Journal of Korea Technical Association of The Pulp and Paper Industry
/
v.30
no.4
/
pp.28-34
/
1998
Polyvinyl acetate emulsion has been widely used as adhesives for wood and paper, paint additives and binders for fiber, leather, and other materials because it is an excellent adhesive with many advantages including low in toxicity risks and manufacturing cost. It is expected the consumption of polyvinyl acetate emulsion as adhesives will increase in cigarette industry as well as in paperboard coating industry. Recently the operation speed of the cigarette tip wrapper increased so substantially that improvement of the emulsion properties is required including good wet tack development, narrow and controlled particle size distribution, low viscosity, etc. In this study the effects of such polymerization conditions as the type and amount of emulsifier, internal or external plasticizing, and emulsification methods on the viscosity and particle size of polyvinyl acetate emulsions were examined. Results showed that polyvinyl alcohol with a high degree of hydrolysis and low molecular weight and nonionic surfactants are superior to anionic surfactant in improving adhesion and emulsion stability. They also tend to produce emulsions with smaller particle size. External plasticization with dipropylene glycol dibenzoate was more effective in improving flexibility than internal plasticization with butyl acrylate. Monomer emulsification under high shear was more effective in decreasing the particle size.
Proceedings of the Korean Institute of Building Construction Conference
/
2017.11a
/
pp.100-101
/
2017
LEFC(Light Emotion Friendly Conceret) was developed in Korea with demands of esthentic requirements in line with the recent developmental trend of concrete technology. The LEFC is made by inserting transparent transparent rods, and this forms a heterogeneous structure in the concrete matrix causing the LEFC substrate to crack due low adhesion between the rod and the cement. In this study, as a way to strengthen the bonding to the rod inserted in the LEFC, high strength vinylon fibers of varying mixture ratios were applied and physical properties were tested accordingly. To study the effect of different spacing of the bars on the LEFC, physical property testing was conducted on respective specimens with two different diameters (5mm, 10mm) inserted in different intervals of spacing (10mm, 15mm, and 20mm).
To evaluate the bonding performance of reinforced glulam, the textile type of glass fiber and aramid fiber, and the sheet type of glass fiber reinforced plastic (GFRP) and carbon fiber reinforced plastic (CFRP) were used as reinforcements. The reinforced glulam was manufactured by inserting reinforcement between the outmost and middle lamination of 5ply glulam. The types of adhesives used in this study were polyvinyl acetate resins (MPU500H, and MPU600H), polyurethane resin and resorcinol resin. The block shear strengths of the textile type in glass fiber reinforced glulam using MPU500H and resorcinol resin were higher than 7.1 N/$mm^2$, and these glulams passed the wood failure requirement of Korean standards (KS). In case of the sheet types, GFRP reinforced glulams using MPU500H, polyurethane resin and resorcinol resin, and CFRP reinforced glulams using MPU500H and polyurethane resin passed the requirement of KS. The textile type of glass fiber reinforced glulam using resorcinol resin after water and boiling water soaking passed the delamination requirement of KS. The only GFRP reinforced glulam using MPU500H after water soaking passed the delamination requirement of KS. We conclude that the bonding properties of adhesive according to reinforcements are one of the prime factors to determine the bonding performance of the reinforced glulam.
Journal of the Korea institute for structural maintenance and inspection
/
v.23
no.1
/
pp.102-112
/
2019
This paper studies impact fracture behavior under temperature variation and compressive flexural strength of cement composites using VAE(vinyl acetate ethylene) powder polymer and PVA(polyvinyl alcohol) fiber. Impact test were conducted in the temperature range selected for the $-35^{\circ}C$, $0^{\circ}C$ and $35^{\circ}C$. In this experimental study, impact test were carried out using a drop impact testing machine (Ceast 9350) to obtain such as displacement, time, and impact fracture energy of normal specimen and and cement composites specimen. As test results, the use of VAE powder polymer and PVA fiber were observed to enhance the flexural strength of mortar. The compressive strength of PVA fibers reinforced cement composites was slightly decreased at 28 days, but the flexural strength was observed to increase 24.4% of normal mortar strength. As a result of the drop impact tests, PVA fiber reinforced cement composites specimens showed microcracks due to energy dispersion and crack prevention with bridge effect of the fibers, and scabbing or perforation by impact was suppressed. On the other hand, the normal mortar and VAE powder polymer cement composites specimens were carried out to the perforation and macro crack. Most of normal mortar and the cement composites subjected to impact load on specimens shows mostly local brittle failure. The impact resistant performance of the specimen with PVA fiber was greatly improved due to the increase of flexure performance.
Kim, Subong;Chung, Yong Sik;Choi, Heung-Soap;Jin, Fan-Long;Park, Soo-Jin
Bulletin of the Korean Chemical Society
/
v.34
no.12
/
pp.3733-3737
/
2013
Polyacrylonitrile (PAN)-based ultrafine fibers and carbon fibers were produced by wet-spinning, and the crystal sizes and thermal and mechanical properties of the fibers were investigated. Scanning electron microscopy revealed that the superfine fibrils in the surfaces of the PAN/polyvinyl acetate (PVA) blend fibers increased slightly with increasing PAN content before removal of the PVA. Differential scanning calorimetry indicated that the PAN and PVA in the blend fibers do not mix and, therefore, each maintains their inherent thermal characteristics. The crystal sizes of the blend fibers prepared by removing PVA with water increased at 5 wt % water. The extent of the reaction of the PAN carbon fibers, as calculated from the FT-IR spectra, is maximized at the stepwise temperature of $230^{\circ}C$, and the density increased significantly above this temperature. The carbon fibers had relatively good mechanical properties, as shown by their tensile strength and modulus values of 2396 MPa and 213 GPa, respectively.
Electrospinning process is the useful and unique method to produce nanofibers from metal precursor and polymer solution by controlled viscosity. In this study, the NiZn ferrite nanofibers were prepared by electrospinning with a aqueous metal salts/polymer solution that contained polyvinyl pyrrolidone and Fe (III) chloride, Ni (II) acetate tetrahydrate and zinc acetate dihydrate in N,N-dimethylformamide. The applied electric field and spurting rate for spinning conditions were 10 kV, 2 ml/h, respectively. The obtained fibers were treated at $250^{\circ}C$ for 1 h to remove the polymer. Finally, the NiZn ferrite fibers were calcined at $600^{\circ}C$ for 3 h and annealed at $900{\sim}1200^{\circ}C$ in air. By tuning the viscosity of batch solution before electrospinning, we were able to control the microstructure of NiZn ferrite fiber in the range of $150{\sim}500\;nm$ at 770 cP. The primary particle size in $600^{\circ}C$ calcined ferrite fiber was about 10 nm. The properties of those NiZn ferrite fibers were determined from X-ray diffraction analysis, electron microscopy, energy dispersive spectroscopy, Fourier transform infrared spectroscopy, thermal analysis, and magnetic measurement.
This study was carried out to investigate the bending strength of the Larix glulam beams which were reinforced with CFRP (Carbon fiber reinforced plastic) of which the reinforcement ratios were 0.7% and 2.1% by volume. In the bending test, the rupture shape of the reinforced glulam shows that the reinforced glulam broke firstly in the lowest bottom layer on which tension was loaded, but did not in the upper part reinforced with the CFRP layer. The upper part of the reinforced layer kept strength and did not break when the reinforced glulam broke firstly at the bottom part of the reinforced layer, but broke secondly as loading was increased. In the glulam beams reinforced with CFRP of which the reinforcement ratio was 0.7% by volume, the bending strength of the reinforced beams was increased by 28% at the first break. When beams broke up to the upper part of the reinforced layer, the bending strength of the reinforced beams was increased by 55%, compared to those of control glulam beams. When the glulam beams were reinforced with CFRP of which the reinforcement ratio was 2.1% by volume, the bending strength of the reinforced beams was increased by 77%, compared to those of control glulam beams. The ratio of the height of calculated neutral axis using failure mode recommended by Romani and the height of actual neutral axis using strain gauge was 1.03 and agreed well.
This study was carried out to investigate the bending strength properties of the unreinforced glulam beams and the GFRP laminated glulam beams according to the volume ratio of GFRP. The 7-layer glulam beams ($10cm(b){\times}14cm(h){\times}180cm(l)$) were manufactured, using Larch (Larix kaempferi Carr.) laminae ($2cm(h){\times}10cm(b){\times}360cm(l)$), which were dried to the moisture content of 8% and specific gravity of 0.54. GPRP of 0.1 and 0.3 cm was reinforced between the outmost layer of bottom and next layer. When the glulam beams were reinforced with GFRP at the volume ratio of 0.7% and 2.1%, respectively, the bending strength was increased by 12% and 28%, respectively, in the reinforced beams than in control glulam beams. Also, the GFRP reinforced layer of the glulam beams with GFRP laminations blocked the progression of rupture, and the unbroken part held about 90% of the bending strength. In the results of glue joints test, the block shear strength is higher than $7.1N/mm^2$, the standard of KS F3021, and in the result of delamination, the adhesive strength is good as the water soaking and boiling delamination was less than 5%.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.