• Title/Summary/Keyword: plasma spray coating

Search Result 224, Processing Time 0.031 seconds

HISTOLOGIC EvALUATION OF BONE HEALING AROUND TITANIUM PLASMA SPRAYED AND HYDROXYAPATITE-COATED IMPLANTS IN DOGS (성경 대퇴골에 매식된 Titanium Plasma Spray 및 Hydroxyapatite 피복임프란트 주위의 골치유 양상)

  • Huh, Ki-Nam;Chung, Hyun-Ju
    • Journal of Periodontal and Implant Science
    • /
    • v.25 no.2
    • /
    • pp.418-437
    • /
    • 1995
  • The effect of the hydroxyapatite coatings on Titanium implants has been the subject of recent investigations. So far, the use of HA coating remains substantially controversial.This study was aimed to evaluate histologically the bone healing patterns around titanium plasm sprayed(TPS) amd HA-coated implant after implantation into the femur neck of ten adult dogs. After implantation, animals were sacrificed at the intervals of 2,4,6,8 and 12 weeks.The fluorescent dyes were injected on the postoperative 4th and 12th week into the animals supposed to be killed at the 12th week. The morphology and direction of new bone formation was similar in both TPS and HA-coated implants.There was a tendency toward more bone formation in the cortical bone area than in the cancellous bone area. Histologically,in the interface of the HA-coated implants, bone response and bone maturation was faster, compared to the TPS implants in the 2nd and 4th week. By fluorescent microscopy, new bone formation was active in the 4th week around both implants and was directed from the periosteum overlying cortical bone to the cancellous bone. These results suggest that the bone formation and maturation is faster during the early healing stage in the interface of the HA-coated implant and where the cortical bone quality is poor, HA coated implant is superior to the TPS implant in the early phase of new bone formation.

  • PDF

전북대학교 소재공정용 다목적 100 kW ICP (RF) 플라즈마 발생 장치 구축

  • Seo, Jun-Ho;Lee, Mi-Yeon;Kim, Jeong-Su;Choe, Chae-Hong;Kim, Min-Ho;Hong, Bong-Geun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.190-190
    • /
    • 2012
  • 전북대학교 고온 플라즈마 응용 연구 센터는 교육과학기술부 기초연구사업 중 고가연구장비 구축사업의 일환으로 소재공정용 다목적 100 kW 플라즈마 발생장치를 구축하고 있다. 100kW급 ICP (RF)형 플라즈마 발생장치는 RF 전력 인출이 이중으로 되어있어 한쪽에서는 수~수십 um 크기의 금속, 세라믹 등 고융점 원료분말을 순간적으로 용해, 기화 및 분해시키고 이들 기화 또는 분해된 증기를 급랭시키는 과정에서 초미분(<1 um)을 합성하는 플라즈마 합성법 연구가 가능하도록 RF 플라즈마 분말 합성 시스템이 연결되어 있고 다른 한쪽으로는 진공 챔버 내에서 고온 고속의 RF 플라즈마 불꽃을 형성 한 후 RF 플라즈마의 축 방향으로 반응성 가스 및 코팅 대상 물질을 주입하여 코팅 할 수 있는 열플라즈마 용사코팅 시스템이 연결되어 있는 다목적 연구 장치이다. 본 장치는 100 kW급 RF 전원 공급기와 유도결합형 플라즈마 토치, 플라즈마 분말 합성 부, 플라즈마 코팅 및 반응성 증착부, 가스 공급부, 냉각수 공급부, 전기 계장/제어부로 구성되어 있다.

  • PDF

Tribological Characteristics of Ceramic Coated High Power Brake Discs (세라믹 코팅 고에너지 제동 디스크의 트라이볼로지적 특성)

  • 이희성;강부병
    • Tribology and Lubricants
    • /
    • v.18 no.4
    • /
    • pp.305-311
    • /
    • 2002
  • Three different kinds of brake discs including two coated brake discs and one steel disc were tested under the same experimental conditions on a reduced scale braking test bench. A braking test bench was specially designed to analyse thermo-mechanical and frictional behaviors of two types of brake with different sizes in stop and hold braking modes. Plasma spray coating technique was also used to coat the discs with ceramic powder. During the test four commercial brake pads were coupled with discs. Ceramic coated discs showed good stability in friction coefficient at high speed and high energy braking conditions. But they caused large wear loss of pad mass compared with the steel disc. It was shown that thermal barrier effect in ceramic coated discs adjusted the thermal partition between pad and disc. For a steel disc. it showed fluctuating friction coefficient at high speed but small wear loss of pad mass compared with ceramic coated discs.

Braking Performance of Ceramic Coated Discs

  • Kang, B.B.;Lee, H.S.
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2002.10b
    • /
    • pp.429-430
    • /
    • 2002
  • In this study, three kinds of brake: discs including two coated brake discs and one steel disc were tested under the same experimental conditions on a reduced scale braking test bench. Plasma spray coating technique was used to coat ceramic powder on the discs. In the test, four commercial sintered brake pads were coupled with discs. Ceramic coated discs have shown good stability in friction coefficient at high speed and high energy braking conditions. However, ceramic coated discs caused more wear loss of pad mass than the steel disc. It was shown that thermal barrier effect in ceramic coated discs adjusted the thermal partition between pad and disc. Steel disc showed fluctuating friction coefficient at high speed but less wear loss of pad mass than ceramic coated discs.

  • PDF

Experimental Analysis of Ceramic Coated High Power Brake Discs (세라믹 코팅 고에너지 제동 디스크의 마찰특성 연구)

  • 강부병;이희성
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1998.04a
    • /
    • pp.97-107
    • /
    • 1998
  • Three different kinds of brake discs including two coated brake discs and one steel disc were tested under the same experimental conditions on a reduced scale braking test bench. Braking test bench was specially designed to analyse thermo-mechanical and frictional behaviors of two sizes of brake discs in stop and hold braking modes. And Plasma spray coating technique was used to coat ceramic powder on the discs. In the test four commercial brake pads were coupled with discs. Ceramic coated discs had shown good stability in friction coefficient at high speed and high energy braking conditions. But they caused large pad mass wear loss compared with the steel disc. It was shown that thermal barrier effect in ceramic coated discs adjusted the thermal partition between pad and disc. For a steel disc, it had shown fluctuating friction coefficient at high speed but a fittie pad mass wear loss compared with ceramic coated discs.

  • PDF

Mechanical Behavior of Layered YSZ Thermal Barrier Coatings using Indentation Test (압입시험법에 의한 YSZ 층상 열차폐 코팅재의 기계적 거동)

  • Lee, Dong-Heon;Lee, Kee-Sung
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.5
    • /
    • pp.396-403
    • /
    • 2011
  • In this study, we investigated the mechanical behaviors of layered thermal barrier coatings by indentations. Various single and double-layered thermal barrier coatings were deposited by air plasma spray process using different type of commercialized YSZ (Yttria stabilized zirconia) starting powders. Indentation stress-strain curve, load-displacement curve and hardness of the single and the double-layered thermal barrier coatings were obtained experimentally and analyzed. The indentation damages at the same loads were compared, and thus, the results depend on the structure of each coating. The result indicates improvement in damage resistances from tailoring of layered structures in the component of gas turbine system is expected.

Ni-BASE ALLOY SYSTEMS AS ALTERNATIVE TO HEXAVALENT CHROMIUM (경질크롬도금 대체용 Ni계 합금도금 기술)

  • Chang, Do-Yon;Lee, Kyu-Hwan;Kwon, Sik-Chol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2003.10a
    • /
    • pp.11-11
    • /
    • 2003
  • Electroplated hexavalent chromium coatings have been used in many technical applications since it was invented by G.J. Sargent in 1920. Because of the environmental problems and health risks associated with the use of hexavalent chromium, there has been an extensive search for alternative coatings with properties such as corrosion resistance and wear resistance, at a reasonable cost. However there is no single substitute that meets all the desirable performance characteristics of chromium. Advanced techniques, such as alloy plating, electroless plating, trivalent chromium plating, plasma and thermal spray coating, PVD and ion implantation, have been applied for replacing hexavalent chromium plating.

  • PDF

Effects of Hot Isostatic Pressing on Bond Strength and Elevated Temperature Characteristics of Plasma sprayed TBC (HIP처리가 플라즈마 용사된 열차폐 코팅층의 접착강도와 고온특성에 미치는 영향)

  • Park, Young-Kyu;Kim, Sung-Hwi;Kim, Doo-Soo;Lee, Young-Chan;Choi, Cheol;Jung, Jin-Sung;Kim, Gil-Moo;Kim, Jae-Chul
    • Korean Journal of Materials Research
    • /
    • v.10 no.4
    • /
    • pp.312-316
    • /
    • 2000
  • A study has been made to investigate the effects of hot isostatic pressing(HIP ping) on bond strength and elevated temperature characteristics of thermal barrier coating(TBC). The specimens were prepared by HIPping of TBC which is composed of the ceramic top coat(8wt%$Y_2$$O_3$-$ZrO_2$) and the metallic bond coat on the matrix of IN738LC superalloy. The results showed that the porosity and microcracks in the ceramic top coat of TBC were significantly decreased by HIP. As a result, the bond strength of the HIPped coating was increased above 48% compared to that of as-coated specimen and microstructure was homogenized. It was found that the thermal cycle resistance of HIPped coating was inferior to that of as-coated specimen. It was considered that this result was mainly caused by the reduction of internal defects in the top coat layer which could play a role in relaxing the thermal stress due to a large difference in thermal expansion between TBC and matrix.

  • PDF

Effect of Heat Treatment on Interface Behavior in Ni-P/Cr Double Layer (열처리 시간에 따른 Ni-P/Cr 이중 도금 층의 계면 거동에 관한 연구)

  • Choi, Myung-Hee;Park, Young-Bae;Rhee, Byong-ho;Byon, Eungsun;Lee, Kyu Hwan
    • Journal of Surface Science and Engineering
    • /
    • v.48 no.6
    • /
    • pp.260-268
    • /
    • 2015
  • The thermal barrier coating (TBC) for inner wall of liquid-fuel rocket combustor consists of NiCrAlY as bonding layer and $ZrO_2$ as a top layer. In most case, the plasma spray coating is used for TBC process and this process has inherent possibility of cracking due to large difference in thermal expansion coefficients among bonding layer, top layer and metal substrate. In this paper, we suggest crack-free TBC process by using a precise electrodeposition technique. Electrodeposited Ni-P/Cr double layer has similar thermal expansion coefficient to the Cu alloy substrate resulting in superior thermal barrier performance and high temperature oxidation resistance. We studied the effects of phosphorous concentrations (2.12 wt%, 6.97 wt%, and 10.53 wt%) on the annealing behavior ($750^{\circ}C$) of Ni-P samples and Cr double layered electrodeposits. Annealing temperature was simulated by combustion test condition. Also, we conducted SEM/EDS and XRD analysis for Ni-P/Cr samples. The results showed that the band layers between Ni-P and Cr are Ni and Cr, and has no formed with heat treatment. These band layers were solid solution of Cr and Ni which is formed by interdiffusion of both alloy elements. In addition, the P was not found in it. The thickness of band layer was increased with increasing annealing time. We expected that the band layer can improve the adhesion between Cr and Ni-P.

Hot Corrosion Behavior of Plasma Sprayed 4 mol% Y2O3-ZrO2 Thermal Barrier Coatings with Volcanic Ash (플라즈마 용사법으로 제작된 4mol% Y2O3-ZrO2 열차폐코팅의 화산재에 의한 고온열화거동)

  • Lee, Won-Jun;Jang, Byung-Koog;Lim, Dae-Soon;Oh, Yoon-Suk;Kim, Seong-Won;Kim, Hyung-Tae;Araki, Hiroshi;Murakami, Hideyuki;Kuroda, Seiji
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.6
    • /
    • pp.353-358
    • /
    • 2013
  • The hot corrosion behavior of plasma sprayed 4 mol% $Y_2O_3-ZrO_2$ (YSZ) thermal barrier coatings (TBCs) with volcanic ash is investigated. Volcanic ash that deposited on the TBCs in gas-turbine engines can attack the surface of TBCs itself as a form of corrosive melt. YSZ coating specimens with a thickness of 430-440 ${\mu}m$ are prepared using a plasma spray method. These specimens are subjected to hot corrosion environment at $1200^{\circ}C$ with five different duration time, from 10 mins to 100 h in the presence of corrosive melt from volcanic ash. The microstructure, composition, and phase analysis are performed using Field emission scanning electron microscopy, including Energy dispersive spectroscopy and X-ray diffraction. After the heat treatment, hematite ($Fe_2O_3-TiO_2$) and monoclinic YSZ phases are found in TBCs. Furthermore the interface area between the molten volcanic ash layers and YSZ coatings becomes porous with increases in the heat treatment time as the YSZ coatings dissolved into molten volcanic ash. The maximum thickness of this a porous reaction zone is 25 ${\mu}m$ after 100 h of heat treatment.