Analysis of Heat Transfer Characteristics by Materials in Closed Conditions Using Acrylic Hemisphere (I): Comparison of Interior Finishing Materials (아크릴 반구를 이용한 밀폐 조건에 따른 재료별 열 이동 특성 분석(I): 실내마감재 종류에 따른 비교)

  • YANG, Seung Min;LEE, Hyun Jae;KANG, Seog Goo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.2
    • /
    • pp.217-230
    • /
    • 2020
  • Global warming has increased interest in reducing greenhouse gas emissions. And a policy has effort to reduce energy consumption as a greenhouse gas reduction plan. In Korea, 25% of total energy is consumed in the building sector. In order to reduce energy consumption of buildings, it is possible to expand the utilization of wood as a structural material or thermal insulation materials with low thermal conductivity. It is also reported that when used as an interior finishing material, the energy consumption of the building is reduced by up to 7% by insulation performance. In this study, the heat transfer characteristics and the heat capacity were compared according to the three type of finishing materials(cement, paulownia coreana, medium density fiberboard) normally used as indoor finish materials. Through this study, most of the heat transfer volumes are transferred in the form of radiant heat, and the result was derived from the highest amount of energy and heat transfer in the use of paulownia coreana. When indoor finishing materials are used as wood, it is deemed that energy efficiency inside the building will be improved.

Manufacture of Calligraphy-carving Artworks Using Carbonized Board (탄화보드를 이용한 서각작품 제작)

  • Park, Sang-Bum;Chong, Song-Ho;Byeon, Hee-Seop;Ryu, Hyun-Soo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.38 no.3
    • /
    • pp.185-190
    • /
    • 2010
  • This study was focused to make a wooden plate that is engraved with writings or pictures on the medium density fiberboard (MDF), and then to produce a calligraphy-carving artwork by carbonization of the carved MDF. The external appearances and anatomical changes were investigated on the carbonized MDF and aesthetic characteristics was also discussed. No split and no twist were found after the carbonization (at $850^{\circ}C$) of the calligraphy-encarved MDF, shrinkages of the MDF were observed with portions of 21.8% in length, 18.8% in width and 43.5% in thickness, and 69.2% of weight loss with density decrease of 14.8% were observed as well. From the observation of the carbonized board by a scanning electron microscope, specific phenomena were found: the adhesives, surrounding the fiber's surface and pits, were carbonized, the woody fibers were changed smoothly, the pits were opened, the fiber' size was uniformized, and the organization was compacted. By the combination of handmade calligraphy-woodcarving and crack-free carbonizing methods, it was able to find a new method for manufacture carbonized calligraphy-woodcarving artwork. It is concluded that the calligraphy-woodcarving artwork using carbonized board can be a new access for the eco-friendly art that has the advantage of the functionality of charcoal and the aesthetic of calligraphy-woodcarving simultaneously.

Core Issues and Tariff Reduction of Timber Products in Non-Agricultural Market Access on WTO/DDA in Korea (WTO/DDA협상 비농산물시장접근분야의 목재류의 주요 쟁점 및 관세 감축 영향)

  • Lee, Seong Youn;Jung, Byung-Heon;Song, Young Gun;Kim, Se Bin;Kwak, Kyung Ho
    • Journal of Korean Society of Forest Science
    • /
    • v.97 no.4
    • /
    • pp.408-416
    • /
    • 2008
  • This study was analyzed the changes of the tariff reduction for the timber products according to the modalities proposed by the chairman of Non-agriculture Market Access. The resulted data would be expected to be used for establishing the strategies for the WTO/DDA negotiation of Korea. As WTO/DDA negotiation was officially resumed in the early 2007. It was necessarily required to develop a strategy how to address debating core issues raised during the negotiation since 2006. For this purpose, major core issues and agenda were arranged and analyzed in this study. In Korea, the results of the analysis show that, in the position of developed members, the applicable tariff rates after the tariff reduction of sawnwood and veneer sheet was not different from that in 2007. However, in the position of developing members, the applicable tariff rate of sawnwood and veneer sheet was increased after the tariff reduction. The unbound tariff lines, wood-based panels such as plywood and medium-density fiberboard, the applicable tariff rate after the tariff reduction was analyzed to be reduced more than 50% in the position of developed members, and therefore is determined to be considerable influenced upon the applicable tariff rates. On the other hand, in the position of developing country the tariff rates after the tariff reduction was higher than that of the applicable tariff rates in 2007. Thus no changes of the tariff reduction by a negotiation agreement was analyzed to be happened.

Static Bending Strength Performances of Hybrid Laminated Woods Composed of Wood-Wood Based Boards (목재와 목질보드 복합적층재의 휨강도성능)

  • Park, Han-Min;Moon, Sung-Jae;Choi, Yoon-Eun;Park, Jung-Hwan;Byeon, Hee-Seop
    • Journal of the Korean Wood Science and Technology
    • /
    • v.37 no.6
    • /
    • pp.546-555
    • /
    • 2009
  • To study an effective use of woods, three-ply hybrid laminated woods instead of crosslaminated woods which are composed of spruce in the face and three kinds of wood-based boards (MDF, PB, OSB) in the core were manufactured, and the effect of constitution elements for the core laminae on bending strength performances was investigated. Bending modulus of elasticity (MOE) of hybrid laminated woods had the highest values for the hybrid laminated wood types arranging OSB laminae in the core, and had the lowest values for those arranging MDF laminae in the core. These values were higher than those of various cross-laminated woods. The estimated bending MOEs of the hybrid laminated woods which were composed of perpendicular-direction lamina of spruce in the faces were similar to their measured values, regardless of wood-based boards in the core. However, those of the hybrid laminated woods which were composed of parallel-direction lamina of spruce in the faces had much higher values than those of their measured values, and it was necessary to revise the measured values. Bending modulus of rupture (MOR) of the hybird laminated woods had the highest value for those arranging OSB laminae in the core, and had the lowest values for those arranging PB laminae in the core unlike the bending MOE. By hybrid laminating, the anisotropy of bending strength performances was markedly decreased, and the differences of strength performances among wood-based boards were also considerably decreased.

CO and Soot Yields of Wood Combustibles for a Kitchen Fire Simulation (주방 화재시뮬레이션을 위한 목재 가연물의 CO 및 Soot Yields)

  • Mun, Sun-Yeo;Hwang, Cheol-Hong;Kim, Sung-Chan
    • Fire Science and Engineering
    • /
    • v.33 no.1
    • /
    • pp.76-84
    • /
    • 2019
  • Experimental studies using an open cone calorimeter were conducted to provide information on the CO and soot yields of wood combustibles required for a kitchen fire simulation of PBD. A total of eight specimens were examined for medium density fiberboard (MDF) and particle board (PB), which are used widely in kitchen furniture production, depending on the water content, surface processing method, and surface color. The thermal penetration time related to the fire spread rate in the depth direction differed significantly according to the surface processing treatment method, even for a specimen of identical thickness. The CO yield ($y_{CO}$) of the MDF and PB series did not change significantly according to the combustion mode and surface treatment process in flaming mode. On the other hand, $y_{CO}$ was approximately 10 times higher in smoldering mode than in flaming mode. The soot yield ($y_{soot}$), however, varied considerably depending on the combustion mode and surface treatment process. In particular, a higher $y_{soot}$ was found in flaming mode and in the surface-treated specimens. Finally, the $y_{CO}$ and $y_{soot}$ of MDF and PB measured for the kitchen fire simulation of PBD were applied.

Performance on Flame-Retardant Polyurethane Coatings for Wood and Wood-based Materials (목재 및 목질재료용 난연성 폴리우레탄수지 도막의 난연성능)

  • Kim, Jong-In;Park, Jong-Young;Kong, Young-To;Lee, Byoung-Hoo;Kim, Hyun-Joong;Roh, Jeang-Kwan
    • Journal of the Korean Wood Science and Technology
    • /
    • v.30 no.2
    • /
    • pp.172-179
    • /
    • 2002
  • In this study, two materials treated with a flame retardant were examined for their fire resistance. The first, MDF (medium density fiberboard) was overlaid by an oak sliced veneer, which was either treated by soaking in a 6wt.% solution of flame retardant chemicals (pentabromine-chlorinated paraffin) or non-treated and then was coated with either a flame retardant polyurethane coating or with a common polyurethane coating. The second material, Pinus koraiensis penal was either treated by a spray treatment using a flame retardant solution or non-treated and then was coated with either a flame retardant polyurethane coating or with a common polyurethane coating. Pentabromine-chorinated paraffin chemicals were added (6 part of urethane resin) as the flame retardant chemicals in the polyurethane coatings. In the fire resistance test, the th𝜃(℃·min) decreased with the flame retardant treatment or/and the flame retardant coatings, compared to the untreated sample Weight loss (%) decreased with the flame retardant treatment or/and the flame retardant coatings. The ignition time (sec.) increased and the residual flame time (sec.) decreased with the flame retardant treatment or/and flame retardant coatings. Therefore, the flame retardant treatment or/and flame retardant polyurethane coatings have excellent incombustibility.

A Study on the Stiffness of CBA(Corner Block with Anchor Bolt) Joint in Knockdown Type Table Furniture (조립식(組立式) 탁자(卓子)의 CBA접합부(接合部) 강성(剛性)에 관(關)한 연구(硏究))

  • Chung, Woo-Yang;Lee, Phil-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.17 no.2
    • /
    • pp.34-64
    • /
    • 1989
  • Corner block with anchor bolt(CBA) joint method used in knock-down type table furniture manufacturing can reduce the packing and transporting cost. Unfortunately. it also has the disastrous defect to be loosend and unstable during the service life mainly due to fatigue and creep(repeated and prolonged loading). So 22 joint groups constructed were tested to evaluate the effect of some design factors related to the size of side rail(apron). block attachment to side rail. and the number of anchor bolt as well as the effect of the type of corner block(mitered type vs. rectangular type) Usable strength from the stiffness coefficients of each joint group were analysed with SPSS /PC+ and described as the criteria of CBA joint construction. The conclusions were as follows: The height of side rail(50, 75 and 100 mm) and the addition of polyvinyl acetate(PVAc) emulsion in the corner block attactment to side rail had the effect on raising the usable strength of CBA joint with remarkable high significance. And the effect of 2 - anchor bolts was also superior to that of 1 - bolt significantly. However. the thickness of side rail(22 mm vs. 25 mm) had no effect on the strengthening the table joint rigidity. Mitered type corner block joint appeared to he recommendable for CBA jointed table construction rather than the rectangular type one regardless of the method of block attachment to side rail. The best result identified from Duncan's multiple comparison was in the construction with 25 mm thick and 100 mm height of side rail fastened using 2 - anchor bolts in mitered type corner block. But it would be reasonable to use 22 mm thick & 75 mm high side rail and mitered corner block with PVAc emulsion & 2 bolts considering the productivity and production cost down in the MDF furniture manufacturing industries.

  • PDF

Bending Creep Performances of Hybrid Laminated Woods Composed of Wood-Wood Based Boards (목재와 목질보드 복합적층재의 휨 크리프 성능)

  • Park, Han-Min;Kang, Dong-Hyun;Choi, Yoon-Eun;Ahn, Sang-Yeol;Ryu, Hyun-Su;Byeon, Hee-Seop
    • Journal of the Korean Wood Science and Technology
    • /
    • v.38 no.1
    • /
    • pp.1-10
    • /
    • 2010
  • In this study, to study an effective use and improve strength performances of woods and wood-based materials, three-ply hybrid laminated woods which are composed of spruce in the face and three kinds of wood-based boards (MDF, PB, OSB) in the core were manufactured, and the effect of constitution elements used for the core laminae on bending creep performances was investigated. The shape of creep curves showed exponential function plots which the upper right side was increased, and differed among the kinds of wood-based boards used for the core laminae of hybrid laminated wood. The creep deformation perpendicular to the grain of faces of hybrid laminated woods was in order $C_{\perp}$(P) > $C_{\perp}$(M) > $C_{\perp}$(O) with PB, MDF and OSB in the core, respectively. It was found that the creep deformation arranged with OSB in the core had 2 times smaller than those arranged with MDF and PB in the core. By hybrid laminating, the creep deformation of spruce perpendicular to the grain was markedly decreased. On the other hand, the creep deformation parallel to the grain of the faces ($C_{\parallel}$ type) of hybrid laminated woods was in order $C_{\parallel}$(P) > $C_{\parallel}$(O) > $C_{\parallel}$(M) with PB, OSB and MDF in the core. The ratios among three hybrid laminated woods were considerably decreased, especially the difference between $C_{\parallel}$(P) and $C_{\parallel}$(O) hybrid laminated woods arranged with PB and OSB in the core was very small. These values showed 0.108~0.464 times smaller than creep deformation of three wood-based boards and it was found that creep deformation of three wood-based boards was considerably decreased by hybrid laminating. Creep anisotropy of hybrid laminated woods was greater in creep deformation than in initial deformation, whereas it was found that the values was much smaller than that of spruce parallel laminated woods.

The Dyeing Properties of Woody Fiber Regenerated from Waste MDF by Reactive Dyes (반응성염료에 의한 폐MDF 재생 목질섬유의 염색특성)

  • Ju, Seon-Gyeong;Roh, JeongKwan
    • Journal of the Korean Wood Science and Technology
    • /
    • v.47 no.2
    • /
    • pp.163-177
    • /
    • 2019
  • This study aims to review the relations between the dyeing conditions (i.e., dye concentration, addition amounts of salt and alkali, and dyeing temperature) and dyeing properties and color fastness to light for identifying the optimal dyeing conditions when dyed regenerated woody fibers were obtained through the defibration of waste medium density fiberboard (MDF) using reactive Red H-E3B (Bis-monochlorotriazine (MCT)/MCT type) and reactive Red RB133% (Bis-MCT/Vinyl sulphone type). The dyeing yield (K/S) obtained using two types of reactive dyes increased as the dye concentration increased by 1-10% (on the weight of fiber (OWF)). In addition, the K/S of H-E3B was higher than that of RB133% irrespective of the dye concentration. The color difference of H-E3B after ultraviolet (UV) radiation was lower than that of RB133%, denoting good resistance to discoloration by UV. As the amount of sodium sulfate increased, the color difference and K/S also increased, and the adequate salt content was determined to be 50-70 g/L. Further, the color difference and K/S significantly increased only the addition of 2 g/L of sodium carbonate; however, almost no difference was observed when more than 2 g/L of sodium carbonate was added. The addition amount of sodium carbonate was adequate 5-10 g/L to dyeing the fiber and the pH at this addition level was 10. The dyeing yield of H-E3B increased when the dyeing temperature increased; however, it subsequently decreased after the dyeing temperature became $80^{\circ}C$. The dyeing yield of RB133% was almost the same up to $60-70^{\circ}C$ but declined subsequently. Thus, the adequate temperatures were $80^{\circ}C$ and $60^{\circ}C$ for H-E3B and RB133%, respectively. If the waste MDF woody fiber was dyed under the aforementioned optimal conditions, dyed regenerated woody fiber can be obtained having the following colors: 1.5 to 2.0R with the H-E3B dye and 9.6 to 10.0 PR with RB133%.