• Title/Summary/Keyword: plasma treatments

Search Result 601, Processing Time 0.037 seconds

Effects as Plasma Treatments on CdS Buffer Layers in CIGS Thin Film Solar Cells

  • Jo, Hyun-Jun;Sung, Shi-Joon;Hwang, Dae-Kue;Bae, In-Ho;Kim, Dae-Hwan
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.08a
    • /
    • pp.171-171
    • /
    • 2012
  • We have studied the effects of plasma treatments on CdS buffer layers in CIGS thin film solar cells. The CdS layers were deposited on CIGS films by chemical bath deposition (CBD) method. The RF plasma treatments of the CdS thin films were performed with Ar, $O_2 and $N_2 gases, respectively. After plasma treatments, the solar cells with Al:ZnO/i-ZnO/CdS/CIGS structures were fabricated. The surface properties of the CdS/CIGS thin films after plasma treatments were investigated with SEM, EDX and AFM measurements. The electrical properties of manufactured solar cell were discussed with the results of current-voltage measurements. The plasma treatments have a strong influence on the open circuit voltage (VOC) and the fill factor of the solar cells. Finally, a correlation between the surface properties of CdS layer and the efficiencies of the CIGS thin film solar cells is discussed.

  • PDF

Effects of Plasma Surface Treatments Using Dielectric Barrier Discharge to Improve Diamond Films

  • Kang, In-Je;Ko, Min-Guk;Rai, Suresh;Yang, Jong-Keun;Lee, Heon-Ju
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.552-552
    • /
    • 2013
  • In our study we consider Al2O3 ceramic substrates for Plasma Surface Treatments in order to improve deposited diamond surface and increase diamond deposition rate by applying DBD (Dielectric Barrier Dischrge) system. Because Plasma Surface Treatments was used as a modification method of material surface properties like surface free energy, wettability, and adhesion. By applying Plasma Surface Treatments diamond films are deposited on the Al2O3 ceramic substrates. DC Arc Plasmatron with mathane and hydrogen gases is used. Deposited diamond films are investigated by SEM (Scanning Electron Microscopy), AFM (Atomic Force Microscopy) and XRD (X-ray Diffractometer). Then the C-H stretching of synthetic diamond films by FTIR (Fourier Transform Infrared Spectroscopy) is studied. As a result, nanocrystalline diamond films were identified by using SEM and diamond properties in XRD peaks at (111, $43.8{\Box}$, (220, $75.3{\Box}$ and (311, $90.4{\Box}$ were shown. Absorption peaks in FTIR spectrum, caused by CHx sp3 bond stretching of CVD diamond films, were identified as well. Finally, we improved such parameters as depostion rate ($2.3{\mu}m$/h), diamond surface uniformity, and impurities level by applying Plasma Surface Treatments. These experimental results show the importance of Plasma Surface Treatments for diamond deposition by a plasma source.

  • PDF

Effect of Low Temperature Plasma Pretreatment on the Color Depth of Wool Fabrics (양모직물의 염착농도에 미치는 저온플라즈마 처리의 영향)

  • 배소영;이문철
    • Textile Coloration and Finishing
    • /
    • v.4 no.2
    • /
    • pp.76-83
    • /
    • 1992
  • Wool tropical and nylon taffeta were treated with low temperature plasma of $O_2$, $N_2$, NH$_3$, CF$_4$ and CH$_4$ for the intervals of 10 to 300 sec, and then dyed with leveling and milling type acid dyes in presence or absence of buffer solution. From the color depth of dyed fabrics, effect of plasma gases, treated time, dyeing time and temperature on dyeing property was studied. The results of the experiment can be summarized as follows: 1) The plasma treatments except methane gas increased the color depth of dyed wool fabrics, but not that of dyed nylon fabrics regardless of the plasma gases used. 2) The color depth of wool fabrics dyed in the dye bath without buffer solution was increased by the low temperature plasma, especially increased much more by CF$_4$ plasma treatment. It is found that with the identification of F- ion in the residual dye bath the hydrogen fluoride gas was adsorbed on wool fabrics in the plasma treatment. 3) The color depth of wool fabrics was increased with the time of $O_2$ and CF$_4$ plasma treatments. 4) In both cases of the leveling and milling type acid dyes, the rate of dyeing was increased in the low temperature plasma treatments, and it is found that the leveling type acid dye increased the color depth at relatively low temperature below 4$0^{\circ}C$, compared with the milling type acid dye.

  • PDF

Effects of the Plasma Treatment on the Physical Property of ZnO Thin Film (플라즈마 처리가 ZnO 박막의 물리적 특성에 미치는 영향)

  • Cho, Jae-Won;Joung, Tae-Young;Rhee, Seuk-Joo
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.3
    • /
    • pp.173-176
    • /
    • 2011
  • The characteristic changes in ZnO thin film according to H- and O- plasma treatments have been studied by Photoluminescence (PL) spectroscopy at room temperature. The red shift of UV peak by 20-30 meV in PL spectra after plasma treatments is identified, which indicates that there are changes in the binding energy of bound exciton and/or the movement of energy levels of lattice defects and impurities. The width of UV peak is decreased after plasma treatments, which is believed to be closely related to the crystal quality of ZnO film. The increase of UV peak intensity after H-plasma treatment is also observed, and this could mean that the radiative recombination is strengthened because the hydrogen atoms in the plasma diffuse into the film where they passivate and neutralize the defects and the impurities.

Helium/Oxygen Atmospheric Pressure Plasma Treatment on Poly(ethylene terephthalate) and Poly(trimethylene terephthalate) Knitted Fabrics: Comparison of Low-stress Mechanical/Surface Chemical Properties

  • Hwang Yoon Joong;McCord Marian G.;Kang Bok Choon
    • Fibers and Polymers
    • /
    • v.6 no.2
    • /
    • pp.113-120
    • /
    • 2005
  • Helium-oxygen plasma treatments were conducted to modify poly(trimethylene terephthalate) (PIT) and poly(ethylene terephthalate) (PET) warp knitted fabrics under atmospheric pressure. Lubricant and contamination removals by plasma etching effect were examined by weight loss $(\%)$ measurements and scanning electron microscopy (SEM) analysis. Surface oxidation by plasma treatments was revealed by x-ray photoelectron spectroscopy (XPS) analyses, resulting in formation of hydrophilic groups and moisture regain $(\%)$ enhancement. Low-stress mechanical properties (evaluated by Kawabata evaluation system) and bulk properties (air permeability and bust strength) were enhanced by plasma treatment. Increasing interfiber and interyarn frictions might play important roles in enhancing surface property changes by plasma etching effect, and then changing low-stress mechanical properties and bulk properties for both fabrics.

Electrical Characteristics of Carbon Nanotubes by Plasma and Microwave Surface Treatments

  • Cho, Sang-Jin;Shrestha, Shankar Prasad;Lee, Soon-Bo;Boo, Jin-Hyo
    • Bulletin of the Korean Chemical Society
    • /
    • v.35 no.3
    • /
    • pp.905-907
    • /
    • 2014
  • The plasma and microwave surface treatments of carbon nanotubes that loaded on plastic substrates were carried out with expecting a change of carbon nanotube dispersion by increasing treatment time. The microwave treatment process was undergone by commercial microwave oven (800 W). The electrical property was measured by hall measurement and resistance was increased by increasing $O_2$ flow rate of plasma, suggesting an improvement of carbon nanotube dispersion and a possibility of controlling the resistances of carbon nanotubes by plasma surface treatment. The resistance was increased in both polyethylene terephthalate and polyimide substrates by increasing $O_2$ flow rate. Resistance changes only slightly with different $O_2$ flow treatment in measure rho for all polyimide samples. Sheet resistance is lowest in polyimide substrate not due to high carbon nanotube loading but due to tendency to remain in elongated structure. $O_2$ or $N_2$ plasma treatments on both polyethylene terephthalate and polyimide substrates lead to increase in sheet resistance.

Effects of Sea Shell Supplementation on Egg Quality in Diets of Laying Hens (산란계 사료내 Sea Shell 첨가로 인한 난각질 향상에 미치는 효과)

  • 권오석;김인호;홍종옥;황일환;홍의철;이상환
    • Korean Journal of Poultry Science
    • /
    • v.27 no.3
    • /
    • pp.221-226
    • /
    • 2000
  • This experiment was conducted to determine the effect of replacing limestone by sea shell on digestibility, egg strength and thickness, Ca and P of serum and Ca and P of tibia in layer hens. A total 54 brown layers was assigned to the treatments. There were six layers per replicate with three replicate per treatment. Treatments were layer diet with 7.5% limestone as control, 7.0% limestone and 0.5% sea shell in diet(SS0.5) and 6.5% limestone and 1.0% sea shell in diet(SS1.0). Digestibility of DM was significantly difference between SS0.5 and SS1.0(P〈0.05). Digestibilities of Ca and P were not affected by treatments(P〉0.05), however, SS1.0 tended to increase Ca and P digestibility compared to control. Egg thickness and egg strength were no differences among the treatments(P〉0.05). Differences of initial and finial period on Ca of plasma were significantly affected in the a.m. between SS0.5 and SS1.0(P〈0.05). However, there was no difference in Ca of plasma in the p.m. among the treatments and Ca of plasma in control had a tendency to decrease in the p.m. compared to that of treatments(P〉0.05). Ca of tibia was significantly increased by SS1.0 compared to control(P〈0.05). However, there was no difference in P of tibia among the treatments(P〉0.05). Based on these results, dietary supplemental sea shell mat have a role to improve the egg quality of layer hens.

  • PDF

Influence of Oxygen Plasma Treatments on Yellowing of Polyester Fabrics (산소 플라즈마 처리가 폴리에스테르 직물의 황변에 미치는 영향)

  • 권영아
    • Textile Coloration and Finishing
    • /
    • v.10 no.6
    • /
    • pp.1-9
    • /
    • 1998
  • The effects of oxygen plasma treatments at different discharge power, reaction pressure, treatment time on yellowing of polyester fabrics were studied. Surface characteristics of the treated fabrics were also investigated by means of SEM and ESCA. The results were as follows : The yellowing of fabrics increases as the power and the treatment time are increased, and decreases as the pressure is increased. The plasma treatment of 100 Watt, 200 mTorr, 5 min. is the optimal condition which is most effective in holding whiteness as well as high weight loss of fabrics.

  • PDF

Duplex Surface Treatments of Plasma Nitrocarburizing and Plasma Oxidation of SKD 11 Steel

  • Lee, In-Sup;Jeong, Kwang-Ho;Cho, Young-Rae
    • Journal of Surface Science and Engineering
    • /
    • v.40 no.6
    • /
    • pp.250-253
    • /
    • 2007
  • Plasma nitrocarburizing and plasma oxidizing treatments were performed to improve the wear and corrosion resistance of SKD 11 steel. Plasma nitrocarburizing was conducted for 12 h at $520^{\circ}C$ in the nitrogen, hydrogen and methane atmosphere to produce the $\varepsilon-Fe_{2-3}(N,C)$ phase. It was found that the compound layer produced by plasma nitrocarburising was predominantly composed of $\varepsilon-phase$, with a small proportion of $\gamma'-Fe_4(N,C)$ phase. The thickness of the compound layer was about $5{\mu}m$ and the diffusion layer was about $150{\mu}m$ in thickness, respectively. Plasma post oxidation was performed on the nitrocarburized samples with various oxygen/hydrogen ratio at constant temperature of $500^{\circ}C$ for 1 hour. The very thin magnetite($Fe_3O_4$) layer $1-2{\mu}m$ in thickness on top of the compound layer was obtained by plasma post oxidation. It was confirmed that the corrosion characteristics of the nitrocarburized compound layer could be further improved by the application of the superficial magnetite layer.

Experimental Study on Reduction of Temporal Dark Image Sticking on Bright Screen in AC-PDPs Using RF-Plasma Treatment on MgO layer

  • Park, Choon-Sang;Kim, Jae-Hyun;Tae, Heung-Sik
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2009.10a
    • /
    • pp.101-103
    • /
    • 2009
  • Minimizing the residual impurity level on the MgO layer is the key factor for reducing temporal dark image sticking on bright screen. In this paper, to reduce the residual impurity level on the MgO layer of 50-in. full-HD ac-PDP with He (35%) - Xe (11%) contents, RF-plasma treatments on the MgO layer are adopted under various gases for plasma treatment. As a result of monitoring the difference in the display luminance between the before and after 5-min. sustain discharge with a square-type image at peak luminance, the Ar and Ar>$O_2$ plasma treatments can reduce the temporal dark image sticking on the bright screen in an ac-PDP.

  • PDF