The Growth of $MgO:LiNbO_3$ Single Crystal by Czochralski Method and its Density Measurement (Czochralski법에 의한 $MgO:LiNbO_3$단결정 성장과 밀도 측정)

  • Kim, Il-Won;Park, Bong-Chan;Kim, Gap-Jin
    • Korean Journal of Crystallography
    • /
    • v.4 no.2
    • /
    • pp.74-85
    • /
    • 1993
  • Single crystals of LiNbO3 have found extensive application in electro-optic and nonlinear optic devices. However, laser-induced refartive index inhomogeneities, which have been labeled opical damage impose limits on device optical damage in LiNbO3 is imporved if more than 4.5 rml% MgO is added to the melt The laser damage thrueshold increased as much as 100 times better then that of undoped crystals. The MgO doped cystal has thus been urterlsiv81y studied since then. In the study, Mgo:LiNbOs(MLA) single crystals dopsd with 0, 2.5, 5.0, 7.5, 10.0 mol% MgO have been grown by the czocrualski technique. The metls were prepared in the platinum crluible and 15∼20mm diameter crystals were grown with a length of 20∼30mm in a resitance heater. The growth rate was 2.5mm/hr, the rotation speed 15rpn. Before sawing MLN single crystals were annealed for 24 hours under atmosphere at a temperature of 1080℃. After sawing, we have found an annual ring cross section of MNA crystals only in the direction of perpendicilar to the c-axis. Nonuniform dispusion of MgO was pointed out that the cuties of the state of oxide were strongly affected by oxygen partial pressure in.

  • PDF