Fabrication and Pore Properties of SUS316L Membrane with Double-Layered Pore Structures by Wet Powder Spraying

  • Min-Jeong Lee;Hyeon-Ju Kim;Manho Park;Jung-Yeul Yun
    • Archives of Metallurgy and Materials
    • /
    • v.67 no.4
    • /
    • pp.1531-1534
    • /
    • 2022
  • In this study, a SUS316L membrane having double layered pore structures was fabricated, and the pore characteristics were analyzed after coating with a spherical powder and a flake-shaped powder on a disk-shaped SUS316L support using a wet powder spraying process. The thickness of the coated layer was checked using an optical microscope, and air permeability was measured using a capillary flow porometer. When the coating amount was similar, the fine porous layer prepared using flake powder was thicker and showed higher porosity. In the case of a similar thickness, the case of using flake powder was half of the amount of spherical powder used. Therefore, it was confirmed that it is possible to manufacture a metal membrane having a high filter efficiency even with a small coating amount when using the flake powder.

A Study on the Pd-Ni Alloy Hydrogen Membrane using the Porous Nickel Metal Support (다공성 Ni 금속 지지체를 사용한 Pd-Ni 합금 수소 분리막 연구)

  • Kim Dong-Won;Um Ki-Youn;Kim Sang-Ho;Park Jong-Su
    • Journal of the Korean institute of surface engineering
    • /
    • v.37 no.5
    • /
    • pp.289-295
    • /
    • 2004
  • A dense palladium-nikel (Pd-Ni) alloy composite membrane has been fabricated on microporous nickel support mixed with submicron/micron nickel powder instead of mesoporous stainless steel support. Plasma treatment process is introduced as pre-treatment process instead of HCI activation. Pd-Ni alloy composite membrane prepared by electro plating was fairly a uniform and dense surface morphology. The membrane was characterized by permeation experiments with hydrogen and nitrogen gases at temperature 773 K and pressure 2.2 psi. The results showed that hydrogen ($H_2$) permeance was 27 ml/$\textrm{cm}^2$ㆍatmㆍmin and hydrogen/ nitrogen ($_H2$$N_2$) selectivity was 8 at 773 K.

Microstructure and Pore Characteristics of a SUS316L Gas Filter Fabricated by Wet Powder Spraying

  • Min-Jeong Lee;Yu-Jeong Yi;Hyeon-Ju Kim;Manho Park;Jungwoo Lee;Jung-Yeul Yun
    • Archives of Metallurgy and Materials
    • /
    • v.67 no.4
    • /
    • pp.1547-1550
    • /
    • 2022
  • In this study, a flake-shaped metal powder was coated on a tube shaped pre-sintered 316L stainless steel support using a wet powder spraying process to fabricate a double pore structure, and the pore characteristics were analyzed according to coating time and tube rotation speed. The thickness of the coated layer was checked via optical microscopy, and porosity was measured using image analysis software. Air permeability was measured using a capillary flow porometer. As a result of the experiment, the optimal rotation speed of the support tube was established as 200 rpm. When the rotation speed was fixed, the coating thickness and the coating amount of the double pore structure increased as the coating time increased. The porosity of the double pore structure was increased due to the irregular arrangement of the flake-shaped powder. The air permeability of the double pore structure decreased with increasing fine pore layer thickness.

The Effect of Porous Support and Intermediate Layer on the Silica-zirconia Membranes for Gas Permeation Performance (실리카-지르코니아 분리막 성능에 대한 다공성 지지체와 중간층의 영향)

  • Lee, Hye Ryeon;Seo, Bongkuk
    • Membrane Journal
    • /
    • v.25 no.1
    • /
    • pp.15-26
    • /
    • 2015
  • In this study, porous metal (O.D. = 10 mm, length = 10 mm, 316 L SUS, Mott Corp.) and ${\alpha}$-alumina tube (O.D. = 10 mm, length = 50 mm, Pall, German) support was modified with suspension sols, which were consisted of $3{\sim}4{\mu}m$ and 150 nm size of ${\alpha}$-alumina particle in the water or silica-zirconia colloidal sol. The porous support was fabricated by dip coating method for 5 seconds with suspension of alumina particles. After drying at $100^{\circ}C$ for 1 h, it was calcined at $550^{\circ}C$ for 30 min. It was repeated several times in order to decrease big pore on support. The surface roughness and largest pore size on the porous support was decreased by increasing coating times with $3{\sim}4{\mu}m$ size of ${\alpha}$-alumina particle and alumina coating with 150 nm size of ${\alpha}$-alumina particle served as further smoothening the surface and decreasing the pore size of the substrate. And the silica-zirconia membranes were successfully prepared on the modified porous metal and ${\alpha}$-alumina supports, and showed hydrogen permeance in the range of $1.8-8.4{\times}10^{-4}mol{\cdot}m^{-2}{\cdot}s^{-1}{\cdot}Pa^{-1}$ and $3.3-5.0{\times}10^{-5}mol{\cdot}m^{-2}{\cdot}s^{-1}{\cdot}Pa^{-1}$, respectively.