The Effects of Sealing Materials in Cone Crack Formation of Soda-lime Glass by Ball Impact (볼 충격을 받는 유리의 콘크랙형성에 대한 실링재료의 영향)

  • Kim, Moon-Saeng;Heo, Jin;Lee, Hyun-Chul;Kim, Ho-Jong
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.20 no.5
    • /
    • pp.156-163
    • /
    • 2003
  • In order to investigate the possibility of punching process of brittle material by ball impact, the effects of sealing materials about impact damage of soda-lime glass by small spheres were evaluated experimentally. The using of sealing materials in the development of perfect cone crack was more effective than no using of sealing materials. At the sealing materials condition, in the case of 5mm-thick specimen, Copper and PMMA sealing were more effective in producing a perfect cone formation than the other sealing materials. And in the case of 8mm-thick specimen, Aluminum sealing was most effective in producing a perfect cone formation. The impact velocity range over which perfect cones were formed was influenced by both the thickness of specimen and sealing materials. By a proper selection of sealing materials, the application fur industrial technology for hole (or nozzle) punching process of brittle materials is expected.

An Experimental Study on the Damage Mechanism of Particle Impact in a Scratched Glass (표면거칠기를 가진 유리의 입자충격 손상기구에 관한 실험적 연구)

  • Suh, Chang-Min;Chung, Seong-Muk;Lee, Mun-Hwan
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.20 no.7
    • /
    • pp.2196-2204
    • /
    • 1996
  • The damage mechanism by the impact of steel ball on the soda-lime glass having a different surface roughness was investigated. An initiation and a propagation behavior of cracks formed by each impact velocity were quantitatively studied. A 4-point bending test was carried out to evaluate the remaining bending strength of a scratched soda-lime glass which impacted by the steel ball. As the surface roughness was increased, the shape of cracks became more irregular rather than those of the smooth specimens. The phenomenon of turning up in the wing of cone cracks occurred even at the lower velocity than the critical velocity caused the crushing. The threshold velocity of cracks initiation generally became lower than those of smooth specimen. An initiation and a propagation behavior of radial cracks had no relation with the direction of scratch on the surface. The remaning benidng strength of the scratched specimen according to impact velocity had no big difference compared with those of the smooth specimen.

Damage Mechanism of Particle Impact in a $Cr_2O_3$ Plasma Coated Soda-lime Glass ($Cr_2O_3$ 플라스마 용사 코팅된 유리의 입자충격에 의한 손상기구)

  • Suh, Chang-Min;Lee, Moon-Whan;Kim, Sung-Ho;Jang, Jong-Yun
    • Journal of Ocean Engineering and Technology
    • /
    • v.12 no.3 s.29
    • /
    • pp.49-59
    • /
    • 1998
  • The damage mechanism of $Cr_2O_3$ plasma coated soda-lime glass and uncoated glass by steel ball particle impact was analyzed in this study. And the shape variation of the cracks was investigated by stereo-microscope according to the impact velocity and steel ball diameter. In order to improve the damage reduction effect by $Cr_2O_3$ coating layer, crack size was measured and surface erosion state was observed for both of two kinds of specimen after impact experiment. And the results were compared with each other. The 4-point bending test was performed according to ASTM D790 testing method to evaluate the effect of coating layer for bending strength variation. As a result, it was found that the crack size of $Cr_2O_3$ coated specimen was smaller than that of uncoated one, because of the impact absorption by interior pores in the coating layer and the load dispersion by the structural characteristic of the coating layer. For the specimens subjected to the steel ball impact, the bending strength of coated specimen was higher than that of uncoated specimen.

  • PDF

Dielectric Characteristics on Filler Content and Sintering Temperature in Pb-Free White Dielectric Layer (Pb-Free 백색유전체에서 필러함량과 소성온도에 따른 유전체 특성)

  • An, Yong-Tae;Choi, Byung-Hyun;Ji, Mi-Jung;Lee, Jung-Min;Kim, Hyun-Sun;Jung, Kyung-Won
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.8
    • /
    • pp.755-759
    • /
    • 2008
  • For the development of a new white dielectric layer in plasma display panel, different $TiO_2$ types as a filler was add to the $Bi_2O_3$-BaO-ZnO glass matrix. The reflectance and dielectric constant of dielectric have been investigated as a function of the mixing content (rutile and anatase), and sintering temperature. The reflectance of dielectric sintered at the 520$^{\circ}C$ appeared most highly and suitable in terms of the adhesion and reflectance of the soda-lime glasses. Also, the thermal expansion coefficient of dielectric was found to be $85.6\times10^{-7}/K$, which was similar to that of the soda-lime glasses. Especially, the dielectric constants were not increased with increasing of $TiO_2$ filler contents.

Elastic properties of ion-assisted Cr films measured by brillouin light scattering (브릴루앙 산란 실험을 이용한 이온빔 보조 증착법의 Cr 박막의 탄성특성)

  • ;;;John R. Dutcher
    • Korean Journal of Optics and Photonics
    • /
    • v.6 no.1
    • /
    • pp.50-55
    • /
    • 1995
  • We have performed Brillouin light scattering experiments to study the elastic properties of Cr films deposited on soda-lime glasses by using Ar-ion assisted deposition techniques. The elastic constants of the films increased as the ion-current density employed during the film deposition increases and they approached to the values of bulk Cr. The best fit values of the elastic constants of the films manufactured with ion current density of $400\muA/cm^{2}$are $c_{11}=296, c_{13}=83, c_{33}=289$, and $c_{55}=c_{44}=108(\times10^9/N/m^{2}}$ and these are 5% lower than those of bulk Cr in hexagonal symmetry. metry.

  • PDF

Vacuum Packaging and Operating Properties of Micro-Tunneling Sensors

  • Park, H.W.;Lee, D.J.;Son, Y. B.;Park, J.H.;Oh, M. H.;Ju, B. K.
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2000.04a
    • /
    • pp.110-110
    • /
    • 2000
  • Cantilever-shaped lateral field emitters were fabricated and their electrical characteristics were tested. As shown in Fig.1, poly-silicon cantilevers were fabricated by the surface micromachining and they were used to the vacuum magnetic field sensors. The tunneling devices were vacuum sealed with the tubeless packaging method, as shown in Fig.2 and Fig.3. The soda-lime glasses were used for better encapsulation, so the sputtered silicon and the glass layers on the soda-lime glasses were bonded together at 1x10$^{-6}$ Torr. The getter was activated after the vacuum sealing fur the stable emissions. The devices were tested outside of the vacuum chamber. Through vacuum packaging, the tunneling sensors can be utilized. Fig.4 shows that the sensor operates with the switching of the magnetic field. When the magnetic field was applied to the device, the anode currents were varied by the Lorentz force. The difference of anode currents can be varied with the strength of the applied magnetic field.

  • PDF

Impact Damage on Brittle Materials with Small Spheres (I) (취성재료의 소구충돌에 의한 충격손상 (I))

  • U, Su-Chang;Kim, Mun-Saeng;Sin, Hyeong-Seop;Lee, Hyeon-Cheol
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.18 no.11
    • /
    • pp.93-100
    • /
    • 2001
  • Brittle materials are very weak for impact because of typical characteristics which happen to be easily fractured with low fracture toughness and crack sensitivity. When brittle materials are subjected to impact due to small spheres, high contact pressure is occurred to impact surface and then local damage on specimen is developed, since there are little plastic deformations due to contact pressure compared to metals. This local damage is a dangerous factor which gives rise to final fracture of structures. In this research, the crack propagation process of soda lime glass by impact of small sphere is explained and the effects of the constraint conditions of impact spheres and materials for the material damage were studied by using soda-lime glass. that is the effects for the materials and sizes of impact ball, thickness of specimen and residual strength. Especially, this research has focused on the damage behavior of ring crack, cone crack and several kinds of cracks.

  • PDF

Production of Foamed Glass by Using Hydrolysis of Waste Glass (I) - Hydrolysis of Waste Glass - (폐 유리의 가수 분해반응에 의한 발포유리의 제조(I) - 폐유리의 가수분해 반응 -)

  • Lee, Chul-Tae;Lee, Hong-Gil
    • Applied Chemistry for Engineering
    • /
    • v.16 no.4
    • /
    • pp.519-526
    • /
    • 2005
  • Hydrolysis of soda-lime waste glass was investigated to test the feasibility for use of waste glass as feed material in the production of foamed glass. The soda-lime glass, such as plate glass and various bottle glasses, was effectively hydrolyzed by steam and water under high pressure. The proper condition for the hydrolysis was found to be reaction temperature of $250^{\circ}C$ and reaction time of 2 h. Under this condition, the water content of hydrated glass through hydrolysis was 7.85~10.04%, allowing successful foaming process for production of foamed glass. Using Na as the modifying agent of glass was effective in the hydrolysis by water. The highest water content of hydrated glass was obtained when weight ratio of NaOH to the glass was 0.04.

The Study on the Fabrication and Characterization of Dielectric Materials of Front and Back Panel for PDP(Plasma Display Panel)

  • Chang, Myeong-Soo;Lee, Yoon-Kwan;Ryu, Byung-Gil;Park, Myung-Ho
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2000.01a
    • /
    • pp.181-182
    • /
    • 2000
  • The glass compositions of $PbO-SiO_2-B_2O_3$ system and $P_2O_5-PbO-ZnO$ system for the transparent dielectric materials for front panel and $P_2O_5-ZnO-BaO$ and $SiO_2-ZnO-B_2O_3$ for the reflective dielectric materials for back panel of PDP(Plasma Display Panel) were investigated. As a transparent dielectric materials for front panel, $PbO-SiO_2-B_2O_3$ glass showed good dielectric properties, high transparency and proper thermal expansion matching to soda-lime glass substrate. And the reflective dielectric materials for back panel were prepared from parent glass of $SiO_2-ZnO-B_2O_3$ system and oxide filler. It was found that these glass-ceramics are useful materials for reflective dielectric layers, as those have a similar thermal expansion to soda-lime glass plate, high reflectance, low sintering temperature.

  • PDF

Strengthening of Substrate Glass for LCD by Single ton Exchange Process (Single Ion Exchange Process에 의한 LCD용 기판유리의 강화)

  • 이회관;오영석;이용수;강원호
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.7
    • /
    • pp.675-679
    • /
    • 2002
  • To produce a strengthened glass, single ion exchange properties such as three-point bend strength and residual stress were investigated in soda-lime-silicate substrate glass for display use. The present work showed that the maximum value of strength was 62.5${\times}$10$\sub$6/ kg/㎡ after, the two-step single ion exchange process at 470$^{\circ}C$ for 1 h and 450$^{\circ}C$ for 24 h. As the result of the fracture analysis after bending test, the residual stress on the fractured surface of the strengthened glass increased the flexibility by means of absorbing the elastic deformation energy in the glass. Also, the effects of absorbing the elastic deformation energy were analysed by curvature change, number of multiple crack branches and brittleness.