• 제목/요약/키워드: luting agent

검색결과 34건 처리시간 0.026초

Effect of surface treatment and luting agent type on shear bond strength of titanium to ceramic materials

  • Karaokutan, Isil;Ozel, Gulsum Sayin
    • The Journal of Advanced Prosthodontics
    • /
    • 제14권2호
    • /
    • pp.78-87
    • /
    • 2022
  • PURPOSE. This study aimed to compare the effect of different surface treatments and luting agent types on the shear bond strength of two ceramics to commercially pure titanium (Cp Ti). MATERIALS AND METHODS. A total of 160 Cp Ti specimens were divided into 4 subgroups (n = 40) according to surface treatments received (control, 50 ㎛ airborne-particle abrasion, 110 ㎛ airborne-particle abrasion, and tribochemical coating). The cementation surfaces of titanium and all-ceramic specimens were treated with a universal primer. Two cubic all-ceramic discs (lithium disilicate ceramic (LDC) and zirconia-reinforced lithium silicate ceramic (ZLC)) were cemented to titanium using two types of resin-based luting agents: self-cure and dual-cure (n = 10). After cementation, all specimens were subjected to 5000 cycles of thermal aging. A shear bond strength (SBS) test was conducted, and the failure mode was determined using a scanning electron microscope. Data were analyzed using three-way ANOVA, and the Tukey-HSD test was used for post hoc comparisons (P < .05). RESULTS. Significant differences were found among the groups based on surface treatment, resin-based luting agent, and ceramic type (P < .05). Among the surface treatments, 50 ㎛ air-abrasion showed the highest SBS, while the control group showed the lowest. SBS was higher for dual-cure resin-based luting agent than self-cure luting agent. ZLC showed better SBS values than LDC. CONCLUSION. The cementation of ZLC with dual-cure resin-based luting agent showed better bonding effectiveness to commercially pure titanium treated with 50 ㎛ airborne-particle abrasion.

Effect of liners and primers on tensile bond strength between zirconia and resin-based luting agent

  • Jo, Eun-Hye;Huh, Yoon-Hyuk;Ko, Kyung-Ho;Park, Chan-Jin;Cho, Lee-Ra
    • The Journal of Advanced Prosthodontics
    • /
    • 제10권5호
    • /
    • pp.374-380
    • /
    • 2018
  • PURPOSE. The effect of silica-based glass-ceramic liners on the tensile bond strength between zirconia and resin-based luting agent was evaluated and compared with the effect of 10-methacryloyloxydecyl dihydrogen phosphate (MDP)-containing primers. MATERIALS AND METHODS. Titanium abutments and zirconia crowns (n = 60) were fabricated, and the adhesive surfaces of the specimens were treated by airborne-particle abrasion. The specimens were divided into 5 groups based on surface treatment: a control group, 2 primer groups (MP: Monobond Plus; ZP: Z Prime Plus), and 2 liner groups (PL: P-containing Liner; PFL: P-free Liner). All specimens were cemented with self-adhesive resin-based luting agent. After 24-hour water storage and thermocycling (5,000 cycles, $5^{\circ}C/55^{\circ}C$), the tensile bond strength was measured using a universal testing machine. Failure mode analysis and elemental analysis on the bonding interface were performed. The data were analyzed using Kruskal-Wallis test, Dunn's post hoc test, and Fisher's exact test. RESULTS. The liner groups and primer groups showed significantly higher tensile bond strengths than that of the control group (P<.05). PFL showed a significantly higher tensile bond strength than the primer groups (P<.05). The percentage of mixed failure was higher in the primer groups than in the control group (P<.001), and all the specimens showed mixed failure in the liner groups (P<.001). A chemical reaction area was observed at the bonding interface between zirconia and liner. CONCLUSION. The application of liner significantly increased the tensile bond strength between zirconia and resin-based luting agent. PFL was more effective than MDP-containing primers in improving the tensile bond strength with the resin-based luting agent.

Efficacy of various cleansing techniques on dentin wettability and its influence on shear bond strength of a resin luting agent

  • Munirathinam, Dilipkumar;Mohanaj, Dhivya;Beganam, Mohammed
    • The Journal of Advanced Prosthodontics
    • /
    • 제4권3호
    • /
    • pp.139-145
    • /
    • 2012
  • PURPOSE. To evaluate the shear bond strength of resin luting agent to dentin surfaces cleansed with different agents like pumice, ultrasonic scaler with chlorhexidine gluconate, EDTA and the influence of these cleansing methods on wetting properties of the dentin by Axisymmetric drop Shape Analysis - Contact Diameter technique (ADSA-CD). MATERIALS AND METHODS. Forty coronal portions of human third molar were prepared until dentin was exposed. Specimens were divided into two groups: Group A and Group B. Provisional restorations made with autopolymerizing resin were luted to dentin surface with zinc oxide eugenol in Group A and with freegenol cement in Group B. All specimens were stored in distilled water at room temperature for 24 hrs and provisional cements were mechanically removed with explorer and rinsed with water and cleansed using various methods (Control-air-water spray, Pumice prophylaxis, Ultrasonic scaler with 0.2% Chlorhexidine gluconate, 17% EDTA). Contact angle measurements were performed to assess wettability of various cleansing agents using the ADSA-CD technique. Bond strength of a resin luting agent bonded to the cleansed surface was assessed using Instron testing machine and the mode of failure noted. SEM was done to assess the surface cleanliness. Data were statistically analyzed by one-way analysis of variance with Tukey HSD tests (${\alpha}$=.05). RESULTS. Specimens treated with EDTA showed the highest shear bond strength and the lowest contact angle for both groups. SEM showed that EDTA was the most effective solution to remove the smear layer. Also, mode of failure seen was predominantly cohesive for both EDTA and pumice prophylaxis. CONCLUSION. EDTA was the most effective dentin cleansing agent among the compared groups.

Core와 시멘트의 종류가 전부주조금관의 유지력에 미치는 영향 (THE RETENTION OF FULL VENEER GOLD CROWN BY CORE MATERIAL AND DENTAL CEMENT)

  • 하점임;조혜원;동진근
    • 대한치과보철학회지
    • /
    • 제30권1호
    • /
    • pp.93-101
    • /
    • 1992
  • The purpose of this study was to evaluate the effectiveness of core materials and luting agents on the retention of full veneer gold crown. The core materials used in this study was dental amalgam, and composite resin, and the luting agents were zinc phosphate cement, polycarboxylate cement, and glass ionomer cement. The obtained results were as follows. 1. In full veneer gold crown supported by composite resin core, the crown retention with zinc phosphate cement was the highest of all. 2. In full veneer gold crown supported by amalgam core, the crown retention was shown no statistical difference by luting agent. 3. There was no statistical difference in the crown retention between the full veneer gold crown supported by composite resin core and dental amalgam core.

  • PDF

Evaluation of the bond strength between aged composite cores and luting agent

  • Polat, Serdar;Cebe, Fatma;Tuncdemir, Aliriza;Ozturk, Caner;Usumez, Aslihan
    • The Journal of Advanced Prosthodontics
    • /
    • 제7권2호
    • /
    • pp.108-114
    • /
    • 2015
  • PURPOSE. The aim of this study was to evaluate effect of different surface treatment methods on the bond strength between aged composite-resin core and luting agent. MATERIALS AND METHODS. Seventy-five resin composites and also seventy-five zirconia ceramic discs were prepared. 60 composite samples were exposed to thermal aging (10,000 cycles, 5 to $55^{\circ}C$) and different surface treatment. All specimens were separated into 5 groups (n=15): 1) Intact specimens 2) Thermal aging-air polishing 3) Thermal aging- Er:YAG laser irradiation 4) Thermal aging- acid etching 5) Thermal-aging. All specimens were bonded to the zirconia discs with resin cement and fixed to universal testing machine and bond strength testing loaded to failure with a crosshead speed of 0.5 mm/min. The fractured surface was classified as adhesive failure, cohesive failure and adhesive-cohesive failure. The bond strength data was statistically compared by the Kruskal-Wallis method complemented by the Bonferroni correction Mann-Whitney U test. The probability level for statistical significance was set at ${\alpha}$=.05. RESULTS. Thermal aging and different surface treatment methods have significant effect on the bond strength between composite-resin cores and luting-agent (P<.05). The mean baseline bond strength values ranged between $7.07{\pm}2.11$ and $26.05{\pm}6.53$ N. The highest bond strength of $26.05{\pm}6.53$ N was obtained with Group 3. Group 5 showed the lowest value of bond strength. CONCLUSION. Appropriate surface treatment method should be applied to aged composite resin cores or aged-composites restorations should be replaced for the optimal bond strength and the clinical success.

Evaluation of removal forces of implant-supported zirconia copings depending on abutment geometry, luting agent and cleaning method during re-cementation

  • Rodiger, Matthias;Rinke, Sven;Ehret-Kleinau, Fenja;Pohlmeyer, Franziska;Lange, Katharina;Burgers, Ralf;Gersdorff, Nikolaus
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권3호
    • /
    • pp.233-240
    • /
    • 2014
  • PURPOSE. To evaluate the effects of different abutment geometries in combination with varying luting agents and the effectiveness of different cleaning methods (prior to re-cementation) regarding the retentiveness of zirconia copings on implants. MATERIALS AND METHODS. Implants were embedded in resin blocks. Three groups of titanium abutments (pre-fabricated, height: 7.5 mm, taper: $5.7^{\circ}$; customized-long, height: 6.79 mm, taper: $4.8^{\circ}$; customized-short, height: 4.31 mm, taper: $4.8^{\circ}$) were used for luting of CAD/CAM-fabricated zirconia copings with a semi-permanent (Telio CS) and a provisional cement (TempBond NE). Retention forces were evaluated using a universal testing machine. Furthermore, the influence of cleaning methods (manually, manually in combination with ultrasonic bath or sandblasting) prior to re-cementation with a provisional cement (TempBond NE) was investigated with the pre-fabricated titanium abutments (height: 7.5 mm, taper: $5.7^{\circ}$) and SEM-analysis of inner surfaces of the copings was performed. Significant differences were determined via two-way ANOVA. RESULTS. Significant interactions between abutment geometry and luting agent were observed. TempBond NE showed the highest level of retentiveness on customized-long abutments, but was negatively affected by other abutment geometries. In contrast, luting with Telio CS demonstrated consistent results irrespective of the varying abutment geometries. Manual cleaning in combination with an ultrasonic bath was the only cleaning method tested prior to re-cementation that revealed retentiveness levels not inferior to primary cementation. CONCLUSION. No superiority for one of the two cements could be demonstrated because their influences on retentive strength are also depending on abutment geometry. Only manual cleaning in combination with an ultrasonic bath offers retentiveness levels after re-cementation comparable to those of primary luting.

Fiber post의 Relining 방법과 시멘트 유형에 따른 Push-out Bond Strength의 비교 (Comparison of Push-out Bond Strengths According to Relining Procedure and Cement Type on Fiber Post)

  • 강현영;조소연;유미경;이광원;김경아
    • 구강회복응용과학지
    • /
    • 제27권3호
    • /
    • pp.253-265
    • /
    • 2011
  • 근관치료된 치아의 수복에서 fiber post 크기와 포스트 공간의 직경이 일치하지 않은 경우, 포스트 공간은 두꺼운 레진 시멘트로 채워지게 된다. 레진 시멘트가 두꺼워지면 시멘트 내에 기포가 형성되어 포스트 분리가 발생되기 쉽다. 이런 문제점을 해결하기 위한 방법은 composite resin을 이용하여 fiber post를 relining하는 것이다. 이렇게 형성된 해부학적 포스트는 포스트 공간에 잘 적합하고 시멘트의 두께를 감소시킨다. 이 연구의 목적은 relining 과정과 임상 과정의 간소화를 위해 사용되고 있는 luting agents 종류에 따른 fiber post의 push-out 결합 강도를 평가하는 것이다. 42개의 발치된 치아는 6개의 그룹(n=7)으로 나누어졌다. (A1: relined fiber post를 Luxacore/all-bond 2로 합착, A2: non-relined fiber post를 Luxacore/all-bond 2로 합착. B1: relined fiber post를 Calibra/XP-bond로 합착. B2: non-relined fiber post를 Calibra/XP-bond로 합착. C1: relined fiber post를 RelyX Unicem으로 합착. C2: non-relined fiber post를 RelyX Unicem으로 합착.) Push-out 결합 강도는 relining procedure와 cement type의 상호작용에 의해 영향을 받는 것으로 나타났다. relined fiber post 그룹이 non-relined fiber post 그룹보다 더 높은 결합 강도를 가지며 fiber post relining 과정은 결합강도에 유의한 영향을 가진다.(p<0.05) Luting agent에 따라 모든 그룹에서 RelyX Unicem의 결합강도가 Luxacore/All-bond 2와 Calibra/XP bond에 의한 것보다 유의하게 더 높았다(p<0.05).

IN VITRO STUDY OF THE TENSILE BOND STRENGTH OF CEMENT-RETAINED SINGLE IMPLANT PROSTHESIS BY THE VARIOUS PROVISIONAL LUTING CEMENTS AND THE SURFACE TREATMENT OF ABUTMENTS

  • Lee, Hwa-Yeon;Lee, Ho-Sang
    • 대한치과보철학회지
    • /
    • 제40권3호
    • /
    • pp.296-305
    • /
    • 2002
  • The main disadvantage of cement-retained implant restorations is their difficulty in retrievability. Advocates of cemented implant restorations frequently state that retrievability of the restoration can be maintained if a provisional cement is used. The purpose of this study was to find the optimal properties of provisional luting cements and the surface treatment of abutments in single implant abutment system. 30 prefabricated implant abutments, height 8mm, diameter 6mm, 3-degree taper per side, with light chamfer margins were obtained. Three commercially available provisional luting agents which were all zinc oxide eugenol type ; Cavitec, TempBond and TempBond NE were evaluated. No cement served as the control. TempBond along with vaseline, a kind of petrolatum (2:1 ratio) was also evaluated. Ten out of thirty abutments were randomly selected and abutment surfaces were sandblasted with $50{\mu}m$ aluminum oxide. Another ten abutments were sandblasted with $250{\mu}m$ aluminum oxide. A vertical groove, 1 mm deep and 5mm long was cut in each twenty abutments. Ten of them were sandblasted with $50{\mu}m$ aluminum oxide. The full coverage casting crowns were cemented to the abutments with the designated provisional luting agent. Specimens were stored in distilled water at $37^{\circ}C$ for 24 hours. Each specimen was attached to a universal testing machine. A crosshead speed of 0.5mm/min was used to apply a tensile force to each specimen. Within the limitations of this in vitro study, the following conclusions were drawn: 1. Tensile bond strength of provisional luting cements in no surface treatment decreased with the sequence of TempBond NE, TempBond, Cavitec, TempBond with vaseline, no cement. 2. Tensile bond strength more increased by surface treatment. Sandblasting with $250{\mu}m$ aluminum oxide exhibited the highest tensile bond strength in the abutment cemented with TempBond NE and sandblasting with $50{\mu}m$ aluminum oxide exhibited the highest tensile bond strength in cemented with TempBond. 3. In the aspect of a groove formation, tensile bond strength significantly increased in TempBond with vaseline only and the others had no significant effect on tensile bond strength.

In vitro study of compressive fracture strength of Empress 2 crowns cemented with various luting agents

  • Kim Min-Ho;Yang Jae-Ho;Lee Sun-Hyung;Chung Hun-Young;Chang Ik-Tae
    • 대한치과보철학회지
    • /
    • 제39권3호
    • /
    • pp.260-272
    • /
    • 2001
  • All-ceramic restorations have had a more limited life expectancy than metal ceramic restorations because of their low strength. Their relatively lower strength and resistance to fracture have restricted the use of all-ceramic crowns to anterior applications where occlusal loads are lower. But there has been increasing interest in all-ceramic restorations because patients are primarily concerned with improved esthetics. Many efforts have been made to in prove the mechanical properties of dental ceramics. This study was designed to elucidate the influence of the luting agent on the strength of the Empress 2 crown (staining technique) cemented on human teeth. Seventy extracted human permanent molar teeth were chosen. Teeth were prepared for Empress 2 crowns with milling machine on a surveyor. A dental bur was placed in the mandrel that was positioned so that the long axis of the bur was perpendicular to the surveyor base. Dimensions of the Empress 2 crown preparation were $6^{\circ}$ taper on each side, $1.5{\pm}0.1mm$ shoulder margin, and 4mm crown height. The luting cements used in this study were as follow: 1. Uncemented 2. Zinc phosphate cements (Confi-Dental) 3. Conventional glass ionomer cement : Fuji 1 (GC) 4. Resin-modified glass ionomer cements : Fuji plus (GC) 5. Adhesive cements : Panavia F (Kuralay), Variolink II (Vivadent), Choice (Bisco). Fracture test using Instron. The crowns were loaded in compressive force to evaluate the effect of these cements on the breaking strength of these all-ceramic crowns. A steel ball with a diameter of 4mm was placed on the occlusal surface and load was applied to the steel ball by a cylindrical bolt with a crosshead speed of 0.5mm per minute until fracture occurred. The fractured surface was examined using Scanning Electron Microscopic Image (SEM) to discover the correlation between fracture strength and bonding capacity. Within the limitation of this in vitro study design, the results were as follows : 1. fomentations significantly increased the fracture resistance of Empress ceramic crowns compared to control. Uncemented (206.9 N): ZPC (812.9 N): Fuji 1 (879.5 N): Fuji Plus (937.7 N): Choice (1105.4 N): Variolink II (1221.1 N): Panavia F (1445.2 N). 2. Resin luting agent, treated by a silane bond enhancing agents, yielded a significant increase in fracture resistance. In some of the Panavia F group, a fracture extended into dentin. 3. According to SEM images of fractured Empress crowns, the stronger the bond at both interfaces(crown and die), the more fracture strength was acquired.

  • PDF

섬유강화 복합레진 포스트의 결합강도에 대한 포스트 공간 적합도 및 접착 시멘트의 영향 (The influence of fitness and type of luting agents on bonding strength of fiber-reinforced composite resin posts)

  • 배꽃별;정혜윤;황윤찬;오원만;황인남
    • 구강회복응용과학지
    • /
    • 제39권4호
    • /
    • pp.187-194
    • /
    • 2023
  • 목적: 포스트와 포스트 공간의 크기 불일치는 포스트 수복 중 흔히 발생하는 문제이며, 이러한 불일치는 섬유강화 복합레진 포스트의 결합강도에 영향을 미치기 때문에 이를 보상할 수 있는 적절한 접착 시멘트가 필요하다. 연구의 목적은 섬유강화 복합레진 포스트의 결합강도에 영향을 미치는 포스트 공간의 적합도와 접착 시멘트 종류에 따른 영향을 평가하는 것이다. 연구 재료 및 방법: 발거된 30개의 하악소구치를 근관 치료한 뒤, 준비된 포스트 공간에 따라 Fitting (F)과 Mismatching (M)의 두 그룹으로 분류했다. 이들 그룹은 접착 시멘트 종류에 따라 다시 RelyX Unicem (ReX), Luxacore dual (Lux) 및 Duolink (Duo)의 세 가지 하위 그룹으로 추가로 분류했다. 이후 시편을 만들어 만능 물성 시험기 상에서 결합 강도를 측정했고 각 시편의 파절 양상을 관찰하여 분류했다. 결과: 실험의 결과로 ReX 및 Duo 하위 그룹에서는 F 그룹의 평균 결합 강도가 더 높았다. 그러나 Lux 하위 그룹은 F 그룹과 M 그룹 간에 큰 차이가 없었다. 파절 양상 분석에서 ReX 하위 그룹은 시멘트와 상아질 사이의 접착 실패만 관찰되었다. 결론: 본 연구 결과, 섬유강화 복합레진 포스트의 결합강도는 접착 시멘트의 종류, 포스트 공간과 포스트 직경의 불일치에 의해 영향을 받는 것으로 나타났다. Rex는 다른 접착 시멘트와 비교 시 유의하게 높은 결합강도를 보였다. 포스트 직경은 모든 그룹에서 F그룹이 M그룹보다 높은 결합강도를 보였으며, 이 값은 ReX와 Duo 두 그룹에서 유의한 것으로 나타났다.