Separation and Utilization of Main Components of Hardwood by Organosolv Pupling (Organosolv 방법(方法)에 의(依)한 활엽수(闊葉樹) 주요(主要) 조성분(組成分)의 분리(分離) 및 이용(利用))

  • Paik, Ki-Hyon;An, Byoung-Jun;Nahm, Won-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.16 no.4
    • /
    • pp.70-78
    • /
    • 1988
  • To separate and utilize the main components of hardwood (Quercus mongolica) by organosov pulping (ester pulping), chips were cooked at various conditions such as; the solvent ratio (acetic acid: ethylacetate: water, 50:25:25; 33:33:34; 25:50:25), maximum temperature (165, 170, $175^{\circ}C$), and cooking times (2, 2.5, 3 hr). The pulps were bleached by the sequences of CEDED, C/DEDED, PEDED. Lignin, sugars, and acetic acid were separated from black liquor and washing liquors. 1. The selective delignification at optimal pulp yield (43-45%) was obtained by cooking at acetic acid: ethylace tate: water ratio of 33:34:34 for 3 hr at $170^{\circ}C$. But in this case, kappa no. of the pulp was not reduced under 60 points. 2. Kappa no. of the pulp could be dropped by an acetone wash to remove reprecipitated lignin a t cooked pulp. 3. The unbleached pulps had a brightness of 45-50%, whereas the bleached pulps gave at 88-93% brightness. Tensile, burst, and tear strengths of the bleached pulps were lower than those of kraft pulp, especially in tear strength. The pulps which were bleached with CEDED sequence were higher in strengths than another bleaching sequences. 4. Lignin of 90-95%(lignin base on wood)was separated from black liquor and washing liquors, while the purified sugars and recovery of acetic acid were a low. An organic phase composed of acetic acid, ethylacetate, and water was separated to a two-phase system by proper adjustment of the solvent ratios.

  • PDF

Properties of Rubbers and Coated Fabrics according to Different Cross-linking Density of Coating Agent (코팅제의 가교 밀도에 따른 고무와 코팅원단의 물성 변화)

  • Suhong Kim;Kisuk Sung;Doohyun Baik
    • Textile Coloration and Finishing
    • /
    • v.35 no.1
    • /
    • pp.8-19
    • /
    • 2023
  • Silicone rubber is widely used in most industries due to diverse advantages like heat stability, UV stability, durability, chemical resistance, environment friendliness, inertness and so on. But there is limitation to expand applications due to relatively weak rubber strengths such as tensile strength and tear strength, especially in fabric coating applications. The purpose of this study is to find influence of coating agent on performances of rubber and coated fabrics and their correlation according to different crosslinking densities of silicone rubbers. Addition cure type of silicones were formulated using crosslinked MQ-type silicone resin consisting of M (R3SiO1/2) and Q (SiO4/2) and linear polymers. Raw materials used were; 1) linear vinyl endblocked polymers and vinyl functional MQ resin as main polymers, 2) linear silicone hydride polymers as crosslinkers, 3) platinum catalyst and 4) inhibitor to control curing speed. Rubber specimens were prepared to check mechanical strength using universal testing machine (UTM). Crosslinking density was calculated using Flory-Rhener equation using solvent swelling method. Differential scanning calorimetry (DSC) and scanning electron microscope (SEM-EDS) were used to characterize rubbers. Consequently, it was found that physical properties of silicone rubbers and coated fabrics can be expected by crosslinking density of rubbers. Silicone rubber formulations that contain 20 ~ 30 wt% of vinyl MQ resin showed strongest balanced performances.

A Study of the Changes for Military Uniform Fabric Properties according to Multiple Washing (전투복 원단 다회 세탁에 따른 물성변화 연구)

  • Kim, Ji-Hoon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.20 no.10
    • /
    • pp.366-373
    • /
    • 2019
  • Combat uniforms require higher tensile and tear strength than civilian products, and applied infrared reflectance from the recently developed nighttime fluoroscopy equipment to ensure combatant survival at night. Unlike other uniforms for civilian use, combat uniforms require durability against laundering because they may not be supplied again, once originally provided. Therefore, this study examined the changes in strength and changes in infrared reflectance after multiple washing of combat uniforms. The experiment confirmed that the strength change after the washing of combat uniforms 15 times was maintained in the same manner as the result after washing five times. In the case of infrared reflectance, the difference in reflectance after multiple washing treatments was greater than that in the case where washing was not performed. Therefore, although the durability in the case of combat uniforms is strong, it is necessary to maintain a reflectance higher than a certain level through the development of materials and the development of dyes.

The Relationship between Blowing Agents and Inner Temperature at the Preparation of Flexible Polyurethane Forams (연질 폴리우레탄 발포체 제조에서 발포제와 내부 온도와의 관계)

  • Lee, S.W.;Kim, J.H.;Kim, K.H.;Yang, Y.K.;Ahn, C.I.;Myong, Y.C.
    • Journal of the Korean Applied Science and Technology
    • /
    • v.16 no.2
    • /
    • pp.179-185
    • /
    • 1999
  • The effect of blowing agents and inner temperature on the machanical properties of the flexible polyurethane foams were investigated. In the study used that chemical blowing agents is $H_2O$ and support blowing agents. CFC-11, HCFC-114b, dichloromethane, n-penthane, iso-pentane, cyclopentane. The flexible polyurethane foams were foamed by the density of $0.015{\pm}0.002g/cm^3$ and $0.024{\pm}0.002g/cm^3$ which were used in mechanical properties measurements. Inner temperature was measure as long as the preparation of the flexible polyurethane foams of each blowing agents. The density, tensile strength, elongation, tear strength, compression strength and compression set were measured after 48 hours hardening. The result of the study was optimized dichloromethane and cyclopentane at the support blowing agents.

Anatomical Structures and Fiber Quality of Four Lesser-Used Wood Species Grown in Indonesia

  • MARBUN, Sari Delviana;WAHYUDI, Imam;SURYANA, Jajang;NAWAWI, Deded Sarip
    • Journal of the Korean Wood Science and Technology
    • /
    • v.47 no.5
    • /
    • pp.617-632
    • /
    • 2019
  • This study aimed to investigate the anatomical structure and fiber quality of four lesser-used wood species namely Benuang (O. sumatrana), Duabanga (D. moluccana), Pisang Merah (H. hellwigii), and Terap (A. odoratissimus). This study evaluated its suitability for raw material in pulp and paper manufacturing. The anatomical structure was observed macro- and microscopically. Macroscopic structures were observed directly to the wood samples, while microscopic characteristics were observed through microtome specimens. Fiber dimension was measured through macerated specimens and fiber quality was analyzed following the Rachman and Siagian's method. Results showed that these four timber species have similarity in the indistinct growth ring, diffuse porous in a radial pattern, rounded solitary vessel outline, 1 to 3 cells of ray width, deposits within the rays, fiber length, and cell wall thickness. Differences were found on vessel diameter, vessel grouping, vessel frequency, tyloses existence, type of axial parenchyma, and ray height. Based on fiber length and its derived values, the wood fibers of all species studied are suitable for pulp and paper manufacturing. They belong to the II quality class. The produced pulp and paper would have good quality, especially in tensile, folding, and tear strength. To promote their utilization, silviculture aspect of these four species has to be well understood.

The Properties of Kenaf/Polyester Blended Nonwovens (케나프/폴리에스테르 혼방 부직포의 특성)

  • Lee, Hye-Ja;Yoo, Hye-Ja;Han, Young-Sook
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.31 no.7
    • /
    • pp.1119-1127
    • /
    • 2007
  • Nonwovens have been widely used in various regions from the households to the industrial, agricultural and medical goods. Synthetic fibers have been used for source of nonwovens commonly because of their useful and economic properties. They are not only main factor causing environmental problems but also spend huge cost to renew the environmental disruption by them. Nonwovens must have both cost-competitiveness and environment-friendly property to be the desirable sources in 21th centuries. For meet these needs, it is suitable for the times that economical and environmentally-safe kenaf fibers would be used as raw materials of nonwovens. Kenaf and polyester fibers were blended in 4 types of ratio : 0/100, 20/80, 40/60, 60/40 were needle-punched. The nonwovens properties such as color values, surface appearance, strength, elongations, stiffness, moisture regain, water and oil absorbency, and electrification were tested. As the results, tensile and tear strengths, water and oil absorbency were maximum at 20/80 kenaf/polyester blend nonwoven, because of effecting by nonwoven structure and fiber properties. The moisture regain were increased according to kenaf were blended and the eletrification reduced in proportion to the kenaf fibers by chemical property of fiber composed nonwovens.

Effective Utilization of Hemp Fiber for Pulp and Papermaking(II) - Characteristics of hemp-wood paper made of hemp fiber cooked at low temperature - (펄프.제지용 원료로서의 삼 섬유 이용에 관한 연구(제2보) -저온 펄프화 삼 섬유의 수초지 특성-)

  • Lee, Myoung-Ku;Kim, Ji-Seop;Yoon, Seung-Lak
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.43 no.5
    • /
    • pp.27-33
    • /
    • 2011
  • Hemp bast pulp cooked at temperature below $100^{\circ}C$ followed by defibration by the knife and the valley beater, respectively was mixed with softwood pulp varying the amount of hemp pulp in order to find the optimum condition for making hemp-wood paper. Both the knife and the valley beaters contributed to the dispersion of pulp fiber well. Lots of shives were found when the knife beater was applied exclusively, but the fibers were dispersed well when freeness dropped to 600 mL CSF and 500 mL CSF by the valley beater. Air resistance decreased drastically below 500 mL CSF where rapid disrupture of pulp fiber occurred. As the values for freeness and hemp fiber content increased, so did roughness and bulk. It was apparent that the tear strength of hemp-wood paper was on the rise drastically as hemp fiber content increased. Nevertheless the optimum hemp fiber content of hemp-wood paper would be 20% considering the decrease in both tensile and burst strengths as well as sheet formation.

Changes of Handsheet Fracture Toughness by Wood and Cotton Fibers Mixing (목재섬유와 면섬유의 혼합에 따른 수초지의 파괴인성 변화)

  • Kim, Jeong-Jung;Jang, Dong-Uk;Yoon, Sang-Gu;Shin, Hyeon-Sik;Park, Jong-Moon
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.46 no.3
    • /
    • pp.81-87
    • /
    • 2014
  • Conditions of paper manufacturing process should be changed depending on the end use and paper properties. Most of the case, mixed pulps with long softwood fibers and short hardwood fibers are used to achieve proper qualities of product with reasonable production cost. For specialty paper manufacture the wood pulp and cotton linter pulp are usually mixed together. The objectives of this study is to analyze physical, mechanical and fracture mechanical properties of paper depending on SwBKP, HwBKP and cotton linter pulp(CLP) mixing. When the mixing ratio of SwBKP was increased, strength properties, such as tensile, tear, and folding endurance, were also increased. When the mixing ratio of SwBKP and HwBKP was increased, stress concentration index was decreased and fracture toughness was increased.

EoP Bleaching of Mixed Office Wastepaper (MOW의 산소-알칼리 첨가 과산화수소 표백)

  • Kim, Seung-Ho;Lee, Hyung;Baek, Ki-Hyun
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.34 no.3
    • /
    • pp.46-52
    • /
    • 2002
  • To produce the raw material used for printing and writing paper or high quality tissue, MOWs that were consisted of white ledger, colored ledger and old newspaper were bleached with EoP and EoPY(FAS) method, the EoP bleaching process gave the improvement in brightness and a high color removal efficiency. Especially, MOW B(initial brightness: 59.1% ISO) that contained much old newspaper showed the higher bleaching efficiency than those of MOW A(initial brightness: 68.3%). After EoPY(FAS) bleaching, MOW's brightness was increased from 68.3% ISO to 84.3∼84.0% ISO, and from 59.1% ISO to 78.7∼79.2% ISO, respectively. Also the tensile and burst index of bleached pulps decreased by 10∼30%. The tear index slightly decreased or halted at the same range as unbleached pulps.

Effect of Chlorinated Polyethylene(cPE) on Morphology and Mechanical Properties of Polypropylene(PP) and Nitrile Rubber(NBR) Blends (염소화폴리에틸렌의 첨가가 폴리프로필렌-니트릴 고무 블렌드의 모폴로지 및 기계적물성에 미치는 영향)

  • Chang, Young-Wook;Won, Jong-Hoon;Joo, Hyun-Seok;Chung, Kyung-Ho
    • Elastomers and Composites
    • /
    • v.40 no.3
    • /
    • pp.204-211
    • /
    • 2005
  • Effect of chlorinated polyethylene(cPE) on the morphology and mechanical properties of isotactic polypropylene(iPP) and nitrile rubber(NBR) blends was investigated. It was found that incorporation of a small amounts of cPE leads to a decrease in domain size of the dispersed phase, and uniform distribution of the dispersed phase in the blends. The PP/NBR/cPE ternary blends showed an improved tensile and tear strength as well as elongation-at-break as compared to binary PP/NBR blends. From the results on morphology and mechanical properties, optimum amount of the cPE is 5-10 wt% with repect to NBR in the blend.