• Title/Summary/Keyword: poly(phenylene benzobisoxazole) (PBO)

Search Result 2, Processing Time 0.017 seconds

Study on the Mechanical Properties of Rubber Composite Materials Contained PBO, Aramid Chopped Fiber (PBO, Aramid Chopped Fiber가 함유된 고무복합재료의 기계적 물성연구)

  • Lee, Jun Hee;Lee, Kwang-Woo
    • Textile Coloration and Finishing
    • /
    • v.33 no.4
    • /
    • pp.327-337
    • /
    • 2021
  • The uniformly dispersed Aramid and Poly (phenylene benzobisoxazole) (PBO) in a variety of rubber was investigated. The mechanical properties of rubber were characterized by hardness, tensile strength, elongation at break, heat resistance, oil resistance, cold resistance, ozone resistance measurements. The 3mm Aramid chopped fiber better tensile strength than the other Chopped fiber. The Aramid of 3mm chopped fiber showed excellent reinforcing in rubber composite because of homogeneous dispersion. Consequently, the best 3mm Aramid chopped fiber and rubber improved the tensile strength and elongation at break of the composite. Also, 3mm Aramid chopped fiber improved the oil-resistant, ozone resistant and cold resistant.

Nondestructive Microfailure and Interfacial Evaluation of Plasma-Treated PBO and Kevlar Fibers/Epoxy Composites using Micromechanical Test and Acoustic Emission (Micromechanical 시험법과 음향방출을 이용한 플라즈마 처리된 PBO와 Kevlar 섬유강화 Epoxy 복합재료의 비파괴적 파단특성 및 계면물성 평가)

  • 박종만;김대식;김성룡
    • Composites Research
    • /
    • v.16 no.4
    • /
    • pp.74-79
    • /
    • 2003
  • Comparison of interfacial properties and microfailure mechanisms of oxygen-plasma treated poly(p-phenylene-2,6-benzobisoxazole(PBO. Zylon) and poly(p-phenylene terephthalamide)(PPTA, Kevlar) fibers/ epoxy composites were investigated using micromechanical technique and nondestructive acoustic emission(AE). Interfacial shear strength(IFSS) and work of adhesion, Wa of PBO or Kevlar fibers/epoxy composites increased by oxygen-plasma treatment. Plasma-treated Kevlar fiber shooed the maximum critical surface tension and polar term, whereas the untreated PBO fiber showed the minimum value. Microfibril fracture pattern of plasma-treated Kevlar fiber appeared obviously. Based on the propagation of microfibril failure toward core region. the number of AE events for plasma-treated PBO and Kevlar fibers increased significantly. The results oi nondestructive AE were consistent well with microfailure modes by optical observation in microdroplet and two-fiber composites tests.