• Title/Summary/Keyword: metallic phase

Search Result 319, Processing Time 0.035 seconds

Room and High Temperature Deformation Behaviors and Estimation on Formability of Zr-based Bulk Metallic Glass Composite (Zr-Nb-Cu-Ni-Al 비정질 복합 재료의 변형거동과 성형성)

  • Jun, H.J.;Lee, K.S.;Kuhn, U.;Eckert, J.;Chang, Y.W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.199-202
    • /
    • 2008
  • In this study, we investigated the thermal properties of $Zr_{66.4}Nb_{6.4}Cu_{10.5}Ni_{8.7}Al_{8.0}$ by using a differential scanning calorimeter (DSC), and then analyzed the composition of dendrite phase by using X-ray diffraction (XRD). A series of uniaxial compression tests has been performed under the strain rates between $10^{-5}/s$ and $10^{-2}/s$ at room temperature and near SLR. This BMGC has higher high temperature strength than other Zr-based monolithic BMGs because in-situ formed crystalline phases hinder a feasible viscous flow of amorphous matrix. Warm formability is also estimated by laboratory-scale extrusion test within supercooled liquid region. It was found that BMGC has poor formability compared with nother Zr-based bulk metallic glass composite presumably due to large volume fraction of 'brittle' crystalline phases distributed within amorphous matrix.

  • PDF

Bioactivity of Calcium Phosphate Ceramic Coatings on Metallic Implants

  • Kim, Cheol-Sang;Ducheyne, P.
    • Journal of Biomedical Engineering Research
    • /
    • v.11 no.1
    • /
    • pp.5-12
    • /
    • 1990
  • Calcium phosphate ceramics have been applied intensively to orthopaedic and dental implants by virtue of their osteoconductive nature. In an attempt to enhance the bone implant intergrity and Eta utility, these ceramics are deposited onto the porous surface of metallic implants. The coating procedure and the ensuing phase transformations of the ceramic alter the mechanical properties and surface chemistry of the ceramic layers as well as those of the substrate. These structural and compositional differences are directly related to the interaction mechanisms at the surface-active ceramicbone interface. Material and processing induced influences on dissolution, electrokinetic behavior, ceramic-metallic substrate interface and boRe growth enhancement are presented.

  • PDF

Visualization of Crack Propagation and Fracture Transition in Bulk Metallic Glass using Mechano-Luminescence (압광을 이용한 금속계 비정질 합금의 균열전파 및 파괴전이 현상 가시화 연구)

  • Kim, Ji-Sik
    • Transactions of Materials Processing
    • /
    • v.20 no.4
    • /
    • pp.303-308
    • /
    • 2011
  • Using a mechano-luminescent(ML) paint, which allows the visualization of fast propagating crack under conventional loading conditions, a catastrophic fracture mechanism associated to crack tip melting and wake bridging in bulk metallic glass, is described in this paper. Fracture occurs in two steps with, first, crack initiation from the mechanically machined sharp notch tip in a rectangular shaped compact tension specimen and melting of its tip due to intense shear deformation within very few deformation bands. Then, the crystalline phase in the glass matrix gradually converts the molten crack into a conventional bridged crack as it propagates.

High Strength Nanostructured Metastable Alloys

  • Eckert, Jurgen;Bartusch, Birgit;Schurack, Frank;He, Guo;Schultz, Ludwig
    • Journal of Powder Materials
    • /
    • v.9 no.6
    • /
    • pp.394-408
    • /
    • 2002
  • Nanostructured high strength metastable Al-, Mg- and Ti-based alloys containing different amorphous, quasicrystalline and nanocrystalline phases are synthesized by non-equilibrium processing techniques. Such alloys can be prepared by quenching from the melt or by powder metallurgy techniques. This paper focuses on one hand on mechanically alloyed and ball milled powders containing different volume fractions of amorphous or nano-(quasi)crystalline phases, consolidated bulk specimens and, on the other hand. on cast specimens containing different constituent phases with different length-scale. As one example. $Mg_{55}Y_{15}Cu_{30}$- based metallic glass matrix composites are produced by mechanical alloying of elemental powder mixtures containing up to 30 vol.% $Y_2O_3$ particles. The comparison with the particle-free metallic glass reveals that the nanosized second phase oxide particles do not significantly affect the glass-forming ability upon mechanical alloying despite some limited particle dissolution. A supercooled liquid region with an extension of about 50 K can be maintained in the presence of the oxides. The distinct viscosity decrease in the supercooled liquid regime allows to consolidate the powders into bulk samples by uniaxial hot pressing. The $Y_2O_3$ additions increase the mechanical strength of the composites compared to the $Mg_{55}Y_{15}Cu_{30}$ metallic glass. The second example deals with Al-Mn-Ce and Al-Cu-Fe composites with quasicrystalline particles as reinforcements, which are prepared by quenching from the melt and by powder metallurgy. $Al_{98-x}Mn_xCe_2$ (x =5,6,7) melt-spun ribbons containing a major quasicrystalline phase coexisting with an Al-matrix on a nanometer scale are pulverized by ball milling. The powders are consolidated by hot extrusion. Grain growth during consolidation causes the formation of a micrometer-scale microstructure. Mechanical alloying of $Al_{63}Cu_{25}Fe_{12}$ leads to single-phase quasicrystalline powders. which are blended with different volume fractions of pure Al-powder and hot extruded forming $Al_{100-x}$$(Al_{0.63}Cu_{0.25}Fe_{0.12})_x$ (x = 40,50,60,80) micrometer-scale composites. Compression test data reveal a high yield strength of ${\sigma}_y{\geq}$700 MPa and a ductility of ${\varepsilon}_{pl}{\geq}$5% for than the Al-Mn-Ce bulk samples. The strength level of the Al-Cu-Fe alloys is ${\sigma}_y{\leq}$550 MPa significantly lower. By the addition of different amounts of aluminum, the mechanical properties can be tuned to a wide range. Finally, a bulk metallic glass-forming Ti-Cu-Ni-Sn alloy with in situ formed composite microstructure prepared by both centrifugal and injection casting presents more than 6% plastic strain under compressive stress at room temperature. The in situ formed composite contains dendritic hcp Ti solid solution precipitates and a few $Ti_3Sn,\;{\beta}$-(Cu, Sn) grains dispersed in a glassy matrix. The composite micro- structure can avoid the development of the highly localized shear bands typical for the room temperature defor-mation of monolithic glasses. Instead, widely developed shear bands with evident protuberance are observed. resulting in significant yielding and homogeneous plastic deformation over the entire sample.

Formation of Icosahedral Phase in Bulk Glass Forming Ti-Zr-Be-Cu-Ni Alloy

  • Park, Jin Man;Lee, Jun Hyeok;Jo, Mi Seon;Lee, Jin Kyu
    • Applied Microscopy
    • /
    • v.45 no.2
    • /
    • pp.58-62
    • /
    • 2015
  • Formation of an icosahedral phase in the bulk glass forming $Ti_{40}Zr_{29}Be_{14}Cu_9Ni_8$ alloy during crystallization from amorphous phase and solidification from melt is investigated. The icosahedral phase with a size of 10 to 15 nm forms as a thermodynamically stable phase at intermediate temperature during the transformation from amorphous to crystalline phases such as Laves and ${\beta}$-(Ti-Zr) phases, indicating that the existence of the icosahedral cluster in the undercooled liquid. On the other hand, the icosahedral phase forms as a primary solidification phase even though the Laves phase is stable at high temperature, which is can be explained based on the high nucleation rate of icosahedral phase relative to that of competing crystalline Laves phase due to lower interfacial energy between icosahedral and liquid phases.

The Study on Explosion Phenomena of a Metal Wire by Rapid Heating in Water (초고속가열에 의한 금속세선의 폭발현상에 관한 연구)

  • Jang, In-Seon;Kim, Jong-Su
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.33 no.1
    • /
    • pp.27-37
    • /
    • 1997
  • The aim of the present study is to investigate experimentally the mechanism of an exploding wire in water and also to observe the bubble motion induced by an exploding wire. The experiment of an exploding wire is carried out in a water tank. As a metallic wire, a tungsten wire of 0.2mm in diameter and 10mm in length is employed. The electric energy of 50-300J is fed to the wire from a capacitor of 100$\mu$F charged up to 1-2.5kV. The explosion is recorded by a CCD camera with the resolution of 1$\mu$sec. The explosion process of metallic wire is divided into three phases. Phase 1 : As the voltage is applied to the wire, the temperature increases due to Joule heating and the wire emits light. Phase 2 : Then the wire melts and the cylindrical plasma is formed between the electrodes. Up to this stage, strong light emission is observed. Phase 3 : The light emission goes out and a vapor bubble begins to grow spherically. The radius of a bubble oscillates in time, but the amplitude of oscillation diminishes in several cycles.

  • PDF

Flow Stress and Deformation Behavior of Zr-based Bulk Metallic Glass Composite in Supercooled Liquid Region (Zr계 비정질 복상 합금의 과냉 액상 영역에서의 유동 음력과 변형거동)

  • Jun, H.J.;Lee, K.S.;Chang, Y.W.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.417-420
    • /
    • 2006
  • The composition and structure of dendrite phase within $Zr_{76.11}Ti_{4.20}Cu_{4.51}Ni_{3.16}Be_{1.49}Nb_{10.53}$ bulk metallic glass (BMG) were confirmed by using an EPMA, XRD and TEM, respectively. The chief elements of dendrite phase were Zr-Ti-Nb and had a BCC structure. The thermal properties of this BMG have been then subsequently investigated by using a differential scanning calorimeter (DSC). The glass transition and crystallization onset temperatures were determined as $339.7^{\circ}C$ and $375.8^{\circ}C$ for this alloy, respectively. Mechanical properties have also been examined by conducting a series of uniaxial compression tests at various temperatures within supercooled liquid region under the strain rates between $10^{-4}/s$ and $3{\times}10^{-2}/s$. The deformation behavior of BMG composite within supercooled liquid region is similar to one of Vit-1 exhibiting amorphous single phase alloy. The flow stresses of BMG composite, however, are entirely higher than those of Vit-1 because dendrite phases are interfere with moving of atoms.

  • PDF

Numerical Study on the Atomization Process of a Supersonic Gas-Metallic Liquid Atomizer (초음속기체-금속액체 분사기의 미립화 과정에 대한 수치해석)

  • Hwang, Won-Sub;Kim, Kui-Soon;Choi, Jeong-Yeol
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.44 no.7
    • /
    • pp.593-602
    • /
    • 2016
  • Numerical simulations on the close-coupled supersonic gas atomizer for metallic powder production were performed in this study. A proper turbulence model was chosen and then VOF(Volume of Fluid) and DPM(Discrete Phase Model) methods were sequentially applied for the simulations of primary and secondary break-up processes of liquid metal. Diameters of parent droplets were calculated by analyzing Level-Set function contour from the VOF result. Finally, the distribution of particle diameter was obtained from the DPM result at exit of the computational domain.

Surface Morphology and Electrical Property of PEMFC (Proton Exchange Membrane Fuel Cell) Bipolar Plates (고분자전해질 연료전지용 바이폴라 플레이트의 표면형상과 전기적 특성)

  • Song, Yon-Ho;Yun, Young-Hoon
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.3
    • /
    • pp.161-166
    • /
    • 2008
  • The multi-films of a metallic film and a transparent conducting oxide (TCO, indium-tin oxide, ITO) film were formed on the stainless steel 316 and 304 plates by a sputtering method and an E-beam method and then the external metallic region of the stainless steel bipolar plates was converted into the metal nitride films through an annealing process. The multi-film formed on the stainless steel bipolar plates showed the XRD patterns of the typical indium-tin oxide, the metallic phase and the metal substrate and the external nitride film. The XRD pattern of the thin film on the bipolar plates modified showed two metal nitride phases of CrN and $Cr_2N$ compound. Surface microstructural morphology of the multi-film deposited bipolar plates was observed by AFM and FE-SEM. The metal nitride film formed on the stainless steel bipolar plates represented a microstructural morphology of fine columnar grains with 10 nm diameter and 60nm length in FE-SEM images. The electrical resistivity of the stainless steel bipolar plates modified was evaluated.

Heat Transfer Characteristics of Aluminium and FeCrAlY Foam

  • Jin, Meihua;Kim, Pil-Hwan;Lee, Hae-Jong;Jeong, Hyo-Min;Chung, Han-Shik
    • Proceedings of the SAREK Conference
    • /
    • 2008.06a
    • /
    • pp.395-401
    • /
    • 2008
  • Since metallic foam will increase the performance of heat exchanger, it have caused many researcher's attention recently. Our research base on the model that metallic foams applied to heat exchanger. In this case, there is three kind of heat transfer mechanisms, heat conduction in fibers, heat transfer by conduction in fluid phase, and internal heat change between solid and fluid phases. In this paper we study both the hydraulic and thermal aspect performance. Pressure drop along air flow direction will be presented. As thermal aspect, we first discuss the acceptance of applying thermal equilibrium among the two phases. then to calculate the dimensionless temperature profile, the heat transfer coefficient and Nu number in 14 metallic foams(7 Aluminium foams, 7 FeCrAlY foams). All these discussion is based on the same velocity u=2 m/s.

  • PDF