• 제목/요약/키워드: potentiodynamic

검색결과 372건 처리시간 0.026초

전기화학적 분석을 통해 산출된 코팅 결함율이 트라이볼로지적 특성에 미치는 영향 평가 (Influence of Coating Defect Ratio on Tribological Behavior Determined by Electrochemical Techniques)

  • 이영제;김우중;안승호;김호건;김정구;조정우
    • Tribology and Lubricants
    • /
    • 제20권6호
    • /
    • pp.306-313
    • /
    • 2004
  • Many of the current development in surface modification engineering are focused on multilayered coatings, which have the potential to improve the tribological properties. Four different multilayered coatings were deposited on AISI D2 steel in this study. The prepared samples are designed as $WC-Ti_{0.6}Al_{0.4}N,\;WC-Ti_{0.53}Al_{0.47}N,\;WC-Ti_{0.5}Al_{0.5}N\;and\;WC-Ti_{0.43}Al_{0.57}N$. The multilayered coatings were investigated with respect to coating surface and cross-sectional morphology, roughness, adhesion, hardness, porosity and tribological behaviors. Especially, wear tests of four multilayered coatings were performed by using a ball-on-disc configuration with a linear sliding speed of 0.017 m/sec and a normal load of 5.38 N load. The tests were carried out at room temperature in air by employing AISI 52100 steel ball $(H_R\;=\;66) $ having a diameter of 10 mm. The surface morphology, and topography of the wear scars of samples and balls have been determined by using scanning electron spectroscopy (SEM). Also, wear mechanism was determined by using SEM coupled with energy-dispersive spectroscopy (EDS). Results have showed an improved wear resistance of the $WC-Ti_{1-x}Al_xN$coatings with increasing of Al (aluminum) concentration.

PEO 처리조건에 따른 마그네슘 합금 AZ91의 표면특성변화에 관한 연구 (Effects of PEO Conditions on Surface Properties of AZ91 Mg Alloy)

  • 박경진;정명원;이재호
    • 마이크로전자및패키징학회지
    • /
    • 제17권3호
    • /
    • pp.71-77
    • /
    • 2010
  • 마그네슘 합금은 낮은 밀도를 가지는 장점을 이용하여 자동차, 항공, 이동전화, 컴퓨터 등에 많이 쓰이고 있으나 기계적 강도가 낮고 내부식성이 좋지 않아 사용이 제한되었다. 마그네슘 합금 표면에 내식성 산화층을 형성하기 위하여 환경 친화적인 전해 플라즈마 산화법(PEO)을 연구에 사용하였다, PEO법은 수용약 중에서 플라즈마를 발생시켜 전기화학적 산화막을 형성시키는 방법이다. 인가전압과 전휴가 산화피마에 미치는 영향에 대하여 고찰하였다, 또한, 직류와 펄스전류를 사용하여 결과를 분석하였다. 펄스전류를 사용하고 정전류법을 사용한 경우에 치밀한 산화막을 얻을 수 있었다, 부식특성 분석을 위하여 양극산화분극방법을 이용하였다. 표면의 강도는 처리전의 AZ9ID에 비하여 5배 이상 증가하였다.

Effectiveness of Calcium Nitrite in Retarding Corrosion of Steel in Concrete

  • Abosrra, L.;Youseffi, M.;Ashour, A.F.
    • International Journal of Concrete Structures and Materials
    • /
    • 제5권1호
    • /
    • pp.65-73
    • /
    • 2011
  • Corrosion of steel bars embedded in concrete admixed with 0%, 2% and 4% calcium nitrite (CN), having compressive strengths of 20 and 46 MPa was investigated. Reinforced concrete specimens were immersed in 3% NaCl solutions for 1, 7 and 15 days where 0.4A external current was applied to accelerate the chemical reactions. Corrosion rate was measured by retrieving electrochemical data via potentiodynamic polarization technique. Pull-out tests of reinforced concrete specimens were then conducted to assess the corroded steel-concrete bond characteristics. Experimental results showed that corrosion rate of steel bars and steel-concrete bond strength were dependent on concrete strength, amount of CN added and accelerated corrosion period. As concrete strength increased from 20 to 46 MPa, corrosion rate of embedded steel decreased. The addition of 2% CN to concrete of 20 MPa was not effective in retarding corrosion of steel at long time of exposure. However, the combination of higher strength concrete and 2% or 4% CN appear to be a desirable approach to reduce the effect of chloride-induced corrosion of steel reinforcement. After 1 day of corrosion acceleration, specimens without CN showed higher bond strength in both concrete mixes than those with CN. After 7 and 15 days of exposure, the higher concentration of CN, the higher bond strength in both concrete mixes achieved, except for the concrete specimen of 20 MPa compressive strength with 2% CN that recorded the highest deterioration in bond strength at 15 days of exposure.

Effect of PO43-, CO32- and F- anions on the electrochemical properties of the air-formed oxide covered AZ31 Mg alloy

  • Fazal, Basit Raza;Moon, Sungmo
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.150.2-150.2
    • /
    • 2017
  • This research was conducted to investigate in detail the effect of $PO_4{^{3-}}$, $CO_3{^{2-}}$ and $F^-$ anions on the electrochemical properties of the thin air-formed oxide film-covered AZ31 Mg alloy. In this work, native air-formed oxide films on AZ31 Mg alloy samples were prepared by knife-abrading method and the changes in the electrochemical properties of the air-formed oxide film were investigated in electrolytes containing 0.01 M, 0.05 M and 0.1 M of $PO_4{^{3-}}$, $CO_3{^{2-}}$ and $F^-$ anions. It was observed that the trend of open circuit potential (OCP) transients changed only in the solution containing $PO_4{^{3-}}$ ions. The Nyquist plots obtained from electrochemical impedance spectroscopy (EIS) showed that the resistance of the new surface films formed in fluoride ion containing bath increased with the increase in concentration of fluoride ions but the resistance of surface films formed in carbonate ion containing bath decreased with the increase in concentration of carbonate ions. The potentiodynamic polarization curves illustrated that under anodic polarization, there was growth of porous passive layer only in fluoride ion containing solution while the surface layer formed in phosphate and carbonate ion containing solutions lost its passivity at high anodic potential of $2.5V_{Ag/AgCl}$.

  • PDF

Electrochemical Behavior of Plasma Electrolytic Oxidized Films Formed in Solution Containing Mn, Mg and Si Ions

  • Lim, Sang-Gyu;Choe, Han Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.80-80
    • /
    • 2017
  • Titanium and its alloys that have a good biocompatibility, corrosion resistance, and mechanical properties such as hardness and wear resistance are widely used in dental and orthopedic implant applications. However, they do not form a chemical bond with bone tissue. Plasma electrolytic oxidation (PEO) that combines the high voltage spark and electro-chemical oxidation is a novel method to form ceramic coatings on light metals such as tita-nium and its alloys. This is an excellent re-producibility and economical, because the size and shape control of the nano-structure is relatively easy. Silicon (Si), manganese (Mn), and magne-sium (Mg) have a useful to bone. Particularly, Si has been found to be essential for normal bone, cartilage growth, and development. Mn influences regulation of bone remodeling be-cause its low content in body is connected with the rise of the concentration of calcium, phosphates and phosphatase out of cells. Pre-studies have shown that Mg plays very im-portant roles in essential for normal growth and metabolism of skeletal tissue in verte-brates and can be detected as minor constitu-ents in teeth and bone. In this study, Electrochemical behavior of plasma electrolytic oxidized films formed in solution containing Mn, Mg and Si ions were researched using various experimental in-struments. A series of Si-Mn-Mg coatings are produced on Ti dental implant using PEO, with the substitution degree, respectively, at 5 and 10%. The potentiodynamic polarization and AC impedance tests for corrosion behav-iors were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat with a scan rate of 1.67mV/s and potential range from -1500mV to + 2000mV. Also, AC impedance was performed at frequencies anging from 10MHz to 100kHz for corrosion resistance.

  • PDF

Corrosion Charateristics of PEO-treated Ti-6Al-4V Alloy in Solution Containing Si and Mg Ions

  • Park, Seon-Yeong;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.153-153
    • /
    • 2017
  • The application of the coating supports the mechanical characteristics of the implant, and various materials and coatings are currently being used in the implant in a way to accelerate adhesion. Especially, plasma electrolytic oxidation (PEO) coating has been proposed continually with good surface treatment of titanium alloys. Also, the PEO process can incorporate Ca and P ions on the titanium surface through variables varied factor. PEO process for bioactive surface has carried out in electrolytes containing Ca and P ions. Natural bone is composed of mineral elements such as Mg, Si, Zn, Sr, and Mn, etc. Especially, Mg and Si of these elements play role in bone formation and growth after clinical implantation of bio-implants. In this study, corrosion charateristics of PEO-treated Ti-6Al-4V alloy in solution containing Si and Mg ions has been investigated using several experimental techniques. The PEO-treated surfaces were identified by X-ray diffraction, using a diffractometer (XRD, Philips X' pert PRO, Netherlands) with Cu $K{\alpha}$ radiation. The morphology was observed by field-emission scanning electron microscopy (FE-SEM, Hitachi 4800, Japan) and energy-dispersive X-ray spectroscopy (EDX, Oxford ISIS 310, England). The potentiodynamic polarization and AC impedance tests for electrochemical degradations were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat with a scan rate of 1.67mV/s and potential range from -1500mV to + 2000mV.

  • PDF

Changes in the electrochemical properties of air-formed oxide film-covered AZ31 Mg alloy in aqueous solutions containing various anions

  • Fazal, Basit Raza;Moon, Sungmo
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.96.2-96.2
    • /
    • 2017
  • This research was conducted to investigate the electrochemical properties of the thin air-formed oxide film-covered AZ31 Mg alloy. In this work, native air-formed oxide films on AZ31 Mg alloy samples were prepared by knife-abrading method and the changes in the electrochemical properties of the air-formed oxide film were investigated in seven different electrolytes containing the following anions $Cl^-$, $F^-$, $SO{_4}^{2-}$, $NO_3{^-}$, $CH_3COO^-$, $CO{_3}^{2-}$ and $PO{_4}^{3-}$. It was observed from open circuit potential (OCP) transients that the potential initially decreased before gradually increasing again in the solutions containing only $CO{_3}^{2-}$ or $PO{_4}^{3-}$ ions, indicating the dissolution or transformation of the native air-formed oxide film into new more protective surface films. The Nyquist plots obtained from electrochemical impedance spectroscopy (EIS) showed that there was growth of new surface films with immersion time on the air-formed oxide film-covered specimens in all the electrolytes; the least resistive surface films were formed in fluoride and sulphate baths whereas the most protective film was formed in phosphate bath. The potentiodynamic polarization curves illustrated that passive behaviour of AZ31 Mg alloy under anodic polarization appears only in $CO{_3}^{2-}$ or $PO{_4}^{3-}$ ions containing solutions and at more than $-0.4V_{Ag/AgCl}$ in $F^-$ ion containing solution.

  • PDF

Electrochemical characteristics of Ca, P, Sr, and Si Ions from PEO-treated Ti-6Al-4V Alloy Surface

  • Yu, Ji-Min;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.154-154
    • /
    • 2017
  • Ti-6Al-4V alloys are widely used as metal-lic biomaterials in dentistry and orthopedics due to its excellent biocompatibility and me-chanical properties. However, because of low biological activity, it is difficult to form bone growth directly on the surface of titanium implants. For this reason, surface treatment of plasma electrolytic oxidation(PEO) was used for dental implants. To enhance bioac-tivity on the surface, strontium(Sr) and sili-con(Si) ions can be added to PEO treated sur-face in the electrolyte containing these ions. The presence of Sr in the coating enhances osteoblast activity and differentiation, where-as it inhibits osteoclast production and prolif-eration. And Si has been found to be essen-tial for normal bone, cartilage growth, and development. In this study, electrochemical characteristics of Ca, P, Sr, and Si ions from PEO-treated Ti-6Al-4V alloy surface was re-searched using various experimental instruments. DC power is used and Ti-6Al-4V al-loy was subjected to a voltage of 280 V for 3 minutes in the electrolyte containing 5, 10, 20M% Sr ion and 5M% Si ion. The morphol-ogies of PEO-treated Ti-6Al-4V alloy by electrochemical anodization were examined by field-emission scanning electron micro-scopes (FE-SEM), energy dispersive x-ray spectroscopy (EDS), x-ray diffraction (XRD) and corrosion analysis using AC impedance and potentiodynamic polarization test in 0.9% NaCl solution at similar body tempera-ture using a potentiostat with a scan rate of 1.67mV/s and potential range from -1500mV to + 2000mV.

  • PDF

용융탄산염 연료전지의 Anode가스 분위기에서 AISI-type 316L stainless steel의 전기화학적 부식 특성 (Electrochemical Corrosion Characteristics of AISI-type 316 L Stainless Steel in Anode-Gas Environment of MCFC)

  • 이갑수;임태훈;홍성안;김화용
    • 전기화학회지
    • /
    • 제5권2호
    • /
    • pp.62-67
    • /
    • 2002
  • 용융탄산염 연료전지의 성능 저하와 수명 감소의 원인이 되는 부식 현상을 규명하고자 분리판 재료로 가장 널리 사용되고 있는 AISI-type 316L stainless steel을 대상으로 62Li/38K계 용융탄산염 내에서의 부식 실험을 수행하였다. 부식의 형태 및 속도는 환경에 의하여 다양하게 변화하게 되며, 용융탄산염 내에서 AISI-type 316L stainless steel의 부식 속도는 부식 반응에 의하여 형성되는 부동태 산화막의 안정성에 의하여 크게 영향을 받는다. 전기화학적 분극 거동을 분석한 결과 용융탄산염 연료전지의 anode가슨 분위기에서는 안정한 부동태 산화막이 형성되지 않았다. 순환 전압전류법과 정전위법을 이용한 부식 생성물의 X-ray분석을 통하여 특정한 전기화학적 전위 영역에서 반응기구와의 인과관계를 규명하고 다양한 형태의 부식 반응들을 분리해 내었다.

합금화된 단일타겟을 마그네트론 스퍼터를 이용하여 합성된 나노복합구조 Al-Ti-X-N (X=Si,Cu,Cr) 코팅의 기계적 특성

  • 정덕형;이한찬;신승용;문경일
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.281-281
    • /
    • 2011
  • 산업 환경에서 친환경 및 에너지효율성을 중요한 조건이 되면서 고효율성 및 다기능을 가진 재료에 대한 연구가 활발히 진행 되고 있다. 특히 Al-Ti-N 코팅은 이미 경도 측면에서 우수 하여 고속 공구 부품에 널리 사용되고 있고 최근에 Al-TiN에서 Si 첨가는 40GPa이상의 고경도와 1000도 이상의 산화온도를 지닌 나노 혼합물 코팅을 형성 시키는 것으로 알려져 있다. 본 연구에서 Al-Ti에 Si, Cu, Cr 을 첨가하였을 때 코팅을 형성하였을 때 바뀌는 물성 변화을 확인하였다. 이러한 연구를 위해 Al-Ti 합금 조성 중 가장 우수한 것으로 알려진 60:40으로 타겟을 만들어 스퍼터 장비를 이용해 코팅을 형성하여 기초 실험을 진행하였다. 그 근거로 하여 3원계인 Si, Cu, Cr 을 첨가하여 각각의 단일 타겟으로 만들고 코팅을 형성하였다. 타겟과 코팅의 성분이 동일한지 확인하기 위해 EPMA분석을 하였고 그 결과 오차 범위 내에 동일한 것으로 확인하였다. 또 내산화성 테스트를 위해 400도에서 1000도로 가열된 대기 중에 코팅 층을 1시간씩 노출시키는 공정을 통해 확인하였고 내식성 테스트는 SUS 304계열 위에 코팅을 하여 Potentiodynamic polarization scan 장비로 비교해 보았다. 표면경도는 3원계 코팅인 경우 질소비율이 증가할수록 30GPa ~ 35GPa까지 증가하였고 XRD 분석 결과와 비교 시 (111), (200) peak가 명확할수록 경도 값이 높은 것으로 확인하였다. 마모테스트 결과 3원계인 코팅 층이 dry상태에서 감소하는 경향을 보였다. 특히 0,26까지 감소한 Si 을 첨가한 코팅 층은 H/E지수도 좋아 마모트랙의 길이도 짧아 우수한 것으로 알 수 있었다. 이런 결과에서 보듯 3원소 이상 첨가 시 특성변화가 차이가 있다는 것을 알 수 있었다.

  • PDF