The formation of a thicker hard alloyed layer have been investigated on the surface of aluminum cast alloy (AC2B) by PTA overlaying process with Cr, Cu and Ni motel powders under the condition of overlaying current 125-200A. overlaying speed 150 mm/min and different powder feeding rate 5-20 g/min. In addition the characteristics of hardening and wear resistance of alloyed layer here been examined in relation to the microstructure of alloyed layer. Main results obtained were summarized as follows: 1) There was an optimum overlaying condition to get a good alloyed layer with smooth surface. This good layer became easy to be formed as increasing overlaying current and decreasing powder feeding rate under a constant overlaying speed. 2) Cu powder was the most superior one in metal powders used due to a wide optimum overlaying condition range, uniform hardness distribution of Hv250-350, good oar resistance and freedom from cracking in alloyed layer with fine hyper-eutectic structure. 3) On the contrary, irregular hardness distribution was usually obtained in Cr ar Ni alloyed layers of which hardness was increased as Cr or Ni contents and reached to maximum hardness of about Hv400-850 at about 60wt%cr or 40wt%Ni in alloyed layer. 4) Cracking occurred in Cr or Ni alloyed layers with higher hardness than Hv250-300 at mere than 20-25wt% of Cr or Ni contents in alloyed layer. Porosity was observed in all alloyed layers but decreased by usage of spherical powder with smooth surface.
Proceedings of the Korean Society for Technology of Plasticity Conference
/
2009.10a
/
pp.358-361
/
2009
The increasing interest in the surface modification technology by the plasma transferred arc overlaying process in the material processing is placing stringent demands on the manufacturing techniques and performance requirements, and the manufacture employs the high quality and efficiency plasma transferred arc overlaying technology. This paper covers recent technical trends of plasma transferred arc overlaying technology including the COMPENDEX DB analysis.
An overlaying of the seating surfaces of engine valves by OAW, GTAW or PTA weldings are common practice. The OAW method of a lower torch energy density compared to GTAW and PTA methods produces smoother deposits but the pain size at the vicinity of the interface is increased remarkably up to $30~50{\mu\textrm{m}}$ (that of base metal is about $10\mu\textrm{m}$). It's grain coarsening and the solute dilution are related to the decarburizing during OAW could be minimized by reducing the preheating temperature and by maintaining the carbide precipitates in base metal prior to welding. The formation of columnar structures and carbide precipitation zone in the vicinity of the GTAW welded interface, because of the high heat concentration, causes weakened zone on the valve seat face. The width of the reaction boundary zone is about $50\mu\textrm{m}$ for PTA and GTAW overlaying, and about $150\mu\textrm{m}$ for OAW welding. The smaller width of the reaction boundary zone is the less the solute-dilution rate. Thereby PTA welding may be recommended for overlaying of the seating surfaces.
Effect of Cr, Cu and Ni metal powders addition on the alloyed layer of aluminum alloy (AC2B) has been investigated with the plasma transferred arc (PTA) overlaying process. The overlaying conditions were 125-200A in plasma arc current, 150mm/min in process speed and 5-20g/min in powder feeding rate. Main results obtained are summarized as follows: 1) It was made clear that formation of thick surface alloyed layer on aluminum alloy is possible by PTA overlaying process. 2) The range of optimum alloying conditions were much wider in case of Cu and Ni powder additions than the case of Cr powder addition judging from the surface appearance and the bead macrostructure. 3) Alloyed layer with Cu showed almost the homogeneous microstructure through the whole layer by eutectic reaction. alloyed layers with Cr and Ni showed needle-like and agglomerated microstructures, the structure of which has compound layer in upper zone of bead by peritectic and eutectic-peritectic reactions, respectively. 4) Microconstituents of the alloyed layer were analyzed as A1+CrA $l_{7}$ eutectics, C $r_{2}$al sub 11/, CrA $l_{4}$, C $r_{4}$A $l_{9}$ and C $r_{5}$A $l_{*}$ 8/ for Cr addition, Al+CuA $l_{2}$(.theta.) eutectics and .theta. for Cu addition, and Al+NiA $l_{3}$ eutectics. NiA $l_{3}$, N $i_{2}$A $l_{3}$ and NiAl for Ni addition. 5) Concerning defect of the alloyed layer, many blow holes were seen in Cr and Ni additions although there was lesser in Cu addition. Residual gas contents in blow hole for Cu and Ni alloyed layer were confirmed as mainly $H_{2}$ and a littie of $N_{2}$ Cracking was observed in compound zone of the alloyed layer in case of Cr and Ni addition but not in Cu alloyed layer.r.r.
Proceedings of the Korean Society of Surveying, Geodesy, Photogrammetry, and Cartography Conference
/
2002.04a
/
pp.25-33
/
2002
Historical maps are precious materials, which show spatial distribution of land use, streets and so on at the time when the maps were produced. In analysis of historical maps, the most practical method is to compare them with the present ones, for instance by overlaying them. However, the low precision, in the geometrical sense, of the historical maps makes the task of comparison very difficult. This drawback brings us the idea to incorporate the historical maps into GIS after rubber-sheet transformation, i.e. geometric correction, of them. It makes comparing and overlaying multiple maps from different time periods. Furthermore, it gives map-scales to the historical maps, which are not in general represented on the old maps, and if we allow ourselves to ignore the changes in terrain from past to present, it will make overlaying of present contour lines on the historical maps. As a result, we can bring the points of view of quantitative consideration and three-dimensional visualization into analyses of historical map. We have addressed incorporating historical maps produced in Edo period (1603-1867) in Japan into our GIS for Tokyo. This article shows the outline of our procedures and some applications, e.g., overlaying different maps from Edo period to present, quantitative analyses of land use in Edo, and visualization of landscape of Edo.
The thick and hard alloyed layer was formed on the surface of Aluminum Cast Alloy(AC2B) by PTA overlaying process with Cr, Cu and Ni metal powders under the condition of overlaying current 150A, overlaying speed 150mm/min and different powder feeding rate 5-20g/min. The characteristics of hardening and were resistance of alloyed layer have been investigated in relation to microstructure of alloyed layer. As a result, it was made clear that Cu powder was the most superier one in three metal powders used due to an uniform hardness distribution of Hv 250-350, good wear resistance and freedom from cracking in alloyed layer of which microstructure consisted of hypereutectic. On the contrary, irregular hardness distribution was usually obtained in Cr or Ni alloyed layers of which hardness was increased as Cr or Ni contents and reached to maximum hardness of about Hv 400-850 at about 60wt% Cr or 40wt% Ni in alloyed layer. However the cracking occurred in these alloyed layers with higher hardness than Hv 250-300 at more than 20-25wt% of Cr or Ni contents in alloyed layer. Wear rate of alloyed layer was decreased to 1/10 in Cu alloyed layer and 1/5 or 1/3 in Cr or Ni alloyed layer with same hardness of about Hv 300 in comparison with that of base metal at higher sliding speed.
The Journal of Korean Institute of Communications and Information Sciences
/
v.35
no.7B
/
pp.1009-1017
/
2010
Offering of different attractive opportunities by different wireless technologies trends the convergence of heterogeneous networks for the future wireless communication system. To make a seamless handover among the heterogeneous networks, the optimization of the power consumption, and optimal selection of interface are the challenging issues. The access of multi interfaces simultaneously reduces the handover latency and data loss in heterogeneous handover. The mobile node (MN) maintains one interface connection while other interface is used for handover process. However, it causes much battery power consumption. In this paper we propose an efficient interface selection scheme including interface selection algorithms, interface selection procedures considering battery power consumption and user mobility with other existing parameters for overlaying networks. We also propose a priority based network selection scheme according to the service types. MN‘s battery power level, provision of QoS/QoE and our proposed priority parameters are considered as more important parameters for our interface selection algorithm. The performances of the proposed scheme are verified using numerical analysis.
Recently, it is necessary fir surface materials to be low cost and to keep well endurable and wear in machinery field. Since most good materials with endurance and wear are expensive, they are being studied hard to modify to surface materials with endurance and wear, which overlay with the surface membrane completely. One of them is PTA(Plasma Transferred Arc Overlaying Process) method, which gets into the spotlight. It is thought to be an optimum method, since this method of overlays properly materials with about 3∼5cm surface membrane. It is necessity for the modified materials with endurance and wear to improve within the agricultural environment. Therefore, this research was used the PTA method to endure and wear a material. This method proved to be a reliable method for overlaying the membrane on the materials of an economical agricultural machinery.
A computer top table was manufactured with the solid wood wastes that has been landfilled, combustion or burnt as a fuel at the present time. The computer table is different in form and size to that of existing fixed rectangular. It is idea1 product not only convenient and functional to use and beautiful design but also processing Performance of edge area and overlaying properties. The main technologies to develop this computer top table are plan for moulder to mould the Product and producing, molding the most suitable material and composition, suitable adhesives selecting and synthetic technology, investigation for the moulding conditions such as temperature, time etc, adequate overlaying materials selecting and overlaying technology have to be chocked.
Effect of Si metal powders addition with the plasma transferred arc(PTA) overlaying process on characteristics of the alloyed layer in aluminum alloy(A5083) has been investigated. The overlaying conditions were 175-250A in plasma arc current, 500mm/min in travel speed, the 5-20g/min in powder feeding rate. Main results obtained are summarized as follows. 1)Sufficient size of molten pool on surface of base metal was required for forming an alloyed layer; in a fixed travel, the formation of alloyed layer with clear and beautiful surface depend upon the plasma arc current and powder feeding rate; the greater plasma arc current and the smaller powder feeding rate were, the better bead was formed. Optimum alloyed conditions by which an excellent alloyed bead obtained was 225A in plasma arc current. PTA process made it possible to form an alloyed layer with up to 67wt% Si. 2)Microstructure in the alloyed layer was in accord with prediction from the Al-Si phase diagram 3)The hardness of the alloyed layer increased in proportion to Si content. 4)As volume fraction of primary Si increased, the specific wearness of the alloyed layer was significantly improved. However, no further improvement was found when the volume fraction was greater than about 30%. 5)Utilizing the PTA process, a crack free alloyed layer with maximum hardness of about Hv 310 could be obtained.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.