• 제목/요약/키워드: nucleation sites

검색결과 99건 처리시간 0.024초

수용액 분사법에 의한 용융아연 도금강판의 미니스팡글 형성 (Minispangling of a Hot Dip Galvanized Sheet Steel by a Solution Spray Method)

  • 김종상;전선호;박정렬
    • 한국표면공학회지
    • /
    • 제27권3호
    • /
    • pp.149-157
    • /
    • 1994
  • The formation of spangles on a hot dip galvanized sheet steel by spray cooling the molten zinc coating with air, water and 2.0wt% $NH_4H_2PO_4$ solution has been studied performing laboratory experiments, and their coating properties have been evaluated. Minimized spangles were easily formed by mist spraying the solution for 1 second at the low nozzle spray pressure onto the molten zinc at 420~$422^{\circ}C$ because the solute $NH_4H_2PO_4$ in the sprayed solution imparted a highly rapid cooling effect to the coating through its endothermic de-composition reactions and because the decomposed products acted as numerous nucleation sites for the mini-mized spangles on the coating. Good surface appearances sand sound coating properties were obtained on this coating. Only regular spangles were formed on the coating by the forced convective air cooling. At the high nozzle spray pressure, zero spangles were formed on the coating by the pure water spray cooling. However, the coating had a dull and rough surface with craters sand cracks.

  • PDF

구상흑연주철(球狀黑鉛鑄鐵)의 3상혼합조직(相混合組織)의 변태거동(變態擧動)에 관(關)한 연구(硏究) (A Study on the Transformation Behaviors of a Multi-phase (Ferrite-Bainite-Martensite) in Ductile Cast Iron)

  • 김석원;김동건;유선경
    • 한국주조공학회지
    • /
    • 제11권5호
    • /
    • pp.406-413
    • /
    • 1991
  • Ductile cast iron(DCI) with a multi-phase(ferrite-bainite-martensite) structures was produced by various special heat treatment. Intercritical heat treatment(I. C.), intermediate heat treatment(I. M.) and step quenching(S. Q.) were used to strengthen and toughen the fracture initiation sites such as graphite-marix interfaces and eutectic cell boundaries in DCI. The purpose of this study was to investigate of DCI by the special heat treatment. (I. C., I. M., and S. Q.) At a result, bainite nucleation rate at higher temperature was higher than that of at lower temperature, and shapes of bainite and martensite became bar /spheroidal type with increase of isothermal transformation time.

  • PDF

과공정 Al-Si합금에서의 초정 및 공정 Si의 동시 미세화 (Simultaneous Refinement of Primary and Eutectic Si in Hypereutectic Al-Si Alloys)

  • 박재영;이재상;나형용
    • 한국주조공학회지
    • /
    • 제15권3호
    • /
    • pp.262-271
    • /
    • 1995
  • It is well known what is impossible to refine primary and eutectic Si simultaneously by addition of both Cu-P and Sr(or Na). Because of the formation of compound $Sr_3P_2(or Na_3P)$ in the melt, in the result, both effects disappear. In this study Al-Cu-P alloy that comprises AlP compounds inside is added in the melt with Sr simultaneously. As AlP compounds that act on nucleation sites of primary Si are not formed but added directly an the melt, it is difficult to form $Sr_3P_2$ by reaction with Sr. Therefore it is possible to refine primary and eutectic Si simultaneously in the general casting process by use of Al-Cu-P alloy and Sr.

  • PDF

Alumina substrate 상의 무전해 도금층의 밀착력에 관한 연구 (A study on adhesion strength of electroless plated deposits on Alumina substrate)

  • 조용균;안균영;박용수
    • 한국표면공학회지
    • /
    • 제24권4호
    • /
    • pp.187-195
    • /
    • 1991
  • Adhesion strength of electroless-plated Ni, Ni-P and Cu deposites on alumina substrate has been studied. Grain boundary spaces produced on the substrate surface by etching treatment provided anchoring sites for enhancing the adhesion strength. Adhesion strengths of Ni-P and Ni deposit were higher than that of Cu deposit, because of higher initial nucleation rates than the latter. The electroless-plated Ni-P and Ni underlayer improved the adhesion strength of the Cu deposit. In could be attributed to the enhanced adhesion between the substrate and those underlayers as well as the satisfactory adhesion between Cu deposits and those underlayers. Heat treatment was also conducted in order to enhance the adhesion strength of Cu layer. The strength was enhanced by about 19% when the treatment was conducted at $150^{\circ}C$ for 2 hours. The enhancement was attributed to relief of internal stress and release of hydrogen.

  • PDF

The simulation of hydration of Portland cement blended with chemical inert filler

  • Xiaoyong, Wang;Lee, Han-Seung
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2008년도 춘계 학술발표회 제20권1호
    • /
    • pp.1041-1044
    • /
    • 2008
  • The addition of chemical inert filler in blended cement, such as limestone or chemical inert silica fume, will produce a physical effect on cement hydration. Due to the high surface area of inert filler in the mixtures, it provides sites for the nucleation and growth of hydration products, thus improving the hydration rate of cement compounds and consequently increasing the strength at early age. This paper proposes a model of hydration of Portland cement blended with chemical inert filler. This model considers the influence of water to cement ratio, cement particle size, cement composition and addition of chemical inert filler on hydration. The heat evolution, degree of hydration and porosity are obtained as accompanied results in hydration process. The prediction results agree well with experiment results.

  • PDF

Microwave Plasma CVD에 의한 Diamond 박막의 성장 (The Study on Growls of diamond thin films Synthesized by Microwave Plasma Enhanced Chemical Vapor Deposition)

  • 이병수;이상희;박구범;박종관;박상현;유도현;이덕출
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 추계학술대회 논문집
    • /
    • pp.373-376
    • /
    • 1997
  • Diamond thin films were deposited on P-type(100) Si wafers using MPECVD. Prior to deposition, mechanical scretching was done to improve density of nucleation sites with diamond paste of 0.25${\mu}{\textrm}{m}$ size. Diamond films were deposited under the following conditions : methane concentration of 0.5~5%, oxygen concentration of 0~70%, process pressure of 70Torr, process temperature of 900~95$0^{\circ}C$, and deposition time 5hrs. The changes of the morphology and the growth rates of the deposits with the experimental conditions are expriend by Scanning Electron Microscopy. Raman Spectroscopy and X-ray Diffraction method.

  • PDF

Effects of Flux Treatment on the Glass Forming Ability and Magnetic Properties of Fe-based Ternary Amorphous Alloys

  • Zuo, Mingqing;Yi, Seonghoon
    • 한국주조공학회지
    • /
    • 제40권4호
    • /
    • pp.113-117
    • /
    • 2020
  • A series of Fe-P-B and Fe-Si-B amorphous alloys with high Fe contents exceeding 90 wt.% was successfully prepared by combining flux treatment and melt-spinning technique. The effects of Fe content and the flux treatment on the thermal and magnetic properties of amorphous alloys were studied. The glass-forming ability and the thermal stability of amorphous ribbons can be improved by a flux treatment, revealing the effective removal of heterogeneous nucleation sites in the ribbons through the flux treatment. It was found that Fe-Si-B ribbons exhibit higher saturation magnetization levels than Fe-P-B ribbons.

High Catalytic Activity and Recyclability of Graphene Oxide Based Palladium Nanocomposites in Sonogashira Reaction

  • Kim, Bo Hyun;Park, Joon B.
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.139.1-139.1
    • /
    • 2013
  • Graphene and graphene oxide (GO) have been modified with palladium nanoparticles (Pd NPs) to develop high performance catalysts for the Sonogashira cross coupling reaction. To understand catalytic performance of Pd NPs on graphene (Pd/G) and Pd NPs on GO (Pd/GO), we monitored their morphological and electronic structural changes before/after Sonogashira reaction using FT-IR, XRD, XPS, and XAFS. Here, we demonstrate that both Pd/G and Pd/GO show high catalytic efficiency toward the Sonogashira reaction, but only Pd/GO revealed excellent recyclability. The remarkable catalytic efficiency of both catalysts is attributed to the high degree of the Pd NP dispersions on supports and thus smaller Pd NPs can provide highly reactive low coordinated Pd atoms. However, we attributed the excellent recyclability of Pd/GO to the presence of oxygen functionalities on GO, which can provide nucleation sites for the detached Pd atoms during the Sonogashira reaction and prevent agglomeration of the Pd NPs since the oxygen functional groups are very reactive to mobile Pd adatoms.

  • PDF

정전 대전된 액적에 의한 용융 아연 도금층의 응고 방법 (Solidification of Hot-Dip Galvanized Layer by Electrostatically Charged Aerosol Particles)

  • 김상헌;김형민;정원철;정원섭
    • 한국표면공학회지
    • /
    • 제33권4호
    • /
    • pp.233-240
    • /
    • 2000
  • A novel electrostatic spraying method to solidify molten zinc coating layer was studied by SEM and measurement of sample's temperature. The sprayed droplets also served as nucleation sites in the solidification reaction of molten zinc but might leave the pitting mark by impinging on its surface especially at high spray pressure. Our experimental results showed that electric field could change the sprayed particle trajectories and assist the fine droplets to attach on the surface. Thus, by reducing the spray pressure and by applying the electric voltage higher than -20 KV to charge the droplets electrostatically, we could produce the spangle free galvanized coating layer without pitting.

  • PDF

용융아연도금강판의 표면특성에 미치는 조질압연 조업조건의 영향 (Effect of Skinpassing Conditions on the Surface Characteristics of Hot-dip Galvanized Steel Sheets)

  • 전선호
    • 한국표면공학회지
    • /
    • 제34권4호
    • /
    • pp.327-336
    • /
    • 2001
  • The skinpassing conditions such as roll type, roll force and roll roughness of the work roll were evaluated to give the surface properties of the galvanized steel sheets that were required for automotive and to get rid of the surface defects that caused with the bad control of galvanized coating process parameters. The surface defects of the galvanized steel sheets such as the ripple mark and the scratch were completely removed as the roll force of SPM work roll was increased and the amount of the transfer of roll surface texture to the strip was also gained a lot. The image clarity of electro discharge textured (EDT) coated steel sheets before and after painting was higher than that of the bright (BRT) and shot blasted (SBT) coated steel sheets because of higher PPI value, lower waviness and uniform surface pattern. Since micro-craters transferred on the surface of the galvanized steel sheets played a role of nucleation sites of chromate reaction, Increase of micro-craters was bring to better corrosion resistance with the increase of the roll force and the use of EDT roll at the skin pass mill.

  • PDF