1
    • /
    • pp.1-14
    • /
    • 2014
  • Physico-chemical changes of the plasma modified titanium alloy [Ti-6Al-4V] surface were studied with respect to their crystallographic changes by X-Ray Diffraction (XRD) and Scanning Electron Microscope (SEM).The plasma-treatment of surface was carried out to enhance adhesion of high performance nano reinforced epoxy adhesive, a phenomenon that was manifested in subsequent experimental results. The enhancement of adhesion as a consequence of improved spreading and wetting on metal surface was studied by contact angle (sessile drop method) and surface energy determination, which shows a distinct increase in polar component of surface energy. The synergism in bond strength was established by analyzing the lap-shear strength of titanium laminate. The extent of enhancement in thermal stability of the dispersed nanosilica particles reinforced epoxy adhesive was studied by Thermo Gravimetric Analysis (TGA), which shows an increase in onset of degradation and high amount of residuals at the high temperature range under study. The fractured surfaces of the joint were examined by Scanning electron microscope (SEM).

A STUDY ON THE FATIGUE AND PHYSICAL PROPERTIES OF TITANIUM USED IN REMOVABLE PARTIAL DENTURES (국소의치용 티나늄의 피로도 및 물리적 성질에 관한 연구)

  • Kim Hak-Sun;Kim Kwang-Nam;Chang Ik-Tae
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.32 no.2
    • /
    • pp.249-267
    • /
    • 1994
  • The purpose of this study was to compare the fatigue, physical properties, flexibility and surface roughness of titanium used in removable partial dentures with those of a type IV and alloy and a cobalt- chromium alloy. Fatigue testing subjected the test specimen to rapid cycling at a given stress until failure occurred by using a small-sized, electrodynamic type bending fatigue testing machine. The S-N curves for the framework materials were generated. For tensile testing, a tensile bar as described in the ADA Specification No.14 was subjected to tensile loading until failure occurred. Load-displacement curves were generated for 18 gauge round specimen and tapered half round specimen. Then the flexibilities were calculated. The surface roughnesses were compared by analyzer. Through analyses of the data, the following conclusions were obtained. 1. The fatigue property of titanium was higher than that of a type IV gold alloy$(p\leq0.05)$, but there was no significant difference between titanium and a cobalt-chromium alloy $(p\geq0.05)$. 2. The yield strength, the ultimate tensile strength and Victors hardness of titanium were higher than those of a type IV gold alloy but lower than those of a coalt-chromium alloy$(p\leq0.05)$. 3. The percentage of elongation and reduction of area of titanium were the highest $(p\leq0.05)$. 4. The surface roughness of titanium was the greatest$(p\leq0.05)$. 5. The flexibility of titanium was lower than that of a type IV gold alloy but higher than that of a cobalt-chromium alloy$(p\leq0.05)$.

  • PDF

Screw joint stability according to abutment screw materials

  • Jeong Yong-Tae;Chung Chae-Heon;Lee Heung-Tae
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.3
    • /
    • pp.297-305
    • /
    • 2001
  • Statement of problem. There have been previous studies about instability according to screw material by means of calculating preload in tightening screw or recording of the torque necessary to loosen screw after tightening screw. Purpose. The purpose of this study was to evaluate screw joint stability through the analysis of fitness at the mating thread surfaces between implant and screw after tightening screws made of different materials. Material and methods. In this study, screws were respectively used to secure a cemented abutment to a hexlock implant fixture; teflon coated titanium alloy screw and titanium alloy screw(Steri-Oss), gold-plated gold-palladium alloy screw and titanium alloy screw(Implant Innovation), gold screw and titanium screw(AVANA Dental Implant System). Each abutment screw was secured to the implant with recommended torque value using a digital torque controller. Each screw was again tightened after 10minutes. All samples were cross sectioned with sandpaper and polished. Then samples were evaluated with an scanning electron microscope analysis. Results. In titanium alloy screw, irregular contact and relatively large gap was present at mating thread surface. Also in teflon-coated titanium screw, incomplete seating and only partially contact was present at the mating thread surface. In gold-plated gold-palladium alloy screw, relatively close and tight contact without the presence of large gap was present by existing of gold coating at the mating thread surfaces. In gold alloy screw, relatively small gap between the mating components was seen. Conclusions. This result suggested that gold plated gold-palladium alloy screw and gold alloy screw achieved a greater degree of contact at the mating thread surfaces compared to titanium alloy screw and teflon-coated titanium alloy screw.

  • PDF

Finite Element Analysis on the Effect of the Surface Roughness on the Tensile Properties of Pure Titanium (순 타이타늄 인장 물성에 미치는 표면 거칠기의 영향에 대한 유한요소해석)

  • Baek, S.M.;Moon, J.H.;Kim, H.S.
    • Transactions of Materials Processing
    • /
    • v.26 no.2
    • /
    • pp.108-114
    • /
    • 2017
  • Titanium based implants are known to improve their osseointegration by controlling surface roughness from nanometers to micrometers. Implants continuously and/or repeatedly receive irregular loads in the human body, and require a deeper understanding of the tensile and fatigue properties that can determine the fracture characteristics of the materials. In this study, the plastic deformation behavior which depends on the surface geometry of the materials during tensile tests was analyzed using the finite element method. As a result, the tensile properties were greatly decreased with increasing the sharpness of the surface. On the other hand, the average roughness had no significant effect on tensile properties. This investigation shed a light on developing titanium implants with improved osseointegration by surface treatments.

Effect of EDM Conditions when wire-EDM for Titanium Alloy (티타늄합금의 와이어 방전가공시 방전가공 조건의 영향)

  • 김종업;왕덕현;이윤경;김원일
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 2001.04a
    • /
    • pp.281-286
    • /
    • 2001
  • Titanium alloy conducted in this experimental study has superior corrosive resistant and is mainly used in aerospace, automotive and petro-chemical industries. It is also treated with important materials of domestic goods due to improvement of the standard of living. In this study specimens were processed in the wire EDM after annealing, solution treatment and aging. Results were obtained through repeated experments of main rough process and finish process with the change of process parameters. Processing characteristics such as surface hardness, surfaces roughness, shape of processed surface and components were measured. The results confirmed that the above mentioned elements were improved in accordance with the number of process. Therefore, the optimal wire EDM condition in accord with processing characteristics is proposed in this experiment.

  • PDF

High speed milling titanium alloy (Ti 합금의 고속가공시 밀링특성에 관한 연구)

  • Ming CHEN;Youngmoon LEE;Seunghan YANG;Seungil CHANG
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 2003.04a
    • /
    • pp.454-459
    • /
    • 2003
  • The paper will present chip formation mechanism and surface integrity generation mechanism based on the systematical experimental tests. Some basic factors such as the end milling cutter tooth number, cutting forces, cutting temperature, cutting vibration, the chip status, the surface roughness, the hardness distribution and the metallographic texture of the machined surface layer are involved. the chip formation mechanism is typical thermal plastic shear localization at high cutting speed with less number og shear ribbons and bigger shear angle than at low speed, which means lack of chip deformation. The high cutting speed with much more cutting teeth will be beneficial to the reduction of cutting forces, enlarge machining stability region, depression of temperature increment, auti-fatigability as well as surface roughness. The burrs always exists both at low cutting speed and at high cutting speed. So the deburr process should be arranged for milling titanium alloy in any case.

  • PDF

An Experimental Study on the Lapping of Titanium Alloy (티타늄합금의 래핑가공에 관한 실험적 연구)

  • Park, Ji-Ho;Kim, Won-Il
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.8 no.1
    • /
    • pp.25-29
    • /
    • 2005
  • Titanium specially has high specific strength, excellent mechanical properties as fatigue strength and fracture ductility, good corrosion resistance, and therefore are broadly applied to the various fields. It is required the developmennt for the skills of wire-cut electrical discharge machining(WEDM), but the WEDMed surface was found to be worst due to the attached components of wire. Therefore precision maching method like lapping is necessary for getting high quilty surface. Roughness of lapped surface, surface hardness to each process depth and improved method of surface shape were stuided experimentally, by changing of grain size of diamond lap material and lapping pressure with constant speed in lapping process.

  • PDF