• 제목/요약/키워드: magnesium particles

검색결과 105건 처리시간 0.029초

질산염 및 황산염 집적 염류 토양의 전기역학적 개량 (Electrokinetic Restoration of Saline Soil Accumulated with Nitrate and Sulfate)

  • 조정민;조성웅;김도형;양중석;백기태
    • 한국지하수토양환경학회지:지하수토양환경
    • /
    • 제16권5호
    • /
    • pp.18-23
    • /
    • 2011
  • The electrokinetic transport characteristics of salts were investigated using nitrate and sulfate accumulated saline greenhouse soil. Within 8 days, 95% of nitrate was removed from the soil, while sulfate removal was 19% for 8 days. The low removal of sulfate came from adsorption reaction on the soil particles or organic matter and precipitation with calcium. Divalent cations such as calcium and magnesium were transported toward cathode via electromigration, and most monovalent cation such as potassium was removed. The pattern of residual electrical conductivity was similar with that of sulfate. Based on the results, electrokinetic technique is effective to restore nitrate-accumulated saline soil, but is not effective to restore sulfate-accumulated soil.

유성밀 분쇄에 의한 사문석과 활석의 물리적 특성변화 (Physical Properties Change of Serpentine and Talc by Planetary Ball Mill)

  • 김동진;정헌생;이재천;이자현
    • 한국재료학회지
    • /
    • 제9권8호
    • /
    • pp.810-816
    • /
    • 1999
  • 유성밀로써 사문석과 활석을 분쇄시 X-ray 회절분석, FT-IR, DSC-TG, 입도분석 그리고 SEM관찰 등을 이용하여 결정조직과 물리적 특성변화를 조사하였다. 분쇄기간이 증가함에 따라 사문석과 활석 원시료의 결정피크가 점처 감소하여 120분 이상 분쇄시 비정질상으로 변하였으며 이와 같은 변화는 마그네슘 결정 조직의 무질서에 기인한다. 분쇄된 시료에서 나타나는 흡열반응의 피크는 원시료보다 낮은 온도에서 관찰되었다. 또한 불규칙한 모양의 원시료는 분쇄처리를 실시함에 따라 구형의 응집체로 변하였다.

  • PDF

전자교반에 의한 Cu-0.5wt%Zr 합금의 반응고 조직제어에 관한 연구 (The Effect of Electromagnetic Stirring on the Semi-Solid Microstructure of Cu-0.15wt%Zr Alloy)

  • 임성철;이흥복;김경훈;권혁천;윤의박
    • 한국주조공학회지
    • /
    • 제26권1호
    • /
    • pp.40-45
    • /
    • 2006
  • Most of the work reported concerned the semi-solid processing of low melting point alloys, and in particular light alloys of aluminum and magnesium. The purpose of this paper is to develop a semi-solid microstructure of Cu alloys using electromagnetic stirring applicable for squirrel cage rotor of induction motor. The size of primary solid particle and the degree of sphericity as a function of the variation in cooling rate, stirring speed, and holding time were observed. By applying electromagnetic stirring, primary solid particles became finer and rounder relative to as-cast sample. As the input frequency increased from 30 to 40 Hz, particle size decreased. The size of primary solid particle was found to be decreased with increasing cooling rate. Also, it decreased with stirring up to 3 minutes but increased above that point. The degree of sphericity became closer to be 1 with hold time. Semi-solid microstructure of Cu alloys, one of the high melting point alloys, could be controlled by electromagnetic stirring.

MgxNiyZn1-x-yFe2O4나노입자 제조를 위한 초음파 습식 자기분류법의 적용 (Application of Ultrasonic Wet-Magnetic Separation Method to Prepare Nano-sized MgxNiyZn1-x-yFe2O4)

  • 구문선;최용
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.201.2-201.2
    • /
    • 2016
  • $Mg_xNi_yZn_{1-x-y}Fe_2O_4$ ferrite powders were prepared by self-propagating high temperature synthesis followed by classified by ultrasonic wet-magnetic separation method to get nano-sized particles with high purity. The $Mg_xNi_yZn_{1-x-y}Fe_2O_4$ ferrites were well formed by using several powders like iron, nickel oxide, zinc oxide and magnesium oxide at 0.1 MPa of oxygen pressure. The ultrasonic wet-magnetic separation of pre-mechanical milled ferrite powders produced the powders with average size of $3.7-0.8{\mu}m$. The addition of a surfactant during the separation process improved productivity more than twice. The coercive force, maximum magnetization and residual magnetization of the $Mg_xNi_yZn_{1-x-y}Fe_2O_4$ nano-powders with 810 nm size were 45.89 Oe, 53.92 emu/gOe, 0.4 emu/Oe, respectively.

  • PDF

Reaction Kinetics with Hydrogen and Temperature Dependence of the Hydriding Rate for a Magnesium-Based Nickel Iron Oxide Alloy

  • Song, Myoung Youp;Baek, Sung Hwan;Park, Hye Ryoung
    • 대한금속재료학회지
    • /
    • 제50권6호
    • /
    • pp.463-468
    • /
    • 2012
  • A 71.5 wt%Mg-23.5 wt%Ni-5 wt%$Fe_2O_3$ (Mg-23.5Ni-$5Fe_2O_3$) sample was prepared by a quite simple process, reactive mechanical grinding, and its hydriding and dehydriding properties were then investigated. The reactive mechanical grinding of Mg with Ni and $Fe_2O_3$ is considered to facilitate nucleation and shorten the diffusion distances of the hydrogen atoms. After the hydriding-dehydriding cycling, the Mg-23.5Ni-$5Fe_2O_3$ sample contained $Mg_2Ni$ phase. Expansion and contraction of the hydride-forming materials (Mg and $Mg_2Ni$) with the hydriding and dehydriding reactions are also considered to increase the hydriding and dehydriding rates of the mixture by forming defects and cracks leading to the fragmentation of the particles. The temperature dependence of the hydriding rate of the sample is discussed.

고상반응법에 의한 아커마나이트 분말의 합성 및 생체활성도 평가 (Synthesis of akermanite bioceramics by solid-state reaction and evaluation of its bioactivity)

  • 고재은;이종국
    • 한국결정성장학회지
    • /
    • 제32권5호
    • /
    • pp.191-198
    • /
    • 2022
  • 치과용 임플란트 재료로 주로 사용되는 지르코니아 및 티타늄 합금은 생체불활성 특징으로 인하여 골유착 및 골형성 능력이 떨어진다. 이러한 문제를 쉽고 간단하게 해결하기 위한 방법으로는 생체활성 물질을 표면에 코팅하여 생체 활성을 높이는 방법이 있다. 본 연구에서는 우수한 골결합 능력을 가진 실리케이트계 세라믹인 아커마나이트(Ca2MgSi2O7)를 고상반응법으로 합성하고, SBF 용액 내 침적실험을 통하여 합성 아커마나이트 분말의 생체활성을 분석하였다. 고상반응 출발원료로는 탄산칼슘(CaCO3), 탄산마그네슘(MgCO3), 이산화규소(SiO2) 분말을 사용하였다. 분말을 혼합 및 건조한 후, 가압 성형하여 디스크 형태로 만든 후, 고상반응 온도를 변화시키며 아커마나이트 상의 합성을 유도하였다. 합성된 아커마나이트 펠릿의 용해 및 생체활성 분석을 위하여 SBF 용액 내 침적 시키고, 침적시간에 따라 아커마나이트의 표면 용해 및 하이드록시아파타이트 석출을 분석하였다. 합성반응 온도가 높아질수록 아커마나이트 상이 뚜렷하게 나타난 반면에, SBF 용액 내 용해는 천천히 진행되었다. 합성된 아커마나이트 분말의 생체활성도는 대체적으로 우수하였으나, 그 중에서도 1100℃에서 고상반응 하여 합성한 분말에서 적절한 용해 및 하이드록시아파타이트 입자의 석출이 잘 일어나는 것으로 분석되었다.

L-글루타민산 생산균 Brevibacterium lactofermentum의 Bacteriophag에 관한 연구 (Studies on the Bacteriophages of Brevibacterium lactofermentum)

  • 이태우
    • 미생물학회지
    • /
    • 제17권3호
    • /
    • pp.97-130
    • /
    • 1979
  • Many industrial processes those employ bacteria are subjected to phage infestations. In L-glutamic acid fermentions using acetic acid, the phage infestations of the organisms have been recently recognized. In efforts to elucidate the sources of phage contamination involved in the abnormal fermentation, a series of study was conducted to isolate the phages both from the contents of abnormally fermented tanks and the soil or sewage samples from the surroundings of a fermentation factory, to define major charateristics of the phage isolates, and finally to determine the correlation between the phage isolates and temperate phages originating from the miscellaneous bacterial species isolated from the soil or sewage samples. The results are summarized as follows; 1) All phages were isolated from the irregular fermentation tanks and soil or sewage samples, and they were designated as phage PR-1, PR-2, PR-3, PR-4, PR-5, PR-6, and PR-7, in the order of isolation. These PR-series phages were proved to be highly specific for the variant strains of Br. lactofermentum only, namely, phage PR-1 and PR-2 for Br. lactofermentum No. 468-5 and phage PR-3~PR-7 for Br. lactofemrentum No. 2256. By cross-neutralization test, the 7 phagescould be subdivided into 3 groups, i. e., phage PR-I and PR-2 the first, phage PR-3, PR-4, PR-5, PR-6 the second, and the phage PR-7 the third. 2) The 7 phages were virulent under the experimental conditions. They produced plaques with clear and relatively sharp margins without distinct halo. The mean sizes of plaques were 1.5mm in diameter for phage PR-1 and PR-2, and 1. Omm for phages PR-3~PR-7. Double layer technique modified by Hongo and described by Adams, was applied to assay of the PR-series phages. The factors influencing the plaques were as follows;young age cells of host bacteria cultured for 3-6 hours represented the largest number and size, optimum was pH 7.0, incubation temperature was $30^{\circ}C$, and agar concentration and amount of overlayer medium were 0.6% and 0.2ml, respectively. 3) PR-series phages were stable in 0.05M tris buffer and 0.1M ammonium acetate buffer solution. The addition of $5{\times}10^{-3}M$ magnesium ion effectively increased the stability. Thermostability experiments indicated that PR-series phages were stable at the teinperture between $50^{\circ}{\sim}55^{\circ}C$ in nutrient medium, $45^{\circ}{\sim}50^{\circ}C$ in buffer solution. However, the phages mere completely inactivated at 603C and 65$^{\circ}$C within 10 minutes. The phages were stable at the range of pH6~9 in nutrient medium and of pH 8-9 in buffer solution, respectively. Exposure of the phages to UV for 25, 60 and 100 seconds resulted in the complete loss of infectivily, respectively. 4) Electron microscopy showed that PR-series phage particles exhibited rather similar morphology, differing in the size All of PR-series phages had a multilateral head and had a simple long tiil about three to five times long as compared with head. By the size, phage PR-1 and PR-2, PR-3, PR-4, PR-5, and PR-6 and PR-7 were classified into same groups, respectively. The head and tail size of phage PR-1, PR-5, PR-5(T) and PR-7 were 85nm, 74nm and 235nm and 350mm, and 72nm and 210nm, respectively. 5) Nucleic acids of PR-series phages were double stranded DNA. The G+C contents of phage PR-1, PR-5 and PR-7 were 56.1, 52.9 and 53.7, respectively. The values of G+C contents derived from the $T_m$ were in agreement with the chemically determined values. 6) PR-series phages effectively adsorbed on their host bacteria at the rate of more than 90% during 5 min. K value for phage PR-1, PR-5 and PR-7 were calculated to be $6{\times}10^9 ml$ per minute, respectiveky. The pH of the medium did effect adsorption rate, but both temperature and age of host cells did not. Generally, optimum adsorption condition of phages seemed to be almost same as optimum growth conditions of host bacteria. 7) In one-step growth experiments, the latent periods at $30^{\circ}C$ for PR-1, and PR-7 were about 70, 50 and 55 min, respectively. The corresponding average burst size was 200, 70 and 90, respectively. Lpsis period according to the multiplicity of infection and a phage series. In case of m. o. i. 100, strain No. 2256 (PR-5) and No. 468-5(PR-1) failed to grow and turbidity decreased after 50 and 70min, respectively. 8) In the lysate of a plaque purified phage PR-5 infected bacteria, there observed 2 types ofphage particles, i. e., phage PR-5 and PR-5 (T) of similar morphology but differing at the length of phage tail, and phage tail like particles. The phage taillike particles could be divided into 4 types by the length. Induction experiments of Br. lactofermentum with UV irradiation, mitomycin C or bacitracin treatment produced neither phage PR-5 (T) or phage tail-like particles. 9) No lysis occured when the growth of 7 strains of miscellaneous bacteria, isolated from soil and sewage samples, were inoculated with either phage PR-5 (T) or phage tail-like particles the inoculation of phage PR-5 pellet resulted in the growth inhibition of the orgainsms in the spot test. The lysates obtained from 3 miscellaneous soil derived bacteria following mitomycin C treatment the growth of Br. lactofermentum, but did not lyze the bacterium.

  • PDF

고용 강화 및 결정립 미세화를 통한 마그네슘 합금 주조재의 기계적 물성 향상 (Improvement in Mechanical Properties of Cast Magnesium Alloy through Solid-solution Hardening and Grain Refinement)

  • 김상훈;문병기;유봉선;박성혁
    • 한국주조공학회지
    • /
    • 제37권6호
    • /
    • pp.207-216
    • /
    • 2017
  • This study investigated the effects of the addition of Zn, Ca, and SiC on the microstructure and mechanical properties of Mg-Al alloys. The tensile properties of homogenized Mg-xAl (x = 6, 7, 8, and 9 wt.%) alloys increased with increasing Zn content by the solid-solution strengthening effect. However, when the added Zn content exceeded the solubility limit, the strength and ductility of the alloys decreased greatly owing to premature fracture caused by undissolved coarse particles or local melting. Among the Mg-xAl-yZn alloys tested in this study, the AZ74 alloy showed the best tensile properties. However, from the viewpoints of the thermal stability, castability, and tensile properties, the AZ92 alloy was deemed to be the most suitable cast alloy. Moreover, the addition of a small amount (0.17 wt.%) of SiC reduced the average grain size of the AZ91 alloy significantly, from $430{\mu}m$ to $73{\mu}m$. As a result, both the strength and the elongation of the AZ91 alloy increased considerably by the grain-boundary hardening effect and the suppression of twinning behavior, respectively. On the other hand, the addition of Ca (0.5-1.5 wt.%) and a combined addition of Ca (0.5-1.5 wt.%) and SiC (0.17 wt.%) increased the average grain size of the AZ91 alloy, which resulted in a decrease in its tensile properties. The SiC-added AZ92 alloy exhibited excellent tensile properties (YS 125 MPa, UTS 282 MPa, and EL 12.3%), which were much higher than those of commercial AZ91 alloy (YS 93 MPa, UTS 192 MPa, and EL 7.0%). The fluidity of the SiC-added AZ92 alloy was slightly lower than that of the AZ91 alloy because of the expansion of the solid-liquid coexistence region in the former. However, the SiC-added AZ92 alloy showed better hot-tearing resistance than the AZ91 alloy owing to its refined grain structure.

Kroll법에 의한 타이타늄 스폰지 생성기구에 관한 연구 (A Study on the Formation Mechanism of Titanium Sponge in the Kroll Process)

  • 정재영;손호상
    • 자원리싸이클링
    • /
    • 제26권5호
    • /
    • pp.54-60
    • /
    • 2017
  • 본 연구에서는 $TiCl_4$ 투입시간의 효과가 $TiCl_4$ and Mg의 주어진 중량비율에서 Kroll반응에 미치는 효과를 조사하였다. 그리고 환원반응은 $TiCl_4$ 투입시간에 따라 온도변화를 측정하고, 반응 후 Ti 스폰지 단면과 외관을 관찰함으로써 조사되었다. Kroll 반응열 생성에 의한 온도 증분은 $TiCl_4$ 투입속도에 직선적으로 비례하는 것으로 파악되었다. $TiCl_4$ 투입시간과 환원조 온도 그래프를 보면, 초기 온도 피크가 주입조건에 무관하게 모두 관찰되었다. 이는 초기 Kroll 반응후 $MgCl_2$ 형성으로 인한 일시적인 반응 중단을 의미하는 것으로 해석된다. 또한 스폰지 단면을 관찰해보면, 구형 Mg 입자상이 $MgCl_2$ 내부에 다량으로 관찰되었다. 우리는 이것이 지속적인 Kroll 반응이 일어나도록 미반응 Mg 표면을 계속적으로 공급하는 과정이라 추론할 수 있다. 주사전자현미경으로 스폰지 외형을 관찰한 결과는 Kroll 반응된 Ti 입자들의 합체나 성장이 냉각속도에 의해 제어될 수 있음을 보여주었다.

해양차량 경량화용 마그네슘합금의 마찰용접 및 AE 특성 (Friction Welding and AE Characteristics of Magnesium Alloy for Lightweight Ocean Vehicle)

  • 공유식;이진경;강대민
    • 한국해양공학회지
    • /
    • 제25권6호
    • /
    • pp.91-96
    • /
    • 2011
  • In this paper, friction welded joints were constructed to investigate the mechanical properties of welded 15-mm diameter solid bars of Mg alloy (AZ31B). The main friction welding parameters were selected to endure reliable quality welds on the basis of visual examination, tensile tests, impact energy test, Vickers hardness surveys of the bonds in the area and heat affected zone (HAZ), and macrostructure investigations. The study reached the following conclusions. The tensile strength of the friction welded materials (271 MPa) was increased to about 100% of the AZ31B base metal (274 MPa) under the condition of a heating time of 1 s. The metal loss increased lineally with an increase in the heating time. The following optimal friction welding conditions were determined: rotating speed (n) = 2000 rpm, heating pressure (HP) = 35 MPa, upsetting pressure (UP) = 70 MPa, heating time (HT) = 1 s, and upsetting time (UT) = 5 s, for a metal loss (Mo) of 10.2 mm. The hardness distribution of the base metal (BM) showed HV55. All of the BM parts showed levels of hardness that were approximately similar to friction welded materials. The weld interface of the friction welded parts was strongly mixed, which showed a well-combined structure of macro-particles without particle growth or any defects. In addition, an acoustic emission (AE) technique was applied to derive the optimum condition for friction welding the Mg alloy nondestructively. The AE count and energy parameters were useful for evaluating the relationship between the tensile strength and AE parameters based on the friction welding conditions.