$Pb(Zn_{1/3}Nb_{2/3})O_3-Pb(Fe_{1/2}Nb_{1/2})O}3$ 계에서의 초전성질에 관한 연구 (Pyroelectric Properties of $Pb(Zn_{1/3}Nb_{2/3})O_3-Pb(Fe_{1/2}Nb_{1/2})O}3$ Ceramics)

  • 김정욱;최성철;이응상
    • 한국세라믹학회지
    • /
    • 제32권6호
    • /
    • pp.748-760
    • /
    • 1995
  • Pyroelectric properties, figure of merits, and the other properties of the Pb(Zn1/3Nb2/3)O3-Pb(Fe1/2Nb1/2)O3 system, as expected to have excellent pyroelectric properties in the operating temperature range of pyroelectric type infrared sensor, were investigated. In the Pb(Zn1/3Nb2/3)O3-Pb(Fe1/2Nb1/2)O3 system, suppression of the pyrochlore phase depended on sintering condition, as like sintering temperature, holding time, sintering atmosphere. The specimen, sintered by the same composition atmosphere powder at 105$0^{\circ}C$ for 1.5h, possessed the best physical property. It was found that the piezoelectric parameters were mainly depended on the amount of spontaneous polarization and then the 0.2PZN-0.8PFN showed the best pyro- and piezoelectric properties. In terms of the experimental method, two pyroelectric-testing methods, i.e. static and dynamic methods, had a same tendency. Also the result of pyroelectric testing by the static method indicated that the diffuse phase transitiion resulted in the temperature difference of phase transition between dielectric constant and pyroelectric coefficient.

  • PDF

Mn Oxide의 첨가에 따른 PSS-PT-PZ 세라믹의 초전특성 (Pyroelectric Properties of Modified PZT Ceramics with $MnO_2$ Addition)

  • 신상현;김영훈;박기운;강동헌;김영호;길상근
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.746-748
    • /
    • 2002
  • The effect of $MnO_2$ addition in $0.05Pb(Sn_{0.5}Sb_{0.5})O_3-0.8PbZrO_3-0.15PbTiO_3$(0.05PSS-0.8PZ-0.15PT) ceramics on crystal structure and electrical properties were studied. The sintering temperature and time were $1230^{\circ}C{\sim}1270^{\circ}C$ and 2hr, respectively. Then crystal structure, dielectric and pyroelectric properties were investigated. All the poled specimens showed the lower dielectric constant and $tan{\delta}$ than the unpoled specimens. Dielectric constant at 1kHz of the 0.05PSS-0.8PZ-0.15PT(MnO2 0.3wt%) system specimen sintered at $1250^{\circ}C$ for 2hr were 270 and showed the lowest $tan{\delta}$ of 0.2% after poling of $2kV_{DC}/mm$ at $150^{\circ}C$ for 30 minutes. Pyroelectric coefficient was maximum value of $50nC/cm^2K$ and Curie temperature was $224^{\circ}C$.

  • PDF

PLT 박막에서 조성에 따른 동적 초전특성의 주파수 의존성에 관한 연구 (A Study on the Effects of the La Concentration on the Frequency Dependence of Dynamic Pyroelectric Properties of PLT Thin Films)

  • 차대은;장동훈;강성준;윤영섭
    • 대한전자공학회논문지SD
    • /
    • 제39권10호
    • /
    • pp.35-42
    • /
    • 2002
  • Modulation frequency dependences of the pyroelectric properties of PLT (P $b_{1-x}$ L $a_{x}$ $Ti_{1-x}$ 4/ $O_3$) thin films with La concentrations of 5, 10 and 15㏖% have been investigated by using the dynamic method. The PLT thin film with 10㏖% of the La concentration (PLT(10) thin film) shows the most excellent pyroelectric properties among the films. For PLT(10) thin film, the pyroelectric coefficient shows the maximum value of 6.6$\times$10$^{-9}$ C/$\textrm{cm}^2$ㆍK without frequency dependence. The figure of merits for the voltage responsivity and specific detectivity are 1.03$\times$10$^{-11}$ Cㆍcm/J and 1.46$\times$10$^{-9}$ Cㆍcm/J, respectively. Voltage responsivity corresponding to the pyroelectric voltage is almost constant at low modulation frequency and decreases in proportional to frequency at high modulation frequency. Voltage responsivity is 5.15 V/W at 8Hz. Noise equivalent power (NEP) and specific detectivity ( $D^{*}$) of the PLT(10) thin film are 9.93$\times$10$^{-8}$ W/H $z^{1}$2/ and 1.81$\times$10$^{6}$ cmH $z^{1}$2/W at the frequency of 100Hz, respectively. The results indicate that PLT(10) thin film is very suitable for pyroelectric IR sensors.s.s.

Ba$_{0.67}$Sr${0.33)2$TiO$_3$ 박편 및 박막의 유전 및 초전 특성 (Dielectric and Pyroelectric Properties of $Ba_{0.67}$Sr${0.33)2$TiO$_3$ Thin Plates and Films)

  • 이문희;조성걸;이상기
    • 한국세라믹학회지
    • /
    • 제35권7호
    • /
    • pp.679-684
    • /
    • 1998
  • Dielectricand pyroelectric properties of {{{{ { { {Ba }_{0.67 }Sr }_{0.33 } }`TiO_{3 } ^{ } }} (BST) thin plates and films were investigated. For BST thin plates maximum dielectric constant and pyrolelectric coefficient were observed at around 24$^{\circ}C$ and pyroelectric characteristics were improved as applied bias field was increased. When the electric field of 4kV/cm was applied to the thin plates sintered at 140$0^{\circ}C$ the pyroelectric coefficients over 4$\times$10-7C/{{{{ { cm}^{2 }K }} were obtained in the range of 0-4$0^{\circ}C$ BST thin films deposited using rf magnetron sputtering showed [001] preferred orientation at substrate temperatures above 50$0^{\circ}C$ On the contrary to the thin plates the dielectric constants of the thin films gradually increased above 15$^{\circ}C$ and decreased as applied bias field in-creased. The pyroelectric coefficients of thin films were lower than 1/10 those of thin plates.

  • PDF

Pyroelectricity of Ni-doped PMNT Ferroelectric for Pyroelectric Detector

  • Kim, Yeon Jung
    • Applied Science and Convergence Technology
    • /
    • 제24권6호
    • /
    • pp.215-218
    • /
    • 2015
  • A pyroelctric properties of Ni(x)-doped PMNT systems were analyzed. Modified PMNT samples were prepared using the columbite structure method. Pyroelectric current, polarization, dielectric constant and dissipation factor of Ni-doped PMNT samples were measured as a function of temperature. By adding a small amount of NiO, pyroelectricity of PMNT is increased. Unlike the normal $ABO_3$ ferroelectric, Ni-doped PMNT showed properties for relaxor ferroelectric of causing the successive phase transition over a wide temperature. The optimum conditions for obtaining compositions with improvement ferroelectric properties are a nominal addition of 0.02 mole% Ni. Also, Ni-doped PMNT ferroelectric showed excellent pyroelectric figures of merit in the vicinity of room temperature. The pyroelectric coefficient ($0.00524C/m^2K$ at $25^{\circ}C$) and figures of merit ($F_v{\sim}0.039m^2/C$ and $F_d{\sim}0.664{\times}10^{-4}Pa^{-1/2}$) of composition PMNT with 0.02 mole% Ni are comparable to the earlier reports on lead-type pyroelectrics.

Dielectric Characteristics of PbSc1/2Nb1/2O3 Prepared by Using the One-step Solid State Reaction

  • Kim, Yeon Jung
    • Applied Science and Convergence Technology
    • /
    • 제25권4호
    • /
    • pp.77-80
    • /
    • 2016
  • The $PbSc_{1/2}Nb_{1/2}O_3$ ceramics at a relatively low temperature of $1300^{\circ}C$ was successful synthesized. Solid state reaction of two-step process is not necessary. The dielectric constant, dielectric loss and admittance of ceramic samples were determined. The pyroelectric characteristics are in good agreement with the dielectric properties. Ferroelectric properties of well-formed the $PbSc_{1/2}Nb_{1/2}O_3$ ceramics are in agreement with broad distribution of relaxation phenomenon. Relatively strong frequency dependent of dielectric constant is observed at about $110^{\circ}C$. The distinct thermal hysteresis was observed in the measurement of the dielectric constant and dielectric loss. The critical exponents of during cooling and heating measurements in the $PbSc_{1/2}Nb_{1/2}O_3$ ceramics were 1.14 and 1.59 at 1 kHz, respectively.

PZN-PT-PZ계 세라믹의 초전특성에 관한연구 (A Study on Pyroelectric Characteristics of PZN-PT-PZ Ceramics)

  • 박정철;전용우;소대화
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 춘계학술대회 논문집
    • /
    • pp.46-50
    • /
    • 1996
  • In this paper, xPb(Zn$\_$1/3/Nb$\_$2/3/)O$_3$-yPbTiO$_3$-zPbZrO$_3$-zPbZrO$_3$ (0.5wt%)MnO$_2$ ceramics were fabricated by the mixed oxide method sintered at 1250$^{\circ}C$ for 2[hrs] and then the dielectric and pyroelectric properties were investigated. In 0.10PZN-0.45PT-0.47PZ sample, dielectric constant was 829 and in the case of 01.5PZN-0.45PT-0.40PZ sample, pyroelectric current and pyroelectric coefficient were 0.95 x 10$\^$-7/ [A] and 7.6 x 10$\^$-1/ [C/$\textrm{cm}^2$$.$$^{\circ}C$]. Figure of merits of pyroelectric current and voltage and detectivity, in same sample, has shown good properties, that were 2.4 x 10$\^$-8/[C$.$cm/J], 5.5 x 10$\^$-11/[C$.$cm/J], 1.6 x 10$\^$-8/ [C$.$cm/J].

  • PDF

화재감지센서용 PZN-PSS-PZT계 초전재료의 전기적 특성에 미치는 Mn $O_2$ 첨가제의 영향 (Effect of Mn $O_2$ additive on the electrical characteristics of PZN-PSS-PZT Pyroelectric materials for the fire detactor)

  • 김용혁;백동현;최일수
    • 한국화재소방학회논문지
    • /
    • 제9권2호
    • /
    • pp.29-36
    • /
    • 1995
  • In this study, the effect of Mn $O_2$ additive on the electrical characteristics of PZN-PSS-PZT Pyroelectric materials for the fire detactor was studies. PZT ceramics used this experimental is 4 composite system $[$Pb(Z $n_{1}$3/ N $b_{2}$3/) $O_3$+Pb(S $n_{1}$3/ S $b_{2}$3/) $O_3$+PbTi $O_3$+PbZr $O_3$$]$The dielectric constants and dissipation factors decreases as to Mn $O_2$ concentration increases. At the Mn $O_2$ 0.5($\omega$t%), Pyroelectric coefficient shows 8(10$^{-8C}$$\textrm{cm}^2$$^{\circ}C$) which have the highst value among other additive contents. It is found that output voltage shows maximum peck at Mn $O_2$0.7($\omega$t%) is associated with the higher pyroelectric coefficient and Lowered dielectric constant.t.

  • PDF

Dielectric and Pyroelectric Properties of Y-modified PSS-PT-PZ Ceramics

  • Lee, Sung-Gap
    • Transactions on Electrical and Electronic Materials
    • /
    • 제6권3호
    • /
    • pp.119-123
    • /
    • 2005
  • $0.10Pb(Sb_{1/2}Sn_{1/2})O_3-0.25PbTiO_3-0.65PbZrO_3$ specimens doped with $ MnO_2\;(0.18\;mol\%)$ and $Y_2O_3\;(0\~0.4\;wt\%)$ were fabricated by the mixed-oxide method. All specimens showed the typical XRD patterns of a perovskite polycrystalline structure and the lattice constant decreased with increasing amount of $Y_2O_3$. The relative dielectric constant and the dielectric loss of the specimens doped with $0.2\;wt\%\;Y_2O_3$ were 704 and 0.0201, respectively. The remanent polarization, the coercive field and the pyroelectric coefficient of the specimen doped with $0.2\;wt\%\;Y_2O_3$ were $10.88\times10^{-2}Cm^{-2},\;11.12\times10^2kVm^{-1}$ and $5.03\times10^{-4}Cm^{-2}K^{-1}$ at $25^{\circ}C$, respectively. The figures of merit, $F_V$ for the voltage responsivity and $F_D$ for the specific detectivity, of the specimen doped with $0.2\;wt\%\;Y_2O_3$ were the good values of $3.04\times10^{-2}\;m^2C^{-1}\;and\;1.50\times10^{-5}\;Pa^{-1/2}$, respectively.

$Y_2O_3$ 첨가에 따른 PZT계 세라믹의 초전특성 (Pyroelectric Properties of PZT System Ceramics with Addition of $Y_2O_3$)

  • 강정민;조현무;이성갑;이상헌;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.329-331
    • /
    • 2003
  • In this paper, $0.10Pb(Sb_{1/2}Sn_{1/2})O_3-0.25PbTiO_3-0.65PbZrO_3$ ceramics were fabricated by the mixed-oxide method. The sintering temperature and time were $1230^{\circ}C$ and 2(hr), respectively. The structural, dielectric and pyroelectric properties with addition of $Y_2O_3$ were studied. The crystal structure of a specimen was rhombohedral. As a result of SEM, the average grain size were decreased with increasing the contents of $Y_2O_3$. Relative dielectric constant and dielectric loss of the specimen doped with 0.2wt% $Y_2O_3$ were 597 and 0.022, respectively. Remanent polarization and coercive field of the specimen doped with 0.4wt% $Y_2O_3$ were $8.5[{\mu}C/cm^2]$ and 10.2[kV/cm], respectively.

  • PDF