• 제목/요약/키워드: thermal shock

검색결과 714건 처리시간 0.025초

전기용융 분말로부터 합성된 $Al_2$TiO$_5$ Ceramics의 열충격 저항성 (Thermal Shock Resistance of $Al_2$TiO$_5$ Ceramics Prepared from Electrofused Powders)

  • 김익진
    • 한국세라믹학회지
    • /
    • 제35권10호
    • /
    • pp.1061-1069
    • /
    • 1998
  • The thermal instability of Al2TiO5 Ceramics was contrlled by solid solution with MgO SiO2 and ZrO2 through electrofusion in an arc furnace. The thermal expansion properties of Al2TiO5 composites show the hysteresis due to the strong anisotropy of The crystal axes of these material. These phenomena are ex-plained by the opening and closing of microcracks. The difference in microcracking temperatures e.g 587.6(ATG2), 405.9(ATG3) and 519.7$^{\circ}C$(ATG4) is caused by the difference in grain size and stabilizer type. The thermal shock behaviour under cyclic conditions between 750-1400-75$0^{\circ}C$ show no change in mi-crostructure and phase assemblage for all three stabilized specimens. After the thermal loading test at 110$0^{\circ}C$ for 100hrs. ATG1 and ATG2 materials decomposes completely to its components corundum and ru-tile in both cases. However with approximatelly 20% retention of the Al2TiO5 Thus in order to prevent decomposition of the stabilized material in the critical temperature range 800-130$0^{\circ}C$ it must be traversed within a short period of time.

  • PDF

플립칩 패키지에서 무연 솔더 조인트 및 UBM의 열충격 특성 해석 (An Analysis on the Thermal Shock Characteristics of Pb-free Solder Joints and UBM in Flip Chip Packages)

  • 신기훈;김형태;장동영
    • 한국공작기계학회논문집
    • /
    • 제16권5호
    • /
    • pp.134-139
    • /
    • 2007
  • This paper presents a computer-based analysis on the thermal shock characteristics of Pb-free solder joints and UBM in flip chip assemblies. Among four types of popular UBM systems, TiW/Cu system with 95.5Sn-3.9Ag-0.6Cu solder joints was chosen for simulation. A simple 3D finite element model was first created only including silicon die, mixture between underfill and solder joints, and substrate. The displacements due to CTE mismatch between silicon die and substrate was then obtained through FE analysis. Finally, the obtained displacements were applied as mechanical loads to the whole 2D FE model and the characteristics of flip chip assemblies were analyzed. In addition, based on the hyperbolic sine law, the accumulated creep strain of Pb-free solder joints was calculated to predict the fatigue life of flip chip assemblies under thermal shock environments. The proposed method for fatigue life prediction will be evaluated through the cross check of the test results in the future work.

질화상압(NPS)법으로 제조한 질화규소의 열충격 저항성 및 내부식성 특성평가 (Thermal Shock and Hot Corrosion Resistance of Si3N4 Fabricated by Nitrided Pressureless Sintering)

  • 곽길호;김철;한인섭;이기성
    • 한국세라믹학회지
    • /
    • 제46권5호
    • /
    • pp.478-483
    • /
    • 2009
  • Thermal shock and hot corrosion resistance of silicon nitride ceramics are investigated in this study. Silicon nitrides are fabricated by nitride pressureless sintering (NPS) process, which process is the continuous process of nitridation reaction of Si metal combined with subsequent pressureless sintering. The results of thermal shock test show it sustains 400MPa of initial strength during test in the designated condition of ${\Delta}T=700{\sim}25^{\circ}C$ up to maximum 4,800 cycles. Hot corrosion tests also reveal that the strength degradation of NPS silicon nitride did not occur at $700^{\circ}C$ with an exposure in Ar, $H_2$, Na and K for 1,275 h.

가압열충격에 대한 원자로용기의 구조건전성 평가프로그램의 개발 (Development of structural integrity evaluation program for reactor vessel under pressurized thermal shock)

  • 정명조
    • 전산구조공학
    • /
    • 제9권2호
    • /
    • pp.153-161
    • /
    • 1996
  • 본 논문에서는 가압열충격의 파괴역학적 해석에 필요한 이론을 조사하였고 원자로용기의 구조건전성을 평가하기 위하여 해석과정을 전산화하였다. 우선 사고 transient에 대하여 원자로용기내의 압력과 주입되는 냉각재의 온도변화가 주어지면 이들로 부터 시간에 따른 용기에서의 온도와 응력분포를 구하고, 중성자 조사량과 용기 재질의 화학성분으로 부터 기준무연성천이온도의 분포가 구해지며 이로부터 파괴인성치 K/sub IA/와 K/sub IC/의 분포가 얻어진다. 또한 응력분포로 부터 균열의 크기 및 형상에 따라 응력확대계수 K/sub I/이 구해지므로 이를 K/sub IA/및 K/sub IC/와 비교함으로써 균열의 성장거동을 예측할 수 있다. 지금까지 보고된 가압열충격을 유발할 수 있는 대표적인 사고 transient가 국내 발전소에 발생할 경우를 가정하여 해석을 수행하였고 그 결과에 대하여 검토하였다.

  • PDF

금속기지 내열 경사기능 복합재료 개발에 관한 연구 (Development of the Heat-Resistant Functionally Gradient Material with Metal Substrate)

  • 김부안;남기우;조문호
    • 한국해양공학회지
    • /
    • 제13권1호통권31호
    • /
    • pp.62-69
    • /
    • 1999
  • 67Ni-22Cr-10Al-1Y and $ZrO_2-8Y_2O_3$ were coated on the substrate surface of ST304 and Al2024 by the plasma spraying method. The adgesion of the films varies depending on the substrates and the laminating method. In the case of STS304, the cracks were observed at thermal shock temperature difference ${Delta}T$ of $900^{circ}C$ in the non functionally gradient material(NFGM) and at $1100^{circ}C$ in the functionally gradient material(FGM). The film adhesion of the FGM is better than that of the NFGM in ST304. The cumulative AE count of the FGM of STS304 increased continuously at the bending test. But the NFGM of STS304 showed discontinuity of the AE count. The total AE count for the FGM of STS304 decreased as the number of thermal shock increased, and this tendency was evident as the thermal shock temperature difference increased.

  • PDF

Thermal Shock Behavior of TiN Coating Surface by a Pulse Laser Ablation Method

  • Noh, Taimin;Choi, Youngkue;Jeon, Min-Seok;Shin, Hyun-Gyoo;Lee, Heesoo
    • 대한금속재료학회지
    • /
    • 제50권7호
    • /
    • pp.539-544
    • /
    • 2012
  • Thermal shock behavior of TiN-coated SUS 304 substrate was investigated using a laser ablation method. By short surface ablation with a pulse Nd-YAG laser, considerable surface crack and spalling were observed, whereas there were few oxidation phenomena, such as grain growth of TiN crystallites, nucleation and growth of $TiO_2$ crystallites, which were observed from the coatings quenched from $700^{\circ}C$ in a chamber. The oxygen concentration of the ablated coating surface with the pulse laser also had a lower value than that of the quenched coating surface by Auger electron spectroscopy and electron probe micro analysis. These results were attributed to the fact that the properties of the pulse laser method have a very short heating time and so the diffusion time for oxidation was insufficient. Consequently, it was verified that the laser thermal shock test provides a way to evaluate the influence of the thermal shock load reduced oxidation effect.

Re-acceleration of Nonthermal Particles at Weak Cosmological Shock Waves

  • 강혜성;류동수
    • 천문학회보
    • /
    • 제36권1호
    • /
    • pp.45.1-45.1
    • /
    • 2011
  • Shock waves form in the intergalactic medium as a consequence of accretion, merger, and turbulent motion during the structure formation of the universe. They not only heat gas but also govern non-thermal processes through the acceleration of cosmic rays (CRs), production of magnetic fields, and generation of vorticity. We examine diffusive shock acceleration of the pre-existing as well as freshly injected populations of nonthermal, CR particles at weak cosmological shocks. Since the injection is extremely inefficient at weak shocks, the pre-existing CR population dominates over the injected population. If the pressure due to pre-existing CR protons is about 5 % of the gas thermal pressure in the upstream flow, the downstream CR pressure can absorb typically a few to 10 % of the shock ram pressure at shocks with the Mach number M<3. Yet, the re-acceleration of CR electrons can result in a substantial synchrotron emission behind the shock. The implication of our findings for observed bright radio relics is discussed.

  • PDF

고온하에서 암석의 열충격, 열팽창 및 열파괴에 관한 연구 (A Study on Thermal Shock, Thermal Expansion and Thermal Cracking of Rocks under High Temperature)

  • 이형원;이정인
    • 터널과지하공간
    • /
    • 제5권1호
    • /
    • pp.22-40
    • /
    • 1995
  • Thermomechanical characteristics of rocks such as thermal shock, thermal expansion, thermal cracking were experimentally investigaed using Iksan granite, Cheonan tonalite and Chung-ju dolomite to obtain the basic data for proper design and Chung-ju dolomite to obtain the basic data for proper design and stability analysis of underground structures subjected to temperature changes. The effect of thermal shock did not appear when the heating speed was under 3$^{\circ}C$/min. and there existed little difference between multi-staged cyclic heating and single-cycled heating. Thermal expansion of rocks was affected by mineral composition, crack porosity and the degree of thermal craking. In quartz-beraring multimineralic rocks such as Iksan granite and Cheonan tonalite, the thermal expansion coefficient increaseed continuously with temperature rise, but that of Chung-ju dolomite which was a monomineralic rock showed a constant value for the temperature above 250$^{\circ}C$, Chung-ju dolomite yielded the lowest critical threshold temperature(Tc) of 100$^{\circ}C$ and unstable thermal cracking was initiated above the new threshold temperature(Tc')of 300$^{\circ}C$. Above Tc' thermal cracks grew but they were not interconnected. Iksan granite showed closing of microcracks to the temperature of 100$^{\circ}C$, then expanded linearly to Tc of 200$^{\circ}C$. Above Tc, thermal cracking was initiated and progressed rapidly and almost all the grain boundaries were cracked at 600$^{\circ}C$. Cheonan tonalite also showed similar behavior to iksan granite except that Tc was 350$^{\circ}C$ and that thermal cracks propagated more rapidly. Thermal expansions calculated by Turner's equation were found to be valid in predicting the thermal expansion and cracking behavior of rocks.

  • PDF

골모세포에서 열자극에 의한 Hsp27 발현에 대한 연구 (HSP27 EXPRESSION IN OSTEOBLAST BY THERMAL STRESS)

  • 임재석;김병렬;권종진;장현석;이의석;전상호;우현일
    • Maxillofacial Plastic and Reconstructive Surgery
    • /
    • 제30권1호
    • /
    • pp.11-21
    • /
    • 2008
  • Aim of the study: Thermal stress is a central determinant of osseous surgical outcomes. Interestingly, the temperatures measured during endosseous surgeries coincide with the temperatures that elicit the heat shock response of mammalian cells. The heat shock response is a coordinated biochemical response that helps to protect cells from stresses of various forms. Several protective proteins, termed heat shock proteins (hsp) are produced as part of this response. To begin to understand the role of the stress response of osteoblasts during surgical manipulation of bone, the heat shock protein response was evaluated in osteoblastic cells. Materials & methods: With primary cell culture studies and ROS 17/2.8 osteoblastic cells transfected with hsp27 encoding vectors culture studies, the thermal stress response of mammalian osteoblastic cells was evaluated by immunohistochemistry and western blot analysis. Results: Immunocytochemistry indicated that hsp27 was present in unstressed osteoblastic cells, but not fibroblastic cells. Primarily cultured osteoblasts and fibroblasts expressed the major hsp in response to thermal stress, however, the small Mr hsp, hsp27 was shown to be a constitutive product only in osteoblasts. Creation of stable transformed osteoblastic cells expressing abundant hsp27 protein was used to demonstrate that hsp27 confers stress resistance to osteoblastic cells. Conclusions: The demonstrable presence and function of hsp27 in cultured bones and cells implicates this protein as a determinant of osteoblastic cell fate in vivo.

초 고온·고압 소결 공정으로 제조된 다결정 다이아몬드 컴팩트(PDC)의 미세조직 및 열충격 특성에 미치는 다이아몬드 입자 비율의 영향 (Effect of Diamond Particle Ratio on the Microstructure and Thermal Shock Property of HPHT Sintered Polycrystalline Diamond Compact (PDC))

  • 김지원;박희섭;조진현;이기안
    • 한국분말재료학회지
    • /
    • 제22권2호
    • /
    • pp.111-115
    • /
    • 2015
  • This study investigates the microstructure and thermal shock properties of polycrystalline diamond compact (PDC) produced by the high-temperature, high-pressure (HPHT) process. The diamond used for the investigation features a $12{\sim}22{\mu}m$- and $8{\sim}16{\mu}m$-sized main particles, and $1{\sim}2{\mu}m$-sized filler particles. The filler particle ratio is adjusted up to 5~31% to produce a mixed particle, and then the tap density is measured. The measurement finds that as the filler particle ratio increases, the tap density value continuously increases, but at 23% or greater, it reduces by a small margin. The mixed particle described above undergoes an HPHT sintering process. Observation of PDC microstructures reveals that the filler particle ratio with high tap density value increases direct bonding among diamond particles, Co distribution becomes even, and the Co and W fraction also decreases. The produced PDC undergoes thermal shock tests with two temperature conditions of 820 and 830, and the results reveals that PDC with smaller filler particle ratio and low tap density value easily produces cracks, while PDC with high tap density value that contributes in increased direct bonding along with the higher diamond content results in improved thermal shock properties.