• Title/Summary/Keyword: mineral synthesis

Search Result 214, Processing Time 0.026 seconds

X-ray Photoelectron Spectroscopy Study of LaFeO3 Powders Synthesized by Solution Combustion (용액연소법으로 제조한 LaFeO3의 XPS 특성)

  • Hwang, Yeon;Kang, Dae-Sik;Park, Mi-Hye;Cho, Sung-Baek
    • Korean Journal of Materials Research
    • /
    • v.18 no.6
    • /
    • pp.313-317
    • /
    • 2008
  • [ $LaFeO_3$ ] powders were synthesized using a method involving solution combustion, and the surface properties of these powders were examined by x-ray photoelectron spectroscopy. As the amount of fuel increased during the synthesis, the $LaFeO_3$ powders became amorphous with a large plate-like shape. It was found that the O 1s spectra were composed of two types of photoelectrons by deconvolutioning the spectra. Photoelectrons with higher binding energy come from adsorbed oxygen ($O^-$) whereas those with lower energy come from lattice oxygen ($O^{2-}$). The ratio of adsorbed and lattice oxygen increased as the ratio of the fuel and nitrate (${\Phi}$) increased. The binding energy of both types of oxygen increased as ${\Phi}$ increased due to the formation of carbonates.

Synthesis of zeolite A from serpentine (사문석으로부터 제올라이트 A의 합성)

  • 김동진;정헌생;이재천;김인회;이자현
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.10 no.1
    • /
    • pp.73-79
    • /
    • 2000
  • Highly porous amorphous silica obtained from a serpentine mineral by hydrochloric acid treatment was used to produce a zeolite A through the hydrothermal reaction under atmospheric pressure. An optimum synthesis condition of the zeolite A was achieved at $80^{\circ}C$ for two hours with a mole ratio of $Na_2O/SiO_2$1.5. Additionally, it was found that a hydroxysodalite zeolite was formed under the experimental conditions over the reaction temperature of $80^{\circ}C$ and the reaction time of 120 minutes even though the crystallization of zeolite proceeds rapidly as the reaction temperature and the alkalinity becomes higher.

  • PDF

Recombinant Human L-ferritin from Saccharomyces cerevisiae: Molecular Characterization and Synthesis of Iron Oxide Nanoparticles (효모에서 생산한 재조합 human L-ferritin의 생화학적 특성 및 나노입자의 철산화물 합성)

  • Kim, Kyung-Suk
    • KSBB Journal
    • /
    • v.26 no.2
    • /
    • pp.119-125
    • /
    • 2011
  • In the synthesis of nanoparticles, much attention has been paid to regulating the particle size. There has been a possible evident that using the central cavity (core) of the protein ferritin has a greatly significant influence on it because the core can generate the nanometer-sized mineral particles of variable metal ions. In this report, recombinant human L-ferritins produced from Saccharomyces cerevisiae were purified and their molecular properties were characterized. The cDNA for human ferritin L chain was also expressed in another host such as Escherichia coli, and the properties of recombinant L-ferritins were compared. From isoelectric focusing experiment, the L-ferritin from the recombinant yeast showed no indication of N-glycosylation. Some post-translational modifications other than N-glycosylation were speculated in the L-ferritins from yeast. A difference was made in the L-ferritins in their iron uptake rates and the initial rate of the L-ferritin from yeast was slightly increased. The reconstitution yield and size distribution of the core minerals were analyzed in the L-ferritins by transmission electron microscopy. The L-ferritin from yeast with higher reconstitution yield (54.5%) showed slightly larger sizes (mean 6.92 nm) with narrower size distribution than the L-ferritin from E. coli. It is, in conclusion, speculated that L-ferritin from yeast is relatively superior to the other, in view of the size of nanoparticle and its relative homogeneity.

A Methylobacillus Isolate Growing Only on Methanol (메탄올만 이용하여 성장하는 Methylobacillus의 분리 및 특성)

  • 김시욱;김병홍;김영민
    • Korean Journal of Microbiology
    • /
    • v.29 no.4
    • /
    • pp.250-257
    • /
    • 1991
  • An obligate methanol-oxidizing bacterium, Methylobacillus sp. strain SK1, which grows only on methanol was isolated from soil. The isolate was nonmotile Gram-negtive rod. It does not have internal membrane system. The colonies were small, whitish-yellow, and smooth. The guanine plus cytosine content of the DNA was 48 mol%. Cellular fatty acids consisted predominantly of large amounts of straight-chain saturated $C_{16:0}$ acid and unsaturated $C_{16:1}$ acid. The major ubiquinone was Q-8, and Q-10 was present as minor component. The cell was obligately aerobic and exhibited catalase, but no oxidase, activity. Poly-.betha.-hydroxybutyrate, endospores, or cysts were not observed. the isolate could grow only on methanol in mineral medium. Growth factors were not required. The isolate was unable to use methane, formaldehyde, formate, methylamine, and several other organic compounds tested as a sole source of carbon and energy. Growth was optimal at 35.deg.C and pH 7.5. It could not grow at 42.deg.C. The doubling time was 1.2h at 30.deg.C when grown with 1.0%(v/v) methanol. The growth was not affected by antibiotics inhibiting cell wall synthesis and carbon monoxide but was completely suppressed by those inhibiting protein synthesis. Methanol was found to be assimilated through the ribulose monophosphate pathway. Cytochromes of b-, c-, and o- types were found. Cell-free extracts contained a phenazine methosulfate-linked methanol dehydrogenase activity, which required ammonium ions as an activator. Cells harvested after the late exponential phase seemed to contain blue protein.ein.

  • PDF

Hydrothermal Mechanism of Na-A Type Zeolite from Natural Siliceous Mudstone (규질 이암으로부터 Na-A형 제올라이트 수열합성 반응기구에 대한 연구)

  • Bae, In-Kook;Jang, Young-Nam;Chae, Soo-Chun;Kim, Byoung-Gon;Ryu, Kyoung-Won;Lee, Sung-Ki
    • Journal of the Mineralogical Society of Korea
    • /
    • v.20 no.3
    • /
    • pp.223-229
    • /
    • 2007
  • The mechanism of hydrothermally synthesizing Na-A zeolite from siliceous mudstone at a $Na_2O/SiO_2$ ratio of 0.6, a $SiO_2/Al_2O_3$ 2.0 and a $H_2O/Na_2O$ 119 has been observed by IR, DTA, XRD and SEM. This mudstone is a tertiary periodic sedimentary rock and widely spreads around the Pohang area. In the early hydrothermal synthesis at $80^{\circ}C$ in an autoclave, sodium silicate and sodium aluminate were found to be preferentially reacted to generate Na-A type zeolite. Gibbsite and bayerite were also formed due to the presence of extra aluminum oxide in the feedstock. As reaction time in-creased up to 50 h, residual sodium aluminatewas reacted with siliceous mudstone, causing the Na-A zeolite crystal to grow and the hydroxylsodalite to generate. Therefore, in the $14{\sim}50\;h$ synthetic time, Na-A zeolite and hydroxylsodalite were formed. Also, if reaction time passed over 50 h, a part of the Na-A zeolite was finally redissolved and reacted with hydroxylsodalite to synthesize Na-P zeolite, generating porous surface of Na-A zeolite and disappearing hydroxylsodalite.

Synthesis of Hollow Silica Particles from Sodium Silicate using Organic Template Particles (유기 주형 입자를 이용한 소디움 실리케이트로부터 중공형 실리카 입자 제조)

  • Lee, Chongmin;Kim, Jiwoong;Chang, Hankwon;Roh, Ki-Min;Jang, Hee Dong
    • Korean Chemical Engineering Research
    • /
    • v.53 no.1
    • /
    • pp.78-82
    • /
    • 2015
  • Hollow silica particles were prepared using sodium silicate and organic templates. Polystyrene latex (PSL) particles produced by dispersion polymerization were used as organic templates. PSL particles ranged from $1{\mu}m$ to $3{\mu}m$ in diameter were synthesized by adjusting the amount of 2,2'-azobisisobutyronitrile (AIBN). The PSL/$SiO_2$ core-shell particles were prepared by coating of silica nanoparticles originated from sodium silicate using sol-gel method. The organic templates were removed by the organic solvent, tetrahydrofuran (THF). Morphology of hollow silica particles was investigated with respect to types of the reaction medium and pH during the process. By changing the solvent from ethanol to water, hollow silica particles were successfully formed. Hollow silica particles with the uniform shell thickness were produced at low pH as well. The reflectivity of the as-prepared silica particles was measured in the range of the wavelength of UV and visible light. Hollow silica particles showed much better reflective properties than the commercial light reflector, Insuladd.

Environment-Friendly Synthesis of Graphene Ball and its Characterization (그래핀 볼의 친환경 제조 및 특성 평가)

  • Park, Su-Ryeon;Jo, Eun Hee;Kim, Sun Kyung;Chang, Hankwon;Jang, Hee Dong
    • Korean Chemical Engineering Research
    • /
    • v.54 no.6
    • /
    • pp.786-791
    • /
    • 2016
  • Spherical graphene balls were fabricated by an aerosol spray drying process after reduced graphene oxide was prepared by the liquid phase reaction using glucose as an environment-friendly reducing agent. Spherical morphology of the as-fabricated particles was observed by FE-SEM analysis. Diffraction patterns of spherical particles were found as graphene by XRD analysis. Sphericity of GB was controlled by the variation of operating temperature, amount of glucose, and addition of $NH_4OH$. Higher sphericity of GB was prepared at higher operating temperature in the presence of $NH_4OH$. As the amount of glucose in the liquid phase reaction increased in the presence of $NH_4OH$, sphericity of GB increased. The highest sphericity of GB was 1.1. GB of higher sphericity showed lower aggregation property than that of lower sphericity. Furthermore, as-prepared GBs were found as a potential electrode material for capacitor.

Synthesis of calcium phosphates from abalone shells via precipitation (전복패각을 침전법의 원료로 이용한 calcium phosphates의 합성)

  • Moon, Sung Wook;Lee, Byeong Woo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.30 no.4
    • /
    • pp.143-149
    • /
    • 2020
  • Calcium phosphates recognized as important bio-materials have been successfully synthesized by simple precipitation using waste abalone shells, which are rich mineral sources of calcium. Calcium hydroxide (Ca(OH)2) originated from abalone shells was used as calcium source (precursor) for the preparation. Synthesis of calcium phosphates was performed by reacting calcium hydroxide with phosphoric acid (H3PO4) in aqueous solution. The initial precursor Ca/P ratios were adjusted to 1.50, 1.59 and 1.67, and the effect of the composition and the heat treatment on the synthesized powders and sintered bodies was investigated. The phases of the sintered ceramics prepared at 1150℃ were hydroxyapatite (HAp), β-tricalcium phosphate (β-TCP), and biphasic phosphate (HAp with β-TCP)), which were determined by the initial precursor Ca/P ratios. The results demonstrate the possibility for the synthesis of high value-added calcium phosphates from economical starting materials with low cost and high availability.

Dual Role of Acidic Diacetate Sophorolipid as Biostabilizer for ZnO Nanoparticle Synthesis and Biofunctionalizing Agent Against Salmonella enterica and Candida albicans

  • Basak, Geetanjali;Das, Devlina;Das, Nilanjana
    • Journal of Microbiology and Biotechnology
    • /
    • v.24 no.1
    • /
    • pp.87-96
    • /
    • 2014
  • In the present study, a yeast species isolated from CETP, Vellore, Tamilnadu was identified as Cryptococcus sp. VITGBN2 based on molecular techniques and was found to be a potent producer of acidic diacetate sophorolipid in mineral salt media containing vegetable oil as additional carbon source. The chemical structure of the purified biosurfactant was identified as acidic diacetate sophorolipid through GC-MS analysis. This sophorolipid was used as a stabilizer for synthesis of zinc oxide nanoparticles (ZON). The formation of biofunctionalized ZON was characterized using UV-visible spectroscopy, XRD, scanning electron microscopy (SEM), and Fourier transform infrared spectroscopy. The antimicrobial activities of naked ZON and sophorolipid functionalized ZON were tested based on the diameter of inhibition zone in agar well diffusion assay, microbial growth rate determination, protein leakage analysis, and lactate dehydrogenase assay. Bacterial pathogen Salmonella enterica and fungal pathogen Candida albicans showed more sensitivity to sophorolipid biofunctionalized ZON compared with naked ZON. Among the two pathogens, S. enterica showed higher sensitivity towards sophorolipid biofunctionalized ZON. SEM analysis showed that cell damage occurred through cell elongation in the case of S. enterica, whereas cell rupture was found to occur predominantly in the case of C. albicans. This is the first report on the dual role of yeast-mediated sophorolipid used as a biostabilizer for ZON synthesis as well as a novel functionalizing agent showing antimicrobial property.

Synthesis of Na-A Type Zeolite and Its Ability to Adsorb Heavy Metals (Na-A형 제올라이트의 합성 및 중금속에 대한 흡착능)

  • Chae, Soo-Chun;Jang, Young-Nam;Bae, In-Kook;Lee, Sung-Ki;Ryou, Kyung-Won
    • Journal of the Mineralogical Society of Korea
    • /
    • v.21 no.1
    • /
    • pp.37-44
    • /
    • 2008
  • This study was performed to synthesize Na-A type zeolite with melting slag from the Mapo incineration site and recycle the zeolite as an environmental remediation agent. The melting slag used had a favorable composition containing 26.6% $SiO_2$, 10.9% $Al_2O_3$ and 2.7% $Na_2O$ for zeolite synthesis although there were high contents of iron oxides, including 19.6% $Fe_2O_3$ and 18.9% FeO, which had been used as a flux for the melting. It was confirmed that the Na-A type zeolite could be successfully synthesized at $80^{\circ}C$ and $SiO_2/Al_2O_3\;=\;0.80{\sim}1.96$. The cation exchange capacities (CEC) of the zeolites was determined to be about 220 cmol/kg leveled off at the synthetic time more than 10hrs. The adsorption capacities of zeolite to heavy metals (Cd, Cu, Mn and Pb) were high except for As arid Cr. It was also confirmed through the Eh and pH analysis that As and Cr existed in the forms of $HAsO_4^{2-}$ and $CrO_4^{2-}$. The low absorption rates of zeolite for As and Cr are attributed to the fact that the pore size ($4\;{\AA}$) of Na-A type is smaller than those of $HAsO_4^{2-}$ and $CrO_4^{2-}$ ions ($4\;{\AA}$ ionic radii and $8\;{\AA}$ diameter).