• Title/Summary/Keyword: polyester fabric

Search Result 344, Processing Time 0.025 seconds

Washing Fastness of Polyester Artificial Suede Fabric According to Reduction Clearing Method (환원세정방법에 따른 스웨드 직물의 세탁견뢰도)

  • 강연희;백진주;서말용;김삼수;허만우;이난형
    • Textile Coloration and Finishing
    • /
    • v.13 no.4
    • /
    • pp.234-240
    • /
    • 2001
  • In order to improve the washing fastness of dyed polyester artificial suede fabric, it was dyed by using auto and anthraguinone type disperse dyes and treated with 3 different reduction clearing methods. The reduction clearing methods used in this study were normal alkaline reduction clearing, $N_2$ gas replacement method, and ultrasonic treatment during normal reduction clearing. The results were as followings ; The washing fastness property of dyed polyester artificial suede fabric was slightly improved by reduction clearing with $N_2$ gas replacement or with ultrasonic treatment comparing with normal alkaline reduction clearing. It was found that the use of $N_2$ gas replacement or ultrasonic treatment during reduction clearing eave effective removal of unfixed dyes on the fiber surface. We also obtained that the azo type disperse dye on polyester artificial fabric suede fabric showed higher wash fastness than anthraquinone type disperse dye.

  • PDF

Finishing of Interior Fabric Using Soluble Micro-fiber and low melting Yarn (용출형 극세사와 저온 융착사를 이용한 인테리어 직물의 가공)

  • Ahn, Young-Moo
    • Journal of Fashion Business
    • /
    • v.13 no.2
    • /
    • pp.78-86
    • /
    • 2009
  • When scouring and contraction finishing at $90^{\circ}C$ using Relaxer or Rotary Washer contraction and weight loss ratio in warp and weft directions were excellent. Also surface state of fabric after drying or sanding treatment was excellent without crease. Low melting polyester fabric showed a complete melting bond by heat setting(P/S) at above $160^{\circ}C$. The alkali hydrolysis reaction of polyester showed the breakpoint in the weight loss behavior test, polyester yarn showed a breakpoint ranging from 25% to 28%. This is due to the difference of the hydrolysis rate between regular polyester and soluble polyester. Initially the soluble polyester was eluted and micro-fibrillized 5 times faster than a regular polyester. At a later time, a regular polyester was reduced weight to impart a proper flexibility and drape property to the fabric. As a result of surface sanding finishing, the surface of interior fabric showed a surface state most stabilized when using Mesh No. 220 in mono 0.2d after elution finishing. When the rotation direction of sanding roller was pro-, pro-, pro-, and retro-direction, a directional effect of tuft was not shown, a writing effect as suede was exhibited and a surface state was even. Sublimation fastness was 3-4 class for polyester and 2-4 class for nylon. Light fastness 3-4 class after lapse of 100 hours and 2-4 class after lapse of 160 hours. Abrasion fastness was 3-4 class on wet and 4-5 class on dry Laundry fastness was 2-4 class. As such, the abrasion fastness is slightly reduced upon wetting and the use thereof for interior is excellent, whereas laundry fastness is slightly lowered.

A Study on the High Functional Finishing of Polyester Flat Fabrics Treated with Chitosan (키토산 처리한 폴리에스테르 편평사 직물의 고기능화 가공에 관한 연구)

  • 이석영;박성우;김삼수
    • Textile Coloration and Finishing
    • /
    • v.16 no.3
    • /
    • pp.22-30
    • /
    • 2004
  • The polyester fabrics were treated with the chitosan with various solubility in optimized treatment condition. The treatment method was discussed to be a high functional finishing for the polyester fabric to obtain the high moisture absorption and anti-microorganism property by evaluating the effect of the chitosan purification method on the yield and anti-microorganism property of the chitosan. On the other hand, soluble polyurethane was added to the chitosan treatment solution and/or plasma pretreatment was done. The addition of soluble polyurethane give a high add-on ratio as well as a linen like effect of treated polyester fabric. The results were as follows: 1. In the treatment of polyester fabric by the chitosan solution, a soluble PU resin and low temperature plasma treatment were done to obtain high binding force between the fabrics and the chitosan. The add-on rate and the moisture absorption ratio of the fabrics treated with the chitosan-PU after treated with the plasma slightly increased more than those of the fabrics treated with the chitosan only. 2. Anti-static property of the fabrics treated with the chitosan decreased rapidly with increasing of the chitosan concentration. The washing fastness of the fabrics treated with the chitosan-PU after treated with the plasma was better than those of the fabrics treated with chitosan only. The wrinkle resistance of the treated fabrics decreased constantly with the concentration of the chitosan. The bending rigidity of the treated fabrics increased greatly. On the treatment of polyester fabric under optimum condition, the microorganism reduction rate kept above 90% after 10times launderings. 3. As the polyester fabrics which has flat yam was used as a weft yams were treated with the chitosan-PU as give a functional finishing effects such as durability, moisture absorption, anti-static and anti- microorganism property. Treated polyester fabric showed a good functional finishing effect and a linen like property.

Effect of Washing Conditions on Dimensional Change and Mechanical Properties in Polyester/Spandex Knit Fabric (세탁조건에 따른 폴리에스터/스판덱스 편성물의 형태안정성과 역학적 특성 변화)

  • Roh, Eui Kyung;Kim, Eunae
    • Fashion & Textile Research Journal
    • /
    • v.20 no.1
    • /
    • pp.93-100
    • /
    • 2018
  • This study comparatively analyzed the changes in the dimensional stability and the mechanical properties of stretch knit fabrics associated with washings conditions in order to determine the most appropriate washing method. Polyester and spandex knit fabrics were washed 25 cycles with nine washing condition profiles that controled detergent, hardness. temperature and RPM. The knit fabrics with repeated washings were evaluated by dimensional stability and measured by the KES-FB system. Polyester and spandex fibers have good chemical resistance. However, the changes in the dimensional stability and the mechanical properties were observed in washed knit fabrics. After repeated washings, the knit fabrics washed in an alkali or neutral detergent had good dimensional stability compared with the knit fabric washed in functional detergent. The washed knit fabrics were extended, stiff, rough, and had a smaller volume. The changes were the result of the rearrange of polyester fibers which twisted around spandex core and chemical interactions involving the detergent and the physical and mechanical forces of washing. Especially, using an alkali detergent resulted in increased stiffness and roughness of the knit fabric. In conclusion, the washing in water with low hardness and a neutral detergent can minimize the changes in dimensional stability and mechanical properties of polyester and spandex knit fabric.

Effect of Binder's Concentration and Fiber Type on Mechanical Properties of Fragrant Fabrics (마이크로캡슐을 이용한 방향가공시 바인더 농도 및 섬유 종류에 따른 물성)

  • 김혜림;송화순
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.28 no.7
    • /
    • pp.1029-1036
    • /
    • 2004
  • The fragrant fabrics were prepared by treatment with eucalyptus microcapsules. 100% cotton fabric, 100% polyester fabric and 100% wool fabric were used as test specimens. Using pad-dry-cure method, microcapsules were attached on each specimen by acrylic binder under conditions of varying concentration. Surface property, stiffness, and air permeability of fragrant fabrics were evaluated. As increasing concentration of binder, add-on yield was increased. Add-on yield was decreased with increasing laundering cycle, especially in polyester fabric. As the concentration of binder was increased, the properties of stiffness and air permeability were decreased. Also it fumed out that pad-dry-cure method was not suitable to polyester fabric.

The Skin Care Finishing of Polyester by Silk Sericin (실크 세리신을 이용한 폴리에스테르의 쾌적가공)

  • 한대만;배도규
    • Journal of Sericultural and Entomological Science
    • /
    • v.41 no.3
    • /
    • pp.185-195
    • /
    • 1999
  • This study was carried out to improve the skin care property of the polyester fabric by finishing with sericin. It was known that skin care function, anti-oxidation, anti-tyrosinase activity and anti-elastase activity can be achieved from sericin finish. But, the moisture regain of the finished fabric was measured simply, because the major cause of the discomfort from polyester fabric has been anounced to be wetness. The effects of various treatment conditions on the properties of the finished fabric were measured, and obtained results were as follows: 1. The moisture regain at 40$^{\circ}C$ 90% RH were increased with the sericin uptake increasing. while it was not significant for the effects on the moisture regain depending on the treatment conditions like the degree of polymerization and treatment concentration of the binder. The moisture release of the fabric having sericin uptake 1%, 2% was faster than non treated fabric. The change of the moisture regain of the finished fabric from 40$^{\circ}C$ 90% RH to room temperature was 4∼5 times higher than that of knitted cotton fabric. 2. The frictional static charge was decreased with the degree of polymerization of the binder increasing. While the sericin uptake and treatment concentration of the binder were not significant. 3. The whiteness value of the fabric was slightly decreased by finishing with sericin and binder. In that cases, W values of the finished fabrics were above 90 while that depending on the degree of polymerization of the binder was not significant. 4. The major cause of the yellowness of the finished fabric was proved to be catalyst. The yellowness of the finished fabric with sulfur containing catalyst was lower than that with amine group containing catalyst. 5. The effects of the treatment concentrations of the cross-linking agent, catalyst and drying time on the wash durability were not significant.

  • PDF

Bedding Fabric Performance Using Polyester, Tencel and Cotton MVS Blended Spun Yarns (PET, Tencel, Cotton MVS 혼방사로 제직된 침구용 직물의 성능평가)

  • Sa, A-Na;Lee, Jung Soon
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.41 no.1
    • /
    • pp.17-27
    • /
    • 2017
  • This study evaluated the performance of bedding fabrics consisting of warp (150d/144f, polyester) and weft (polyester, Tencel and cotton MVS blended spun yarn) with blend ratio of weft. We measured electrostatic propensity, moisture properties, pilling properties and mechanical properties of the fabrics for this study. F-P fabric showed outstanding moisture properties and pilling properties. However, tensile properties and electrostatic propensity were relatively inferior to other characteristic values. Significant static electricity may make F-P fabric uncomfortable. F-P7C3 fabric showed outstanding moisture properties and pilling properties. Static electricity may make F-P7C3 fabric uncomfortable; in addition, F-P5C5 fabric showed outstanding moisture properties and pilling properties. Rough and stiff hand feel were expected to increase because tensile properties decreased and surface properties increased. F-C fabric showed outstanding pilling properties and electrostatic propensity. However, it showed inferior moisture control properties. F-P5T4C1 fabric showed outstanding moisture properties, pilling properties and electrostatic propensity. Several properties are outstanding; however, the hand feels are very rough and stiff from bending. The water evaporation and static electricity increased with increasing polyester content. As the content of cotton increased, tensile properties were improved. However, water evaporation and static electricity decreased. The addition of Tencel increased the thickness and compression energy so that it exhibited a soft characteristic upon compression and an excellent moisture control properties, but the surface became somewhat coarse.

The Effects of Water-and Oil-Repellent Finishes on the Surface Characteristics of Polyester Fabrics (발수발유 가공처리가 폴리에스테르 직물의 표면 특성에 미치는 영향)

  • 하희정
    • Journal of the Korean Home Economics Association
    • /
    • v.35 no.3
    • /
    • pp.275-286
    • /
    • 1997
  • The effects of water-and oil-repellent finishes on the surface characteristics of polyester fabrics were investigated in this study. Three kinds of fluoropolyment were selected as water=and oil-repellent finishing agents. The effects of water-and oil-repellent finishes were determined by the water repellency and oil repellency. The surface properties of untreated and treated polyester fabrics were evaluated with respects to crease resistance, contact angle and wicking time. The results of this study were as follows: 1. The polyester fabrics treated with fluoropolymers showed much higher water repellency and oil repellency than those of untreated polyester fabrics. Water-and oil-repellency of fabrics were increased with the crystallinity and the hydrophobic-hydrophillic components of fluoropolymers. 2. Water repellency of fabrics treated with fluoropolymer with hydrophobic components was the highest. Oil repellency of fabrics treated with fluoropolymer with high crystallinity was the highest. Water-and oil-repellency of fabrics treated with fluoropolymer with hydrophyllic components was low comparatively. 3. The crease resistance of polyester fabrics treated with fluoropolymer nearly approached to that of untreated polyester fabric. 4. The water-and oil-repellent finishes improved contact angle markedly. Especially the contact angle of ployester fabric treated with fluropolymer with hydrophobic component was the biggest. 5. The wicking time of polyester fabric treated with fluropolymer with hydrophobic component was the longest.

  • PDF

Synthesis of Temporarily Solubilized Reactive Disperse Dyes and Their Application to the Polyester/Cotton Blend Fabric

  • Lee, Jung-Jin;Han, Nam-Keun;Lee, Won-Jae;Park, Jae-Hong;Kim, Jae-Pil
    • Fibers and Polymers
    • /
    • v.3 no.3
    • /
    • pp.85-90
    • /
    • 2002
  • Five temporarily solubilized reactive disperse dyes were synthesized and characterized. They were applied to polyester/cotton blend fabric using one-bath dyeing method without dispersing agent. The dye that has azonaphthalene chro-mophore seemed to not only be exhausted on polyester but also react with cotton. But other dyes were selectively dyed on polyester and showed limited uptake on cotton. Good levelling as well as moderate to good colour fastness was obtained with the dyes on P/C blend fabric.

Antimicrobial Activity and Physical Properties of Polyester Fabric Treated with Mixture of Chitosan and Collagen (키토산과 콜라겐의 혼합물로 처리한 폴리에스테르 직물의 항균성 및 물성)

  • 박수미;오수민;송화순
    • Textile Coloration and Finishing
    • /
    • v.11 no.4
    • /
    • pp.31-38
    • /
    • 1999
  • The purpose of this study is to develop multifunctional fabric that has improved antimicrobial activity and reduction rate of gas by treatment of mixture of chito colla and crosslinking material for polyester. The surface morphology of treated PET fabric was studied by scanning electron microscopy(SEM). The properties of the PET fabric, such as antimicrobial activity, whiteness, moisture regain, water absorption and static voltage, and handle were investigated. Antimicrobial activity of treated PET fabric was proved 99%. The surface of treated PET fabric showed harshness and irregularity. The whiteness of treated PET fabric on the baking condition was decreased as time and temperature was increased. The moisure regain of treated PET fabric equally was maintained. Water absorption and static voltage of treated PET fabric were improved. KOSHI of treated PET fabric was increased compared with the untreated PET fabric H/W of treated PET fabric was improved compared with the untreated PET fabric and 2HB/B of treated PET fabric were reduced.

  • PDF