  • An Eectrolytic Corrosion(EC) test method was evaluated by the comparison with Copper Accelerated Acetic Salt Spray(CASS) and Neutral Salt Spray(SS) tests. Those methods were applied in order to evaluate corrosion resistance of Ni-Cr plated and Zn-plated Fe substrates. The correlations between results obtained by different test methods were investigated. Results showed that the electrochemical method such as the EC test method was superior to the conventional methods such as CASS and SS, in terms of the quantitative accuracy and the test-time span. Furthermore, the EC test method provided the useful means to estimate the initiation of corrosion of each layer by monitoring the rest potentials of the coated layers such as Ni, Cr, and Zn on Fe substrate. With regard to test time spans, the EC test provided the 78 times and 182 times faster results than the CASS test in cases of $Fe+5{\mu}m$ $Ni+0.5{\mu}m$ Cr and $Fe+20{\mu}m$ $Ni+0.5{\mu}m$ Cr respectively, while the EC test was 85 times faster results than the Salt Spray test in the case of $Fe+20g/m^2$ Zn. Therefore, the EC test can be the better method to evaluate the resistance to corrosion of coated layers than the conventional methods such as the SS test and the CASS.

0.5wt% 탄소강을 이용한 해안 야외부식시험과 염수분무시험, 가속부식시험의 가속계수에 대한 연구 (The Study on the Acceleration Factor of Coastal Outdoor Corrosion test, Salt Spray Test and Accelerated Corrosion Test using 0.5wt% carbon steel)

  • 조의열;권기봉;조대형;김종렬
    • Corrosion Science and Technology
    • /
    • 제12권5호
    • /
    • pp.209-214
    • /
    • 2013
  • In the industry, accelerated corrosion test is used for the life time prediction. When anti-corrosion test proceeds in real environments, it is difficult that we predict and evaluate the corrosion life time because of the long test time such as 10 years or more time. Accelerated corrosion test and Salt spray test are able to test corrosion life time of products in the laboratory instead of outdoor corrosion test. Experimental procedure is selected for the corrosion standard specimen, exposure of the specimens, measurements of the mass loss and evaluating the mass loss data. As a result, the acceleration factor of the accelerated corrosion test to the outdoor corrosion test is 414.8. Therefore we can predict the corrosion life time of carbon steel during a short time period.

아연 전기 도금 강의 환경친화적인 화성처리 기술 개발 (Development of chemical conversion coating technology by environment friendly method for Zn electroplated steel)

  • 김성종;김정일;장석기
    • 한국마린엔지니어링학회:학술대회논문집
    • /
    • 한국마린엔지니어링학회 2006년도 전기학술대회논문집
    • /
    • pp.271-272
    • /
    • 2006
  • Zinc confers high corrosion resistance by acting as a sacrificial anode, and a zinc coating improves the appearance of steel. Chromate conversion coating (CCC) films are still one of the most efficient surface treatments for steel. Although such films can self-repair via the dissolution of Cr(VI), dissolved Cr(VI) have adverse effects on humans, and the environment. Therefore, we examined the corrosion protection property and morphology of colloidal silica conversion films as an alternative to CCC films. The corrosion behavior was investigated in 3% NaCl solution using electrochemical techniques, including electrochemical impedance spectroscopy, open circuit potential, and the salt spray test(SST). Corrosion was implied by the appearance of red rust on the specimen surface. In corrosion resistance at 3% NaCl solution, red rust appeared at 15-20, 55-70, and 83-98 days on Zn-electroplated steel, colloidal silica conversion-coated specimens, and CCC-coated specimens, respectively. In the salt spray test, the colloidal silica film provided better corrosion protection than CCC films, i.e., red rust appeared at 96 hours on the Zn-electroplated steel sheet, at 432 hours with the CCC films, and at 888 hours with silica conversion coating.

  • PDF

마그네슘-알루미늄 합금의 화성처리 공정 개발과 그 내식성 평가 (Development of chemical conversion coating process for Mg-Al alloy and its anti-corrosion property)

  • 김성종
    • 한국마린엔지니어링학회:학술대회논문집
    • /
    • 한국마린엔지니어링학회 2006년도 전기학술대회논문집
    • /
    • pp.265-266
    • /
    • 2006
  • The chemical conversion coating formed on magnesium alloy investigated for low cost and harmless in environment by using the colloidal silica as the main component. The film formed in 298 K is thick, the film, which was thought combination of Si-O, was formed. The film formed in 313 K is thinner than that in 298 K. The quantity of film formed at high temperature such as 333 K and 353 K is smaller than dissolved quantity. At the anodic polarization experiment, corrosion resistance in sealing by hot water after chemical conversion treatment in basic solution condition get worse than that in comparison with basic solution condition. In salt spray test, the ratio of black rust on specimen that did not conducted chemical conversion treatment was five times or more compared with those of chemical conversion treated specimen. The film thickness of chemical conversion coating produced by alkali treatment process is thinner than in comparison with that of specimen produced in basic chemical conversion treatment solution condition. It is thought, however, that it showed good corrosion resistance during salt spray test because the area of microcracks is small.

  • PDF

Accelerated and Outdoor Exposure Tests of Aluminum Coated Steel Sheets

  • Kim, Jongmin;Lee, Jaemin;Lim, Sangkyu;Jung, Choonho
    • Corrosion Science and Technology
    • /
    • 제10권6호
    • /
    • pp.199-204
    • /
    • 2011
  • Hot dip metallic coated steels like as galvanized (GI), zinc-aluminium (GL) and aluminium coated steels are mostly used where corrosion resistance is needed. There are two kinds (type 1 and type 2) of aluminium coated steel being commercially used among them. Type 1 aluminium coated steel is coated with an Al-5~11 wt%Si alloy and Type 2 aluminium coated steel consists of commercially pure aluminium. Type 1 Al coated steel is generally used in automotive components and electrical appliances while type 2 aluminium coated steel is mainly used in construction applications such as building cladding panels, air conditioning and ventilation system. In this study, Type 1 aluminium coated steels have tested by accelerated conditions (salt spray or corrosive gas) and outdoor exposure condition in order to understand their corrosion behaviour. Due to the distinct corrosion mechanism of Al which exposes to the severe chloric condition, Salt Spray Test cannot predict the ordinary atmospheric corrosion of Al based coated materials. In addition, the test results and their corrosion feature of Al coated steel sheets will be discussed comparing with other metallic coated steel sheets of GI and GL.

The Effect of $Bi(OH)_3$ on Corrosion-Resistant Properties of Automotive Epoxy Primers

  • Yang, Wonseog;Min, Sungki;Hwang, Woon-suk
    • Corrosion Science and Technology
    • /
    • 제7권6호
    • /
    • pp.370-374
    • /
    • 2008
  • In this study, we evaluated anti-corrosion properties of both commercial unleaded and lead epoxy primer for automotive substrate before applying to actual painting lines by salt spray test, and cyclic corrosion test, potentiodynamic test and electrochemical impedance spectroscopy. The difference in the corrosion resistance between automotive epoxy primers contained $Bi(OH)_{3}$ and leaded one was investigated. And it was also discussed the effect of zinc phosphate pretreatment to the epoxy primers. The specimen coated epoxy primer contained $Bi(OH)_{3}$ showed 0.5 V higher corrosion potential than that of bare steel. The result of salt spray test did not indicate remarkable difference of corrosion resistance in all specimens above $10{\mu}m$ thickness up to 1200 hours. In the cyclic corrosion test, epoxy primers contained $Bi(OH)_{3}$ on phosphated substrate performed good corrosion properties until 800 hours. The epoxy primer contained $Bi(OH)_{3}$ performed the equivalent corrosion resistance as leaded coating on phosphated steel, but slightly inferior to that of leaded on bare steel. These results show that the pre-treatment of zinc phosphate is effective as well as pigment changing in performing anti-corrosion properties in automotive bodies.

Synthesis and Characterization of Al2O3/ZrO2, Al2O3/TiO2 and Al2O3/ZrO2/TiO2 Ceramic Composite Particles Prepared by Ultrasonic Spray Pyrolysis

  • Shim, In-Soo;Lee, Chang-Seop
    • Bulletin of the Korean Chemical Society
    • /
    • 제23권8호
    • /
    • pp.1127-1134
    • /
    • 2002
  • Fine ceramic particles of zirconia toughened alumina (ZTA), titania toughened alumina (TTA), and zirconia-titania toughened alumina (ZTTA) have been synthesized by ultrasonic spray pyrolysis (USP) at various temperatures from starting salt solutio ns of various compositions aiming for the development of catalytic material. These particles were characterized for properties such as shape, size and size distribution, diffraction pattern, and chemical and phase composition of elements by scanning electron microscopy (SEM), particle size analyzer (PSA), x-ray diffraction (XRD), and inductively coupled plasma-atomic emission spectroscopy (ICP-AES). Chemical compositions and sizes of ceramic composites have been controled by the stoichiometry of salt solutions and the flow rate of spraying solutions. The optimum experimental conditions for the various composite particle syntheses have been proposed.

회전형 미세입자 분무장치의 입자 분포 특성에 관한 기초 연구 (A Basic Study on Particle Distribution Characteristics of Rotary Mist Spraying Device)

  • 유영선;장재경;김형권;김영화;이태석;오성식;진병옥;오경민;강태경
    • 생물환경조절학회지
    • /
    • 제28권4호
    • /
    • pp.454-460
    • /
    • 2019
  • 이 연구에서는 염수를 증발냉각법을 이용하여 담수를 생산할 목적으로 회전형 미세입자 분무장치를 설계 제작하여 회전체의 표면조도, BLDC 시로코 팬의 회전수 그리고 염수 공급량의 변화에 따른 분무입자의 크기와 분포 특성을 실험적으로 분석하고자 하였다. 회전체의 표면조도 $Ra=0.27{\sim}7.65{\mu}m$인 경우 분무입자 크기는 $0.117{\sim}1.360{\mu}m$ 였고, 분무입자의 90% 가 $0.50{\mu}m$ 이하인 것으로 나타났다. $Ra=12.70{\sim}22.84{\mu}m$인 경우에는 분무입자 크기가 $2.51{\sim}184.79{\mu}m$의 범위에 분포하였고, 분무입자의 98%가 $13.59{\mu}m$ 이하인 것으로 나타났다. BLDC 시로코 팬의 회전수가 분무입자의 크기와 분포에 미치는 영향을 분석하기 위하여 표면조도 $Ra=0.27{\mu}m$로 고정한 상태에서 염수 공급량을 일정하게 유지하면서 팬의 회전수를 3,800~5,600rpm 로 변화시켜가며 실험을 수행한 결과 염수 공급량이 2.77~8.28mL/min 인 경우에는 분무입자의 크기가 $0.314{\sim}0.541{\mu}m$의 범위에 분포하였다. 또한 염수공급량이 9.74mL/min 이고 회전수가 5,600rpm인 경우에는 분무입자의 98.23% 이상이 $2.51{\sim}13.59{\mu}m$의 범위에 분포하였다.

복합재료의 기계적 거동에 염수환경이 미치는 영향에 관한 연구 (Effects of salt water environment on the mechanical behavior of composites)

  • 문진범;김수현;김천곤
    • Composites Research
    • /
    • 제23권1호
    • /
    • pp.44-50
    • /
    • 2010
  • 본 연구에서는 염수 침수 실험과 염수 분무 실험이라는 두 가지의 실험을 위그선의 구조재료로 사용될 3가지 다른 복합재료 시스템에 대해서 해수와의 접촉에 의한 물성저하를재현하기 위해 수행하였다. 140일간 염수환경하에서 노화시킨 후 탄소섬유 복합재료와유리섬유 복합재료의 인장, 압축, 전단 강성과 강도 및 층간 전단 강도를 측정하였다. 기본 물성파의 비교를 통해서 염수환경이 복합재료의 기계적 물성에 미치는 영향이 평가되었다. 실험을 통해 염수 분무환경과 침수 환경의 차이는 거의 영향을 미치지 않음을 확인하였다. 탄소섬유 복합재료의 경우 인장 물성에 적은 손실이 발생한 반면 유리섬유 복합재료에서는 인장물성의 저하률이 탄소섬유 복합재료에 비해서 큼을 확인하였다. 그리고 모재 지배적 물성들의 큰 물성저하가 관찰되었다. 이를 통해, 염수는 복합재료의 섬유와 모재 사이의 계면을 퇴화시키고, 또한 모재 자체 물성과 유리섬유의 물성을 저하시킬 수 있음을 확인하였다.