Influence of Fly Ash Quality on Rheological Properties of Cement Paste (플라이애시 품질이 시멘트 페이스트 레올로지 특성에 미치는 영향)

  • Baek, Byung-Hoon;Han, Dongyeop
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.2
    • /
    • pp.183-189
    • /
    • 2017
  • The aim of the research is to provide rheological properties of cement paste with various qualities of coal ash including fly ash, raw ash, and reject ash. Generally, fly ash is the well known supplementrary cementitious materials for concrete and is used to improve various properties. Although fly ash is obtained as a byproduct of fire powder plant, still reject ash is wasted from raw ash. In this research, thus, to provide a fundamental information on using not only fly ash but also raw ash or reject ash for cementitious materials, a rheological properties of cement paste was studied with three different coal ash. This research was conducted from particle conditions of three different coal ashes to rheological properties in cement paste phase. According to the expeirment, reject ash was consisted with large and coagulated particles although fly ash was consisted with a small and spherical shaped particles. based on the particle conditions of various coal ashes, rheological behaviors were tested, and it was shown as the coal ashes improved the fluidity of cement paste. Specifically, depending on the particle distributions of cement paste, it is considered that the viscosity of paste can be controlled.

Effect of addition of methanol on rheological properties of silk formic acid solution

  • Bae, Yu Jeong;Um, In Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.40 no.1
    • /
    • pp.28-32
    • /
    • 2020
  • Recently, many studies have been undertaken on the wet spinning and electrospinning of silk because wet-spun fibers and electrospun webs of silk can be applied in the biomedical and cosmetic fields owing to the good biocompatibility of silk. The rheological properties of silk solution are important because they strongly affect the spinning performance of the silk solution and the structures of resultant fibrous materials. Therefore, as a preliminary study on the effect of solvent composition on the rheological properties of silk fibroin (SF) solution and structure of the resultant film, in the reported work, methanol was added to the SF formic acid solution. A small amount of methanol (i.e. 2%) added to the SF formic acid solution significantly altered the rheological properties of the solution: its shear viscosity increased by 10 folds at low shear and decreased on increasing the shear rate, demonstrating shear thinning behavior of the SF solution. Dynamic tests for the SF solution indicated that the addition of 2% methanol altered the viscous state of the SF formic acid solution to elastic. However, the molecular conformation (i.e. β-sheet conformation) of the regenerated SF film cast from formic acid remained unchanged on the addition of 2% methanol.

Self Diffusions and Rheological Properties of Polyamide Polymer Materials in Various Solvents (용매 환경에서의 폴리아미드 고분자 재료의 자체확산과 유변학적인 특성)

  • Kim, Nam Jeong
    • Journal of the Korean Applied Science and Technology
    • /
    • v.36 no.4
    • /
    • pp.1050-1059
    • /
    • 2019
  • The self diffusion, hole volume, and flow thermodynamic parameters of polyamide fibers were calculated from rheological parameters and crystallite size in order to study of flow segments in amorphous region. The stress relaxation of polyamide filament fibers were carried out in air and various solvents at various temperatures using the tensile tester with the solvent chamber. The rheological parameters were obtained by applying the experimental stress relaxation curves to the theoretical equation of the Ree-Eyring and Maxwell non-Newtonian model. It was observed that the rheological parameters of these polyamide filament fibers are directly related to the relaxation spectra, self diffusion, viscosities, and activation energies of flow segments.

Study on Rheological Characterization of Polyacrylonitrile/Dimethyl Sulfoxide Solution with Change of Storage Times and Temperatures (시간 및 온도변화에 따른 폴리아크릴로니트릴/디메틸술폭시드 중합체 용액의 유변학적 특성 연구)

  • Yang, Jae-Yeon;Lee, Byoung-Min;Kuk, Yun-Su;Kim, Byoung-Suhk;Seo, Min-Kang
    • Composites Research
    • /
    • v.32 no.1
    • /
    • pp.71-77
    • /
    • 2019
  • In this study, the structural and rheological characterizations of polyacrylonitrile(PAN)/dimethyl sulfoxide(DMSO) solutions for PAN fiber were investigated according to the change of storage times and temperatures. As a result, PAN/DMSO solutions exhibited a very characteristic rheological behavior with variation of temperature. The solutions showed an increase of complex viscosity and a decrease of loss tangent($tan{\delta}$) as temperature was increased over the temperature range of 40 and $70^{\circ}C$ and it could be seen that the viscosity rapidly increased at low frequency. These results indicated that the gel polymer and denser gel structure were formed due to the intermolecular hydrogen bonding of water in the polymer solution depending on the storage time.

Computer Simulation for Die Filling Behavior of Semi-Solid Slurry of Mg Alloy

  • Lee, Dock-Young;Moon, Jung-Hwa;Seok, Hyun-Kwang;Kim, Sung-Bin;Kim, Ki-Bae
    • Journal of Korea Foundry Society
    • /
    • v.27 no.1
    • /
    • pp.31-35
    • /
    • 2007
  • In order to develop the semi-solid forming technology for magnesium alloy the rheological and thixotropic behavior of Mg alloy slurry with varying shear rates and cooling rates was investigated and simulated with considering the viscosity based on microstructures and processing variables. The viscosity of slurry of Mg alloy (AZ91D) in semi-solid region was exponentially increased with a solid fraction, and was decreased with increasing a shear rate. In order to analyze precisely the rheological behavior, the ANYCAST program modified with the Carreau model and the different heat transfer coefficient between the cast and mold was used to simulate the flow behavior of Mg semi-solid slurry during the injection into a casting mold in a high pressure diecasting machine. The simulated rheological behavior of Mg alloy slurry was matched well with the experimental results.

Synthesis and characterization of thiolated hexanoyl glycol chitosan as a mucoadhesive thermogelling polymer

  • Cho, Ik Sung;Oh, Hye Min;Cho, Myeong Ok;Jang, Bo Seul;Cho, Jung-Kyo;Park, Kyoung Hwan;Kang, Sun-Woong;Huh, Kang Moo
    • Biomaterials Research
    • /
    • v.22 no.4
    • /
    • pp.249-258
    • /
    • 2018
  • Background: Mucoadhesive polymers, which may increase the contact time between the polymer and the tissue, have been widely investigated for pharmaceutical formulations. In this study, we developed a new polysaccharide-based mucoadhesive polymer with thermogelling properties. Methods: Hexanoyl glycol chitosan (HGC), a new thermogelling polymer, was synthesized by the chemical modification of glycol chitosan using hexanoic anhydride. The HGC was further modified to include thiol groups to improve the mucoadhesive property of thermogelling HGC. The degree of thiolation of the thiolated HGCs (SH-HGCs) was controlled in the range of 5-10% by adjusting the feed molar ratio. The structure of the chemically modified polymers was characterized by $^1H$ NMR and ATR-FTIR. The sol-gel transition, mucoadhesiveness, and biocompatibility of the polymers were determined by a tube inverting method, rheological measurements, and in vitro cytotoxicity tests, respectively. Results: The aqueous solution (4 wt%) of HGC with approximately 33% substitution showed a sol-gel transition temperature of approximately $41^{\circ}C$. SH-HGCs demonstrated lower sol-gel transition temperatures ($34{\pm}1$ and $31{\pm}1^{\circ}C$) compared to that of HGC due to the introduction of thiol groups. Rheological studies of aqueous mixture solutions of SH-HGCs and mucin showed that SH-HGCs had stronger mucoadhesiveness than HGC due to the interaction between the thiol groups of SH-HGCs and mucin. Additionally, we confirmed that the thermogelling properties might improve the mucoadhesive force of polymers. Several in vitro cytotoxicity tests showed that SH-HGCs showed little toxicity at concentrations of 0.1-1.0 wt%, indicating good biocompatibility of the polymers. Conclusions: The resultant thiolated hexanoyl glycol chitosans may play a crucial role in mucoadhesive applications in biomedical areas.

Manufacture of Aluminum Alloy Rheology Materials Using Spiral Stirring Equipment (나선형 기계 교반 장치를 이용한 Al 합금 레오로지 소재의 제조)

  • Bae, J.W.;Han, S.H.;Kang, C.G.
    • Transactions of Materials Processing
    • /
    • v.17 no.1
    • /
    • pp.9-12
    • /
    • 2008
  • Recently, industries and academic institutes have been interested in the rheology forming technology for light weight materials. However, this rheocasting process has advantages such as the high initial investment cost and the lower mechanical properties than thixocasting. In this study, the continuous fabrication of rheological material with a spiral stirring equipment(mechanical stirring system) was newly devised to overcome the disadvantages of rheocasting process. The experimental parameters were stirring time($0{\sim}1200sec$), stirring velocity ($0{\sim}100rpm$) and stirring temperature($650{\sim}680^{\circ}C$). The optimal conditions for fabricated rheological material of A6061 alloy were stirring time at 300sec, stirring velocity at 60rpm and stirring temperature at $650^{\circ}C$. At these results, the equivalent diameter was $45{\sim}65{\mu}m$, mean roundness was $1.4{\sim}1.6$ and Vickers hardness was 60Hv.