• Title/Summary/Keyword: retained volume

Search Result 102, Processing Time 0.025 seconds

Development of Control Technology of Austempered Ductile Iron with High Strength and High Toughness for Gear Parts. (고강도 ADI의 기어부품 개발에 관한 연구)

  • Kim, Won-Yong;Kim, Kwang-Bae;Kang, In-Chan;An, Sang-Uk
    • Journal of Korea Foundry Society
    • /
    • v.13 no.2
    • /
    • pp.187-193
    • /
    • 1993
  • In this study, it was examined the relationship between the microstructure, fatigue properties, mechanical properties and retained austenite volume of Mo-Ni ADI corresponding to various austempering temperatures. When the austempering temperature is increased to $370^{\circ}C$, acicular bainite structure was found to be transformed to feathery bainite structure. But at the austempering temperature of $420^{\circ}C$, the dissolved bainite lath was showned. Up to the austempering temperature of $370^{\circ}C$, the volume of retained austenite was increased. However at the austempering temperature of $420^{\circ}C$ a large amount of retained austenite was decreased. In this study, the retained austenite volume was determined by XRD(X-ray diffraction). It was observed that the optimum fatigue properties can be obtained at the condition of austempering temperature $370^{\circ}C$. Under the such conditions, fatigue limit determined as the value of 290 MPa, tensile strength 877MPa elongation 6%, hardness 285(BHN), impact values(CVN) 9.2J and retained austenite volume 30.3%, respectively.

  • PDF

Effect of Retained and Reversed Austenite on the Damping Capacity in High Manganese Stainless Steel (고 Mn 스테인리스강의 감쇠능에 미치는 잔류 및 역변태 오스테나이트의 영향)

  • Kim, Y.H.;Lee, S.H.;Kim, S.G.;Kang, C.Y.
    • Korean Journal of Materials Research
    • /
    • v.25 no.1
    • /
    • pp.9-15
    • /
    • 2015
  • The effect of retained and reversed austenite on the damping capacity in high manganese stainless steel with two phases of martensite and austenite was studied. The two phase structure of martensite and retained austenite was obtained by deformation for various degrees of deformation, and a two phase structure of martensite and reverse austenite was obtained by reverse annealing treatment for various temperatures after 70 % cold rolling. With the increase in the degree of deformation, the retained austenite and damping capacity rapidly decreased, with an increase in the reverse annealing temperature, the reversed austenite and damping capacity rapidly increased. With the volume fraction of the retained and reverse austenite, the damping capacity increased rapidly. At same volume of retained and reversed austenite, the damping capacity of the reversed austenite was higher than the retained austenite. Thus, the damping capacity was affected greatly by the reversed austenite.

Effect of Cu on the mechanical Properties and damping capacity of austempered ductile cast iron (오스템퍼링 처리한 구상흑연주철의 기계적 성질 및 감쇠능에 미치는 Cu의 영향)

  • Lee, K.H.;Kang, C.Y.
    • Journal of Power System Engineering
    • /
    • v.12 no.3
    • /
    • pp.72-77
    • /
    • 2008
  • This study was investigated to know the effect of Cu addition on austempered ductile cast iron at various temperatures and times. Test results showed that the volume fraction of retained austenite and the carbon contents of retained austenite showed the greatest value at $400^{\circ}C$. Also, in case of specimens having more Cu contents, the volume fraction of retained austenite and the carbon contents of retained austenite showed the lower value. After austempering treatment, tensile strength and Impact value increased, but elongation decreased. With increasing austempering treatment temperature, tensile strength, elongation, and impact value decreased. In case of specimen having more Cu contents, tensile strength showed the higher value, but elongation showed the lower value. Damping capacity was decreased by austempering treatment and was not affected on austempering temperature and time. In case of specimen having more Cu contents, damping capacity showed the higher value.

  • PDF

Elevated Temperature Tensile Properties of Austempered Ductile Irom (Mo-Ni-Cu계 오스템퍼 구상흑연주철의 고온특성)

  • Yi, Young-Sang;Kang, In-Chan
    • Journal of Korea Foundry Society
    • /
    • v.11 no.4
    • /
    • pp.323-330
    • /
    • 1991
  • The relationships between the microstructure changes, retained austenite volume and elevated temperature tensile properties of Mo-Ni-Cu ADI corresponding to various austempering temperatures and time were investigated, After the $250^{\circ}C$ tensile test for the test piece austempered at $270^{\circ}C$ the accicular bainite structure was observed blunted under room temperature microscope. In the case of $370^{\circ}C$ austempering, the feathery bainite lath spacing was observed broadened. But after the $450^{\circ}C$ tensile test, bainitic features could not be observed. As the testing temperature increased, retained austenite volume tested at room temperature decreased. Especially, after the $450^{\circ}C$ tensile test retained austenite volume approached nearly to zero. A little higher tensile properties appeared at $250^{\circ}C$ testing than those at room temperature.

  • PDF

Effects of Mo on the Mechanical Properties of Ductile Cast Iron with Cu Austempered at 380℃ (Cu가 함유된 구상흑연주철의 380℃에서 오스템퍼링 시 Mo이 기계적 특성에 미치는 영향)

  • Kim, G.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.26 no.5
    • /
    • pp.219-224
    • /
    • 2013
  • In this study, we investigated effect of Mo addition on mechanical properties of Cu added ADI. Ductile cast iron specimens were austenitized at $900^{\circ}C$ for 150 min and then austempered at $380^{\circ}C$ for the various time periods from 15 min to 480 min. Mo added ADI had a higher volume fraction of retained austenite, and the volume fraction of retained austenite was determined by XRD analysis. As decreasing volume fraction of retained austenite, the elongation was also decreased as expected. But the UTS and yield strength were not decreased.

Effect of Cryogenic Treatment on the Phase Change and Mechanical Property in STD11 steel for Die and Tool (STD11강의 상변화 및 기계적 성질에 미치는 초심냉처리의 영향)

  • Kim, H.J.;Jang, W.Y.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.28 no.3
    • /
    • pp.139-145
    • /
    • 2015
  • Effects of austenitizing, cryogenic treatment and tempering conditions on the phase change, microstructure and Vickers hardness value have been studied in STD11 steel for tool and die. The volume fraction of retained austenite increased with a rise in austenitizing temperature, while the volume fraction of eutectoid $M_7C_3$ carbides decreased. The retained austenite could be reduced by cryogenic treatment i.e., maintaining at $LN_2$ temperature ($-196^{\circ}C$) for 12hrs but a little amount of retained austenite did not transform to martensite further although holding time increased to 24 hrs or more. The microstructure of the quenched and then cryogenictreated specimen showed nano-sized and needle-shaped carbides in matrix due to the decomposition of martensite by tempering, but that of the one without cryogenic treatment still revealed retained austenite by tempering even at $500^{\circ}C$.

A Study on the Retained Austenite and Tensile Properties of TRIP Type High Strength Steel Sheet with Cu (Cu 함유 TRIP형 고장력 강판의 잔류오스테나이트 및 인장특성에 관한 연구)

  • Kang, C.Y.;Kim, H.J.;Kim, H.G.;Sung, J.H.;Moon, W.J.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.12 no.3
    • /
    • pp.231-239
    • /
    • 1999
  • Volume fraction and morphology of retained austenite, tensile properties of TRIP type high strength steel sheet with Fe-C-Si-Mn-Cu chemical composition have been investigated. The retained austenite of granular, bar and film type existing in specimen was obtained after intercritical annealing and austempering. The granular type retained austenite increased with increase of intercritical annealing and austempering temperature. With increase of intercritical annealing temperature, retained austenite and carbon contents increased. Maximum contents of retained austenite was obtained by austempering at $400^{\circ}C$. The maximum tensile strength was obtained by austempering at $450^{\circ}C$ and maximum elongation was obtained at $400^{\circ}C$. T.S${\times}$E.L value increased with increase of retained austenite contents due to the elongation strongly controlled by contents of retained austenite, but tensile strength was affected with various factors such as bainitic structure etc.

  • PDF

Effect of Retained Austenite on Rolling Contact Fatigue of Nitrocarburized High-Carbon Chromium Bearing Steel (침질탄화처리한 고탄소 크롬 베어링강의 회전접촉 피로거동에 미치는 잔류오스테나이트의 영향)

  • Choi, Byung Young;Kim, Dong Keon;Kim, Chang Seok;Jin, Jai Koan
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.9 no.3
    • /
    • pp.169-176
    • /
    • 1996
  • Effect of retained austenite on rolling contact fatigue of nitrocarburized high-carbon chromium bearing steel has been investigated to develop surface-hardened bearing steel with imprved resistance to rolling contact fatigue. Fatigue tests were conducted in elesto-hydrodynamic lubricating conditions at a shaft speed of 5,000rpm, under max, hertzian stress of $492kg/mm^2$. Volume fraction of retained austenite in austenitic nitrocarburized STB2 steel was controlled by tempering at various temperature, $200{\sim}250^{\circ}C$. It was observed using TEM that decomposition of retained austenite during tempering at $250^{\circ}C$ was the highest in quantity, resulted in formation of lower bainite. Rolling contact fatigue life of the specimens with lower bainite, formed by decomposition of retained austenite, was improved in comparison with there of specimens with more amount of retained austenite.

  • PDF

Effect of Martensite on the Mechanical Properties of Austempered Ductile Cast Iron with Cu (Cu를 갖는 오스템퍼드 구상흑연주철의 기계적 성질에 미치는 마르텐사이트의 영향)

  • Kang, C.Y.;Lee, J.M.;Soon, D.W.;Kwoon, S.K.;Kim, I.S.;Sung, J.H.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.15 no.6
    • /
    • pp.255-259
    • /
    • 2002
  • Effect of martensite on the mechanical properties of austempered ductile cast iron was investigated after obtained the martensite by subzero treatment. Retained austenite was transformed to martensite by subzero treatment, and with decreasing subzero treatment temperature, volume fraction of martensite was increased. With increasing of the volume fraction of martensite, tensile strength was increased and elongation was decreased, ratio of increasing of strength and decreasing of elongation was higher in case of specimens with lot's of Cu contents. With increasing of the volume fraction of martensite, hardness slowly increased until only about 5% and it rapidly increased in a straight proportion when it is above 5%, while impact value was rapidly decreased until about 7% but it had a little change when it is above 7%.

Microstructure and Mechanical Properties of P Added 0.15C-1.5Mn-1.5Al TRIP Aided Cold Rolled Steel (P 첨가 0.15C-1.5Mn-1.5Al TRIP형 냉연강판의 미세조직과 기계적 성질)

  • Ahn M. W.;Cho K. M.;Suh D. W.;Oh C. S.;Kim S. J.
    • Transactions of Materials Processing
    • /
    • v.14 no.8 s.80
    • /
    • pp.712-717
    • /
    • 2005
  • Microstructure and mechanical properties are investigated for 0.15C-1.5Mn-1.5Al TRIP aided cold rolled steels containing $0.05wt\%P$ and $0.1wt\%P$. Despite of the complete replacement of Si by Al, the TRIP steel shows tensile strength of 700MPa and total elongation of $35\%$ by addition of $0.1wt\%$ P. Tensile strength of P added TRIP steels is not only affected by the solid solution hardening but also the volume fraction of retained austenite. As P content increases from $0.05wt\%$ to $0.1wt\%$, tensile strength and volume fraction of retained austenite are increased, but elongation is decreased. The lower stability of austenite in $0.1wt\%$ P added steel is responsible for the decrease of the elongation.