Influence of different fatigue loads and coating thicknesses on service performance of RC beam specimens with epoxy-coated reinforcement

  • Wang, Xiao-Hui;Gao, Yang;Gao, Run-Dong;Wang, Jing;Liu, Xi-La
    • Computers and Concrete
    • /
    • 제19권3호
    • /
    • pp.243-256
    • /
    • 2017
  • Epoxy-coated reinforcing bars are widely used to protect the corrosion of the reinforcing bars in the RC elements under their in-service environments and external loads. In most field surveys, it was reported that the corrosion resistance of the epoxy-coated reinforcing bars is typically better than the uncoated bars. However, from the experimental tests conducted in the labs, it was reported that, under the same loads, the RC elements with epoxy-coated reinforcing bars had wider cracks than the elements reinforced with the ordinary bars. Although this conclusion may be true considering the bond reduction of the reinforcing bar due to the epoxy coating, the maximum service loads used in the experimental research may be a main reason. To answer these two phenomena, service performance of 15 RC beam specimens with uncoated and epoxy-coated reinforcements under different fatigue loads was experimentally studied. Influences of different coating thicknesses of the reinforcing bars, the fatigue load range and load upper limit as well as fatigue load cycles on the mechanical performance of RC test specimens are discussed. It is concluded that, for the test specimens subjected to the comparatively lower load range and load upper limit, adverse effect on the service performance of test specimens with thicker epoxy-coated reinforcing bars is negligible. With the increments of the coating thickness and the in-service loading level, i.e., fatigue load range, load upper limit and fatigue cycles, the adverse factor resulting from the thicker coating becomes noticeable.

A new strength model for the high-performance fiber reinforced concrete

  • Ramadoss, P.;Nagamani, K.
    • Computers and Concrete
    • /
    • 제5권1호
    • /
    • pp.21-36
    • /
    • 2008
  • Steel fiber reinforced concrete is increasingly used day by day in various structural applications. An extensive experimentation was carried out with w/cm ratio ranging from 0.25 to 0.40, and fiber content ranging from zero to1.5 percent by volume with an aspect ratio of 80 and silica fume replacement at 5%, 10% and 15%. The influence of steel fiber content in terms of fiber reinforcing index on the compressive strength of high-performance fiber reinforced concrete (HPFRC) with strength ranging from 45 85 MPa is presented. Based on the test results, equations are proposed using statistical methods to predict 28-day strength of HPFRC effecting the fiber addition in terms of fiber reinforcing index. A strength model proposed by modifying the mix design procedure, can utilize the optimum water content and efficiency factor of pozzolan. To examine the validity of the proposed strength model, the experimental results were compared with the values predicted by the model and the absolute variation obtained was within 5 percent.

인장철근의 겹침이음에서 횡보강근의 효과에 관한 실험적 연구 (An Experimental Study on Effects Transverse Reinforcement in Lap-Spliced Tension Reinforcing Bars)

  • 이호준;최선아;연규원;박찬수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회 논문집(II)
    • /
    • pp.879-884
    • /
    • 2000
  • In this study, an experimental work is conducted to evaluate the bond performance between reinforcing bars and surrounding concrete in a lapped splice. The major variable of this test is a transverse reinforcement in lap-spliced tension reinforcing bars. The test results indicate that the bond strength per unit splice length increases with an increase in the transverse reinforcement factor $K_{\alpha}$. The specimens taken less than (c+$K_{tr}$)/$d_b$=3.0 tend to be very brittle at failure. But the specimens taken longer than (c+$K_{tr}$)/$d_b$=3.0 tend to be somewhat ductile at failure.

Belite 시멘트를 이용한 고성능 콘크리트의 철근 부착성능 실험연구 (An experimental study on Bond strength of Reinforcing steel to High-performance Concrete using Belite Cement)

  • 조필규;김상준;강지훈;김영식;최완철
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 가을 학술발표회 논문집
    • /
    • pp.408-415
    • /
    • 1997
  • Bond strength of reinforcing bar to high-performance concrete using Belite cement is explored using beam end test specimen. The key parameters for the bond test are slump of concrete, top bar effect, and strength of concrete in addition to concrete covers. Specimen failed in the typical brittle bond failure splitting the concrete cover as the wedging action. The test results show that for the group with portland cement I using superplasticizer additional slump does not decrease the bond strength of the top bar is less than bond strength of bottom bar, but the top bar factor satisfy the modification factor for top reinforcement. The result also show that bond strength is function of square root of concrete compressive strength and cover thickness. More detailed evaluation will be conducted from the test specimen with high strength concrete using the belite cement.

  • PDF

기초지반의 지지력보강공법에 관한 연구 (Studies on the Development of Bearing Capacity Reinforcement for the Foundation of Soil)

  • 유동환;최예환;유연택
    • 한국농공학회지
    • /
    • 제30권1호
    • /
    • pp.38-49
    • /
    • 1988
  • This paper presented as follows results of laboratory model tests with various shaped footings on soil bed reinforced with the strips on the base of behaviour of soil structure according to the loads and triaxial test results reinforced with geotextiles. Their parameters studied were the effects on the bearing capacity of a footing of the first layer of reinforcement, horizontal and vertical spacing of layers, number of layers, tensile strength of reinforcement and iclination load to the vertical 1.Depending on the strip arrangement, ultimate bearing capacity values could be more improved than urreinforced soil and the failure of soil was that the soil structure was transfered from the macrospace to microspase and its arrangement, from edge to edge to face to face. 2.The reinforcement was produced the reinforcing effects due to controlling the value of factor of one and permeable reinforcement was never a barrier of drainage condition. 3.Strength ratio was decreased as a linear shape according to increment of saturation degree of soil used even though at the lower strength ratio, the value of M-factor was rot influenced on the strength ratio but impermeable reinforcement decreased the strength of bearing capacity. 4.Ultimate bearing capacity under the plane-strain condition was appeared a little larger than triaxial or the other theoretical formulars and the circular footing more effective. 5.The maximum reinforcing effects were obtained at U I B=o.5, B / B=3 and N=3, when over that limit only acting as a anchor, and same strength of fabric appeared larger reinforcing effects compared to the thinner one. 6.As the LDR increased, more and more BCR occurred and there was appeared a block action below Z / B=O.5, but over the value, decrement of BCR was shown linear relation, and no effects above one. 7.The coefficient of the inclination was shown of minimum at the three layers of fabrics, but the value of H / B related to the ultimate load was decreased as increment of inclination degree, even though over the value of 4.5 there wasn't expected to the reinforcing effects As a consequence of the effects on load inclination, the degree of inclination of 15 per cent was decreased the bearing capacity of 70 per cent but irnproved the effects of 45 per cent through the insertion of geotextile.

  • PDF

CFRP 보강근 보강 콘크리트 슬래브 휨설계의 효율성에 관한 연구 (Investigation for the Efficiency in Flexural Design of CFRP Bar-Reinforced Concrete Slab)

  • 강수태;양은익;최명성
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제26권4호
    • /
    • pp.81-90
    • /
    • 2022
  • 이 연구에서는 일방향 콘크리트 슬래브를 대상으로 하여, 철근을 사용한 경우와 CFRP 보강근을 사용한 경우에 대해 보강근 사용량에 따른 휨강도와 처짐 및 균열폭을 비교하여 평가하였으며, CFRP 보강근 콘크리트 슬래브의 휨설계의 지배적인 성능과 효율적인 휨설계 방안에 대해 검토하였다. CFRP 보강근을 사용한 콘크리트 슬래브는 철근을 사용한 경우에 비해 동일한 보강근량에서 더 큰 설계휨강도를 얻을 수 있는 반면, 처짐 및 균열폭은 상대적으로 훨씬 크게 발생한다. CFRP 보강근을 사용한 콘크리트 슬래브에서는 최대균열폭이 설계의 지배적인 요인으로 작용하는 것으로 확인하였으며, 효율적 휨설계를 위해서는 허용균열폭을 0.7 mm로 완화하여 적용할 필요가 있으며, 작은 직경의 보강근 적용을 검토할 필요가 있음을 제시하였다.

건설기계·장비의 안전재해 네트워크 및 위험도 분석 (An Analysis on the Safety Accident Network and Risk Level of Construction Machine and Equipment)

  • 신원상;손창백
    • 대한건축학회논문집:구조계
    • /
    • 제34권5호
    • /
    • pp.35-42
    • /
    • 2018
  • In order to seek out methods to reduce safety accidents caused by construction machinery and equipment, this study collects data about safety accidents and draws main risk factors by construction from the data, through SNA. It aimed to suggest safety management points to be used in future construction fields, by analyzing risk index of such factors. The finding can be summarized: First, Backhoe Bucket is the risk factor for crash accidents of average workers in earth works; boring machines-maintenance is the risk factor for fall accidents of construction machinery operators in foundation works; bending machine-reinforcing rod processing is the risk factor for jamming accidents of reinforcing rod engineers in frame works; and mobile crane-hook is the risk factor for crash accidents of average workers in lifting works. Second, works can be arranged in turn, according to the risk index: earth, lifting, frame and foundation works. Risk factors can be also arranged according to the risk index: Backhoe in earth works, pile drivers in foundation works, bending machines in frame works and mobile cranes in lifting works. This study has some limits, in that it only analyzed main machinery/equipment, among various kinds of them, for earth, foundation, frame and temporary works (lifting works) and used data collected over three years. Therefore, it is necessary to conduct an analysis using big data, by collecting additional data about a lot of machinery/equipment in future construction fields.

GFRP Rebar 보강 콘크리트 보의 급속노화환경에서의 휨 거동에 관한 연구 (Flexural Behaviors of GFRP Rebars Reinforced Concrete Beam under Accelerated Aging Environments)

  • 박연호;최열
    • 콘크리트학회논문집
    • /
    • 제25권2호
    • /
    • pp.137-144
    • /
    • 2013
  • 철근콘크리트(reinforced concrete) 구조부재에서 철근의 부식으로 인한 문제점을 개선하고자 섬유보강 복합재료(FRP) 보강근(rebar)을 사용하는 것에 대한 연구가 꾸준히 진행되어져 오고 있다. 하지만 이러한 FRP 보강근을 사용한 콘크리트 부재의 환경에 대한 장기거동에 대한 연구가 아직도 미흡한 수준이다. 이 연구는 GFRP(glass fiber reinforced polymer) 보강근을 사용한 콘크리트 부재를 온도 약 $46^{\circ}C$와 습도가 80%인 인위적인 실험실에서 최대 300일까지 노출시킨 후의 장기 거동에 대한 실험적 연구를 제시하였다. 비교를 위하여 두가지 서로 다른 GFRP 보강근과 철근을 보강한 콘크리트 보 시험체를 제작하였다. 실험 결과, 장기 노출환경에서도 GFRP 보강근을 보강한 콘크리트 보 시험체의 파괴형태는 철근 보강 콘크리트 보시험체와 매우 유사한 파괴형태를 나타내었으며, 노출 시간에 따른 하중저항 감소값은 철근이 보강된 경우가 GFRP 보강근이 보강된 경우보다 하중저항 감소값이 크게 일어났다. 또한 GFRP 보강근 보강 콘크리트 보 시험체를 설계할 시에는 철근 보강보다 취성파괴에 대한 충분한 대비가 요구됨을 알 수 있었다. 그리고 압축파괴에 대한 변형도 계수(deformability factor)는 모든 경우에서 노출시간에 관계없이 큰 변화가 없음을 알 수 있었다.

지하 원유 저장기지 터널굴착공사 (Tunneling project of Oil Storage in Underground Base)

  • 김융태
    • 화약ㆍ발파
    • /
    • 제9권2호
    • /
    • pp.13-18
    • /
    • 1991
  • It was described Several Tuneling method for applying petrolum oil storage. The most Important factor of Tunneling is not only reinforcing works such as pre-grouting and after grouting but also rock bolting and shotcrete. The efficent works should be done by professional skillman, and also the classification of rock should be decided by professional engineers.

  • PDF

구속상세가 SD400 및 SD500 확대머리 이형철근의 겹침이음에 미치는 영향에 관한 실험적 연구 (Experimental Study on Effect of Confinement Details for Lap Splice of Headed Deformed Reinforcing Bars in Grade SD400 and SD500)

  • 김승훈
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제19권1호
    • /
    • pp.62-71
    • /
    • 2015
  • KCI 2012와 ACI318-11에서 확대머리 이형철근에 대한 정착길이 산정식을 제시하고 있지만 확대머리 이형철근을 이용한 겹침이음상세에 대한 규정은 없다. 또한, 정착길이 산정에 있어서 횡보강근 효과는 고려하지 않고 있다. 본연구에서는 400MPa과 500MPa 설계기준항복강도를 가지는 확대머리 이형철근에 대하여 겹침이음구간에 대한 구속상세를 평가하기 위하여 겹침이음실험을 실시하였다. 겹침이음 구간내 적용되는 구속상세는 스터럽과 Tie-down 철근이다. 실험결과, 스터럽만으로 보강된 실험체들에서 겹침이음강도 증가에 큰 영향이 없어 취성적인 파괴를 나타낸 반면에, 스터럽과 Tie-down 철근으로 보강된 실험체들은 공칭휨강도 이상의 실험휨강도와 휨거동을 나타내었다. 따라서 스터럽과 Tie-down 철근 상세는 400MPa과 500MPa의 확대머리 이형철근에 대한 겹침이음 성능향상에 기여할 수 있는 것으로 사료된다.