  • Porous basalt aggregate is commonly used in roadbed engineering, but its application in concrete has rarely been studied. This paper studies the application of porous basalt in concrete. Porous basalt aggregate is assessed for its effects on mechanical strength and durability of prepared C50 concrete; because it has a hole structure, porous basalt aggregate is known for its porosity, and porous basalt aggregates can be made full of water through changing the content of saturated basalt; after full-water condition is achieved in porous basalt aggregate mixture of C50 concrete, we discuss its mechanical properties and durability. The effects of C50 concrete prepared with basalt aggregate on the compressive strength, water absorption, and electric flux of concrete specimens of different ages were studied through experiments, and the effects of different replacement rates of saturated porous basalt aggregate on the properties of concrete were also studied. The results show that porous basalt aggregate can be prepared as C50 concrete. For early saturated porous basalt aggregate concrete, its compressive strength decreases with the increase of the replacement rate of saturated aggregate; this occurs up to concrete curing at 28 d, when the replacement rate of saturated basalt aggregate is greater than or equal to 40 %. The compressive strength of concrete increases with the increase of the replacement rate of saturated aggregate. The 28 d electric flux decreases with the increase of the replacement rate of saturated aggregate, indicating that saturated porous basalt aggregate can improve the chloride ion permeability resistance of concrete in later stages.

Fundamental Properties of Porous Concrete by Aggregate Size

  • Kim, Moo-Han;Kim, Gyu-Yong;Baik, Yong-Kwan;Kim, Jae-Hwan;Cho, Bong-Suk
    • International Journal of Concrete Structures and Materials
    • /
    • 제18권2E호
    • /
    • pp.117-124
    • /
    • 2006
  • Porous concrete has been used recently for the purpose of decreasing the load on the earth environment. It consists solely of cement, water and coarse aggregate of uni form size. Its fundamental properties are considerably affected by the physical properties of aggregate because the aggregate is the main material for the most part in its mix proportion. Because of this reason, this study carried out an investigation of the influence of the size and type of aggregate on the fundamental properties of porous concrete. It is shown that the fundamental properties of porous concrete was seldom affected by the size of aggregate except for the case of using $2.5{\sim}5mm$ aggregate but varied significantly by the type of aggregate. In particular, the compressive strength of porous concrete using $2.5{\sim}5mm$ aggregate was much higher than that using other aggregate, and its void ratio and coefficient of permeability was lower. Moreover, the capacity to maintain the permeability of porous concrete was found to vary by the size and type of aggregate. Of particular notice was that it decreased greatly when $2.5{\sim}5mm$ aggregate was used. Unlike ordinary concrete, porous concrete exhibited very high dynamic modulus of elasticity at early age and continued to increase but slowly afterwards.

골재의 종류에 따른 포러스콘크리트의 특성에 관한 실험적 연구 (An Experimental Study on the Characteristic of Porous Concrete using different Aggregates)

  • 정시진
    • 한국건축시공학회지
    • /
    • 제4권1호
    • /
    • pp.89-96
    • /
    • 2004
  • Porous concrete is used of various parts by advantage of porous. Example of growing of plant is possible, and dwelling of creature, and filter functions of various contaminant, and decrease of noise, and so on. This research is for porous concretes that were used by four aggregate rubble, refreshing aggregate, expanded clay, orchid stone. This research estimate that physical and mechanical characteristics of fresh concrete and hardened concrete. The purpose of this research is to make environment-friendly porous concrete. This research's conclusion is as following : 1. Porous Concrete's slump was measured 12~14cm with rubble, 12~16cm with refreshing aggregate, 11~13cm with expanded clay, 11~13cm with orchid stone. Weight of aggregate was bigger, slump price appeared by bigger thing. Because placed Porous Concrete is low viscosity and small resistance between aggregate, it estimated that have high workability. 2. Porous Concrete's unit weight was measured 1.71~1.75t/$\textrm{m}^3$ with rubble, 1.58~1.62t/$\textrm{m}^3$ with refreshing aggregate, 1.19~1.20t/$\textrm{m}^3$ with expanded clay, 0.98~1.06t/$\textrm{m}^3$ with orchid stone. Showed aspect such as weight of aggregate. 3. Porous Concrete's compressive strength was measured 76~102kgf/$\textrm{cm}^2$ with rubble, 51~60kgf/$\textrm{cm}^2$ with refreshing aggregate, 30~40kgf/$\textrm{cm}^2$ with expanded clay, 13~16kgf/$\textrm{cm}^2$ with orchid stone. 4. Tendency of tensile strength and bending strength showed generally similarly with compressive strength, but showed low value fewer than 15kgf/$\textrm{cm}^2$ Therefore, wire mesh, reinforcing rod, such as establishment of frame is considered to need in reinforcement about tensility or flexures in case receive tensility or produce product of thin absence form. It concludes by speculating on the consequences of extrapolating the results of study to remodelling the office building being already existence.

동제련 슬래그를 혼입한 포러스 콘크리트의 강도 및 투수성능에 관한 연구 (A Study on Strength and Permeability of Cooper Slag mixed Porous Concrete)

  • 심병주;김영수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 춘계 학술논문 발표대회 1부
    • /
    • pp.69-72
    • /
    • 2011
  • The purpose of this study is to identify basic property of porous concrete using cooper slag as fine aggregate. The specimens were made with cooper slag with various mixing ratio(10, 20, 30, 50%), porous concrete and porous concrete containing river fine aggregate and crushed fine aggregate, which W/B ratio fixed 0.25. Compressive strength, Flexural strength, coefficient of permeability. From the test results, various fine aggregate mixing ratio improves compressive strength and flexural strength, but cooper slag fine aggregate mixing ratio over 20%, concrete indicates trend to decrease performance of permeability. Concrete containing fine aggregate is improved the performance of permeability and strength compared to other specimen, when age 28days, and cooper slag mixing ratio less than 20% concrete indicates better performance than cooper slag mixing ratio 20% over.

  • PDF

산업부산물을 사용한 포러스 콘크리트의 수질정화 특성에 관한 실험적 연구 (An Experimental Study on Water-Purification Properties of Porous Concrete Using Industrial By-Products)

  • 조영수;김정환;권혁준;박승범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 봄 학술발표회 논문집
    • /
    • pp.717-722
    • /
    • 2002
  • The results of an experiment on the water purification of the porous concrete and its influence on the compressive strength are reported in this paper. Two different sizes of coarse aggregate of 5-10, and 10-20mm, and three absolute volume ratios of paste to aggregate of 30, 40 and 50 percent for a given size of aggregate were used. For the compressive strength, the concrete with the aggregate size of 5-10mm showed much higher strength than that with the aggregate size of 10-20mm. But, the compressive strength is higher when the ratio of paste to aggregate is smaller. In the water purification experiment, the amount of attached an organism on the porous concrete surface indirectly is examined by measuring the consumption of the Dissolved Oxygen (DO). The ability of the water purification is evaluated by the removal amount of the Total Phosphorus(T-P) and Total Nitrogen(T-N). The ability of the removal of the T-N and T-P in the test water is superior to a porous concrete with a smaller size of aggregate and a higher void content. These results are owing to a large specific surface area of the specimen. As a result, porous concrete using by-products has sufficient performance of water purification.

  • PDF

골재 크기에 따른 포러스콘크리트의 기초물성에 관한 실험적 연구 (Fundamental Properties of Porous Concrete According to the Sizes of Aggregate)

  • 김무한;백용관;강석표;김용로;김재환
    • 콘크리트학회논문집
    • /
    • 제13권5호
    • /
    • pp.438-446
    • /
    • 2001
  • 최근 지구환경부하 저감을 목적으로 포러스콘크리트의 수요가 점점 증대되고 있지만 낮은 강도수준으로 인해 사용용도에 제약을 받고 있으며, 또한 대부분 그 기능성을 무시한 채 강도 및 색채에 의해서만 관리되고 있어 그 기능성(특히 투수성능)에 많은 문제를 유발시키고 있다. 이에 본 연구에서는 포러스콘크리트의 배합상 대부분을 차지하는 골재가 포러스콘크리트의 기초물성에 미치는 영향을 파악하여 강도 및 투수성능 향상을 위한 기초적 자료를 제시하고자 하였다. 그 결과 포러스콘크리트의 강도, 공극율 및 투수계수는 동일 단위시멘트량에서 골재 크기에 관계없이 유사하게 나타났으나 2.5~5mm 골재를 사용한 경우에는 다른 골재에 비하여 크게 다른 값을 보이고 있으며, 동일 조건에서도 골재 종류에 따라 다르게 나타났다. 또한 혼탁액 투과에 의한 투수계수 감소율은 골재 크기가 작을수록 크게 되며, 특히 2.5~5mm 골재의 경우에는 급격히 저하하였다. 또한 골재 종류에 따라서도 그 값은 다르게 나타나 포러스콘크리트의 장기 투수성능 확보를 위해서는 재료선정시 골재 크기 및 입형을 충분히 고려해야 할 것으로 판단된다. 포러스콘크리트의 압축강도와 초음파속도 및 동탄성계수 사이에는 높은 상관성을 보이고 있으며 또한 단위용적중량에 의한 포러스콘크리트의 공극율 추정이 가능한 것으로 나타났다. 또한 포러스콘크리트의 동탄성계수는 일반콘크리트에 비하여 초기재령부터 매우 높게 발현되고 있으며, 재령 7일 이후 동탄성계수의 상승구배는 매우 완만하게 나타났다.

포러스콘크리트의 골재입도 및 공극률에 따른 식생능력평가 (Planting-Ability Properties of Porous Concrete as Gradation and Void Ratio)

  • 윤덕열;김정환;조영수;표구영;박승범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.243-248
    • /
    • 2002
  • As a notion of environment protection changes throughout the world, construction engineers, as part of the effort to resolve environmental problems, have been actively doing research on environmental friendly porous concrete using large and non-uniform aggregate. Porous Concrete enables water and air to pass through a firmly hardened material and allows required nutrients to reach roots of plants. The purpose of this study is to analyze planting ability when the change of aggregate gradation and void ratio. The results of an experiment from the planting ability of the porous concrete to its influence on the compressive strength are reported in this paper. As a result of the experiment, the compressive strength is higher when the gradation of aggregate is smaller, and it also goes higher when the void ratio gets smaller The planting ability of porous concrete is decided by the germination and the grass length of Indigofera pseudo-tinctoria(IPT). The length of IPT is longer when the gradation of aggregate is greater and the void ratio gets smaller.

  • PDF

아스팔트순환골재를 이용한 투수성 콘크리트의 역학적 특성 (The Mechanical Properties of Porous Concrete using Recycled Asphalt Aggregate)

  • 이동욱;윤중만;김남식;강영민
    • 한국지반신소재학회논문집
    • /
    • 제10권1호
    • /
    • pp.37-42
    • /
    • 2011
  • 본 연구에서는 아스팔트순환골재를 이용한 투수성 콘크리트의 역학적 특성을 알아보기 위하여 투수성 콘크리트의 단위시멘트량, 잔골재 비율, 물시멘트(w/c)비의 혼합율 변화에 따른 역학적 특성과 구조체로서 요구되는 소요강도에 대하여 분석하고자 하였다. 순환골재의 사용성을 높이기 위하여 입도조정 없이 13mm 아스팔트순환골재를 사용하였으며, 물시멘트비는 빈배합이 되도록 결정하였다. 분석결과 압축강도는 18.2~19.5Mpa을 보였으며 투수계수는 평균적으로 8.0E-02cm/sec 값을 나타내었다.

재생골재의 혼입률과 목표공극률에 따른 포러스콘크리트의 흡음특성에 관한 연구 (A Study on the Sound Absolution Properties of Porous Concrete by Recycled Aggregate Contents and Target Void Ratio)

  • 박승범;서대석;이준
    • 콘크리트학회논문집
    • /
    • 제16권4호
    • /
    • pp.541-548
    • /
    • 2004
  • 본 연구는 도로, 철도, 주택가 및 도심지역의 소음저감과 건설부산물로 발생하는 폐콘크리트 재생골재의 유효이용을 위하여 포러스콘크리트의 목표공극률과 재생골재 혼입률에 따른 물리 역학적 특성 및 흡음특성을 평가하였다. 시험결과, 목표공극률과 실측공극률과의 차이는 1.7% 이내로 나타났고 압축강도는 목표공극률이 25%, 재생골재의 혼입률이 50%를 초과하는 경우에는 급격한 강도저하 경향을 나타냈다. 또한, 폐콘크리트 재생골재를 사용한 포러스콘크리트의 흡음 특성은 NRC의 경우 목표 공극률이 25%에서 가장 우수한 흡음특성을 나타냈으며, 재생골재의 혼입률에 따른 영향은 작은 것으로 나타났다. 따라서, 포러스콘크리트의 강도 및 흡음특성을 고려하였을 때 적정 목표공극률은 25%, 폐콘크리트 재생골재의 혼입률은 50% 정도가 유효한 것으로 판단된다.

랜덤입사방법에 의한 포러스 콘크리트의 흡음특성에 관한 실험적 연구 (The Study on Sound Absorbing Characteristics of Porous Concrete according to Reverberation Room Methods)

  • 서대석;박승범;조광연;장영일;김형석;이윤선
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 춘계 학술발표회 제16권1호
    • /
    • pp.568-571
    • /
    • 2004
  • This research estimated the physical. mechanical characteristic and the character of sound absorption according to target void ratio of porous concrete and the mixing ratio of recycled aggregate for the valid utilization of recycled aggregate using waste concrete and sound reduction out of a road, a railway, a residential street, and a downtown area. As a result of the test, compressive strength tended to be a radical strength fall when target void ratio was $25\%$ and contents of recycled aggregate exceeded over $50\%$. Also, the character of sound absorption of porous concrete which used recycled aggregate using waste concrete was the most excellent when target void ratio was $25\%$, and the influence by contents of recycled aggregate was trivial. Therefore, when the strength and the character of sound absorption of porous concrete are considered, it is proved valid that proper target void ratio was $25\%$ and contents of recycled aggregate using waste concrete was $50\%$ or so.

  • PDF