The possibility of manufacturing titanium hollow cylinder tank for ramjet engine was demonstrated with superplastic forming of subscale article. An innovative manufacturing method to produce complex configuration from titanium multi-sheets by low hydrostatic pressure was presented. Finite element analysis on superplastic blow forming process has been carried out in order to improve the forming process when manufacturing subscale hollow cylinder structure using Ti-6Al-4V multi-sheets. The simulation focused on the reduction of forming time and obtaining finally required shape throughout investigating the deformation mode of sheet according to the forming conditions and die geometry. From pre-sized titanium sheets, near net shape of hollow cylinder tank is obtained by superplastic blow forming conducted using gas pressure of 15bar at 1148K. The result shows that the manufacturing method with superplastic forming of multi-sheets of titanium alloy has been successful for near net shape forming of subscale hollow cylinder tank of ramjet engine.
The present study was carried out to evaluate the microstructural and mechanical properties of cross-roll rolled pure copper sheets, and the results were compared with those obtained for conventionally rolled sheets. For this work, pure copper (99.99 mass%) sheets with thickness of 5 mm were prepared as the starting material. The sheets were cold rolled to 90% thickness reduction and subsequently annealed at $400^{\circ}C$ for 30 min. Also, to analyze the grain boundary character distributions (GBCDs) on the materials, the electron back-scattered diffraction (EBSD) technique was introduced. The resulting cold-rolled and annealed sheets had considerably finer grains than the initial sheets with an average size of 100 ${\mu}M$. In particular, the average grain size became smaller by cross-roll rolling (6.5 ${\mu}M$) than by conventional rolling (9.8 ${\mu}M$). These grain refinements directly led to enhanced mechanical properties such as Vickers micro-hardness and tensile strength, and thus the values showed greater increases upon cross-roll rolling process than after conventional rolling. Furthermore, the texture development of <112>//ND in the cross-roll rolling processed material provided greater enhancement of mechanical properties relative to the case of the conventional rolling processed material. In the present study, we systematically discuss the enhancement of mechanical properties in terms of grain refinement and texture distribution developed by the different rolling processes.
The AA5182/polypropylene/AA5182 (AA/PP/AA) sandwich sheets have been developed for the application for automotive body panels in the future light weight vehicles with significant weight reduction. It has been reported that the 5182 aluminum sheet shows Luders band because of dissolved Mg atoms that causes fabrication process problem, especially surface roughness. The examination of serration behavior has been made after the tensile deformation of the AA/PP/AA sandwich sheets as well as that of the 5182 aluminum skin at room and elevated temperatures. All sandwich sheets and the 5182 aluminum skin showed serration phenomena on their flow curves. However, the magnitude of the serration was significantly diminished in the sandwich sheet with the high volume fraction of the polypropylene core. According to the results of the surface roughness analysis after the tensile test, the sandwich sheet evidently showed lower Luders band depth than the 5182 aluminum skin. Strain rate sensitivity, m-value, of the 5182 aluminum skin was -0.006. By attaching this skin with polypropylene core which has relatively large positive value, 0.050, m-value of the sandwich sheets was changed to the positive value. The serration reduction of the sandwich sheets was quantitatively investigated in the point of the effect on the polypropylene core thickness variation, that on the strain rate sensitivity. It was found that the serration reduction degree from the experimental results of the sandwich sheet was higher than that from the calculated values by the rule of mixture based on volume fraction of the skins and the core.
두께 1 ${\mu}m$ 정도의 연자성 Fe-Si-Cr 합금 박편을 편상화 가공을 실시한 그대로 및 500과 $700^{\circ}C$에서 1시간 어닐링한 후 이를 폴리머 중에 분산시켜 준마이크로파 대역의 전자파 노이즈 억제용 복합 시트를 제조하여, 자성 합금의 열처리가 전자파 전송 손실(전력 손실)에 미치는 영향을 조사하였다. 합금 분말을 어닐링하지 않은 것이 어닐링한 분말을 사용한 경우보다 수 GHz의 주파수 대역에서 전력 손실의 크기가 증가하였다. 이 때 복소 투자율의 허수항 크기도 어닐링을 하지 않았을 때 더 큰 값을 나타내었는바 편상화 가공 상태의 자성 분말을 사용한 복합 시트가 우수한 전자파 노이즈 흡수 특성을 가지며, 이에는 그의 높은 복소 투자율의 허수항 크기가 기여하고 있는 것으로 판단되었다. 반면 편상화 시킨 합금 박편을 어닐링 한 경우에는 와전류 효과의 증대에 따라 복소 투자율이 낮아지고 따라서 전력 손실도 저하되는 것으로 생각되었다.
This paper is concerned with the development of multi-action die or multiple sliding die for the forming process of serrated sheets. Serrated sheets is used as a toothed or serrated seal for securing together overlapping portions of steel or plastic strapping ligature and have been produced conventionally in several methods such as rolling and indentation. Recently, longitudinally oriented thermoplastic materials have been widely used in the strapping industry, while such materials are quite slippery. Provided projections on a seal biting into the strap should overcome the slipperiness and also the tooth configuration must be closely controlled to avoid too much transverse penetration of the strap which could result in the shredding of the strap when it is placed under tension. The seal includes a central portion with a plurality of teeth which bite into one strap portion and a pair of reversely bent legs with a plurality of teeth which bite into the other strap portion. Forming processes applicable for serrated sheets have reviewed in qualitative sense to find possibility in terms of applicability of one of existing processes to the serrated sheet forming process. Existing seal products have been analyzed with enlarged picture of strap contacting surface of the seal by microscope. Based on the analyses of the existing forming processes and seal products, a new forming process is proposed for serrated sheets. The proposed process requires a multislide die which enables inclined indentation or cut-in into the seal material as well as scratching processes sequentially in a single action press.
Tahouneh, Vahid;Naei, Mohammad Hasan;Mashhadi, Mahmoud Mosavi
Steel and Composite Structures
/
제34권2호
/
pp.261-277
/
2020
The main objective of this research paper is to consider vibration analysis of vacancy defected graphene sheet as a nonisotropic structure via molecular dynamic and continuum approaches. The influence of structural defects on the vibration of graphene sheets is considered by applying the mechanical properties of defected graphene sheets. Molecular dynamic simulations have been performed to estimate the mechanical properties of graphene as a nonisotropic structure with single- and double- vacancy defects using open source well-known software i.e., large-scale atomic/molecular massively parallel simulator (LAMMPS). The interactions between the carbon atoms are modelled using Adaptive Intermolecular Reactive Empirical Bond Order (AIREBO) potential. An isogeometric analysis (IGA) based upon non-uniform rational B-spline (NURBS) is employed for approximation of single-layered graphene sheets deflection field and the governing equations are derived using nonlocal elasticity theory. The dependence of small-scale effects, chirality and different defect types on vibrational characteristic of graphene sheets is investigated in this comprehensive research work. In addition, numerical results are validated and compared with those achieved using other analysis, where an excellent agreement is found. The interesting results indicate that increasing the number of missing atoms can lead to decrease the natural frequencies of graphene sheets. It is seen that the degree of the detrimental effects differ with defect type. The Young's and shear modulus of the graphene with SV defects are much smaller than graphene with DV defects. It is also observed that Single Vacancy (SV) clusters cause more reduction in the natural frequencies of SLGS than Double Vacancy (DV) clusters. The effectiveness and the accuracy of the present IGA approach have been demonstrated and it is shown that the IGA is efficient, robust and accurate in terms of nanoplate problems.
A cold roll-bonding process is applied to fabricate an AA6061/AA5052/AA6061 three-layer clad sheet. Two AA6061 and one AA5052 sheets of 2 mm thickness, 40 mm width, and 300 mm length are stacked, with the AA5052 sheet located in the center. After surface treatment such as degreasing and wire brushing, sample is reduced to a thickness of 1.5 mm by multi-pass cold rolling. The rolling is performed at ambient temperature without lubricant using a 2-high mill with a roll diameter of 400 mm at rolling speed of 6.0 m/sec. The roll bonded AA6061/AA5052/AA6061 complex sheet is then hardened by natural aging(T4) and artificial aging(T6) treatments. The microstructures of the as-roll bonded and age-hardened Al complex sheets are revealed by optical microscopy; the mechanical properties are investigated by tensile testing and hardness testing. After rolling, the roll-bonded AA6061/AA5052/AA6061 sheets show a typical deformation structure in which grains are elongated in the rolling direction. However, after T4 and T6 aging treatment, there is a recrystallization structure consisting of coarse equiaxed grains in both AA5052 and AA6061 sheets. The as roll-bonded specimen shows a sandwich structure in which an AA5052 sheet is inserted into two AA6061 sheets with higher hardness. However, after T4 and T6 aging treatment, there is a different sandwich structure in which the hardness of the upper and lower layers of the AA6061 sheets is higher than that of the center of the AA5052 sheet. The strength values of the T4 and T6 age-treated specimens are found to increase by 1.3 and 1.4 times, respectively, compared to that value of the starting material.
본 연구에서는 유리섬유시트로 휨보강된 RC 보의 파괴 양상을 분석하고, 부착파괴를 방지하기 위한 실험 연구를 수행하였다. 부착파괴를 방지하기 위한 방법으로 부착길이를 증가시키는 방법과 U형 보강 방법 및 에폭시 전단키 보강 상세에 대하여 검증하였다. 유리섬유시트의 부착길이는 콘크리트 계면과 보강재 사이의 부착강도를 가정하여 계산하였다. U형 보강 방법은 콘크리트 밑면에 부착된 유리섬유시트의 단부 혹은 중앙부를 U형으로 감싸서 보강하였다. 콘크리트 하부에 매립된 전단키는 유리섬유시트의 인장력에 대하여 충분한 부착력을 제공하도록 하였다. 단부 U 보강과 중앙부 U 보강은 부착파괴를 방지하기 위해 기존에 제안된 방법이며, 에폭시 전단키는 본 연구에서 제시된 새로운 방지 상세이다. 유리섬유시트의 부착파괴 방지 상세에 대한 효과를 검증하기 위하여 총 6개의 실험체를 제작 실험하였다. 본 실험 결과에 의하면 부착길이 및 단부 U 보강 상세를 적용하는 방법은 조기 부착파괴를 억제하지 못하는 것으로 나타났다. 반면 중앙부 U 보강 상세는 보강재를 따라 발생하는 박리균열의 진행을 억제시키기 때문에 부착파괴를 지연하는 효과가 있으며, 전단키의 경우는 부착파괴를 충분히 방지하며 유리섬유시트의 파단을 유도하는 것으로 나타났다.
In this paper, we consider performance assessment methods of mathematics and investigate some difficulties which teachers have been grading of performance assessment of mathematics. And also, using fuzzy theory, we define fuzzy grade sheets for performance assessment of mathematics and discuss some usefulness and simple examples of this new definition.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.