In this study, Y3Al5O12:Eu3+ red phosphors were synthesized at different temperatures using a solid state reaction method. The crystal structures, surface and optical properties of the Y3Al5O12:Eu3+ red phosphors were investigated using X-ray diffraction (XRD), field emission scanning electron microscope (FE-SEM), and photoluminescence (PL) analyses. From XRD results, the crystal structure of the Y3Al5O12:Eu3+ red phosphors was determined to be cubic. The maximum emission spectra were observed for the Y3Al5O12:Eu3+ red phosphor prepared by annealing for 4h at 1,700 ℃. The 565~590 nm photoluminescent spectra of the Y3Al5O12:Eu3+ red phosphors is associated with the 5D0 → 7F2 magnetic dipole transition of the Eu3+ ions. The intensity of the photoluminescent spectra in the red phosphors is more dominant for the magnetic dipole transition than the electric dipole transition with increasing annealing temperature. The International Commission on Illumination (CIE) coordinates of Y3Al5O12:Eu3+ red phosphors prepared by 1,700 ℃ annealing temperature are X = 0.5994, Y = 0.3647.
본 연구에서는 이종의 디지털 방사선사진술이 수복물의 방사선불투과성 비교에 적절하게 이용될 수 있는지의 여부를 평가하고, 이 기법을 이용하여 수종의 compomer 및 유동성 레진의 방사선불투과도를 측정, 비교하고자 하였다. Aluminum step wedge를 방사선사진촬영 하여 기 존의 transmission densitometer와 CD-Dent (phosphor scanning system) 및 RVG$^{(R)}$ (CCD system) 등 두 종류의 디지털 방사선사진술과의 광학밀도 상관관계를 평가하였고, 두께 2mm, 지름 5mm인 원형의 금속주형을 이용하여 Dyract$^{(R)}$ AP, Compoglass$^{(R)}$ 및 Dyract flow$^{(R)}$ 등 3종의 compomer와 Ultraseal-XT$^{(R)}$ plus$^{TM}$, Revolution$^{TM}$, Aeliteflo$^{TM}$ 및 Tetric-flow$^{(R)}$ 등 4종의 유동성 레진의 시편을 각각 5개씩 제작후 방사선불투과성을 측정하고 비교, 평가하여 다음과 같은 결과를 얻었다. 1. Aluminum step wedge를 사용한 광학밀도 측정곡선을 비교한 바, 통상적인 방사선사진술로 얻은 필름의 상에서 transmission densitometer로 방사선불투과도를 측정 한 곡선과 CD-Dent 및 RVG$^{(R)}$ 등 디지털 방사선사진술로 얻은 상에서 CADIA로 불투과도를 측정한 곡선들 사이에서 각각 매우 높은 역상관관계가 나타났다(${\gamma}$=-0.95, ${\gamma}$=-0.98 ; p<0.05). 2. 모든 수복채 공히 상아질과 유사하거나 높은 방사선불투과도를 나타내었고 (p<0.05), compomer인 Dyract$^{(R)}$ AP와 Compoglass$^{(R)}$, 그리고 유동성 레진인 Tetric-flow$^{(R)}$는 통상적인 방사선사진술 및 2종의 디지털 방사선사진술에서 공히 유동성 레진인 Revolution$^{TM}$과 Aeliteflo$^{TM}$, 그리고 상아질에 비해 유의하게 높은 방사선불투과도를 나타내었다 (p<0.05). 3. Compomer인 Dyract$^{(R)}$ AP와 Compoglass$^{(R)}$, 그리고 유동성 레진인 Tetric-flow$^{(R)}$는 통상적인 방사선사진술 및 CD-Dent 디지털 방사선사진술에서 공히 법랑질에 비해 높은 방사선불투과도를 나타내었고(p<0.05), compomer인 Dyract flow$^{(R)}$는 통상적인 방사선사진술에서만 법랑질에 비해 높은 방사선불투과도를 나타내었다(p<0.05).
Carbon nanotubes (CNTs) belong to an ideal material for field emitters because of their superior electrical, mechanical, and chemical properties together with unique geometric features. Several applications of CNTs to field emitters have been demonstrated in electron emission devices such as field emission display (FED), backlight unit (BLU), X-ray source, etc. In this study, we fabricated a CNT cathode by using filtration processes. First, an aqueous CNT solution was prepared by ultrasonically dispersing purified single-walled CNTs (SWCNTs) in deionized water with sodium dodecyl sulfate (SDS). The aqueous CNT solution in a milliliter or even several tens of micro-litters was filtered by an alumina membrane through the vacuum filtration, and an ultra-thin CNT film was formed onto the alumina membrane. Thereafter, the alumina membrane was solvated by acetone, and the floating CNT film was easily transferred to indium-tin-oxide (ITO) glass substrate in an area defined as 1 cm with a film mask. The CNT film was subjected to an activation process with an adhesive roller, erecting the CNTs up to serve as electron emitters. In order to measure their luminance characteristics, an ITO-coated glass substrate having phosphor was employed as an anode plate. Our field emitter array (FEA) was fairly transparent unlike conventional FEAs, which enabled light to emit not only through the anode frontside but also through the cathode backside, where luminace on the cathode backside was higher than that on the anode frontside. Futhermore, we added a reflecting metal layer to cathode or anode side to enhance the luminance of light passing through the other side. In one case, the metal layer was formed onto the bottom face of the cathode substrate and reflected the light back so that light passed only through the anode substrate. In the other case, the reflecting layer coated on the anode substrate made all light go only through the cathode substrate. Among the two cases, the latter showed higher luminance than the former. This study will discuss the morphologies and field emission characteristics of CNT emitters according to the experimental parameters in fabricating the lamps emitting light on the both sides or only on the either side.
AISI 4600계 철 분말에 F$e_2$P 분말을 사용하여 인(P)을 0~1.0% 그리고 흑연 분말을 사용하여 탄소를 0~0.8% 첨가하여 회전혼합기를 사용하여 혼합하였다. 흔합분말을 양단압금형에서 800MPa로 가압하여 성형체를 만들었다. 성형체는 진공 또는 수소와 질소 혼합가스 분위기에서 115$0^{\circ}C$에서 30분간 소결하였다. 소결체를 연마하고 2% 질산용액으로 에칭하였다. 소결체 조직을 Image Analyzer와 금속현미경으로 관찰하였다. 밀도는 ASTM B3l2로, 경도는 미세 비커스경도기로 측정하였다. 얻어진 결과는 다음과 같다. (1) F$e_2$P 첨가량이 증가하면, 소결체 조직은 치밀화되고 입자 크기는 더 커졌다. (2) $Fe_2P량과$ 함께 기공의 형상은 둥글고, 그 숫자는 감소하였으나 평균크기는 더 커졌다. (3) 입자의 크기는 F$e_2$P와 흑연분말을 동시에 첨가한 경우가 각각 단독으로 첨가한 경우보다 커졌다. (4) 미세조직에 미치는 소결분위기의 영향은 거의 없었다. (5) 경도는 인과 탄소량이 증가하면 상승하였다.
본 연구에서는 간단 고상합성법(solid state reaction method)을 이용하여 $Yb^{3+}$, $Er^{3+}$ 이온이 동시도핑된 $NaGd(MoO4)_2$ ($NaGd(MoO_4)_2:Yb^{3+}/Er^{3+}$)를 성공적으로 합성하였으며, 결정구조 및 광학적 특성을 면밀히 분석하였다. 980nm의 근적외선 레이저를 합성된 NaGd(MoO4)2 파우더에 조사하였을 때 $NaGd(MoO_4)_2:Yb^{3+}/Er^{3+}$ 분말은 540 및 550 nm 부근에서 강한 녹색 발광과 함께 650 및 670 nm 부근에서의 매우약한 적색 발광을 하였으며 이러한 업컨버젼 발광 현상은 $Er^{3+}$ 이온 내의 infra 4f transition에 의한 현상임을 확인할 수 있었다. 또한, $Yb^{3+}$ 및 $Er^{3+}$ 이온의 최적 도핑 농도는 각각 (10.0/10.0 mol%)로 확인되었으며, 그에 따른 upconversion 발광 메커니즘에 대하여 상세히 논의하였다.
Sol-gel method로 합성한 anatase상의 $TiO_2$와 Yb와 Er을 codoping한 $TiO_2:Yb^{3+},\;Er^{3+}$ 파우더의 열적안정성과 이에 따른 광촉매 특성의 변화를 비교하였다. XRD 분석을 통하여 $TiO_2$ 결정성 및 상변화에 $Yb^{3+},\;Er^{3+}$ ions이 미치는 영향을 온도에 따라 비교하였으며 anatase $TiO_2$와 rutile $TiO_2$의 광학적 성질을 UV-Vis을 통하여 비교하였다. UV-Vis 분석결과 anatase $TiO_2:Yb^{3+},\;Er^{3+}$ ions도핑에 의하여 $TiO_2$의 밴드갭이 미세하게 감소함을 확인하였고 이를 통해 광촉매 작용을 향상시킬 수 있음을 확인하였다. $Yb^{3+}$ 이온과 $Er^{3+}$ 이온이 도핑된 $TiO_2:Yb^{3+},\;Er^{3+}$ 파우더를 980 nm에서 PL 분석하여 녹색 및 적색 형광을 하는 up-converting 형광특성을 분석하였다.
$Eu^{3+}$- or $Sm^{3+}$-doped $La_2MoO_6$ phosphors were synthesized with different concentrations of activator ions via a solid-state reaction. The X-ray diffraction patterns exhibited that crystalline structures of all the phosphors were tetragonal systems with the dominant peak occurring at (103) plane, irrespective of the concentration and the type of activator ions. The crystallites showed the pebble-like crystalline shapes and the average crystallite size increased with a tendency to agglomerate as the concentration of $Eu^{3+}$ ions increased. The excitation spectra of $Eu^{3+}$-doped $La_2MoO_6$ phosphors contained an intense charge transfer band centered at 331 nm in the range of 250-370 nm and three weak peaks at 381, 394, and 415 nm, respectively, due to the $^7F_0{\rightarrow}^5L_7$, $^7F_0{\rightarrow}^5L_6$, and $^7F_0{\rightarrow}^5D_3$ transitions of $Eu^{3+}$ ions. The emission spectra under excitation at 331 nm exhibited a strong red band centered at 620 nm and two weak bands at 593 and 704 nm. As the concentration of $Eu^{3+}$ increased from 1 to 20 mol%, the intensities of all the emission bands gradually increased. For the $Sm^{3+}$-doped $La_2MoO_6$ phosphors, the emission spectra consisted of an intense emission band at 607 nm arising from the $^4G_{5/2}{\rightarrow}^6H_{7/2}$ transition and three relatively small bands at 565, 648, and 707 nm originating from the $^4G_{5/2}{\rightarrow}^6H_{5/2}$, $^4G_{5/2}{\rightarrow}^6H_{9/2}$, and $^4G_{5/2}{\rightarrow}^6H_{11/2}$ transitions of $Sm^{3+}$, respectively. The intensities of all the emission bands approached maxima when concentration of $Sm^{3+}$ ions was 5 mol%. These results indicate that the optimum concentrations for highly-luminescent red and orange emission are 20 mol% of $Eu^{3+}$ and 5 mol% of $Sm^{3+}$ ions, respectively.
A series of Dy3+, Sm3+, and Dy3+/Sm3+ doped Gd2WO6 phosphors were synthesized by the conventional solid-state reaction. The X-ray diffraction patterns revealed that all of the diffraction peaks could be attributed to the monoclinic Gd2WO6 crystal structure, irrespective of the type and the concentration of activator ions. The photoluminescence (PL) excitation spectra of Dy3+-doped Gd2WO6 phosphors contained an intense charge transfer band centered at 302 nm in the range of 240-340 nm and two weak peaks at 351 and 386 nm. Under an excitation wavelength of 302 nm, the PL emission spectra consisted of two strong blue and yellow bands centered at 482 nm and 577 nm. The PL emission spectra of the Sm3+-doped Gd2WO6 phosphors had a series of three peaks centered at 568 nm, 613 nm, and 649 nm, corresponding to the 6G5/2 → 6H5/2, 6G5/2 → 6H9/2, and 6G5/2 → 6H11/2 transitions of Sm3+, respectively. The PL emission spectra of the Dy3+- and Sm3+-codoped Gd2WO6 phosphors showed the blue and yellow emission lines originating from the 4F9/2 → 6H15/2 and 4F9/2 → 4H13/2 transitions of Dy3+ and reddish-orange and red emission bands due to the 4G5/2 → 6H7/2 and 4G5/2 → 6H9/2 transitions of Sm3+. As the concentration of Sm3+ increased from 1 to 15 mol%, the intensities of two PL spectra emitted by the Dy3+ ions gradually decreased, while those of the three emission bands due to the Sm3+ ions slowly increased, thus producing the color change from white to orange. The CIE color coordinates of Gd2WO6:5 mol% Dy3+, 1 mol% Sm3+ phosphors were (0.406, 0.407), which was located in the warm white light region.
An, Seo-Young;An, Chang-Hyeon;Choi, Karp-Sik;Huh, Kyung-Hoe;Yi, Won-Jin;Heo, Min-Suk;Lee, Sam-Sun;Choi, Soon-Chul
Imaging Science in Dentistry
/
제48권2호
/
pp.97-101
/
2018
Purpose: This study evaluated the radiopacity of contemporary luting cements using conventional and digital radiography. Materials and Methods: Disc specimens (N=24, n=6 per group, ø$7mm{\times}1mm$) were prepared using 4 resin-based luting cements (Duolink, Multilink N, Panavia F 2.0, and U-cem). The specimens were radiographed using films, a complementary metal oxide semiconductor (CMOS) sensor, and a photostimulable phosphor plate (PSP) with a 10-step aluminum step wedge (1 mm incremental steps) and a 1-mm-thick tooth cut. The settings were 70 kVp, 4 mA, and 30 cm, with an exposure time of 0.2 s for the films and 0.1 s for the CMOS sensor and PSP. The films were scanned using a scanner. The radiopacity of the luting cements and tooth was measured using a densitometer for the film and NIH ImageJ software for the images obtained from the CMOS sensor, PSP, and scanned films. The data were analyzed using the Kruskal-Wallis and Mann-Whitney U tests. Results: Multilink (3.44-4.33) showed the highest radiopacity, followed by U-cem (1.81-2.88), Panavia F 2.0 (1.51-2.69), and Duolink (1.48-2.59). The $R^2$ values of the optical density of the aluminum step wedge were 0.9923 for the films, 0.9989 for the PSP, 0.9986 for the scanned films, and 0.9266 for the CMOS sensor in the linear regression models. Conclusion: The radiopacities of the luting materials were greater than those of aluminum or dentin at the same thickness. PSP is recommended as a detector for radiopacity measurements because of its accuracy and convenience.
ZnS:Cu,Cl 형광체를 이용하여 ITO/glaas 기판위에 스크린인쇄법으로 적층형과 혼합형 구조로된 2종류의 교류전계 발광소자를 제작한 후 인가전압과 주파수에 따른 광학적, 전기적 특성을 조사, 비교하였다. 적층헝의 경우 발광휘도는 400Hz, 200V 구동전압에서 약 55 cd/$\m^2$를 나타내었다. 인가전압의 주파수를 400Hz에서 30Hz로 증가시킬 경우 휘도는 420 cd/$\m^2$로 크게 향상되었다. 혼합형의 경우 400Hz의 주파수에서 문턱전압은 45V이었고, 200V, 30KHz 주파수의 동작조건에서 최대휘도는 670 cd/$\m^2$ 이었다. 휘도-전압 특성 측정결과 적층형구조 보다 혼합형 소자구조에서 발광강도가 약 1.5배 증가하였다. 주파수에 따른 주발광 파장의 변화는 양쪽시료 모두 유사하게 나타났다. 1KHz이하의 저주파에서는 652 nm의 청녹색 발광과장을 나타내었으며 5KHz이상에서는 452 nm과장의 청색발광을 나타내었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.