Unexpected Chemical and Thermal Stability of Surface Oxynitride of Anatase TiO2 Nanocrystals Prepared in the Afterglow of N2 Plasma

  • Jeon, Byungwook;Kim, Ansoon;Kim, Yu Kwon
    • Applied Science and Convergence Technology
    • /
    • v.26 no.4
    • /
    • pp.62-65
    • /
    • 2017
  • Passivation of surface defects by the formation of chemically inert structure at the surface of $TiO_2$ nanocrystals can be potentially useful in enhancing their photocatalytic activity. In this regard, we have studied the surface chemical states of $TiO_2$ surfaces prepared by a treatment in the afterglow of $N_2$ microwave plasma using X-ray photoemission spectroscopy (XPS). We find that nitrogen is incorporated into the surface after the treatment up to a few atomic percent. Interestingly, the surface oxynitride layer is found to be chemically stable when it's in contact with water at room temperature (RT). The surface nitrogen species were also found to be thermally stable upon annealing up to $150^{\circ}C$ in the atmospheric pressure. Thus, we conclude that the treatment of oxide materials such as $TiO_2$ in the afterglow of $N_2$ plasma can be effective way to passivate the surface with nitrogen species.

Calcium Aluminate Phosphor Supported $TiO_2$ Nanoparticles (산화(酸化)티탄 나노입자(粒子)가 담지(擔持)된 칼슘 알루미늄 형광체(螢光體))

  • Thube, Dilip R.;Kim, Jin-Hwan;Kang, Suk-Min;Ryu, Ho-Jin
    • Resources Recycling
    • /
    • v.18 no.4
    • /
    • pp.24-30
    • /
    • 2009
  • Rare earth based calcium aluminate phosphor ($CaAl_2O_4:Eu^{2+}$, $Nd^{3+}$) supported $TiO_2$ nanoparticles are synthesized by using sol-gel method, which are further characterized using powder X-ray diffraction (XRD), fourier transform infrared (FT-IR), diffuse reflectance UV-Visible spectroscopy (DRS UV-Vis) and transmission electron microscopy (TEM). The XRD pattern of as-prepared and sintered phosphor supported $TiO_2$ does not show the tendency to change the crystal structure from anatase to rutile phase up to $600^{\circ}C$. This indicates that the phosphor support might inhibit the densification and crystallite growth by providing dissimilar boundaries. The diffuse reflectance spectral (DRS) measurements showed shift towards longer wavelength indicating reduction in the band-gap energy as compared to free $TiO_2$. The FT-IR spectra of phosphor supported $TiO_2$ nanoparticles show shift in the peak positions to lower wavelengths. This indicates that the $TiO_2$ nanoparticles are not free, but covalently bonded to the phosphor support. TEM micrographs show presence of crystalline and spherical $TiO_2$ nanoparticles (8 - 15 nm diameter) dispersed uniformly on the surface of phosphor.