이온성 망상구조막에 기반한 전기 활성 고분자 구동기 (Electro-Active Polymer Actuator by Employing Ionic Networking Membrane of Poly (styrene-alt-maleic anhydride)-Incorporated Poly (vinylidene fluoride))

  • 여군;김상균;이선우;오일권
    • 한국소음진동공학회:학술대회논문집
    • /
    • 한국소음진동공학회 2007년도 추계학술대회논문집
    • /
    • pp.714-717
    • /
    • 2007
  • In this study, a novel actuator was developed by employing the newly-synthesized ionic networking membrane (INM) of poly (styrene-alt-maleic anhydride) (PSMAn)-incorporated poly (vinylidene fluoride) (PVDF). Based on the same original membrane, various samples of INM actuator were prepared through different reduction times with the electroless-plating technique. The as-prepared INM actuators were tested in terms of surface resistance, platinum morphology, resonance frequency, tip displacement, current and blocked force, and their performance was compared to that of the widely-used traditional Nafion actuator. Scanning electron microscope (SEM) and transmission electron microscopy (TEM) revealed that much smaller and more uniform platinum particles were formed on the surfaces of the INM actuators as well as within their polymer matrix. Although excellent harmonic response was observed for the newly-developed INM actuators, this was found to be sensitive to the applied reduction times during the fabrication. The mechanical displacement of the INM actuator fabricated after optimum reduction times was much larger than that of its Nafion counterpart of comparable thickness under the stimulus of constant and alternating current voltage.

  • PDF

시멘트 모르타르용 cPSMA-PSMA 마이크로캡슐 흡수제 제조 및 적용 (Synthesis and Application of cPSMA-PSMA Microcapsule Absorbent for Cement Mortars)

  • 황기섭;장석수;정용욱;이승한;하기룡
    • 폴리머
    • /
    • 제36권2호
    • /
    • pp.216-222
    • /
    • 2012
  • 콘크리트 제조 시 잉여수의 지연 흡수를 위하여 가교된 crosslinked poly(styrene-$alt$-maleic anhydride)(PSMA)가 core이고, PSMA가 shell인 마이크로캡슐 흡수제를 침전중합법으로 제조하였다. Shell의 두께를 조절하기 위하여 (core 단량체의 질량)/(shell 단량체의 질량) 비가 1/1, 1/2 및 1/3이 되도록 하여 cPSMA-PSMA를 중합하였다. FTIR spectrometer를 사용하여 시멘트 포화 수용액 내에서 PSMA가 가수 분해 반응이 일어남을 확인하였다. TEM 분석으로 core/shell 단량체 비가 1/2(cPSMA #3)일 때 마이크로캡슐 구조를 잘 형성하는 것을 관찰하였고, 1/1(cPSMA #2)과 1/3(cPSMA #4)은 불완전한 마이크로캡슐 구조임을 관찰하였다. 시멘트 포화 수용액에서 cPSMA #3의 팽윤비는 초기 20분까지 증가한 후 2시간까지는 감소하였으며, 그 후 24시간까지는 다시 증가하였다. 제조된 cPSMA #3을 시멘트 페이스트에 첨가한 후 시간에 따른 점도 측정 결과 1시간까지는 거의 변화가 없었지만, 그 후 급격한 점도 증가가 일어났다. Core로만 구성된 cPSMA #1을 0.5 wt% 첨가한 시멘트 모르타르의 압축강도는 무첨가 시멘트 모르타르에 비해 약 5% 높게 나타났으며, cPSMA #3을 첨가한 모르타르는 약 7% 증가로 가장 높게 나타났다.