Won Jong-Pil;Sung Sang-Kyoung;Park Chan-Gi;Cho Yong-Jin;Choi Seok-Won;Park Hae-Geun
Proceedings of the Korea Concrete Institute Conference
/
2004.11a
/
pp.253-256
/
2004
Recently, construction works of scale are getting larger with economic growth. Shotcreting is one of major processes in tunnels construction. Accelerator is used in tunnel and underground structures to ensure early strength of shotcrete. Silicate based accelerator and aluminate based accelerator is getting widely in the field. But these accelerators have many problems due to decesase of long-term strength and low quality of the hardened shotcrete. in order to solve these problems, recently developed powder types cement mineral accelerator. In this study, we tested chloride permeability, freezing and thawing and accelerated carbonation of shotcrete. As a result of the test, wet-mixed shotcrete with powder types cement mineral accelerator exhibited durability improvement compared to the conventional shotcrete accelerator.
This investigation is carried out of inqurie into the effects of the accelerator on the setting time and haedness when it is used with plaster products. Plaster($\beta$), dental hard stone($\alpha$), and limproved dental hard stone($M{\alpha}$) are selected as the objects of the investigation, since they are most common materials for dental plaster products. Setting time is gauged by means of Vicket Needle and Gilmore Needle, and hardness is gauged by means of Brinell and Vicket Hardness machines. Samples of each material are made in the standerd water powder ratio and with the accelerator repectively, Every material is tested five times each. The results of the tests are as fallow : 1) In each case the setting time is shortened when the accelerator is used. 2) Of the three materials the hardness of the plaster was lowest A($\beta$) < B($\alpha$) < C($M{\alpha}$)} 3) In each case the hardness of the samples made in the standard water powder ratio were higher than that of the sample made with the accelerator. A1 > A2 ; B1>B2 ; C1>C2 4) Final Conclusion : Higher quality cast is expected when it is made in the standard water powder ratio.
Proceedings of the Korea Concrete Institute Conference
/
2003.05a
/
pp.609-617
/
2003
The use of Shotcrete(Sprayed concrete) for the support of underground excavations was pioneered by the Civil engineering industry. Permanent shotcrete tunnel linings such as Single-shell, NMT(Norwegian Method of Tunnelling) have been constructed in many countries for reducing construction time and lowering construction costs instead of conventional in-situ concrete linings. Among essential technologies for successful application of Permanent Shotcrete Linings, high performance shotcrete having high strength, high durability, better pumpability has to be developed in advance. This paper presents the ideas and the first field test results of wet-mixed Steel Fiber Reinforced Shotcrete(SFRS) with powder types cement mineral accelerator. From the results, wet-mix SFRS with powdered accelerator exhibited good early strength improvement and less rebound ratio compared to the ordinary accelerator.
Journal of the Korea institute for structural maintenance and inspection
/
v.24
no.2
/
pp.86-93
/
2020
Shotcrete concrete is generally used in the form of ready-mixed concrete products using type I ordinary portland cement(hereinafter referred to as OPC) and about 5% of accelerator mixed separately in the field. In this study, we tested the effect of addition of slag powder(SP) and limestone powder(LSP) on a penetration resistance, compressive strength of binder for shotcrete using calcium aluminate type accerlerator. And we analysed hydrates and pore structure effects on mortar performance. In the future, it is expected to be useful for manufacturing optimized composite cement as a binder for shotcrete.
Lee Chol Woong;Mun Kyoung Ju;Xu Xiang Yu;Park Won Chun;Choi Nak Woon;Soh Yang Seob
Proceedings of the Korea Concrete Institute Conference
/
2005.11a
/
pp.555-558
/
2005
The purpose of this study is to evaluate the chemical resistance of polymer powder-modified mortars with special accelerator component. Polymer powder-modified mortars with the accelerator are prepared with various polymer-binder ratios, and tested for flexural and compressive strengths and mass change. Chemicals resistance was tested by dealing with $10\%$ HCl and $5\%\;H_2SO_4$ aqueous solution. As a result, the weight reduction ratio of the mortars decreased with increasing polymer-binder ratio. However, in the viewpoint of strength reduction by chemical attacks, the maximum chemical resistance of the mortars was shown at a polymer-binder ratio of $5\%$.
Jo, Young-Chul;Choi, Nak-Woon;Lee, Chol-Woong;Yang, Suk-Woo;So, Yang-Seob
Proceedings of the Korea Concrete Institute Conference
/
2004.11a
/
pp.731-734
/
2004
Admixture compounds for reducing setting time and accelerating early strength development of redispersible polymer powder-modified mortars were made by mixing various inorganic accelerating inorganic materials. Redispersible polymer powder-modified mortars are prepared with various accelerator contents, and it was tested for setting time, flexural and compressive strengths. As a result, the accelerators contribute to strength development of the mortars in the early curing age of 12h or less. In the viewpoint of early strength development of redispersible polymer powder-modified mortars, an accelerator content of $20\%$ is recommended.
Proceedings of the Korean Institute of Building Construction Conference
/
2012.05a
/
pp.259-262
/
2012
Recently, as the national policy of green growth is promoted, construction field also makes an effort to reduce CO2 gas released when producing cement continuously. In other words, as the method solving environmental pollution and resources exhaustion, lots of mineral material compounds such as blast furnace slag powder which is industrial by-product, fly ash, red mud, etc. are examined to bo used as the substitute good of cement Therefore this study is to investigate the hardening characteristics of alumino-silicate inorganic binder using red-mud used as a accelerator of industrial by-product such as fly ash and blast furnace slag powder according to curing temperature. As a result, it is effective to use red-mud as the accelerator of inorganic binder with other additory accelerators.
From the early 1980's, the New Austrian Tunnelling Method (NATM) has been developed as a one of the standard tunneling method in Korea. Owing to the results of many researches, the practical problems of shotcrete has been improved for a last decade. However, the excess amount of rebound still remains one of the critical problems in shotcrete technology. In order to improve for this rebound problem, recently developed cement mineral accelerator has been successfully applied to several NATM tunnels in Korea. An experimental investigation was carried out in order to verify the rebound characteristics of wet-mix Steel Fiber Reinforced Shotcrete (SFRS) with powder types cement mineral accelerator. Mortar setting test, SEM analysis, bonding test under spring water condition and rebound test were conducted. From the result, wet-mix SFRS with cement mineral acelerator exhibited excellent bonding characteristics even spring water condition and less rebound ratio compared to the conventional liquid accelerator.
Magazine of the Korean Society of Agricultural Engineers
/
v.42
no.5
/
pp.125-132
/
2000
This study was performed to evaluate the physical properties of reinforced soil mixture powder. Soil sample was prepared by passing into the standard sieve of No. 200 and reinforcement materials were calcium carbonate, quicklime and portland cement. Fineness, setting time, and compressive strength test for reinforced soil mixture powder were performed and analyzed to investigate their physical properties. The main results were summarized as follow. The compressive strength of soil mixture powder itself and most reinforced was reinforced according to increasing in the mixture rate of reinforcement and the rate of increase was remarkably higher in the cement reinforced soil moisture powder. It was appeared that the early compressive strength is considering higher in the cement reinforced soil moisture powder with 2% of moisture rate of accelerator.
Journal of the Korea Institute of Building Construction
/
v.15
no.3
/
pp.265-271
/
2015
This study is intended to produce a PC (Precast Concrete) member without a steam curing process in developing the high early strength concrete satisfying the condition of 10MPa in compressive strength at the age of 6 hours, and is intended to ensure economic feasibility by increasing the turnover rate of concrete form. Hence, high early strength cement with high $C_3S$ content and the hardening accelerator of powder type accelerating the hydration of $C_3S$ was used. And the properties of concrete were evaluated according to the hardening accelerator mixing ratio (0, 1.2, 1.6, 2.0). No big difference was found from the tests of both slump and air content. When 1.6 % or higher amounts of the hardening accelerator were mixed, the compressive strength of 10MPa was achieved at the age of 6 hours. From the test results of autogenous (drying) shrinkage and plastic shrinkage, it can be seen that there was a difference according to hydration reaction rate due to the addition of the hardening accelerator. However, it was shown that no problem arose with crack and durability. And it was shown that resistance to freezing-thawing, carbonation, and penetration were excellent.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.