Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT ceramics with the amount of $WO_3$ addition (저온소결 PMN-PNN-PZT세라믹스의 $WO_3$첨가에 따른 압전 및 유전특성)

  • Kim, Kook-Jin;Yoo, Joo-Hyun;Chung, Young-Ho
    • Proceedings of the KIEE Conference
    • /
    • 2006.10a
    • /
    • pp.61-62
    • /
    • 2006
  • In this study, in order to develop the low temperature sintering ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics using ${Fe_2}{O_3}$ and $WO_3$ as sintering aids were manufactured with the amount of $WO_3$ addition, and the specimens were sintered at 900, 930, $960^{\circ}C$, respectively. Thereafter, their dielectric and piezoelectric properties were investigated. The sintering aids were proved to lower the sintering temperature of piezoelectric ceramics due to the effects of ${Fe_2}{O_3}$ and $WO_3$ liquid phase. At 0.3wt% $WO_3$ added specimen sintered at $930^{\circ}C$, kp, Qm, dielectric constant and $d_{33}$ showed the optimum values of 0.60, 1402, 1440 and 360[pC/N], respectively, for multilayer piezoelectric actuator application.

  • PDF

The Dielertric and Piezoelectric Properties of PZT-PCNS Piezoelectric Ceramics with Zr/Ti Mole Ratio (Zr/Ti 몰비에 따른 PZT-PCNS 압전 세라믹의 압전 및 유전 특성)

  • Lee, S.Y.;Lee, Y.H.;Lee, M.J.;Lee, J.S.;Lim, K.J.
    • Proceedings of the KIEE Conference
    • /
    • 2001.11a
    • /
    • pp.100-102
    • /
    • 2001
  • In this paper, the piezoelectric and dielectric properties of $Pb(Zr_xTi_{1-x)O_3$ - $Pb(Co_{1/3}Nb_{1/3})O_3)$ piezoelectric ceramics have been investigated as a function of Zr/Ti mole ratio. From the results, when Zr/Ti mole ratio is 49/51, electromechanical coupling coefficient($k_p$), piezoelectric strain constant($d_{33}$) mechanical quality factor($Q_m$), and Permittivity(${{\varepsilon}_{33}}^T/{\varepsilon}_0$) is 64[%], 469[PC/N], 360 and 2000, respectively. Morphotropic Phase Boundary is Zr/Ti mole ratio(49/51) from XRD analysis. Also. From SEM observation, when sintering temperature is 1150[$^{\circ}C$], grain size is about $1{\sim}2[{\mu}m]$ and maximum sintering density is 7.85[$g/cm^3$].

  • PDF

The Piezoelectric and Dielectric Properties of PZT-PMN Ceramics (PZT-PMN 압전 세라믹의 압전 및 유전 특성)

  • Lee, J.S.;Lee, Y.H.;Hong, J.K.;Jeong, S.H.;Chai, H.I.;Lim, K.J.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05c
    • /
    • pp.131-134
    • /
    • 2001
  • In this paper, the piezoelectric and dielectric properties as a function of x and a in $aPbZr_xTi_{1-x}O_3-(1-a)Pb(Mn_{1/3}Nb_{2/3})O_3$ + ywt%MgO is investigated. As a results, when a is 0.95 and x is 0.505, electromechanical coupling factor$(k_p)$, permittivity${\varepsilon}_33^T/{\varepsilon}_0$, piezoelectric strain constant$(d_{33})$ and mechanical quality factor$(Q_m)$ are 58 %, 1520, 272 pC/N and 1550, respectively. From XRD analysis, when x is 0.505, it is MPB which present rhombohedral and tetragonal phase in same quantity. Also, From SEM observation, when sintering temperature is $1150^{\circ}C$, grain size is about $2\;{\mu}m$. As a results added MgO dopant in the ternary piezoelectric ceramic, when MgO content is 0.1 wt%, $k_p$ increases to 63[%].

  • PDF

Effect of CuO on the Low Temperature Sintering Properties of PSN-PNN-PZT Ceramics

  • Jeong, Yeong-Ho;Yoo, Ju-Hyun;Nam, Seung-Hyon;Lee, Su-Ho;Chung, Kwang-Hyun;Lee, Duck-Chool
    • Transactions on Electrical and Electronic Materials
    • /
    • v.5 no.3
    • /
    • pp.109-112
    • /
    • 2004
  • In this study, in order to develop the low temperature sintering ceramics for ultrasonic vibrator, Pb(Sb$\_$$\frac{1}{2}$/Nb$\_$$\frac{1}{2}$/) O$_3$-Pb(Ni$\_$1/3/Nb$\_$2/3/)O$_3$-Pb(Zr$\_$0.48/Ti$\_$0.52/)O$_3$ ceramics were manufactured as a function of the amount of CuO addition, and their dielectric and piezoelectric characteristics were investigated. With increasing CuO addition, the grain size and density increased up to 0.3 wt% CuO addition. Taking into consideration electromechanical coupling factor(k$\_$p/) of 0.53, mechanical quality factor(Q$\_$m/) of 423, dielectric constant($\varepsilon$$\_$r/) of 1,759 and piezoelectric constant(d$\_$33/) of 362pC/N, it could be concluded that 0.5 wt% CuO added composition ceramic sintered at 920$^{\circ}C$ was suitable for ultrasonic vibrator application.

Piezoelectric Properties of Pb-free Bi(Na,K)$TiO_3-SrTiO_3$ Ceramics with the Amount of $CeO_2$ Addition ($CeO_2$첨가에 따른 무연 Bi(Na,K)$TiO_3-SrTiO_3$ 세라믹스의 압전특성)

  • Lee, Hyun-Seok;Yoo, Ju-Hyun;Park, Chang-Yub;Jeong, Yeong-Ho;Hong, Jae-Il;Im, In-Ho;Yoon, Hyun-Sang
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.590-594
    • /
    • 2004
  • In this study, lead-free piezoelectric ceramics were investigated for pressure sensor applications as a function of the amount of $CeO_2$ addition at Bi(Na,K)$TiO_3-SrTiO_3$ system. With increasing the amount of $CeO_2$ addition, the density and dielectric constant increased. Electromechanical coupling factor($k_p$) showed the maximum value(kp, 0.39) at 0.1wt% $CeO_2$ addition and decreased above 0.1wt% $CeO_2$ addition., Density, dielectric constant(${\varepsilon}_r$) increased but mechanical quality factor(Qm), piezoelectric constant(d33) decreased in $CeO_2$ addition, respectively.

  • PDF

Effects of Thermal Annealing on Dielectric and Piezoelectric Properties of Pb(Zn, Mg)1/3Nb2/3O3-PbTiO3 System in the Vicinity of Morphotropic Phase Boundary

  • Hyun M. Jang;Lee, Kyu-Mann
    • The Korean Journal of Ceramics
    • /
    • v.1 no.1
    • /
    • pp.13-20
    • /
    • 1995
  • Effects of thermal annealing on the dielectric/piezoelectric properties of $Pb(Zn, Mg)_{1/3}Nb_{2/3}O_3-PbTiO_3$ ceramics (PZMNPT) with Zn/Mg=6/4) were examined across the rhombohedral/tetragonal morphotropic phase boundary (MPB). Both the relative dielectric permittivity ($\varepsilon$r)and the piezoelectric constant($d_33$)/electromechanical coupling constant ($k_p$)were increased by thermal annealing ($800^{\circ}$~$900^{\circ}C$) after sintering at $1150^{\circ}C$ for 1 hr. Based on the dielectric analysis using the series mixing model and the concept of a random distribution of the local Curie points, the observed improvements in the dielectric and piezoelectric properties of PZMN-PT were interpreted in terms of the elimination of PbO-rich amorphous intergranular layers(~1nm) induced by thermal annealing. A concrete evidence of the presence of amorphous grain-boundary layers in the unannealed (as-sintered) specimen was obtained by examining the structure of intergranular region using a TEM.

  • PDF

Piezoelectric and Dielectric Characteristics of $NaKNbO_3$ ceramics according to the poling condition (분극조건에 따른 무연 $NaKNbO_3$ 세라믹스의 압전 및 유전 특성)

  • Lee, Sang-Ho;Yoo, Ju-Hyun;Lee, Kab-Soo
    • Proceedings of the KIEE Conference
    • /
    • 2005.11a
    • /
    • pp.157-159
    • /
    • 2005
  • In this study, in order to develop Pb-free piezoelectric ceramics, $[Li_{0.04}(Na_{0.44}K_{0.52)-(Nb_{0.86}Ta_{0.10}Sb_{0.04})]O_3$ ceramics were fabricated by conventional mixed oxide method and their piezoelectric characteristics were investigated according to the poling condition. The transition temperature from orthorhombic phase to tetragonal phase observed at $93[^{\circ}C]$ and Curie temperature was $346[^{\circ}C]$. At $50[^{\circ}C]$ poling temperature, dielectric constant, electromecha nical coupling factor kp, piezoelectric $d_{33}$ const ant, coercive field Ec, remanant polarization Pr and mechanical quality factor Qm showed the optimum value of 737, 0.45, 209[pC/N], 1l.34[kV/cm], $7.14[{\mu}C/cm^2]$ and 205, respectively.

  • PDF

Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT Ceramics with the amount of PNN substitution (PNN 변화에 따른 저온소결 PMN-PNN-PZT 세라믹스의 유전 및 압전특성)

  • Kim, Kook-Jin;Lee, Gap-Soo;Kim, Do-Hyung;Yoo, Ju-Hyun
    • Proceedings of the KIEE Conference
    • /
    • 2007.07a
    • /
    • pp.1337-1338
    • /
    • 2007
  • In this study, in order to develop low temperature sintering ceramics for multilayer piezoelectric actuator, 0.07Pb$(Mn_{1/3}Nb_{2/3})O_{3}-xPb(Ni_{1/3}Nb_{2/3})O_{3}-(0.93-x)Pb(Zr,Ti)O_{3}$ ceramics system were fabricated using $Li_{2}CO_{3}-Bi_{2}O_{3}$-CuO sintering aids and the specimens were sintered at $930^{\circ}C$. Thereafter their piezoelectric and dielectric characteristics were investigated with the amount of PNN substitution. At 9[mol%] PNN substitution, electromechanical coupling factor (kp), mechanical quality factor (Qm) and piezoelectric constant ($d_{33}$) showed the optimum value of 0.60, 1323 and 387pC/N, respectively.

  • PDF

Aging Phenomena of Multilayered PMN-PZT Ceramic Actuator (적층형 PMN-PZT 세라믹 압전 액추에이터의 열화특성)

  • Song, Jae-Sung;Jeong, Soon-Jong;Kim, In-Sung;Lee, Won-Jae;Lee, Dong-Yun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.5
    • /
    • pp.445-449
    • /
    • 2005
  • Aging phenomena of 0.2PMN-0.8PZT multilayered ceramic actuators(MCA) have been investigated at the room temperature. The piezoelectric materials were synthesized as conventional ceramic process, and MCA were fabricatedby tape casting methods. The crystalline structures and lattice parameters were investigated by X-ray diffraction analysis, showing the structure was tetragonal and c/a was about 1.01. And, the effective electromechanical coupling coefficient keff and pseudo-piezoelectric constant $d_{33}$were measured. Variable unipolar electric fields, $2{\sim}4kV/mm$, were applied to MCh to investigate the aging characteristics. After 2 kV/mm unipolar electric field, keff and $d_{33}$ were 0.454 and 4.44 respectively. The measured and simulated values using for aging phenomena analysis, had a good fit to the linear logarithmic stretched exponential law.

Characteristics of Piezoelectric and dielectric of PMWN-PZT Ceramics (PMWN-PZT계 압전세라믹의 압전 및 유전특성)

  • 홍종국;이종섭;채홍인;윤만순;정수현
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.6
    • /
    • pp.455-459
    • /
    • 2001
  • In this paper, the dielectric and pizoelectric properties of 0.05Pb(M $n_{04}$ $W_{0.2}$N $b_{0.4}$) $O_3$-0.95(PbZ $r_{x}$ $Ti_{1-x}$ ) $O_3$+yN $b_2$ $O_{5}$ , are investigated as a function of the mole ratio of Zr and the amount of N $b_2$ $O_{5}$ . Also, the phase is analyzed by XRD. When the mole ratio of Zr is 0.51, the electromechanical coupling coefficient( $k_{p}$ ), relative dielectric constant ($\varepsilon$$^{T}$ $_{33}$ /$\varepsilon$$_{0}$ ), piezoelectric stain constrain ( $d_{33}$ and dielectric loss tangent show maximum, while the mechanical quality factor shows minimum value ; $k_{p}$ =56.5%, $d_{33}$ =258pC/N, $\varepsilon$$^{T}$ $_{33}$ /$\varepsilon$$_{0}$ =1170, $Q_{m}$ =1150, tan$\delta$=0.51%. At that composition, MPB which rhombohedral and tetragonal phase coexist in this ternary system is shown by the results of XRD analysis. Also, when the amount of N $b_2$ $O_{5}$ is 0.3wt%, the mechanical quality factor is increased to about 2000. The phase transition temperature of the ternary piezoelectric ceramic system showed about 35$0^{\circ}C$.TEX>.>.>.

  • PDF