Early-Age Shrinkage and Durability of Shotcrete with Expansive Agent (팽창재를 혼입한 숏크리트의 초기수축 및 내구성 평가)

  • Nam-Gung, Kyeong;Kang, Moon-Sik;Hur, In;Yun, Kyong-Ku
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.13 no.10
    • /
    • pp.4884-4890
    • /
    • 2012
  • In this dissertation, the shrinkage and durability of shotcrete were examined. Analysis and comparison of shrinkage against the strength of shotcrete was investigated after performing actual shotcrete shooting for each mix of different percentage of expansive agent. The research on restrained shrinkage with different percentages of expansive agent used (3%, 7%, 11% and 15%) shows that the maximum shrinkage in all samples occurred in between 13-15 hrs after shotcrete shooting. And it is noticed that increasing the percentage of expansive agent can lower the shrinkage. And hence, the 15% of expansive agent not only lowered the shrinkage But it also lowered the strength.

Interfacial properties of composite shotcrete containing sprayed waterproofing membrane

  • Park, Byungkwan;Lee, Chulho;Choi, Soon-Wook;Kang, Tae-Ho;Kim, Jintae;Choi, Myung-Sik;Jeon, Seokwon;Chang, Soo-Ho
    • Geomechanics and Engineering
    • /
    • v.16 no.4
    • /
    • pp.385-397
    • /
    • 2018
  • This study evaluates the interfacial properties of composite specimens consisting of shotcrete and sprayed waterproofing membrane. Two different membrane prototypes were first produced and tested for their waterproofing ability. Then composite specimens were prepared and their interfacial properties assessed in direct shear and uniaxial compression tests. The direct shear test showed the peak shear strength and shear stiffness of the composites' interface decreased as the membrane layer became thicker. The shear stiffness, a key input parameter for numerical analysis, was estimated to be 0.32-1.74 GPa/m. Shear stress transfer at the interface between the shotcrete and membrane clearly emerged when measuring peak shear strengths (1-3 MPa) under given normal stress conditions of 0.3-1.5 MPa. The failure mechanism was predominantly shear failure at the interface in most composite specimens, and shear failure in the membranes. The uniaxial compression test yielded normal stiffness values for the composite specimens of 5-24 GPa/m. The composite specimens appeared to fail by the compressive force forming transverse tension cracks, mainly around the shotcrete surface perpendicular to the membrane layer. Even though the composite specimens had strength and stiffness values sufficient for shear stress transfer at the interfaces of the two shotcrete layers and the membrane, the sprayed waterproofing membrane should be as thin as possible whilst ensuring waterproofing so as to obtain higher strength and stiffness at the interface.

Experimental Study on the Improvement of Shotcrete Performance by Addition of Calcium Aluminate Based Accelerator and Metakaolin (시멘트 광물계 급결제와 메타카올린에 의한 숏크리트의 고성능화에 대한 실험적 연구)

  • Bae, Gyu-Jin;Chang, Soo-Ho;Park, Hae-Geun;Won, Jong-Pil
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.8 no.3
    • /
    • pp.237-247
    • /
    • 2006
  • The use of high-performance shotcrete lining is indispensable to improve long-term durability of a tunnel and to apply the single-shell tunnelling method. Among a lot of shotcrete admixtures, pozzolan materials such as silica fume have positive effects on increasing the strength and the durability of shotcrete. It is also well known that a cement-based accelerator is much faster in setting time and more eco-friendly than conventional accelerators. This study aimed to improve the properties of wet-mix shotcrete by incorporating with Metakaolin and the calcium aluminate based accelerator. To compare Metakaolin with silica fume, mixing ratios of each material were varied as 4% and 8% of cement weight. Moreover, Metakaolin was blended with silica fume, and their binder was also set to 4% and 8% of cement weight. At each mixing condition, setting time, compressive strength, flexural strength, permeability and freezing-thawing resistance were measured. From the experiments, it was revealed Metakaolin could be a substituting material for silica fume.

Numerical Study on Failure Mechanism of Tunnel Shotcrete Lining (터널 숏크리트 라이닝 파괴 메커니즘에 대한 수치해석적 고찰)

  • Shin, Hyusoung;Shin, Dongin;Bae, Gyujin;Kim, Donggyu
    • Journal of the Korean GEO-environmental Society
    • /
    • v.10 no.7
    • /
    • pp.167-177
    • /
    • 2009
  • This study investigates a failure mechanism of a tunnel shotcrete lining with respect to a concentrated load due to blocky rock mass. First of all, it is carried out to survey relevant researches to shotcrete failures by literature reviews and to numerically re-investigate the failure modes of shotcrete lining given by previous researches. Through this study, the failure modes are relocated with the conditions which induce each failure mode newly proposed by this study. In addition to this, the arching shape of tunnel lining, which has not been considered in the previous research despite of inherent geometrical characteristics in tunnels, is taken into consideration in numerical investigation on lining failure in this study. As a result, it is shown that more simplified failure modes can be found on the tunnel boundary condition and the corresponding failure condition to each mode can be different from ones of the previous study due to a tunnel arching effect.

  • PDF

The Non-destructive Inspection Using Infrared Thermal Technique on Reinforced Slopes by Shotcrete (적외선 열화상을 이용한 숏크리트 보강사면의 비파괴점검)

  • Shin, Chang-Gun;Lee, Song;Ahn, Sang-Ro
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.11 no.1
    • /
    • pp.95-102
    • /
    • 2007
  • It needs to Prevent damage as aging shotcrete itself exists as a dangerous component to comuting vehicles or infrastructure due to scaling, spaling, and loosening. However, it is hard to make an approach owing to a steep slope and high work, and there has been indicated a limit that it is difficult to grasp the internal condition of shotcrete on the surface. This study aimed to research internal defects that cannot be observed from the surface, by measuring a subtle thermal transfer on the shotcrete surface by using infrared thermography for overcoming such a technical limit. As a result of conducting an inspection through an analysis on measured data and fieldwork using an endoscope camera, it was impossible to accurately determine the wet part because of an excessive coating of shotcrete, yet, This study is proposed effictively extract a void part of the inside with non-destructive and non-touching method.

Evalution for Mechanical Property and Durability of Miner's Shotcrete (광산용 숏크리트의 역학적 특성 및 내구성 평가)

  • Nam-Gung, Kyeong;Ma, Sang-Joon;Lee, Kyeo-Re;Yun, Kyong-Ku
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.2
    • /
    • pp.1461-1468
    • /
    • 2015
  • Mostly mine support(Rock bolt and Support) which is currently general for reinforcements of a large scale tunnel is applied, Some executing a reinforcement to Poor ground by cast-in-place shotcrete. However On domestic mine conditions that couldn't having every time after mine tunnel excavation, it couldn't ensure the field batch plant which is a fixed in an issue of economies and site security, constructing it by supply gets from shotcrete materials combined in neighborhood ready mixed concrete manufacturing plants. carried shotcrete in ready mixed concrete manufacturing plants as migration length and time are falling off in quality. But, it is difficult for construction quality control By quality control arbitrariness absence at on-scene. In the present study, carry out Laboratory Test by kinds and percentages of accelerating agent for evalution of Mechanical Property and Durability of Shotcrete.

Evaluation of bonding state of tunnel shotcrete using impact-echo method - numerical analysis (충격 반향 기법을 이용한 숏크리트 배면 접착 상태 평가에 관한 수치해석적 연구)

  • Song, Ki-Il;Cho, Gye-Chun;Chang, Seok-Bue
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.10 no.2
    • /
    • pp.105-118
    • /
    • 2008
  • Shotcrete is one of the main support materials in tunnelling. Its bonding state on excavated rock surfaces controls the safety of the tunnel: De-bonding of shotcrete from an excavated surface decreases the safety of the tunnel. Meanwhile, the bonding state of shotcrete is affected by blasting during excavation at tunnel face as well as bench cut. Generally, the bonding state of shotcrete can be classified as void, de-bonded, or fully bonded. In this study, the state of the back-surface of shotcrete is investigated using impact-echo (IE) techniques. Numerical simulation of IE technique is performed with ABAQUS. Signals obtained from the IE simulations were analyzed at time, frequency, and time-frequency domains, respectively. Using an integrated active signal processing technique coupled with a Short-Time Fourier Transform (STFT) analysis, the bonding state of the shotcrete can be evaluated accurately. As the bonding state worsens, the amplitude of the first peak past the maximum amplitude in the time domain waveform and the maximum energy of the autospectral density are increasing. The resonance frequency becomes detectable and calculable and the contour in time-frequency domain has a long tail parallel to the time axis. Signal characteristics with respect to ground condition were obtained in case of fully bonded condition. As the ground condition worsens, the length of a long tail parallel to the time axis is lengthened and the contour is located in low frequency range under 10 kHz.

  • PDF

Performance Improvement and Durability Evaluation of Shotcrete for Permanent Tunnel Support (터널 영구 지보재로서의 숏크리트 고성능화 및 내구성 평가에 관한 연구)

  • Lee, Sang-Pil;Ryu, Jong-Hyun;Lee, Sang-Don;Jeon, Seok-Won;Lee, Chung-In
    • Tunnel and Underground Space
    • /
    • v.17 no.4
    • /
    • pp.266-284
    • /
    • 2007
  • Recently, many efforts have been made to construct the first unlined tunnel, without in-situ concrete lining, in Korea. However, the lack of reliability in the performance of shotcrete as permanent tunnel support prevented from its realization. Shotcrete has been regarded to have significant problems in field application and long term performance because of unsatisfactory strength level and durability compared to those of European countries. In this study, the high strength shotcrete satisfying compressive strength over 40 MPa and flexural strength over 4.5 MPa was developed from optimized mix design. The type of accelerators and the amount of silica fume were selected as the main factors in mixing process and the analyses were carried out up to the elapsed time of 2 years. In order to evaluate the short term durability of shotcrete, an array of laboratory test consisting of freeze-thaw, carbonation chloride penetration and permeability test was performed. For long-term durability tests, specimens have been put in an operated highway tunnel to expose them to the similar environment when they are actually used as an unlined tunnel support. From the strength and durability tests, it was found that only alkali-free based accelerator satisfied the target strength of this study and also, the developed shotcrete showed very high performance in its durability.

Stress analysis for shotcrete lining on uneven tunnel perimeter (비평탄 굴착벽면의 숏크리트 라이닝에 대한 응력해석)

  • Lee, Seungdo;Moon, Hyun-Koo
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.17 no.6
    • /
    • pp.597-604
    • /
    • 2015
  • When a tunnel is constructed by drilling and blasting operation, the excavated perimeter becomes uneven due to overbreak at the drill holes so that the thickness of shotcrete tends to be irregular. In this case, the conventional stress analyses for tunnel lining of a uniform thickness cannot be readily applicable. In this study, the profile of tunnel perimeter assumed to be sinusoidal in order to simulate the uneven tunnel perimeter and to control the thickness of shotcrete by using the amplitude and wavelength. By adopting the sinusoidal function to a theoretical solution of stress analysis for uniform lining, the range of axial stress of irregular shotcrete can be estimated. The applicability of the approximate solution has been verified by performing a series of numerical analyses for various conditions. It is shown that the axial stress of shorcrete is highly dependent upon the irregularity of shotcrete, together with the ground property and initial stress conditions. It is also shown the shear stress is dependent upon the wavelength, and the stress condition becomes unfavorable where the thickness of shotcrete is relatively small. The approach developed in this study shows that the stress state where the thickness is relatively small is unfavourable, and it is necessary to take complementary measures when installing shotcrete after blasting.