Vapor Permeation Characteristics of TiO2 Composite Membranes Prepared on Porous Stainless Steel Support by Sol-Gel Method

  • Lee, Yoon-Gyu;Lee, Dong-Wook;Kim, Sang-Kyoon;Sea, Bong-Kuk;Youn, Min-Young;Lee, Kwan-Young;Lee, Kew-Ho
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권5호
    • /
    • pp.687-693
    • /
    • 2004
  • Composite membranes with a titania layer were prepared by soaking-rolling method with the titania sol of nanoparticles formed in the sol-gel process and investigated regarding the vapor permeation of various organic mixtures. The support modification was conducted by pressing $SiO_2$ xerogel of 500 nm in particle size under 10 MPa on the surface of a porous stainless steel (SUS) substrate and designed the multi-layered structure by coating the intermediate layer of ${\gamma}-Al_2O_3$. Microstructure of titania membrane was affected by heat-treatment and synthesis conditions of precursor sol, and titania formed at calcination temperature of 300$^{\circ}C$ with sol of [$H^+$]/[TIP]=0.3 possessed surface area of 210 $m^2$/g, average pore size of 1.25 nm. The titania composite membrane showed high $H_2/N_2$ selectivity and water/ethanol selectivity as 25-30 and 50-100, respectively. As a result of vapor permeation for water-alcohol and alcohol-alcohol mixture, titania composite membrane showed water-permselective and molecular-sieve permeation behavior. However, water/methanol selectivity of the membrane was very low because of chemical affinity of permeants for the membrane by similar physicochemical properties of water and methanol.

솔젤법에 의한 메조기공 티타니아/알루미나 막의 제조 및 기체투과 특성 (Synthesis and Characterization of Sol-Gel Derived Mesoporous Titania/Alumina Membranes)

  • 권혁택;김진수
    • 멤브레인
    • /
    • 제21권3호
    • /
    • pp.229-235
    • /
    • 2011
  • 본 연구에서는 메조기공 티타니아/알루미나 막을 솔-젤법을 이용하여 제조하였다. 티타니아/알루미나 막의 기공구조 및 결정상은 하소 온도에 따라 조절될 수 있었다. 티타니아에 알루미나를 첨가하는 것은 티타니아 결정상이 아나타제상에서 루타일상으로 상변화 되는 것을 지연시켜 기공구조의 열적 안정화를 가져왔다. 5번 딥코팅하여 제조된 막의 두께는 $10.3{\mu}m$였으며, 평균 기공크기는 5 nm이었다. 기체 투과 실험 결과는 수소와 질소의 permeance는 각각 $17.1{\tiems}10^{-7}mol/m^2{\cdot}s{\cdot}Pa$$4.7{\tiems}10^{-7}mol/m^2{\cdot}s{\cdot}Pa$이었다. 이 결과는 Knudsen 확산에 의해 설명될 수 있었다.

Photocatalytic Membrane Reactor for VOC Decomposition Using Pt-Modified Titanium Oxide Membranes

  • Toshinori Tsuru;no, Takehiro-Kan;Tomohisa Yoshioka;Masashi Asaeda
    • 한국막학회:학술대회논문집
    • /
    • 한국막학회 2004년도 Proceedings of the second conference of aseanian membrane society
    • /
    • pp.39-42
    • /
    • 2004
  • Ceramic membranes have attracted a great attention because they have excellent resistance to most organic solvents and can be used over a wide temperature range. Especially, titania (titanium oxide, TiO$_2$) shows excellent chemical resistance and can be used both acidic and alkali solutions, and therefore, titania is one of the most promising materials for the preparation of porous membranes; titania membranes having pore sizes in the range of nanofiltration (NF) to ultrafiltration (UF) membrane have been prepared by the sol-gel process (Tsuru 2001).(omitted)

  • PDF

Preparation and characterization of TiO2 membrane on porous 316 L stainless steel substrate with high mechanical strength

  • Mohamadi, Fatemeh;Parvin, Nader
    • Membrane and Water Treatment
    • /
    • 제6권3호
    • /
    • pp.251-262
    • /
    • 2015
  • In this work the preparation and characterization of a membrane containing a uniform mesoporous Titanium oxide top layer on a porous stainless steel substrate has been studied. The 316 L stainless steel substrate was prepared by powder metallurgy technique and modified by soaking-rolling and fast drying method. The mesoporous titania membrane was fabricated via the sol-gel method. Morphological studies were performed on both supported and unsupported membranes using scanning electron microscope (SEM) and field emission scanning microscope (FESEM). The membranes were also characterized using X-ray diffraction (XRD) and $N_2$-adsorption / desorption measurement (BET analyses). It was revealed that a defect-free anatase membrane with a thickness of $1.6{\mu}m$ and 4.3 nm average pore size can be produced. In order to evaluate the performance of the supported membrane, single-gas permeation experiments were carried out at room temperature with nitrogen gas. The permeability coefficient of the fabricated membrane was $4{\times}10^{-8}\;lit\;s^{-1}\;Pa^{-1}\;cm^{-1}$.

Prepartion and Characterization of the Pt doped $TiO_2$ Membranes

  • Bae, Dong-Sik;Han, Kyong-Sop;Choi, Sang-Hael
    • The Korean Journal of Ceramics
    • /
    • 제3권1호
    • /
    • pp.52-56
    • /
    • 1997
  • The Pt doped $TiO_2$ composite membranes were prepared by the sol-gel process. The Pt doped titania sol was peptized with hydrochloric acid in the pH range of 1.23 to 1.32 at 5$0^{\circ}C$. The average particle size of the Pt doped titania sol was shown to be below 15nm and well dispersed in the solution. XPS show the Pt elements continuous and homogeneous dispersed in the $TiO_2$ membrane. The mean particle size of the Pt doped $TiO_2$ composite membrane has smaller than that of the undoped $TiO_2$ composite membrane. The average pore size of the Pt doped $TiO_2$ composite membrane was increased from 58 to 193 $\AA$ with firing temperature changed from 550 to 85$0^{\circ}C$. It was observed that the Pt doped $TiO_2$ composite membranes showed crack-free and homogeneous microstructue as well as narrow particle size distribution up to above 75$0^{\circ}C$.

  • PDF

일체형 포토어노드를 활용한 메틸렌블루의 분해 (Photocatalytic Degradation of MB with One-body Photoanode)

  • 심은정;배상현;윤재경;주현규
    • 한국수소및신에너지학회논문집
    • /
    • 제18권1호
    • /
    • pp.40-45
    • /
    • 2007
  • Methylene blue(MB) was photocatalytically degraded with one-body photoanode and solar simulator to investigate the possible application to both environmental purification and photoelectrochemical cell for hydrogen production. Photoactive titanium dioxide was formed on both sides of Ti plate following steps such as rinsing-annealing-calcination or anodizing(20 V, 30 V)-annealing($350^{\circ}C$, $450^{\circ}C)$ after etching. The prepared titania plate($2cm{\times}2\;cm$, ca 1.6 mg $TiO_2$ on the basis of $1\;{\mu}m$ thickness) was used to degrade MB(10 ppm in 200 mL solution). The reaction tended to follow the Langmuir-Hinshelwood kinetics with zero order. Comparative experiments with Degussa P25 showed the same zero order kinetics when 2 mg of P25 had been used, while the first order kinetics when 200 mg used. This concludes the feasibility of the prepared titania plate as a material for the purification of low-level harmful organics and an electrode or a membrane for photoelectrochemical system for hydrogen production.

Treatment of dyeing wastewater by membrane process

  • Kim, In-Chul;Ka, Young-Hyun;Joo Young park;Lee, Kew-Ho
    • 한국막학회:학술대회논문집
    • /
    • 한국막학회 2003년도 The 4th Korea-Italy Workshop
    • /
    • pp.95-97
    • /
    • 2003
  • The main purpose of this work is to investigate the performance of membranes for treatment of dyeing wastewater. The microfiltration (MF) membranes (titania-blended polysulfone & alumina) were prepared. The nanofiltration (NF) and reverse osmosis (RO) membranes were kindly supplied by the Sae-Han. In order to reuse the wastewater for dyeing, the effluents were treated by the high flux RO and the fouling resistant RO (FRM) membranes. Also, the NF membrane was used for water reuse in rinsing.

  • PDF

금속/세라믹 중공사형 복합 한외여과막의 제조 (Preparation of Metal/Ceramic Composite Ultrafiltration Hollow Fiber Membranes)

  • 김인철;정보름;이동욱;박주영;권자영;이규호
    • 멤브레인
    • /
    • 제19권1호
    • /
    • pp.47-53
    • /
    • 2009
  • 본 연구의 목적은 금속 중공사형 필터에 무기 입자를 코팅하여 금속/세라믹 복합 한외여과막을 제조하는 것이다. 직경이 2.0 mm이며 기공 크기가 $2{\sim}8{\mu}m$ 범위를 갖는 니켈 중공사 필터에 급냉건조법과 침지-건조법으로 실리카 졸과 티타니아 졸을 코팅하여 금속쎄라믹 복합 한외여과막을 제조하였다. SEM과 PMI 결과로부터 기공 크기가 50 nm 수준을 갖는 것을 확인하였다. 기공 크기는 입자 크기, 소성시간 및 온도에 따라 차이를 보였다.

코팅용 알루미타, 티타니아솔 제조에 관한 연구 (A Study on the Preparation of Aluina & Titania Sols for Coatings)

  • 김추희;최형수;조영상;임종주
    • 한국재료학회지
    • /
    • 제4권3호
    • /
    • pp.319-328
    • /
    • 1994
  • 솔-제법에 의한 고분자솔 제조를 위하여 금속 알콕사이드에 $\beta$-diketonate(DKT)기의 유기 리간드를 치환시켜 만든 전구체를 합성한 결과, 가수분해와 축합 반응의 속도 조절이 가능하였고, 이를 이용하여 코팅에 적합한 nm단위의 입자 크기를 갖는 알루미나, 티타니아 솔을 제조하고 그 물성을 파악하였다. 코팅에 적합한 알루미나 솔의 최적조건은 알콕사이드 1몰당 물 1몰, 산 0.3-0.4몰이었다. 티타니아 솔의 제조시는 물/알콕사이드의 몰비가 1이고, 산의 양은 치환수에 따라 달라 1개와 2개 치환된 전구체의 경우 1목의 알콕사이드당 각각 0.25, 0.20몰 이하였다. Dynamic light scattering 장치를 이용하여 제조한 솔의 평균 입자 크기를 측정한 결과 수 nm단위의 미세한 입자를 갖고 있었다. 슬라이드 글라스 위에 코팅하여 $450^{\circ}C$에서 소결한 막을 SEM으로 관찰한 결과 알루미나와 타타니아의 경우 각각 4-4.5$\mu \textrm{m}$, 2-2.5$\mu \textrm{m}$두께의 매끄럽고 균열이 없는 막이 형성되었음을 알 수 있었다. 이때의 입자 크기는 TEM사진을 통하여 알 수 있었으며 티타니아의 경우 수 nm에서 최대 30nm, 알루미나는 1-2nm이하 심지어 수 $\AA$정도의 입자들로 이루어졌음을 관찰하였다. 또한 회절무늬 분석 결과 알루미나는 $\gamma$구조, 티타니아는 anastase결정임을 알 수 있었다.