Suggestion for Determination of Minimum $S_D$ for Rut-Resistable Asphalt Concretes (고온 내변형 아스팔트혼합물 선정을 위한 변형강도 임계치 결정 방안)

  • Kim, Kwang-W.;Cho, Byung-J.;Lee, Soon-Jae;Doh, Young-S.
    • International Journal of Highway Engineering
    • /
    • v.9 no.4
    • /
    • pp.193-204
    • /
    • 2007
  • Deformation strength($S_D$) is a property which shows relatively good correlation with rut resistance of asphalt mixtures at high temperature. The Asphalt Pavement Analyzer (APA) is widely used as an equipment for estimating rut resistance of asphalt mixtures. The APA was used as corresponding property of the $S_D$ to estimate rutting resistance of asphalt mixtures. Many data were collected to establish the correlation of $S_D$ with APA. For $S_D$ test, the specimen is submerged into the $60^{\circ}C$ water for 30 minutes before applying a vertical load at the speed of 50mm/min to obtain peak load (P) and deformation (y) for $S_D$ calculation. For the same materials, APA test was performed. Relation of the $S_D$ with APA rut depth was evaluated using regression analysis. The $R^2$ value was 0.76, indicating this simple test procedure being a possible method for predicting deformation resistance of asphalt concretes at high temperature. It was also shown that, using the regression model, minimum value(s) of $S_D$ of surface course asphalt mixture or binder course for a particular road level can be determined. The limit values may be possible to use as cut-off value(s) of asphalt mixtures for the layer after further elaborated studies.

  • PDF

Evaluation of Fatigue Resistance of Selected Warm-mix Asphalt Concrete (준고온 아스팔트 콘크리트 피로저항성 평가)

  • Kim, Sungun;Lee, Sung-Jin;Kim, Kwang W.
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.62 no.3
    • /
    • pp.29-38
    • /
    • 2020
  • Since some warm-mix asphalt (WMA) concretes were known to show poorer rut resistance than the hot-mix asphalt (HMA) concretes, many studies were performed in efforts of improving its performance at high temperature. The reason is assumed to be due to the moisture remaining in aggregates dried at lower temperature. Therefore, not only the rut resistance, the crack resistance of WMA concrete was also in question. In this study, fatigue life of WMA concrete was evaluated in comparison with HMA using 3-point bending (3PB) beam test. The asphalt mixtures were prepared based on Korean mix-design guide using a 13 mm dense-graded aggregate and 6 binders; two HMA binders and four WMA binders. By 3PB fatigue test, normal (unmodified) and polymer-modified WMA concretes were evaluated in comparison with normal and polymer-modified HMA concretes at a low temperature (-5℃). The results showed that most of WMA concretes showed longer fatigue lives than HMA concretes, even though the same PG binders were used for HMA and WMA. This result indicates that the WMA concretes have stronger resistance against fatigue cracking than HMA at the low temperature, and this result is in contrast to the high-temperature performance test.

Evaluation of the Effect of PE Wax on Asphalt Binder Properties (PE Wax를 첨가한 아스팔트 바인더의 물리적 특성)

  • Kim, Boo-Il;Jeon, Sung-Il;Lee, Moon-Sup;Cho, Yoon-Ho
    • International Journal of Highway Engineering
    • /
    • v.8 no.4 s.30
    • /
    • pp.101-113
    • /
    • 2006
  • Generally, asphalt binder modifier increases the viscosity at high temperature as well as at mixing and paving temperature, so that higher temperature is required to produce the hot-mix asphalt. Otherwise, wax is able to improve workability by means of decreasing the viscosity of asphalt binder. In this study, the effect of PE wax used to modify the asphalt binder was evaluated in laboratory. The properties of PE wax modified binder were compared with those of SBS and Crumb Rubber Modified binders. The results showed that wax type I has an effect on strengthening rut resistance as well as improving workability. However, wax type I weaken crack resistance due to making binder harder at intermediate temperature. The results also showed that wax type II has an effect on improving workability and on strengthening crack resistance due to making binder softer.

  • PDF

Specimen Size Effect in Estimation of Rut Resistance based on Deformation Strength (공시체 크기가 변형강도를 이용한 소성변형 추정에 미치는 영향)

  • Lee, Moon-Sup;Choi, Sun-Ju;Doh, Young-Soo;Kim, Kwang-Woo
    • International Journal of Highway Engineering
    • /
    • v.6 no.2 s.20
    • /
    • pp.1-13
    • /
    • 2004
  • This study dealt with size effect of specimen in measuring deformation strength and estimating rut resistance of asphalt concretes under static loading using Kim test. Two aggregates, a normal asphalt (pen 60-80) and 6 polymer-modified asphalt (PMA) binders were used for preparation of 14 dense-graded mixtures. Mixtures were prepared based on optimum asphalt content by Marshall compactor (S= 10cm) and gyratory compactor (S= 15cm) for Kim test and for wheel tracking test. In statistical analysis by general linear model (GLM) procedure of SAS, the diameter of specimen was found not to be a significant factor that affect the Kim test result. Therefore, it was found that either loom-diameter or 15cm-diameter of specimen gave no significant difference in deformation strength ($K_D$) values in Kim test for any aggregate mixture. However, the thickness of specimen was found to be a significant factor in determining $K_D$. It is estimated that $K_D$ is a function of y, vertical deformation, and y has something to do with thickness of specimen. Therefore, it is suggested that the thickness of specimen should not be higher than 6.6cm, and the correction factor depending on the thickness value should be developed in the future study.

  • PDF

Evaluating Rutting Performance of High-Durability Asphalt Concrete Mixtures and Epoxy Used for Installation of High-Speed Weigh-In-Motion System (고속축중기 시스템의 도입을 위한 고기능 아스팔트 혼합물 및 에폭시의 내구성 평가)

  • Kwon, Hong Jun;Lee, Jong Sub;Kwon, Oh Sun;Kwon, Soon Min
    • International Journal of Highway Engineering
    • /
    • v.20 no.4
    • /
    • pp.7-13
    • /
    • 2018
  • PURPOSES : In order to apply high-speed weigh-in-motion (HS WIM) systems to asphalt pavement, three high-durability asphalt concrete mixtures installed with a WIM epoxy are evaluated. METHODS : In this study, dynamic stability, number of loading repetitions to reach the rut depth of 1 mm, and rut depth measurements of three asphalt mixtures at $60^{\circ}C$ were compared using an Asphalt Pavement Analyzer (APA). Laboratory-fabricated material and field core samples were prepared and tested according to KS F2374. RESULTS : Through the laboratory tests, it was found that all three modified asphalt mixtures (stone-mastic, porous, and semi-rigid) with WIM epoxy showed favorable permanent deformation results and passed the dynamic stability criterion of 3000 loading repetitions per 1 mm. In addition, it was confirmed that the modified SMA mixtures cored from the field construction yields satisfactory rutting testing results using the APA. Finally, the epoxy used for the HS WIM installation shows good adhesion with the three asphalt mixtures and permanent deformation resistance.

Performance Evaluation of Long-Life Asphalt Concrete Overlays Based on Field Survey Monitoring in National Highways (일반국도 현장조사 모니터링을 통한 장수명 아스팔트 덧씌우기 포장의 공용성 분석)

  • Baek, Jongeun;Lim, Jae Kyu;Kwon, Soo Ahn;Kwon, Byung Yoon
    • International Journal of Highway Engineering
    • /
    • v.17 no.3
    • /
    • pp.69-76
    • /
    • 2015
  • PURPOSES : Performance evaluation of four types of asphalt concrete overlays for deteriorated national highways. METHODS : Pavement distress surveys for crack rate and rut depth have been conducted annually using an automated pavement survey vehicle since 2007. Linear and non-linear performance prediction models of the asphalt concrete overlays were developed for 43 sections. The service life of the asphalt overlays was defined as the number of years after which a crack rate of 30% or rut depth of 15mm is observed. RESULTS : The service life of the asphalt overlays was estimated as 17.4 years on an average. In 90.7% of the sections, the service life of the overlays was 15 years or more which is 1.5 times the life of conventional asphalt concrete overlays used in national highways. The performance of the overlays was dependent on the type of asphalt mixture, traffic volume levels, and environmental conditions. CONCLUSIONS : The usage of stone mastic asphalt (SMA) and polymer-modified asphalt (PMA) for the overlays provided good resistance to cracking and rutting development. It is recommended that appropriate asphalt concrete overlays must be applied depending on the type of existing pavement distress.

Reliability Evaluation of Rubber Wheel and Steel Wheel for Wheel Tracking Test of Bituminous Concretes (역청 콘크리트 반복주행시험에서 고무바퀴와 강재바퀴의 신뢰성 비교 연구)

  • Hong, Joon-Pyo;Doh, Young-Soo;Kim, Kwang-Woo
    • International Journal of Highway Engineering
    • /
    • v.7 no.2 s.24
    • /
    • pp.97-107
    • /
    • 2005
  • Since the purpose of wheel tracking test is to find out relative difference of mixture's rut resistance, the wheel is an important part in the test for obtaining a consistent output. This study is performed to examine efficiency of different wheel material, rubber and steel in wheel tracking test. The rubber was inserted as a ring on the outer face of the steel wheel, and thickness of rubber ring was 15mm and 7.5mm and 0mm (steel wheel without rubber), making the total outer diameter 200mm. The objective of this study was to select reliable wheel material type in wheel tracking test at $60^{\circ}C$ based on variance in output (rut depth and dynamic stability) and correlation with SD (deformation strength). The result of regression analysis of rut depth with Sd showed that $R^2$ values of wheel rubber thickness of 15mm, 7.5mm and 0mm were 0.7, 0.8 and over 0.9, respectively. In a case of steel wheel (0mm), the highest $R^2$ value was 0.9569. Therefore, the wheel without rubber ring was the best in output consistency level and coefficient of determination $(R^2)$ with deformation strength. Therefore, the steel wheel without rubber ring is suggested as the best choice for wheel tracking test of asphalt concrete.

  • PDF

Analysis of Apparatus Variables for Deformation Strength Test of Asphalt Concrete Based on Correlation with Rutting and Prediction Model for Rutting (소성변형과의 상관성 및 추정모델을 통한 변형강도 시험장치 변수 분석)

  • Kim, Kwang-Woo;Lee, Moon-Sup;Kim, Sung-Tae;Lee, Soon-Jae
    • International Journal of Highway Engineering
    • /
    • v.4 no.4 s.14
    • /
    • pp.41-52
    • /
    • 2002
  • This study dealt with analysis of size effect of testing apparatus for Kim test which measures rut resistance characteristics of asphalt mixture under static loading. Two columns in different diameter with each column having different radios of round cut (Curvature) at the bottom were used for testing asphalt mixture. Deformation load ($P_{max}$) and deformation strength ($K_D$) were found to have relatively high correlation with rut depth and dynamic stability of asphalt concrete. Diameter of specimen was not a significant factor in this test. From the statistical correlation analysis with rutting properties, the radius of curvature and diameter of loading column were found to be important factor affecting the results of the test. Among the radios (r) of curvatures, r=0.5cm and 1.0cm showed much higher correlation than the column without curvature, and r=1.0cm being better between the two. The column with diameter of 4cm showed better correlation than diameter of 3cm. Therefore, the column of 4cm diameter with r=1.0cm was found to be the best among various apparatus sizes. Prediction models for rut depth and dynamic stability were developed for each aggregate mixture based on Kim test variables using SAS STEPWISE procedure. Therefore, if this test method is validated through further study, Kim test can be used for selecting asphalt mixture with the highest resistance against permanent deformation.

  • PDF