A study on adhesion properties between composite material and aluminum according to the physical surface treatment technique (물리적 표면처리 기법에 따른 복합소재 및 알루미늄간 접합특성 연구)

  • Kim, Moosun
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.11
    • /
    • pp.334-339
    • /
    • 2020
  • In this study, the adhesion properties between aluminum and composite materials, composite materials, and composite materials were compared according to the physical surface treatment to improve mechanical bonding at the bonding surface when considering carbon fiber and glass fiber-reinforced composite materials. Bonded specimens were classified into the type of base material and the surface treatment method of the bonding surface. Sandpaper, sandblasting, and plasma were applied as physical surface treatment methods. The bonded specimen was prepared as a single lap joint test specimen. An experiment to measure the lap shear strength was conducted, and the results were compared. The experimental results confirmed that the mechanical abrasion and sandblasting treatment improved the lap shear strength approximately 4 to 5 fold compared to the general specimen without physical surface treatment. In plasma treatment, the experiment was conducted by defining the respective plasma output and treatment time as follows: 150 W and 5 minutes, 150 W and 10 minutes, and 300 W and 3 minutes. Moreover, the lap shear strength results were similar to the previous mechanical surface treatments. On the other hand, the effect on the adhesion properties was small, depending on the plasma treatment conditions.

Effect of chain structure of polypropylenes on the melt flow behavior

  • Lee, Young-Jun;Sohn, Ho-Sang;Park, Seung-Ho
    • Korea-Australia Rheology Journal
    • /
    • v.12 no.3_4
    • /
    • pp.181-186
    • /
    • 2000
  • Rheological Properties of polypropylenes having different molecular structures (linear polypropylene (PPL) and branched one (PPB)) were studied. Both the extensional flow and oscillatory shear flow properties were checked. Especially, the melt strength of polypropylenes having various shear history were investigated by using in-house-made Rheometer (called SMER). Compared to linear polypropylene, the branched polypropylene shows enhanced melt strength during extensional flow due to the retarded relaxation of molecules. When the slope of melt tension was plotted against take up speed of melt strand, the characteristic peak was observed in case of branched polypropylene, while the linear polypropylene shows only monotonously decreasing pattern. This entanglement was partially disrupted by physical forces such as shear during melt extrusion. However, the melt strength of PPB after multiple extrusion is still higher than PPL, implying the loss of elasticity during multiple extrusion is not so comprehensive. On dynamic experiments, PPB shows typical shear thinning behavior and the tangent delta of PPB is lower than PPL, reflecting high elasticity of PPB.

  • PDF

Effect of Textile Care on Physical Properties and Biodegradability of Cellulose Fabrics (관리 방법에 따른 섬유소계 직물의 물리적 특성 변화 및 생분해성 평가)

  • 이혜원;박정희
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.25 no.1
    • /
    • pp.173-182
    • /
    • 2001
  • The physical properties and biodegradability of cellulose fabrics, such as cotton and rayon, are expected to vary with textile care. In this study cotton and rayon fabrics were washed repeatedly with detergents, bleaches, or softeners. The changes of physical properties were investigated by measuring retention of breaking strength, shrinkage, handle, and the fiber surface was observed by SEM. The biodegradability of fabrics was also estimated by soil burial test. The results were as follows. Cotton fabrics laundered repeatedly by detergents and bleaches lost virtually no strength. The breaking strength of the rayon fabrics decreased by about 17%∼25% after repeated launderings. Shrinkage in weft direction was much larger than that in warp direction. Bending rigidities of both fabrics decreased remarkably within 10 wash cycles. Shear rigidity in cotton fabrics increased continuously with repeated washing cycles, however, that in rayon fabrics did not show any change as washing went on. Friction coefficient increased in both fabrics after 10 wash cycles, and this is thought to be attributed to the wrinkle, interlocking of hairs, surface damage resulted from repeated washings. In cotton fabrics made of staple yarns, short hairs on the yarn surface entangled together with repeated launderings. This resulted in the continuous increase in % shrinkage, shear rigidity, friction coefficient. Rayon fabrics made of filament yarns, however, did not show this phenomenon. Softener treated fabrics showed the lowest values in bending rigidity, shear rigidity and friction coefficient because the cationic surfactants adsorbed on the fiber surface behaved like lubricants. The biodegradability of fabrics was noticeably affected by the composition of washing solutions. The fabrics washed with detergents and bleaches were decomposed faster than those washed with the others were and the cotton fabrics washed with detergents and softeners hardly degraded. The fabrics soiled with milk were decomposed almost completely and those soiled with Palmitic acid did not degrade greatly.

  • PDF

Evaluating the Influence of Post-Earthquake Rainfall on Landslide Susceptibility through Soil Physical Properties Changes (지진이후 강우의 산사태 발생 영향성 평가를 위한 토양물성값 변화 분석)

  • Junpyo Seo;Song Eu;KiHwan Lee;Giha Lee;Sewook Oh
    • Journal of the Society of Disaster Information
    • /
    • v.20 no.2
    • /
    • pp.270-283
    • /
    • 2024
  • Purpose: Considering the rising frequency of earthquakes in Korea, it is crucial to revise the rainfall thresholds for landslide triggering following earthquake events. This study was conducted to provide scientific justification and preliminary data for adjusting rainfall thresholds for landslide early warnings after earthquakes through soil physical experiments. Method: The study analyzed the change in soil shear strength by direct shear tests on disturbed and undisturbed samples collected from cut slopes. Also, The study analyzed the soil strength parameters of remolded soil samples subjected to drying and wetting conditions, focusing on the relationship between the degree of saturation after submergence and the strength parameters. Result: Compaction water content variation in direct shear tests showed that higher water content and saturation in disturbed samples led to a significant decrease in cohesion (over 50%) and a reduction in shear resistance angle (1~2°). Additionally, during the ring shear tests, the shear strength was observed to gradually decrease once water was supplied to the shear plane. The maximum shear strength decreased by approximately 65-75%, while the residual shear strength decreased by approximately 53-60%. Conclusion: Seismic activity amplifies landslide risk during subsequent rainfall, necessitating proactive mitigation strategies in earthquake-prone areas. This research is anticipated to provide scientific justification and preliminary data for reducing the rainfall threshold for landslide initiation in earthquake-susceptible regions.

EFFECT OF PRE-HEATING ON SOME PHYSICAL PROPERTIES OF COMPOSITE RESIN (중합 전 열처리가 복합레진의 일부 물성에 미치는 영향)

  • Jin, Myoung-Uk;Kim, Sung-Kyo
    • Restorative Dentistry and Endodontics
    • /
    • v.34 no.1
    • /
    • pp.30-37
    • /
    • 2009
  • The purpose of this study was to evaluate the effect of pre-heating on some physical properties of composite resin. Eighty extracted, noncarious human molars were used in the present study. Four different temperatures of composite resin were used: $4^{\circ}C$, $17^{\circ}C$, $48^{\circ}C$, and $56^{\circ}C$. The $4^{\circ}C$ and $17^{\circ}C$ values represented the refrigerator storage temperature and room temperature respectively. For $48^{\circ}C$ and $56^{\circ}C$, composite resin was heated to the temperatures. As physical properties of composite resin, shear bond strength, microhardness, and degree of conversion were measured. The data for each group were subjected to one-way ANOVAs followed by the Tukey's HSD test at 95% confidence level. Both in enamel and dentin, among composite resin of $4^{\circ}C$, $17^{\circ}C$ $;48^{\circ}C$, and $56^{\circ}C$, the pre-heated composite resin up to $56^{\circ}C$ revealed the highest shear bond strength, and pre-heated composite resin to the higher temperature revealed higher shear bond strength. Microhardness value was also higher with composite resin of higher temperature. Degree of conversion was also higher with composite resin of the higher temperature. In this study, it seems that pre-heating composite resin up to the higher temperature may show higher shear bond strength, higher microhardness value, and higher degree of conversion. Therefore, when using composite resin in the clinic, preheating the composite resin could be recommended to have enhanced physical properties of it.

Rheological and mechanical properties of ABS/PC blends

  • Khan M.M.K.;Liang R.F.;Gupta R.K.;Agarwal S.
    • Korea-Australia Rheology Journal
    • /
    • v.17 no.1
    • /
    • pp.1-7
    • /
    • 2005
  • Acrylonitrile-Butadiene-Styrene (ABS), polycarbonate (PC) and their alloys are an important class of engineering thermoplastics that are widely used for automotive industry, computer and equipment housings. For the process of recycling mixtures of ABS and PC, it is desirable to know how sensitive the blend properties are to changes in compositions. It was for this reason that blends of virgin ABS and virgin PC at five different compositions, namely, $15\%,\;30\%,\;50\%,\;70%$ and $85\%$ by weight of ABS were prepared and characterised by rheological and mechanical measurements. Rheological properties of these blends in steady, oscillatory and transient step shear and mechanical properties, namely, tensile strength, elongation-at-break and Izod impact strength are reported. The results show that PC behaves in a relatively Newtonian manner, but ABS exhibits significant shear thinning. The ABS-rich blends show a trend that is similar to that of ABS, while PC-rich blends, namely $0\%$ and $15\%$, exhibit a nearly Newtonian behaviour. However, at a fixed shear rate or frequency, the steady shear or the dynamic viscosity varied respectively in a non-mono-tonic manner with composition. Except for $15\%$ blend, the viscosities of other blends fall into a narrow band indicating a wide-operation window of varying blend ratio. The blends exhibited a lower viscosity than either of the two pure components. The other noticeable feature was that the blends at $70\%$ and $85\%$ ABS content had a higher G' than pure ABS, indicating an enhancement of elastic effect. The tensile yield strength of the blends followed the 'rule of mixtures' showing a decreasing value with the increase of ABS content in PC. However, the elongation-at-break and the impact strength did not appear to obey this 'rule of mixtures,' which suggests that morphology of the blends also plays a significant role in determining the properties. Indeed, scanning electron micrographs of the fracture surfaces of the different blends validate this hypothesis, and the $15\%$ blend is seen to have the most distinct morphology and correspondingly different behaviour and properties.

A STUDY ON THE SHEAR BOND STRENGTH OF COMPOMER ACCORDING TO SURFACE TREATMENT (Compomer의 치면처리방법에 따른 전단 결합 강도에 관한 연구)

  • Kim, Jin-Yong;Hong, Chan-Ui
    • Restorative Dentistry and Endodontics
    • /
    • v.23 no.1
    • /
    • pp.247-256
    • /
    • 1998
  • To evalutate the change in shear bond strength according to dentin surface treatment, 4 materials were divided into control group(A) and experimental group(B). Group A was treated according to the instruction of manufacture. Group B was treated with 32% phosphoric acid. After dentin surface treatment, each material was bonded and stored in 100% humidity during 7 days, and then, the shear bond strength was evaluated. The results were as follows: 1. In the case of treatment according to the instruction of manufacture, the shear bond strength according to material showed Z-100 to be highest with 12.42 MPa, Compoglass had the lowest shear bond strength with 4.23 MPa and there was significant difference between Compoglass and Z-100, Dyract (p<0.01). 2. The group treated with 32% phosphoric acid showed lower shear bond strength than that of the group treated according to the instruction of manufacture but there was no statistical significance. 3. As a result of observation under SEM, the fracture pattern was a mixture of cohesive and adhesive failure in group 1, and there was more adhesive failure in group 2, and in group 3 and 4 there was cohesive failure of material or tooth structure. From the results above Dyract showed shear bond strength levels between resin and resin -modified glass ionomer but Compoglass showed much lower shear bond strength than that of resin-modified glass ionomer thus indicating that even though they are the same type of material they show evident differences in physical properties. And it is thought that the treatment of dentin surface with phosphoric acid did not increase the shear bond strength, unlike enamel.

  • PDF

Physical and Mechanical Properties of Waterwaste Sludge and Stabilized Sludge (슬러지 및 안정화시킨 하수 슬러지의 물리적.역학적 특성)

  • 송창섭
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.41 no.6
    • /
    • pp.97-104
    • /
    • 1999
  • An experimental investigation was carried out to study the feasibility of using the stabiliozed sludge, as a backfill and cutoff-water materials for embankment structures. For stabilizing of sludge, hydrated lime and quick lime were used as additive, and a series of tests were performed on the sludge and the stabilized sludge to examine their physical and mechanical properties , compaction, compressive strength, hydraulic conuctivity and consolidation characteristics. From the test results, physical and mechanical properties of the stabilized sludge were improved as compared with the sludge. Especially from the viewpoint of physcial property, consolidation or settlement and cutoff-water, quick lime is more effective than the hydrated lime as a stabilization addtive. But, viewpoint of compaction and shear strength, hydrated lime is more effective than the quick lime as a atabilization additive. As a result of this study, it was found that the stabilized sludge can be developed the backfill and cutoff-water materials, improved the stabilizing method of sludge.

  • PDF

Characteristics Correlations Between Fiber-Reinforced and Interfacial Adhesion in Carbon fiber reinforced Cement composite Prepared by Slurry Method. (슬러리법에 의한 탄소섬유보강 시멘트복합체의 제조에서 보강섬유와 계면결착제와의 상관특성)

  • Choi, Eung-Kyoo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.2 no.3
    • /
    • pp.131-138
    • /
    • 2002
  • The objective of the study is to examine the characteristic correlations between reinforcing carbon fiber and interfacial adhesion agent since the interfacial adhesion strength between reinforcing carbon fiber and matrices is believed to be an essential element influencing the physical properties in carbon fiber reinforced cement composite using slurry method. The integrity of interfacial adhesion between reinforcing fiber and cement not only affects the quality of fiber reinforced cement composite but also influences to a large degree the physical properties of the cement composite when producing carbon fiber reinforced cement composite using slurry method. Having analyzed the physical properties 1.e., water content, tensile strength, flexural strength and flexural toughness of carbon fiber reinforced cement composite specimens, C-PAM(cation polyacrylamide) was determined to be an optimum interfacial adhesion agent. The study has also demonstrated that interfacial adhesion strength varies largely on the content and type of the reinforcing fiber. Judging from magnified view of the tensile shear cross-section using VMS(video microscope system), interfacial adhesion strength between reinforcing fiber and matrices is affected by the type of interfacial adhesion agent. According to the result of the experiments, C-PAM was determined to be an ideal interfacial adhesion agent when using carbon fiber in producing carbon fiber reinforced cement composite with the optimum content of carbon fiber being established.

Coconut shell waste as an alternative lightweight aggregate in concrete- A review

  • Muhammad Fahad, Ejaz;Muhammad ,Aslam;Waqas, Aziz;M. Jahanzaib, Khalil;M. Jahanzaib, Ali;Muhammad, Raheel;Aayzaz, Ahmed
    • Advances in materials Research
    • /
    • v.11 no.4
    • /
    • pp.299-330
    • /
    • 2022
  • This review article highlights the physical, mechanical, and chemical properties of coconut shells, and the fresh and hardened properties of the coconut shell concrete are summarized and were compared with other types of aggregates. Furthermore, the structural behavior in terms of flexural, shear, and torsion was also highlighted, with other properties including shrinkage, elastic modulus, and permeability of the coconut shell concrete. Based on the reviewed literature, concrete containing coconut shell as coarse aggregate with normal sand as fine showed the 28-day compressive strength between 2 and 36 MPa with the dried density range of 1865 to 2300 kg/m3. Coconut shell concretes showed a 28-day modulus of rupture and splitting tensile strength values in the ranges of 2.59 to 8.45 MPa and 0.8 to 3.70 MPa, respectively, and these values were in the range of 5-20% of the compressive strength. The flexural behavior of CSC was found similar to other types of lightweight concrete. There were no horizontal cracks on beams which indicate no bond failure. Whereas, the diagonal shear failure was prominent in beams with no shear reinforcements while flexural failure mode was seen in beams having shear reinforcement. Under torsion, CSC beams behave like conventional concrete. Finally, future recommendations are also suggested in this study to investigate the innovative lightweight aggregate concrete based on the environmental and financial design factors.