Structural and Electrical Properties of Amorphous 2Ti4O12 Thin Films Grown on TiN Substrate (TiN 기판 위에 성장시킨 비정질 BaSm2Ti4O12 박막의 구조 및 전기적 특성 연구)

  • Park, Yong-Jun;Paik, Jong-Hoo;Lee, Young-Jin;Jeong, Young-Hun;Nahm, Sahn
    • Korean Journal of Materials Research
    • /
    • v.18 no.4
    • /
    • pp.169-174
    • /
    • 2008
  • The structural and electrical properties of amorphous $BaSm_2Ti_4O_{12}$ (BSmT) films on a $TiN/SiO_2/Si$ substrate deposited using a RF magnetron sputtering method were investigated. The deposition of BSmT films was carried out at $300^{\circ}C$ in a mixed oxygen and argon ($O_2$ : Ar = 1 : 4) atmosphere with a total pressure of 8.0 mTorr. In particular, a 45 nm-thick amorphous BSmT film exhibited a high capacitance density and low dissipation factor of $7.60\;fF/{\mu}m2$ and 1.3%, respectively, with a dielectric constant of 38 at 100 kHz. Its capacitance showed very little change, even in GHz ranges from 1.0 GHz to 6.0 GHz. The quality factor of the BSmT film was as high as 67 at 6 GHz. The leakage current density of the BSmT film was also very low, at approximately $5.11\;nA/cm^2$ at 2 V; its conduction mechanism was explained by the the Poole-Frenkel emission. The quadratic voltage coefficient of capacitance of the BSmT film was approximately $698\;ppm/V^2$, which is higher than the required value (<$100\;ppm/V^2$) for RF application. This could be reduced by improving the process condition. The temperature coefficient of capacitance of the film was low at nearly $296\;ppm/^{\circ}C$ at 100 kHz. Therefore, amorphous BSmT grown on a TiN substrate is a viable candidate material for a metal-insulator-metal capacitor.

Processing of Water Activity Controlled Fish Meat Paste by Dielectric Heating 1. Formulation and Processing Conditions (내부가열을 이용한 보장성어육(고등어) 연제품의 가공 및 제품개발에 관한 연구 1. 원료${\cdot}$첨가물의 배합 및 가공조건)

  • LEE Kang-Ho;LEE Byeong-Ho;You Byeong-Jin;SUH Jae-Soo;JO Jin-Ho;JEONG In-Hak;JEA Yoi-Guan
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.17 no.5
    • /
    • pp.353-360
    • /
    • 1984
  • As an effort to expand the utilization of mackerel which has been thought disadvantageous to processors due to the defects in bloody dark color of meat, high content of lipid, and low stability of protein, and to develope a new type of product, so called, preservative fish meat paste, the processing method was studied in which dielectric heating was applied by means of cooking, pasteurization, dehydration, and control of water activity. The principle of this method is based on that dielectric heating can initiate a rapid dispersion or displacement of moisture in the meat tissue so that the level of water acivity can be controlled by dehydration with hot air meanwhile the product is cooked, pasteurized, and texturized. And the product is finally heated with electric heaters and vacuum sealed to stabilize water activity and storage stability. In present paper, a formula for preparing the fish meat-stach paste, the conditions of dielectric heating and dehydration, shape and size of the product, and other parameters were tested to optimize the process operation. A formula of the fish meat-starch paste to provide proper textural properties and water activity was $10\%$ starch, $1.5\%$ salt, $3\%$ soybean, $0.6\%$ MSG, $2\%$ sucrose, and $3\%$ sorbitol against the weight of fish meat. A proper shape and size of the product to avoid foaming and case hardening during heating was sliced disc of 8 cm $diameter{\times}0.8$ cm thickness or $10{\times}10$ cm square plate with 1.0 cm thickness. The disc shape was recommended because it resulted more uniform heating, minimum foaming and case hardening. And it was also advantageous that disc was simply provided when the fish meat disc was stuffed in the same, solidified in boiling water for 2 to 3 minutes, and sliced. Condition of dielectric heating was critical to decide the levels of sterility, water activity, and textural property of the product. The temperature at the center of the meat disc slices was raised up to $95^{\circ}C$ in 1.5 minutes so that continuous exposure to microwave caused expanded tissue and hardening ending up with a higher water content. Heating for 5 to 6 minutes was adequate to yield the final water activity of 0.86 to 0.83(35 to $40\%$ moisture). It is important, however, that heating had to be done periodically, for instance, in the manner of 2.0, 1.5, 1.5, and 1.0 minute to give enough time to displace or evaporate moisture from the meat tissue. The product was dehydrated for 2 to 3 minutes by hot air of $60^{\circ}C$, 3 to 5m/sec and finally exposed to electric heaters for 5 to 6 minutes until the surface was roasted deep brown. These conditions of heating and dehydration resulted in a complete reduction of total plate count from an initial count of $5.3{\times}10^6/g$ to less than $3{\times}10^2/g$. General composition of the product was $40.1\%$ moisture, $20.8\%$ protein, $17.4\%$ lipid, $16.2\%$ carbohydrate, and $5.5\%$ ash. Textural properties revealed folding test AA, hardness 42, cohesiveness 0.53, toughness 4.6, and elasticity 0.8.

  • PDF

Effect of V$_2$O$_5$ Addition on Microwave Dielectric Properties of (Zr$_{0.8}$,Sn$_{0.2}$)TiO$_4$ (V$_2$O$_5$의 첨가가 (Zr$_{0.8}$,Sn$_{0.2}$)TiO$_4$의 마이크로파 유전특성에 미치는 영향)

  • 이경호
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.8 no.1
    • /
    • pp.27-32
    • /
    • 2001
  • The effect of $V_2O_5$, a donor-type dopant on the degradation of quality factor of ($Zr_{0.8}, Sn_{0.2})TiO_4$was compared with Ta$_2$O$_{5}$ doped ($Zr_{0.8}, Sn_{0.2})TiO_4$ in terms of microstructure, electrical conductivity, and oxidation state of the dopant. It is well known that the addition of the donor type species such as $Ta_2O_5,Nb_2O_5, Sb_2O_5, WO_{3}$, increases the quality factor of ($Zr_{0.8}, Sn_{0.2})TiO_4$due to decrease the oxygen vacancy concentration. Unlike other dopants, however, the addition of $V_2O_5$ decreased the quality factor. The degradation of quality factor of ($Zr_{0.8}, Sn_{0.2})TiO_4$was resulted from the formation of grain boundary phase and $V_2O_5$rich fiber shaped secondary phase, and the increasing the oxygen vacancy concentration due to unstability of oxidation state of vanadium ions in ($Zr_{0.8}, Sn_{0.2})TiO_4$ceramic.c.

  • PDF

Effects of $B_2O_3$ Additives on the Sintering Temperature and Microwave Dielectric Properties of $Ba(Zn_{1/3}Nb_{2/3})O_3$ Ceramics ($B_2O_3$의 첨가가 $Ba(Zn_{1/3}Nb_{2/3})O_3$ 세라믹스의 소결 온도와 고주파 유전 특성에 미치는 영향)

  • Kim, Min-Han;Son, Jin-Ok;Nahm, Sahn;Yoo, Myong-Jae;Park, Jong-Cheol;Lee, Hwack-Joo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.611-614
    • /
    • 2004
  • [ $Ba(Zn_{1/3}Nb_{2/3})O_3$ ] (BZN) 세라믹스의 소결 온도는 약 $1350^{\circ}C$ 이다. 그러나 $B_2O_3$가 첨가된 경우, BZN 세라믹스는 $900^{\circ}C$에서 소결되었다. $BaB_4O_7$, $BaB_2O_4$ 그리고 $BaNb_2O_6$ 이차상이 $B_2O_3$가 첨가된 BZN 세라믹스에서 관찰되었다. $BaB_4O_7$$BaB_2O_4$ 이차상은 약 $900^{\circ}C$에서 공정 온도를 가지기 때문에 $B_2O_3$를 첨가한 BZN 세라믹스론 $900^{\circ}C$에서 소결하는 동안 액상으로 존재할 것으로 여겨지며, 그것이 BZN 세라믹스의 소결온도를 낮출 것으로 생각된다. 소결 온도의 증가에 따라 유전 상수 ($\varepsilon_r$)와 품질 계수 ($Q{\times}f$)의 값은 증가하였는데, 이는 밀도의 증가에 기인한다. 그러나 $B_2O_3$의 첨가량이 많은 경우 Q 값은 감소하는데, 이는 이차상의 존재가 품질계수의 저하를 초래한다고 생각된다. 2.0 mol% $B_2O_3$가 첨가된 BZN 세라믹스를 $950^{\circ}C$에서 2시간 동안 소결하는 경우, $Q{\times}f$=13.600 GHz, $\varepsilon_r$=37.6 그리고 공진 주파수 온도계수 ($\tau_f$) = 19 ppm/$^{\circ}C$의 유전특성을 얻을 수 있었다.